Osteogenic and Antibacterial Metal-Polyphenol Drug-Loaded Coating on Biodegradable Zinc for Orthopedic Implants Application
Received date: 2023-02-02
Revised date: 2023-03-31
Online published: 2023-04-13
Supported by
National Key Research and Development Program of China(2016YFC1102500);Science and Tech-nology Program of Sichuan Province(2020YFH0077);Science and Tech-nology Program of Sichuan Province(2024YFHZ0310);Open Fund Project of Sichuan Provincial Key Laboratory for Material Corrosion and Protection(2022CL07)
Biodegradable metallic Zn materials are being considered for orthopedic implant applications because of their moderate degradation rate and potential bio-functionalities. Nevertheless, their clinical use is limited due to inadequate osteogenic properties owing to Zn2+ burst release, premature mechanical failure caused by non-uniform corrosion, and poor antibacterial ability. Therefore, to overcome these issues, a metal-polyphenol drug-loaded coating was functionalized on the surface using an alternating chemical deposition method out of tannic acid/metformin molecules and active metallic ions via coordination/chelation reactions. The coating was characterized by homogeneous compactness, which enhanced the corrosion resistance of the Zn substrate, adjusted the corrosion mode, suppressed the release of Zn2+, and regulated metformin release. The in vitro pre-osteoblasts (MC3T3-E1) culture results showed that the coated Zn samples exhibited excellent osteogenic ability. The antibacterial assays with coated Zn samples demonstrated strong antibacterial efficiency.
LIN Xue , QIAN Junyu , ZHANG Wentai , WANG Peng , WAN Guojiang . Osteogenic and Antibacterial Metal-Polyphenol Drug-Loaded Coating on Biodegradable Zinc for Orthopedic Implants Application[J]. Acta Metall Sin, 2024 , 60(11) : 1545 -1558 . DOI: 10.11900/0412.1961.2023.00035
| 1 | Zheng Y F, Wu Y H. Revolutionizing metallic biomaterials [J]. Acta Metall. Sin., 2017, 53: 257 |
| 郑玉峰, 吴远浩. 处在变革中的医用金属材料 [J]. 金属学报, 2017, 53: 257 | |
| 2 | Shi Z Z, Gao X X, Zhang H J, et al. Design biodegradable Zn alloys: Second phases and their significant influences on alloy properties [J]. Bioact. Mater., 2020, 5: 210 |
| 3 | Fang H, Qi X Y, Zhou S C, et al. High-efficient vacuum ultraviolet-ozone assist-deposited polydopamine for poly (lactic-co-glycolic acid)-coated pure Zn toward biodegradable cardiovascular stent applications [J]. ACS Appl. Mater. Interfaces, 2021, 14: 3536 |
| 4 | Su Y C, Wang K, Gao J L, et al. Enhanced cytocompatibility and antibacterial property of zinc phosphate coating on biodegradable zinc materials [J]. Acta Biomater., 2019, 98: 174 |
| 5 | Zhang W T, Li P, Shen G, et al. Appropriately adapted properties of hot-extruded Zn-0.5Cu-xFe alloys aimed for biodegradable guided bone regeneration membrane application [J]. Bioact. Mater., 2021, 6: 975 |
| 6 | Han H S, Loffredo S, Jun I, et al. Current status and outlook on the clinical translation of biodegradable metals [J]. Mater. Today, 2019, 23: 57 |
| 7 | Sheng Y Y, Yang J J, Zhao X Y, et al. Development and in vitro biodegradation of biomimetic zwitterionic phosphorylcholine chitosan coating on Zn1Mg alloy [J]. ACS Appl. Mater. Interfaces, 2020, 12: 54445 |
| 8 | Su Y C, Yang H T, Gao J L, et al. Interfacial zinc phosphate is the key to controlling biocompatibility of metallic zinc implants [J]. Adv. Sci., 2019, 6: 1900112 |
| 9 | Guillory R J, Sikora-Jasinska M, Drelich J W, et al. In vitro corrosion and in vivo response to zinc implants with electropolished and anodized surfaces [J]. ACS Appl. Mater. Interfaces, 2019, 11: 19884 |
| 10 | Mo X S, Qian J Y, Chen Y Q, et al. Corrosion and degradation decelerating alendronate embedded zinc phosphate hybrid coating on biodegradable Zn biomaterials [J]. Corros. Sci., 2021, 184: 109398 |
