Hot Isostatic Densification of Inconel 718 Powder Alloy and Elimination of Prior Particle Boundaries
Received date: 2022-09-28
Revised date: 2023-02-08
Online published: 2023-06-07
Supported by
National Science and Technology Major Project of China(J2019-VⅡ-0005-0145);NStrategic Priority Research Program of the Chinese Academy of Sciences(XDA22010102);CAS Project for Young Scientists in Basic Research(YSBR-025)
Inconel 718 alloy is widely used in aeronautical fields owing to its excellent mechanical properties and high-temperature resistance. Hot isostatic pressing (HIPing) is a powder metallurgy (PM) processing technology that produces near or net-shape components and solves the problems of macro-segregation and microstructure inhomogeneity. However, the application of PM Inconel 718 alloys has been limited by prior particle boundaries (PPBs), which can negatively impact mechanical properties, such as elongation at elevated temperatures and impact properties. To address this issue, the formation of PPBs can be suppressed during HIPing, or they can be eliminated through subsequent processing. Pre-alloyed powder of Inconel 718 was prepared using the electrode induction melting gas atomization (EIGA) method, and PM Inconel 718 alloys were prepared through the HIPing route. The resulting compacts were subjected to special high-temperature heat treatment, and their mechanical properties were tested. The mechanical properties of PM Inconel 718 test bars were found to be comparable to those of the wrought version of the alloy. However, large and complex components of PM Inconel 718 can contain undesirable PPBs due to mold shielding and insufficient degassing, resulting in poor ductility and impact properties after standard heat treatment. Special high-temperature heat treatment can effectively eliminate the PPBs in the compacts, leading to a substantial improvement in tensile ductility and impact properties. This improvement makes it possible to prepare large and complex components through HIPing with improved mechanical properties.
TIAN Xiaosheng , LU Zhengguan , XU Lei , WU Jie , YANG Rui . Hot Isostatic Densification of Inconel 718 Powder Alloy and Elimination of Prior Particle Boundaries[J]. Acta Metall Sin, 2024 , 60(11) : 1487 -1498 . DOI: 10.11900/0412.1961.2022.00481
| 1 | Chamanfar A, Sarrat L, Jahazi M, et al. Microstructural characteristics of forged and heat treated Inconel-718 disks [J]. Mater. Des., 2013, 52: 791 |
| 2 | Baccino R, Moret F, Pellerin F, et al. High performance and high complexity net shape parts for gas turbines: The ISOPREC? powder metallurgy process [J]. Mater. Des., 2000, 21: 345 |
| 3 | Hosseini E, Popovich V A. A review of mechanical properties of additively manufactured Inconel 718 [J]. Addit. Manuf., 2019, 30: 100877 |
| 4 | Bai Q, Lin J, Tian G, et al. Review and analysis of powder prior boundary (PPB) formation in powder metallurgy processes for nickel-based super alloys [J]. J. Powder Metall. Min., 2015, 4: 1000127 |
| 5 | Xu L, Tian X S, Wu J, et al. Hot isostatic densification of Inconel 718 powder alloy, and microstructure and mechanical properties [J]. Acta Metall. Sin., 2022, 59: 693 |
| 徐 磊, 田晓生, 吴 杰 等. Inconel 718粉末合金的热等静压成形和组织性能 [J]. 金属学报, 2022, 59: 693 | |
| 6 | Tian X S, Wu J, Lu Z G, et al. Effect of powder size segregation on the mechanical properties of hot isostatic pressing Inconel 718 alloys [J]. J. Mater. Res. Technol., 2022, 21: 84 |
| 7 | Ning Y Q, Yao Z K, Guo H Z, et al. Investigation on hot deformation behavior of P/M Ni-base superalloy FGH96 by using processing maps [J]. Mater. Sci. Eng., 2010, A527: 6794 |
| 8 | Ning Y Q, Fu M W, Yao W. Recrystallization of the hot isostatic pressed nickel-base superalloy FGH4096. II: Characterization and application [J]. Mater. Sci. Eng., 2012, A539: 101 |
| 9 | Zhao F, Yao C G, Fan K C, et al. Prior particle boundary precipitation in powder metallurgy GH4169 [J]. Aerosp. Mater. Technol., 2012, 42(1): 92 |
| 赵 丰, 姚草根, 范开春 等. 粉末GH4169合金中的原始颗粒边界问题 [J]. 宇航材料工艺, 2012, 42(1): 92 | |
| 10 | Mao J, Yu K L, Zhou R F. Effect of pre-heat treatment on P/M René95 superalloy microstructure [J]. Powder Metall. Technol., 1989, 7: 213 |
| 毛 健, 俞克兰, 周瑞发. 粉末预热处理对HIP René95粉末高温合金组织的影响 [J]. 粉末冶金技术, 1989, 7: 213 | |
| 11 | Chang L T. Preparation and hot isostatic press compaction of superalloy powder with less ceramic inclusions [D]. Shenyang: Institute of Metal Research, Chinese Academy of Sciences, 2014 |
