Construction of Hot Processing Map of Solutionized Mg-10Gd-6Y-1.5Zn-0.5Zr Alloy and Microstructure Evolution
Received date: 2023-05-18
Revised date: 2023-08-28
Online published: 2023-10-17
Supported by
Fellowship of China Postdoctoral Science Foundation(2021M703592);Special Funded Project of Chongqing Postdoctoral Research Program(2021XM1022);Qingnian Project of Science and Technology Research Program of Chongqing Education Commission of China(KJQN202101141);Postgraduate Innovation Project of Chongqing(CYS22640);Graduate Science Research Project of Chongqing University of Technology(KLA21024)
Mg-rare earth (RE)-Zn alloys with long period stacking ordered (LPSO) phases have received extensive attention in the past few years because of their excellent mechanical properties compared with conventional wrought Mg alloys. However, the corresponding hot deformation behaviors and microstructure characteristics of Mg-RE-Zn alloys are rather complex. An in-depth investigation into this would broaden their engineering applications. In this work, hot compression experiments of solutionized Mg-10Gd-6Y-1.5Zn-0.5Zr alloys at 350-500 oC and a strain rate of 0.001-1 s-1 have been conducted to investigate the hot deformation behavior, construct the hot processing map, and determine the hot working window. Afterward, the interaction between dynamic recrystallization (DRX) and kink deformation of LPSO phase during hot deformation has been studied through microstructure characterization. Results show that the flow stress decreases with the increase of temperature and the decrease of strain rate. When deformed at a relatively high strain rate, the sensitivity of flow stress to temperature is evident. When deformed at a relatively low temperature, the sensitivity of flow stress to strain rate is prominent. The corresponding hot processing map was constructed based on Murty criterion. Under a strain of 0.7, two optimal processing areas are found at 400-450 oC (0.001-0.027 s-1) and 450-487 oC (0.12-1 s-1). The accuracy of the constructed hot processing map has been verified by using microstructure characterization (via volume fraction analysis of recrystallized grains) of deformed samples, which correspond to different regions in the constructed hot processing map. By analyzing the softening stress of the flow curve at different temperatures (peak stress minus state stress), DRX volume fraction and kinking angle of the lamellar LPSO phase, the degree of kink deformation of the lamellar LPSO phase decreases with the increase of deformation temperature. In addition, the DRX volume fraction increases with the increase of deformation temperature. Moreover, the kink deformation of the lamellar LPSO phase has an inhibitory effect on DRX and the softening stress of the flow curve could be jointly affected by DRX and the kink deformation of the lamellar LPSO phase.
BAO Chengli , LI Hao , HU Li , ZHOU Tao , TANG Ming , HE Qubo , LIU Xiangguo . Construction of Hot Processing Map of Solutionized Mg-10Gd-6Y-1.5Zn-0.5Zr Alloy and Microstructure Evolution[J]. Acta Metall Sin, 2025 , 61(4) : 632 -642 . DOI: 10.11900/0412.1961.2023.00225
| 1 | Wang C, Ma A B, Liu H, et al. Research progress on heat resistance of magnesium-rare earth alloys reinforced by long period stacking ordered phase [J]. Mater. Rep., 2019, 33: 3298 |
| 王 策, 马爱斌, 刘 欢 等. LPSO相增强镁稀土合金耐热性能研究进展 [J]. 材料导报, 2019, 33: 3298 | |
| 2 | Zhang R Q, Wang J F, Huang S, et al. Substitution of Ni for Zn on microstructure and mechanical properties of Mg-Gd-Y-Zn-Mn alloy [J]. J. Magnes. Alloy., 2017, 5: 355 |
| 3 | Liu H, Bai J, Yan K, et al. Comparative studies on evolution behaviors of 14H LPSO precipitates in as-cast and as-extruded Mg-Y-Zn alloys during annealing at 773 K [J]. Mater. Des., 2016, 93: 9 |
| 4 | Liao H X, Kim J, Lv J B, et al. Microstructure and mechanical properties with various pre-treatment and Zn content in Mg-Gd-Y-Zn alloys [J]. J. Alloys Compd., 2020, 831: 154873 |
| 5 | Li X, Mao P L, Wang F, et al. A literature review on study of long-period stacking ordered phase and its effect on magnesium alloys [J]. Mater. Rep., 2019, 33: 1182 |
| 李 响, 毛萍莉, 王 峰 等. 长周期有序堆垛相(LPSO)的研究现状及在镁合金中的作用 [J]. 材料导报, 2019, 33: 1182 | |
| 6 | Deng Y H. Research progress and development trend in Mg-RE alloys [J]. Chin. Rare Earths, 2009, 30(1): 76 |
| 邓永和. 稀土镁合金研究现状与发展趋势 [J]. 稀土, 2009, 30(1): 76 | |
