Research paper

Influence of Initial Microstructure and Cold Rolling Reduction on Transformation Texture and Magnetic Properties of Industrial Low-Grade Electrical Steel

  • YANG Ping ,
  • MA Dandan ,
  • GU Chen ,
  • GU Xinfu
Expand
  • School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083, China
YANG Ping, professor, Tel: (010)82376968, E-mail: yangp@mater.ustb.edu.cn

Received date: 2022-08-20

  Revised date: 2023-02-17

  Online published: 2023-03-22

Supported by

National Natural Science Foundation of China(51931002)

Abstract

Compared with high-grade electrical steel, low-grade electrical steel has the advantages of low cost and high production quantity but low profits. Therefore, researchers often focus on studying high-grade electrical steel without phase transformation. The microstructure evolution of low-grade electrical steel is more complicated compared to high-grade steel due to the three transformation stages— casting, hot rolling, and final annealing—that are present between austenite and ferrite during their processing. During continuous casting, the <100> columnar grains commonly formed in the low-grade electrical steel cast slabs with phase transformation illustrate the characteristics of the pronounced transformation delay and suppression. In such conditions, the change in hot rolling temperature will cause diversity in hot-rolled microstructures and textures and affect the subsequent cold rolling and annealing microstructure and texture. Based on the previous studies on the effect of hot rolling processes on the transformation texture of industrial low-grade electrical steel and the observation of the transformation delay and suppression of columnar grains in cast slabs, this work further investigates the influence of the initial microstructures before cold rolling and cold rolling reduction on the transformation texture and explores the law of texture inheritance. In particular, the idea of retaining {100} texture using metastable ferrite hot rolling is proposed to improve magnetic properties. The results show that there are more {100} deformed grains in the hot-rolled plate heated at low temperature, and the {100} texture inheritance is obvious after cold rolling and transformation annealing, which effectively improves the magnetic properties. The {100} transformation texture is weakened with the increase in rolling reduction because the initial {100} grains gradually disappear with increasing rolling reduction. An analysis shows that although the {100} transformation texture induced by the surface effect is hindered by the alloying Al and P elements in the used industrial electrical steel, the favorable initial {100} texture produced using low-temperature hot rolling promotes the memory-type transformation texture. In addition, the transformation texture obtained at a high annealing temperature is still better than the recrystallization texture obtained at a low annealing temperature. The significance of these results lies in the possible future practice of enhancing {100} texture in hot rolled plate by metastable ferrite rolling to improve magnetic properties in final annealed sheets.

Cite this article

YANG Ping , MA Dandan , GU Chen , GU Xinfu . Influence of Initial Microstructure and Cold Rolling Reduction on Transformation Texture and Magnetic Properties of Industrial Low-Grade Electrical Steel[J]. Acta Metall Sin, 2024 , 60(3) : 377 -387 . DOI: 10.11900/0412.1961.2022.00406

