Research paper

Effects of Cu Content on the Microstructure and Tensile Property of K4061 Alloy

  • CAO Shuting ,
  • ZHAO Jian ,
  • GONG Tongzhao ,
  • ZHANG Shaohua ,
  • ZHANG Jian
Expand
  • 1.Shi -changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    2.School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China
    3.Xi'an Aerospace Propulsion Institute, Xi'an 710100, China
ZHANG Shaohua, associate professor, Tel: (024)23748882, E-mail: zhangshaohua@imr.ac.cn

Received date: 2022-08-31

  Revised date: 2022-12-21

  Online published: 2023-05-04

Supported by

National Natural Science Foundation of China(52150233,52203301);Key Research Program of the Chinese Academy of Sciences(ZDRW-CN-2021-2-1)

Abstract

The LOX (liquid oxygen)/kerosene rocket engine is widely used in heavy launch vehicles owing to its low cost, high performance, and high reliability. However, the next-generation LOX/kerosene rocket engine requires a new superalloy that can resist oxygen-rich combustion. The K4061 alloy is a second-generation superalloy that has better resistance to oxygen-rich combustion compared to the first-generation superalloy due to the addition of the Cu element in its composition. However, there is limited research on the role of the Cu element in the superalloy. This study investigates the effect of Cu content (mass fraction) ranging from 1% to 10% on the microstructure and Cu distribution of K4061 alloy using thermodynamic calculations along with DSC, SEM, and TEM experiments. The results show that during the equilibrium solidification of K4061 alloy, the γ matrix precipitates first, followed by precipitating MC carbides at the end of solidification. The addition of Cu does not affect the equilibrium solidification path of the alloy; however, it lowers the solidus and liquidus temperatures of the alloy and the precipitation temperature of MC. During the nonequilibrium solidification, the δ phase is also precipitated at the late solidification stage. The types of precipitated phases of K4061 alloy with different Cu contents remain unchanged, consistent with thermodynamic calculations. However, Cu-rich phases are not found in the sample, and Cu does not dissolve in MC in large quantities or segregate into grain boundaries. TEM results show that Cu is enriched in the strengthening phases, and the size of the strengthening phases slightly increases with the addition of Cu during aging heat treatment. Additionally, the addition of Cu reduced the room temperature and 750°C tensile strength of the alloy.

Cite this article

CAO Shuting , ZHAO Jian , GONG Tongzhao , ZHANG Shaohua , ZHANG Jian . Effects of Cu Content on the Microstructure and Tensile Property of K4061 Alloy[J]. Acta Metall Sin, 2024 , 60(9) : 1179 -1188 . DOI: 10.11900/0412.1961.2022.00427