| 7 | Xu D K, Han E H, Xu Y B. Effect of long-period stacking ordered phase on microstructure, mechanical property and corrosion resistance of Mg alloys: A review [J]. Prog. Nat. Sci. Mater. Int., 2016, 26: 117 |
| 8 | Chen Z Y, Li Q A, Chen X Y, et al. Research status and application of Zn-containing magnesium alloys and influence of LPSO on alloy properties [J]. J. Chin. Soc. Rare Earths, 2021, 39: 860 |
| 陈籽佚, 李全安, 陈晓亚 等. 含锌镁合金的研究现状与应用及其LPSO相对合金性能的影响 [J]. 中国稀土学报, 2021, 39: 860 | |
| 9 | Xing Q Y, Meng L G, Yang S J, et al. Research progress of new magnesium-rare earth alloy [J]. Foundry, 2018, 67: 317 |
| 邢清源, 孟令刚, 杨守杰 等. 新型稀土镁合金的研究进展 [J]. 铸造, 2018, 67: 317 | |
| 10 | Ullmann M, Kittner K, Prahl U. Hot deformation and dynamic recrystallisation behaviour of twin-roll cast Mg-6.8Y-2.5Zn-0.4Zr magnesium alloy [J]. Materials, 2021, 14: 307 |
| 11 | Esmaeilpour H, Zarei-Hanzaki A, Eftekhari N, et al. Strain induced transformation, dynamic recrystallization and texture evolution during hot compression of an extruded Mg-Gd-Y-Zn-Zr alloy [J]. Mater. Sci. Eng., 2020, A778: 139021 |
| 12 | Bao C L, Zhou T, Shi L X, et al. Hot deformation behavior and constitutive analysis of as-extruded Mg-6Zn-5Ca-3Ce alloy fabricated by rapid solidification [J]. Metals, 2021, 11: 480 |
| 13 | Nie Y J F, Zheng J, Han R, et al. Hot deformation behaviour and constitutive equation of Mg-9Gd-4Y-2Zn-0.5Zr alloy [J]. Materials, 2022, 15: 1779 |
| 14 | Zhang L, Wu X Y, Zhang X F, et al. Constitutive model and recrystallization mechanism of Mg-8.7Gd-4.18Y-0.42Zr magnesium alloy during hot deformation [J]. Materials, 2022, 15: 3914 |
| 15 | Xia X S, Chen Q, Li J P, et al. Characterization of hot deformation behavior of as-extruded Mg-Gd-Y-Zn-Zr alloy [J]. J. Alloys Compd., 2014, 610: 203 |
| 16 | Chen B, Zhou W M, Li S, et al. Hot compression deformation behavior and processing maps of Mg-Gd-Y-Zr alloy [J]. J. Mater. Eng. Perform., 2013, 22: 2458 |
| 17 | Xu W C, Jin X Z, Shan D B, et al. Study on the effect of solution treatment on hot deformation behavior and workability of Mg-7Gd-5Y-0.6Zn-0.8Zr magnesium alloy [J]. J. Alloys Compd., 2017, 720: 309 |
| 18 | Xue T X, Yu J B, Wang Z, et al. Investigation on hot workability of Fe-6.5Si-2Cr-12Ni high-silicon steel based on processing map and microstructural evolution [J]. Metall. Mater. Trans., 2023, 54A: 2227 |
| 19 | Li B, Teng B G, Xu W C. Hot deformation characterization of homogenized Mg-Gd-Y-Zn-Zr alloy during isothermal compression [J]. JOM, 2019, 71: 4059 |
| 20 | Liu H N, Li Y J, Zhang K, et al. Microstructure, hot deformation behavior, and textural evolution of Mg-3wt%Zn-1wt%Ca-0.5wt% Sr alloy [J]. J. Mater. Sci., 2020, 55: 12434 |
| 21 | Hu L, Lang M A, Shi L X, et al. Study on hot deformation behavior of homogenized Mg-8.5Gd-4.5Y-0.8Zn-0.4Zr alloy using a combination of strain-compensated Arrhenius constitutive model and finite element simulation method [J]. J. Magnes. Alloy., 2023, 11: 1016 |
| 22 | Li K, Chen Z Y, Chen T, et al. Hot deformation and dynamic recrystallization behaviors of Mg-Gd-Zn alloy with LPSO phases [J]. J. Alloys Compd., 2019, 792: 894 |
| 23 | Jeong H T, Kim W J. The hot compressive deformation behavior of cast Mg-Gd-Y-Zn-Zr alloys with and without LPSO phase in their initial microstructures [J]. J. Magnes. Alloy., 2022, 10: 2901 |
| 24 | Murty S V S N, Rao B N. On the development of instability criteria during hotworking with reference to IN 718 [J]. Mater. Sci. Eng., 1998, A254: 76 |
| 25 | Prasad Y V R K, Gegel H L, Doraivelu S M, et al. Modeling of dynamic material behavior in hot deformation: forging of Ti-6242 [J]. Metall. Trans., 1984, 15A: 1883 |
| 26 | Prasad Y V R K, Seshacharyulu T. Processing maps for hot working of titanium alloys [J]. Mater. Sci. Eng., 1998, A243: 82 |
| 27 | Srinivasan N, Prasad Y V R K, Rao P R. Hot deformation behaviour of Mg-3Al alloy—A study using processing map [J]. Mater. Sci. Eng., 2008, A476: 146 |
| 28 | Wang L, Sabisch J, Lilleodden E T. Kink formation and concomitant twin nucleation in Mg-Y [J]. Scr. Mater., 2016, 111: 68 |
| 29 | Liu C, Yang X H, Peng J C, et al. In-situ and ex-situ investigation of deformation behaviors of a dual-phase Mg-Ni-Y alloy [J]. Scr. Mater., 2023, 226: 115264 |
| 30 | Zhou Y C, Luo Q, Jiang B, et al. Strength-ductility synergy in Mg98.3Y1.3Ni0.4 alloy processed by high temperature homogenization and rolling [J]. Scr. Mater., 2022, 208: 114345 |
/
| 〈 |
|
〉 |