Evolution and Healing Mechanism of 1Cr22Mn16N High Nitrogen Austenitic Stainless Steel Interface Microstructure During Plastic Deformation Bonding
Received date: 2023-01-09
Revised date: 2023-03-22
Online published: 2023-04-11
Supported by
National Key Research and Development Program of China(2018YFA0702900);National Natural Science Foundation of China(52173305);National Natural Science Foundation of China(52101061);National Natural Science Foundation of China(52233017);National Natural Science Foundation of China(52203384)
High nitrogen austenitic stainless steels (HNASSs) are widely used for their good wear resistance and high strength, plasticity, and corrosion resistance. Among these steels, 1Cr22Mn16N HNASS improves the cost effectiveness because of the incorporation of a N element in place of the expensive Ni element. In addition, the overall mechanical properties of the steel are further improved because of the solid solution-strengthening effect of the N element. However, the traditional welding methods such as arc welding, tungsten gas shielded welding, and friction stir welding are not suitable for 1Cr22Mn16N HNASS welding because of the different solubility of N in the liquid and solid phases. N easily spills out during the welding process, which considerably degrades the mechanical properties of the welded joints. Therefore, a new welding method needs to be explored to solve the problems in 1Cr22Mn16N welding. In this work, the bonding technology of plastic deformation was introduced to solve the poor performance problems of 1Cr22Mn16N HNASS welded joints. The experiments were conducted through the Glebble 3500 thermomechanical simulation in the temperature range of 1050-1250oC and a strain range of 10%-40% with a strain rate of 0.1 s-1. The microstructure evolution of the bonding interface was characterized and investigated using OM, EBSD, and TEM; the interface healing mechanism was discussed, and the bonding strength of the joint was evaluated by tensile test. The results show that the bonding level of the interface substantially increases with the increase in deformation and temperature. When the deformation temperature reached 1200oC and the strain reached 40%, the mechanical properties of the bonding interface reached up to the same level as the matrix. During the process of deformation, discontinuous dynamic recrystallization (DDRX) occurred at the interface because of thermomechanical coupling; meanwhile, dislocations accumulated and entanglement occurred under the action of stress, forming a large number of subgrain boundaries within the original grain boundaries near the interface, which, lead to continuous dynamic recrystallization (CDRX). The healing of the interface was achieved by the synergistic effect of CDRX and DDRX.
YANG Ruize , ZHAI Ruzong , REN Shaofei , SUN Mingyue , XU Bin , QIAO Yanxin , YANG Lanlan . Evolution and Healing Mechanism of 1Cr22Mn16N High Nitrogen Austenitic Stainless Steel Interface Microstructure During Plastic Deformation Bonding[J]. Acta Metall Sin, 2024 , 60(7) : 915 -925 . DOI: 10.11900/0412.1961.2023.00015
| 1 | Zhang X Y, Zhou Q, Wang K H., et al. Study on microstructure and tensile properties of high nitrogen Cr-Mn steel processed by CMT wire and arc additive manufacturing [J]. Mater. Des., 2019, 166: 107611 |
| 2 | Gavriljuk V G, Berns H. High Nitrogen Steels [M]. Berlin: Springer, 1999: 135 |
| 3 | Lang Y P, Zhou Y, Rong F, et al. Hot working of high nitrogen austenitic stainless steel [J]. J. Iron Steel Res. Int., 2010, 17: 45 |