References

1 Gu C, Yang P, Mao W M. The influence of rolling process on the microstructure, texture and magnetic properties of low grades non-oriented electrical steel after phase transformation annealing [J]. Acta Metall. Sin., 2019, 55: 181
  顾 晨, 杨 平, 毛卫民. 轧制工艺对低牌号无取向电工钢相变退火组织、织构与磁性能的影响 [J]. 金属学报, 2019, 55: 181
2 Liu H T, Li H L, Schneider J, et al. Effects of coiling temperature after hot rolling on microstructure, texture, and magnetic properties of non-oriented electrical steel in strip casting processing route [J]. Steel Res. Int., 2016, 87: 1256
3 Wu S J, Li H, Yue C X, et al. Effect of finishing temperature on magnetic properties of medium and low grade non-oriented silicon steel [J]. Trans. Mater. Heat Treat., 2019, 40(9): 89
  吴圣杰, 李 慧, 岳重祥 等. 终轧温度对中低牌号无取向硅钢磁性能的影响 [J]. 材料热处理学报, 2019, 40(9): 89
4 An L Z, Liu H T, Wang G D. Effects of hot-rolled coiled temperature on microstructure, texture and magnetic properties of low silicon non-oriented electrical steels [J]. Electr. Steel, 2021, 3(1): 15
  安灵子, 刘海涛, 王国栋. 热轧卷取温度对低硅无取向硅钢组织、织构及磁性能的影响 [J]. 电工钢, 2021, 3(1): 15
5 An L Z, Wang Y P, Wang G D, et al. Fabrication of high-performance low silicon non-oriented electrical steels by a new method: Low-finishing-temperature hot rolling combined with batch annealing [J]. J. Magn. Magn. Mater., 2022, 546: 168907
6 Yashiki H, Okamoto A. Effect of hot-band grain size on magnetic properties of non-oriented electrical steels [J]. IEEE Trans. Magn., 1987, 23: 3086
7 Wu X L, Yang P, Gu X F, et al. Effects of normalizing treatment on microstructure, texture and magnetic properties of 50 W800 electrical steel [J]. Electr. Steel, 2019, 1(1): 29
  武晓龙, 杨 平, 顾新福 等. 常化处理对50W800电工钢组织、织构与磁性的影响 [J]. 电工钢, 2019, 1(1): 29
8 Xie L, Yang P, Xia D S, et al. Microstructure and texture evolution in a non-oriented electrical steel during γα transformation under various atmosphere conditions [J]. J. Magn. Magn. Mater., 2015, 374: 655
9 Xie L, Yang P, Zhang N, et al. Formation of {100} textured columnar grain structure in a non-oriented electrical steel by phase transformation [J]. J. Magn. Magn. Mater., 2014, 356: 1
10 Xie L, Yang P, Zhang N, et al. Texture optimization for intermediate Si-containing non-oriented electrical steel [J]. J. Mater. Eng. Perform., 2014, 23: 3849
11 Yang P, Xia D S, Wang J H, et al. Influence of processing parameters on microstructures, textures and magnetic properties in a Fe-0.43Si-0.5Mn electrical steel subjected to phase transformation treatment [A]. Proceeding of the 11th Annual Chinese Iron and Steel Congress [C]. Beijing Metallurgical Industry Press, 2017: 1
  杨 平, 夏冬生, 王金华 等. 相变法制备Fe-0.43Si-0.5Mn电工钢时工艺参数对组织结构和磁性能的影响 [A]. 第十一届中国钢铁年会论文集 [C]. 北京: 冶金工业出版社, 2017: 1
12 Yang P, Zhang L W, Wang J H, et al. Improvement of texture and magnetic properties by surface effect induced transformation in non-oriented Fe-0.82Si-1.37Mn steel sheets [J]. Steel Res. Int., 2018, 89: 1800045
13 Sung J K, Lee D N, Wang D H, et al. Efficient generation of cube-on-face crystallographic texture in iron and its alloys [J]. ISIJ Int., 2011, 51: 284
14 Sung J K, Koo Y M. Magnetic properties of Fe and Fe-Si alloys with {100} <0vw> texture [J]. J. Appl. Phys., 2013, 113: 17A338
15 Sung J K, Lee D N. Evolution of crystallographic texture in pure iron and commercial steels by γ to α Transformation [J]. Mater. Sci. Forum, 2012, 706-709: 2657
16 Wu X L, Gu C, Yang P, et al. Transformation delay and texture memory effect of columnar grained cast slab in low grades non-oriented electrical steels [J]. ISIJ Int., 2021, 61: 1669
17 Wu X L, Yang P, Gu X F, et al. Effect of the initial columnar-grained inhomogeneity of electrical steels on the transformation temperature [J]. Steel Res. Int., 2022, 93: 2100388
18 Wu X L, Jiang W N, Yang P, et al. Formation of {100} subgrain variants and Σ3 variants during phase transformation of columnar grains in electrical steel: Texture memory and variant selection [J]. Steel Res. Int., 2022, 93: 2100594
19 Yang P, Ma D D, Gu X F, et al. On the transformation textures influenced by deformation in electrical steels, high manganese steels and pure titanium sheets [J]. Front. Mater. Sci., 2022, 16: 220582
20 Tomida T, Wakita M, Yasuyama M, et al. Memory effects of transformation textures in steel and its prediction by the double Kurdjumov-Sachs relation [J]. Acta Mater., 2013, 61: 2828
21 Xie L, He M T, Sun L Y, et al. Columnar grain growth in non-oriented electrical steels via plastic deformation of an initial columnar-grained solidification microstructure [J]. Mater. Lett., 2020, 258: 126797
22 Xie L, Liu S J, He M T, et al. Growth and strain behavior of columnar grains in Fe-0.5%Mn alloy by hot-rolling [J]. J. Alloys Compd., 2021, 877: 160257
23 Cheng L, Yang P, Fang Y P, et al. Preparation of non-oriented silicon steel with high magnetic induction using columnar grains [J]. J. Magn. Magn. Mater., 2012, 324: 4068
24 Cheng L, Zhang N, Yang P, et al. Retaining {100} texture from initial columnar grains in electrical steels [J]. Scr. Mater., 2012, 67: 899
25 Zhang N, Yang P, Mao W M. {001}<120>-{113}<361> recrystallization textures induced by initial {001} grains and related microstructure evolution in heavily rolled electrical steel [J]. Mater. Charact., 2016, 119: 225
26 Zhang N, Yang P, Mao W M. Through process texture evolution of new thin-gauge non-oriented electrical steels with high permeability [J]. J. Magn. Magn. Mater., 2016, 397: 125
Outlines

/