References

1 Kudrin A A, Zuev D S, Ponomareva L L, et al. Influence of microalloying on the plasticity of KhN58MBYuD-VI nickel alloy [J]. Steel Transl., 2008, 38: 252
2 Nedashkovskii K I, Zheleznyak O N, Gromyko B M, et al. Effect of low temperatures on mechanical and physical properties of high-strength nickel alloy éK61-ID and stainless maraging steel Ek49-VD [J]. Met. Sci. Heat Treat., 2003, 45: 233
3 Polyanskii A M, Polyanskii V M. Structural changes in alloy éK-61 due to cyclic deformation at elevated temperature [J]. Met. Sci. Heat Treat., 2010, 52: 279
4 Sorokina N A, Gal'tsova V I. High-temperature ductility of nickel alloys type KhN55MBYu with a high iron content [J]. Met. Sci. Heat Treat., 1994, 36: 476
5 Huang J, Xu G H, Qin H Y, et al. Correlation between fracture morphology and microstructural evolution during long-term aging of EK61 superalloy [J]. Scanning, 2020, 2020: 1087024
6 Mignanelli P M, Jones N G, Pickering E J, et al. Gamma-gamma prime-gamma double prime dual-superlattice superalloys [J]. Scr. Mater., 2017, 136: 136
7 Alam T, Chaturvedi M, Ringer S P, et al. Precipitation and clustering in the early stages of ageing in Inconel 718 [J]. Mater. Sci. Eng., 2010, A527: 7770
8 Slama C, Abdellaoui M. Structural characterization of the aged Inconel 718 [J]. J. Alloys Compd., 2000, 306: 277
9 Semenov V N, Akimov N V, Glushko V P. Formation of cracks in éP202 and éK61 alloys in welding of structures of liquid rocket engines [J]. Weld. Int., 2013, 27: 159
10 Monroe R W, Bates C E, Pears C D. Metal combustion in high-pressure flowing oxygen [A]. The Symposium on Flammability and Sensitivity of Materials in Oxygen-Enriched Atmospheres [C]. West Conshohocken: ASTM, 1983: 126
11 Holt R T, Wallace W. Impurities and trace elements in nickel-base superalloys [J]. Int. Met. Rev., 1976, 21: 1
12 Davis S E. An elementary overview of the selection of materials for service in oxygen-enriched environments [A]. The Symposium on Flammability and Sensitivity of Materials in Oxygen-Enriched Atmospheres: 13th Volume [C]. West Conshohocken: ASTM, 2012: 1
13 Li Y M, Hu W, Chen Y. Effect of copper on solidification process and segregation in K4169 superalloy [J]. Spec. Cast. Nonferrous Alloys, 2013, 33: 895
  李亚敏, 胡 伟, 陈 毅. Cu对K4169合金凝固过程及凝固偏析的影响 [J]. 特种铸造及有色合金, 2013, 33: 895
14 Li Y M, Zhang Y Y, Zhao W, et al. First-principles study on the effect of Cu on Nb segregation in Inconel 718 alloy [J]. Acta Metall. Sin., 2022, 58: 241
  李亚敏, 张瑶瑶, 赵 旺 等. Cu对Inconel 718合金Nb偏析影响机理的第一性原理研究 [J]. 金属学报, 2022, 58: 241
15 Gwalani B, Choudhuri D, Soni V, et al. Cu assisted stabilization and nucleation of L12 precipitates in Al0.3CuFeCrNi2 fcc-based high entropy alloy [J]. Acta Mater., 2017, 129: 170
16 Detrois M, Pei Z R, Rozman K A, et al. Partitioning of tramp elements Cu and Si in a Ni-based superalloy and their effect on creep properties [J]. Materialia, 2020, 13: 100843
17 He Y W. Study on the effect and mechanism of V, Cu in a new Ni-Cr-Fe-Nb superalloy [D]. Shenyang: Northeastern University, 2016
  贺玉伟. V、Cu在新型Ni-Cr-Fe-Nb高温合金中的作用机理研究 [D]. 沈阳: 东北大学, 2016
18 Pan J S, Tong J M, Tian M B. Fundamentals of Materials Science [M]. Beijing: Tsinghua University Press, 2011: 96
  潘金生, 仝健民, 田民波. 材料科学基础 [M]. 北京: 清华大学出版社, 2011: 96
19 Oblak J M, Paulonis D F, Duvall D S. Coherency strengthening in Ni base alloys hardened by DO22 γ'' precipitates [J]. Metall. Trans., 1974, 5: 143
20 Han D W, Yu L X, Liu F, et al. Effect of heat treatment on the microstructure and mechanical properties of the modified 718 alloy [J]. Acta Metall. Sin. (Engl. Lett.), 2018, 31: 1224
21 Goodfellow A J. Strengthening mechanisms in polycrystalline nickel-based superalloys [J]. Mater. Sci. Technol., 2018, 34: 1793
22 Roth H A, Davis C L, Thomson R C. Modeling solid solution strengthening in nickel alloys [J]. Metall. Mater. Trans., 1997, 28A: 1329
Outlines

/