| 11 | Qian J Y, Zhang W T, Chen Y Q, et al. Osteogenic and angiogenic bioactive collagen entrapped calcium/zinc phosphates coating on biodegradable Zn for orthopedic implant applications [J]. Biomater. Adv., 2022, 136: 212792 |
| 12 | Zhu L, Tong X, Ye Z Q, et al. Zinc phosphate, zinc oxide, and their dual-phase coatings on pure Zn foam with good corrosion resistance, cytocompatibility, and antibacterial ability for potential biodegradable bone-implant applications [J]. Chem. Eng. J., 2022, 450: 137946 |
| 13 | Wang B B, Li Y C, Wang S S, et al. Electrodeposited dopamine/strontium-doped hydroxyapatite composite coating on pure zinc for anti-corrosion, antimicrobial and osteogenesis [J]. Mater. Sci. Eng., 2021, C129: 112387 |
| 14 | Li X J, Shi H, Pan K, et al. Improved biocompatibility and antibacterial property of zinc alloy fabricated with γ-polyglutamic acid-g-dopamine/copper coatings for orthopedic implants [J]. Prog. Org. Coat., 2022, 173: 107215 |
| 15 | Pan K, Zhang W, Shi H, et al. Facile fabrication of biodegradable endothelium-mimicking coatings on bioabsorbable zinc-alloy stents by one-step electrophoretic deposition [J]. J. Mater. Chem., 2022, 10B: 3083 |
| 16 | Lu R F, Zhang X Q, Cheng X X, et al. Medical applications based on supramolecular self-assembled materials from tannic acid [J]. Front. Chem., 2020, 8: 583484 |
| 17 | Bigham A, Rahimkhoei V, Abasian P, et al. Advances in tannic acid-incorporated biomaterials: Infection treatment, regenerative medicine, cancer therapy, and biosensing [J]. Chem. Eng. J., 2022, 432: 134146 |
| 18 | Gan D L, Xing W S, Jiang L L, et al. Plant-inspired adhesive and tough hydrogel based on Ag-Lignin nanoparticles-triggered dynamic redox catechol chemistry [J]. Nat. Commun., 2019, 10: 1487 |
| 19 | Kaczmarek B. Tannic acid with antiviral and antibacterial activity as a promising component of biomaterials—A minireview [J]. Materials, 2020, 13: 3224 |
| 20 | Wu Y, Yan R, Duan Y Y, et al. An environmental-friendly tannic acid/Zn conversion film with a good corrosion protection for iron [J]. Surf. Interfaces, 2021, 24: 101078 |
| 21 | Asgari M, Yang Y, Yang S, et al. Mg-phenolic network strategy for enhancing corrosion resistance and osteocompatibility of degradable magnesium alloys [J]. ACS Omega, 2019, 4: 21931 |
| 22 | He M, Yang B, Huo F J, et al. A novel coating with universal adhesion and inflammation-responsive drug release functions to manipulate the osteoimmunomodulation of implants [J]. J. Mater. Chem., 2021, 9B: 5272 |
| 23 | Chen H Y, Zhan J H, Man L, et al. High foliar retention tannic acid/Fe3+ functionalized Ti-pillared montmorillonite pesticide formulation with pH-responsibility and high UV stability [J]. Appl. Surf. Sci., 2023, 620: 156838 |
| 24 | Sharma A, Verma C, Mukhopadhyay S, et al. Development of sodium alginate/glycerol/tannic acid coated cotton as antimicrobial system [J]. Int. J. Biol. Macromol., 2022, 216: 303 |
| 25 | O'Neill E, Awale G, Daneshmandi L, et al. The roles of ions on bone regeneration [J]. Drug Discov. Today, 2018, 23: 879 |
| 26 | Duan J W, Chen Z G, Liang X Y, et al. Construction and application of therapeutic metal-polyphenol capsule for peripheral artery disease [J]. Biomaterials, 2020, 255: 120199 |
| 27 | Lei T, Deng S W, Chen P, et al. Metformin enhances the osteogenesis and angiogenesis of human umbilical cord mesenchymal stem cells for tissue regeneration engineering [J]. Int. J. Biochem. Cell Biol., 2021, 141: 106086 |
| 28 | Zhang R, Liang Q Y, Kang W Y, et al. Metformin facilitates the proliferation, migration, and osteogenic differentiation of periodontal ligament stem cells in vitro [J]. Cell Biol. Int., 2020, 44: 70 |
| 29 | Lin Q X, Zhou Y J, Yin M, et al. Hydroxyapatite/tannic acid composite coating formation based on Ti modified by TiO2 nanotubes [J]. Colloids Surf., 2020, 196B: 111304 |
| 30 | Zhang H, Luo R F, Li W J, et al. Epigallocatechin gallate (EGCG) induced chemical conversion coatings for corrosion protection of biomedical MgZnMn alloys [J]. Corros. Sci., 2015, 94: 305 |