| 4 | Bott A H, Pickering F B, Butterworth G J. Development of high manganese high nitrogen low activation austenitic stainless steels [J]. J. Nucl. Mater., 1986, 141-143: 1088 |
| 5 | Simmons J W. Overview: High-nitrogen alloying of stainless steels [J]. Mater. Sci. Eng., 1996, A207: 159 |
| 6 | Harzenmoser M. Welding of high nitrogen steels [J]. Mater. Manuf. Processes, 2004, 19: 75 |
| 7 | Du Toit M, Pistorius P C. Nitrogen control during autogenous arc welding of stainless steel—Part 1: Experimental observations [J]. Trans. Weld. J.., 2003, 82:219 |
| 8 | Mohammed R, Reddy G M, Rao K S. Welding of nickel free high nitrogen stainless steel: Microstructure and mechanical properties [J]. Def. Technol., 2017, 13: 59 |
| 9 | Zhao L, Tian Z L, Peng Y, et al. Laser welding of high nitrogen steel 1Cr22Mn16N Ⅲ. Microstructure and mechanical properties of welding heat-affected zone [J]. Trans. China Weld. Inst., 2007, 28(12): 26 |
| 赵 琳, 田志凌, 彭 云 等. 1Cr22Mn16N高氮钢的激光焊接Ⅲ.焊接热影响区组织和性能 [J]. 焊接学报, 2007, 28(12): 26 | |
| 10 | Kamiya O, Chen Z W, Kikuchi Y. Microporosity formation in partially melted zone during welding of high nitrogen austenitic stainless steels [J]. J. Mater. Sci., 2002, 37: 2475 |
| 11 | Qiang W, Wang K H. Shielding gas effects on double-sided synchronous autogenous GTA weldability of high nitrogen austenitic stainless steel [J]. J. Mater. Process. Technol., 2017, 250: 169 |
| 12 | Zhang H, Wan D, Xue P, et al. Research advances on homogenization manufacturing of heavy components by metal additive forging [J]. J. Mater. Sci. Technol., 2018, 34: 2183e8 |
| 13 | Sun M Y, Xu B, Xie B J, et al. Research progress of homogenized construction and forming of heavy forgings [J]. Chin. Sci. Bull., 2020, 65: 3043 |
| 孙明月, 徐 斌, 谢碧君 等. 大锻件均质化构筑成形研究进展 [J]. 科学通报, 2020, 65: 3043 | |
| 14 | Zhang J Y, Xu B, Tariq N H, et al. Microstructure evolutions and interfacial bonding behavior of Ni-based superalloys during solid state plastic deformation bonding [J]. J. Mater. Sci. Technol., 2020, 46: 1 |
| 15 | Zhou L Y, Feng S B, Sun M Y, et al. Interfacial microstructure evolution and bonding mechanisms of 14YWT alloys produced by hot compression bonding [J]. J. Mater. Sci. Technol., 2019, 35: 1671 |
| 16 | Xie B J, Sun M Y, Xu B, et al. Dissolution and evolution of interfacial oxides improving the mechanical properties of solid state bonding joints [J]. Mater. Des., 2018, 157: 437 |
| 17 | Xie B J, Sun M Y, Xu B, et al. Oxidation of stainless steel in vacuum and evolution of surface oxide scales during hot-compression bonding [J]. Corros. Sci., 2019, 147: 41 |
| 18 | Zhang J Y, Sun M Y, Xu B, et al. Evolution of the interfacial microstructure during the plastic deformation bonding of copper [J]. Mater. Sci. Eng., 2019, A746 : 1 |
| 19 | Jiang H Y, Sun M Y, Wu M F, et al. Microstructure and properties of 7075 aluminum alloy hot compress bonding joint [J]. Heat Treat. Met., 2020, 45(2): 46 |
| 江海洋, 孙明月, 吴铭方 等. 7075铝合金热变形连接接头的组织与性能 [J]. 金属热处理, 2020, 45(2): 46 | |
| 20 | Ren S F, Zhang J Y, Zhang X F, et al. Evolution of interfacial microstructure of Ni-Co base superalloy during plastic deformation bonding and its bonding mechanism [J]. Acta Metall. Sin., 2022, 58: 129 |
| 任少飞, 张健杨, 张新房 等. 新型Ni-Co基高温合金塑性变形连接中界面组织演化及愈合机制 [J]. 金属学报, 2022, 58: 129 | |
| 21 | Miura H, Ozama M, Mogawa R, et al. Strain-rate effect on dynamic recrystallization at grain boundary in Cu alloy bicrystal [J]. Scr. Mater., 2003, 48: 1501 |
| 22 | Wang Y, Shao W Z, Zhen L, et al. Flow behavior and microstructures of superalloy 718 during high temperature deformation[J]. Mater. Sci. Eng., 2008, A497: 479 |