| 常立涛. 洁净高温合金粉末的制备及其热等静压工艺研究 [D]. 沈阳: 中国科学院金属研究所, 2014 | |
| 12 | Chang L T, Sun W R, Cui Y Y, et al. Preparation of hot-isostatic-pressed powder metallurgy superalloy Inconel 718 free of prior particle boundaries [J]. Mater. Sci. Eng., 2017, A682: 341 |
| 13 | Rao G A, Srinivas M, Sarma D S. Effect of solution treatment temperature on microstructure and mechanical properties of hot isostatically pressed superalloy Inconel* 718 [J]. Mater. Sci. Technol., 2004, 20: 1161 |
| 14 | Rao G A, Srinivas M, Sarma D S. Influence of modified processing on structure and properties of hot isostatically pressed superalloy Inconel 718 [J]. Mater. Sci. Eng., 2006, A418: 282 |
| 15 | Wu J, Guo R P, Xu L, et al. Effect of hot isostatic pressing loading route on microstructure and mechanical properties of powder metallurgy Ti2AlNb alloys [J]. J. Mater. Sci. Technol., 2017, 33: 172 |
| 16 | Xu L, Guo R P, Bai C G, et al. Effect of hot isostatic pressing conditions and cooling rate on microstructure and properties of Ti-6Al-4V alloy from atomized powder [J]. J. Mater. Sci. Technol., 2014, 30: 1289 |
| 17 | Rao G A, Srinivas M, Sarma D S. Effect of thermomechanical working on the microstructure and mechanical properties of hot isostatically pressed superalloy Inconel 718 [J]. Mater. Sci. Eng., 2004, A383: 201 |
| 18 | Arzt E, Ashby M F, Easterling K E. Practical applications of hotisostatic pressing diagrams: Four case studies [J]. Metall. Trans., 1983, 14A: 211 |
| 19 | Li W B, Easterling K E. Cause and effect of non-uniform densification during hot isostatic pressing [J]. Powder Metall., 1992, 35: 47 |
| 20 | Li W B, Ashby M F, Easterling K E. On densification and shape change during hot isostatic pressing [J]. Acta Metall., 1987, 35: 2831 |
| 21 | Nair S V, Tien J K. Densification mechanism maps for hot isostatic pressing (HIP) of unequal sized particles [J]. Metall. Mater. Trans., 1987, 18A: 97 |
| 22 | Zhang M D, Liu J T, Zhang Y W, et al. Relationship between prior particle boundary of powder metallurgy superalloy and solubility of MC carbides [J]. Trans. Mater. Heat Treat., 2021, 42(5): 50 |
| 张梦迪, 刘建涛, 张义文 等. 粉末高温合金原始颗粒边界与MC型碳化物溶解度的关系 [J]. 材料热处理学报, 2021, 42(5): 50 | |
| 23 | Hou J, Dong J X, Yao Z H, et al. Influences of PPB, PPB affect zone, grain boundary and phase boundary on crack propagation path for a P/M superalloy FGH4096 [J]. Mater. Sci. Eng., 2018, A724: 17 |
| 24 | Cai C, Pan K K, Teng Q, et al. Simultaneously enhanced strength and ductility of FGH4097 nickel-based alloy via a novel hot isostatic pressing strategy [J]. Mater. Sci. Eng., 2019, A760: 19 |
| 25 | Qiu C L, Attallah M M, Wu X H, et al. Influence of hot isostatic pressing temperature on microstructure and tensile properties of a nickel-based superalloy powder [J]. Mater. Sci. Eng., 2013, A564: 176 |
| 26 | Tillmann W, Schaak C, Nellesen J, et al. Hot isostatic pressing of IN718 components manufactured by selective laser melting [J]. Addit. Manuf., 2017, 13: 93 |
| 27 | Ye C W, Zhang X H, Wang L, et al. Effect of re-HIPing on microstructure of HIPed TC4 alloy [J]. Trans. Mater. Heat Treat., 2013, 34(6): 99 |
| 叶呈武, 张绪虎, 王 亮 等. 二次热等静压对TC4合金组织的影响 [J]. 材料热处理学报, 2013, 34(6): 99 | |
| 28 | Chang L T, Sun W R, Cui Y Y, et al. Influences of hot-isostatic-pressing temperature on microstructure, tensile properties and tensile fracture mode of Inconel 718 powder compact [J]. Mater. Sci. Eng., 2014, A599: 186 |
| 29 | Teng Q, Wei Q S, Xue P J, et al. Effects of processing temperatures on FGH4097 superalloy fabricated by hot isostatic pressing: Microstructure evolution, mechanical properties and fracture mechanism [J]. Mater. Sci. Eng., 2019, A739: 118 |
| 30 | Fayman Y C. Microstructural characterization and elemental partitioning in a direct-aged superalloy (DA 718) [J]. Mater. Sci. Eng., 1987, 92: 159 |
| 31 | Rao G A, Kumar M, Srinivas M, et al. Effect of standard heat treatment on the microstructure and mechanical properties of hot isostatically pressed superalloy inconel 718 [J]. Mater. Sci. Eng., 2003, A355: 114 |
| 32 | Pfaendtner J A, McMahon Jr C J. Oxygen-induced intergranular cracking of a Ni-base alloy at elevated temperatures—An example of dynamic embrittlement [J]. Acta Mater., 2001, 49: 3369 |
| 33 | Krupp U. Dynamic embrittlement-time-dependent quasi-brittle intergranular fracture at high temperatures [J]. Int. Mater. Rev., 2005, 50: 83 |
/
| 〈 |
|
〉 |