| 31 | Qiu H, Tu Q F, Gao P, et al. Phenolic-amine chemistry mediated synergistic modification with polyphenols and thrombin inhibitor for combating the thrombosis and inflammation of cardiovascular stents [J]. Biomaterials, 2021, 269: 120626 |
| 32 | Al-Saif F A, Refat M S. Synthesis, spectroscopic, and thermal investigation of transition and non-transition complexes of metformin as potential insulin-mimetic agents [J]. J. Therm. Anal. Calorim., 2013, 111: 2079 |
| 33 | Refat M S, Al-Azab F M, Al-Maydama H M A, et al. Synthesis, spectroscopic and antimicrobial studies of La(III), Ce(III), Sm(III) and Y(III) Metformin HCl chelates [J]. Spectrochim. Acta, 2015, 142A: 392 |
| 34 | Thompson K H, McNeill J H, Orvig C. Vanadium compounds as insulin mimics [J]. Chem. Rev., 1999, 99: 2561 |
| 35 | Tao S, Hong B, Kerong Z. An infrared and Raman spectroscopic study of polyanilines co-doped with metal ions and H+ [J]. Spectrochim. Acta, 2007, 66A: 1364 |
| 36 | Zhan W W, Gao L, Fu X, et al. Green synthesis of amino-functionalized carbon nanotube-graphene hybrid aerogels for high performance heavy metal ions removal [J]. Appl. Surf. Sci., 2019, 467-468: 1122 |
| 37 | Pourzolfaghar H, Hosseini S, Zuki F M, et al. Recent advancements to mitigate zinc oxide formation in zinc-air batteries: A technical review [J]. Mater. Today Commun., 2021, 29: 102954 |
| 38 | Zhang B, Yao R J, Li L H, et al. Green tea polyphenol induced Mg2+-rich multilayer conversion coating: Toward enhanced corrosion resistance and promoted in situ endothelialization of AZ31 for potential cardiovascular applications [J]. ACS Appl. Mater. Interfaces, 2019, 11: 41165 |
| 39 | Xu K, Zhou M, Li M, et al. Metal-phenolic networks as a promising platform for pH-controlled release of bioactive divalent metal ions [J]. Appl. Surf. Sci., 2020, 511: 145569 |
| 40 | Yan Y, Chu X, Luo X E, et al. A homogenous microstructural Mg-based matrix model for orthopedic application with generating uniform and smooth corrosion product layer in Ringer's solution: Study on biodegradable behavior of Mg-Zn alloys prepared by powder metallurgy as a case [J]. J. Magnes. Alloys., 2021, 9: 225 |
| 41 | Zhang W T, Zhao S, Mo X S, et al. Mg ions incorporated phytic acid (PA) and zoledronic acid (ZA) of metal-organic complex coating on biodegradable magnesium for orthopedic implants application [J]. Surf. Coat. Technol., 2021, 413: 127075 |
| 42 | Almeida L C, Correia R D, Palys B, et al. Comprehensive study of the electrochemical growth and physicochemical properties of polycatecholamines and polycatechol [J]. Electrochim. Acta, 2021, 386: 138515 |
| 43 | Kasprzak M M, Erxleben A, Ochocki J. Properties and applications of flavonoid metal complexes [J]. RSC Adv., 2015, 5: 45853 |
| 44 | Wang X M, Yin Z Z, Yu X T, et al. Comparison of corrosion resistance of phenylalanine, methionine, and asparagine-induced Ca-P coatings on AZ31 magnesium alloys [J]. Acta Metall. Sin., 2021, 57: 1258 |
| 王雪梅, 殷正正, 于晓彤 等. AZ31镁合金表面苯丙氨酸、甲硫氨酸和天冬酰胺诱导Ca-P涂层耐蚀性能比较 [J]. 金属学报, 2021, 57: 1258 | |
| 45 | Yin Z Z, Zhao W, Xu J, et al. Corrosion resistance of superhydrophobic Mg(OH)2/calcium myristate composite coating on magnesium alloy AZ31 [J]. Acta Metall. Sin. (Engl. Lett.), 2021, 34: 1618 |
| 46 | Tu Q F, Shen X H, Liu Y W, et al. A facile metal-phenolic-amine strategy for dual-functionalization of blood-contacting devices with antibacterial and anticoagulant properties [J]. Mater. Chem. Front., 2019, 3: 265 |
| 47 | Boanini E, Gazzano M, Bigi A. Ionic substitutions in calcium phosphates synthesized at low temperature [J]. Acta Biomater., 2010, 6: 1882 |
| 48 | Pan H B, Li Z Y, Wang T, et al. Nucleation of strontium-substituted apatite [J]. Cryst. Growth Des., 2009, 9: 3342 |
| 49 | Choi S, Murphy W. The effect of mineral coating morphology on mesenchymal stem cell attachment and expansion [J]. J. Mater. Chem., 2012, 22: 25288 |
/
| 〈 |
|
〉 |