| 23 | Mandal S, Jayalakshmi M, Bhaduri A K, et al. Effect of strain rate on the dynamic recrystallization behavior in a nitrogen-enhanced 316L(N) [J]. Metall. Mater. Trans., 2014, 45A: 5645 |
| 24 | Wang X Y, Wang D K, Jin J S, et al. Effects of strain rates and twins evolution on dynamic recrystallization mechanisms of austenite stainless steel [J]. Mater. Sci. Eng., 2019, A761: 138044 |
| 25 | Humphrey F J, Hatherly M. Recrystallization and Related Annealing Phenomena [M]. 2nd Ed., Amsterdam: Elsevier, 2004: 427 |
| 26 | Sakai T, Belyakov A, Kaibyshev R, et al. Dynamic and post-dynamic recrystallization under hot, cold and severe plastic deformation conditions [J]. Prog. Mater. Sci., 2014, 60: 130 |
| 27 | Sakai T, Jonas J J. Overview no.35 Dynamic recrystallization: Mechanical and microstructural considerations [J]. Acta Metall., 1984, 32: 189 |
| 28 | Jonas J J, Sellars C M, Tegart W J M. Strength and structure under hot-working conditions [J]. Metall. Rev., 1969, 14: 1 |
| 29 | Doherty R D, Hughes D A, Humphreys F J, et al. Current issues in recrystallization: A review [J]. Mater. Sci. Eng., 1997, A238: 219 |
| 30 | Huang K, Logé R E. A review of dynamic recrystallization phenomena in metallic materials [J]. Mater. Des., 2016, 111: 548 |
| 31 | Hu G D, Wang P, Li D Z, et al. Effects of nitrogen on precipitation and tensile behaviors of 25Cr 20Ni austenitic stainless steels at elevated temperatures [J]. Mater. Sci. Eng., 2019, A752: 93 |
| 32 | Zhong X T, Wang L, Liu F. Study on formation mechanism of necklace structure in discontinuous dynamic recrystallization of Incoloy 028 [J]. Acta Metall. Sin., 2018, 54: 969 |
| 钟茜婷, 王 磊, 刘 峰. Incoloy 028合金不连续动态再结晶中链状组织形成机理研究 [J]. 金属学报, 2018, 54: 969 | |
| 33 | Souza R C, Silva E S, Jorge A M, et al. Dynamic recovery and dynamic recrystallization competition on a Nb- and N-bearing austenitic stainless steel biomaterial: Influence of strain rate and temperature [J]. Mater. Sci. Eng., 2013, A582: 96 |
| 34 | Sakai T. Dynamic recrystallization microstructures under hot working conditions [J]. J. Mater. Process. Technol., 1995, 53: 349 |
| 35 | Hu G X, Cai X, Rong Y H. Fundamentals of Materials Science [M]. 3rd Ed., Shanghai: Shanghai Jiao Tong University Press, 2010: 5 |
| 胡赓祥, 蔡 珣, 戎咏华. 材料科学基础 [M]. 第 3版, 上海: 上海交通大学出版社, 2010: 5 | |
| 36 | Paggi A, Angella G, Donnini R. Strain induced grain boundary migration effects on grain growth of an austenitic stainless steel during static and metadynamic recrystallization [J]. Mater. Charact, 2015, 107: 174 |
| 37 | Dudova N, Belyakov A, Sakai T, et al. Dynamic recrystallization mechanisms operating in a Ni-20%Cr alloy under hot-to-warm working [J]. Acta Mater., 2010, 58: 3624 |
| 38 | Xie B C, Yu H, Sheng T, et al. DDRX and CDRX of an as-cast nickel-based superalloy during hot compression at γ′ sub-/super-solvus temperatures [J]. J. Alloys Compd., 2019, 803: 16 |
| 39 | Kubota M, Ushioda K, Miyamoto G, et al. Analysis of recrystallization behavior of hot-deformed austenite reconstructed from electron backscattering diffraction orientation maps of lath martensite [J]. Scr. Mater., 2016, 112: 92 |
| 40 | Kim J M, Kim S J, Kang J H. Effects of short-range ordering and stacking fault energy on tensile behavior of nitrogen-containing austenitic stainless steels [J]. Mater. Sci. Eng., 2022, A836: 142730 |
| 41 | Kumar S, Samantaray D, Aashranth B, et al. Dependency of rate sensitive DRX behaviour on interstitial content of a Fe-Cr-Ni-Mo alloy [J]. Mater. Sci. Eng., 2019, A743: 148 |
/
| 〈 |
|
〉 |