Research paper

Effects of V and B on the Microstructure Evolution and Deformation Mechanisms of Ti-44Al-5Nb-1Mo Alloys

  • LI Tianrui ,
  • XU Yuqian ,
  • WU Wenping ,
  • GAN Wenxuan ,
  • YANG Yong ,
  • LIU Guohuai ,
  • WANG Zhaodong
Expand
  • 1 College of Metallurgical Engineering, Anhui University of Technology, Ma'anshan 243000, China
    2 State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819, China
YANG Yong, Tel: 18955536223, E-mail: yyang@ahut.edu.cn

Received date: 2022-11-01

  Revised date: 2023-02-15

  Online published: 2023-03-01

Supported by

National Natural Science Foundation of China(52301028);National Natural Science Foundation of China(52071065);Fundamental Research Funds for the Central Universities(N2007007);Natural Science Foundation of Anhui Province(2208085QE147);Scientific Research Planning Project of Anhui Province(2022AH050333);Foundation of Anhui University of Technology(QZ202102)

Abstract

TiAl alloys are considered potential structural materials because of their low density, good high-temperature strength, and creep resistance. However, their low-temperature brittleness and poor high-temperature workability lead to narrow processing windows, which hinder their industrial applications, low pressure turbine blades of high-performance engines and thermal protection system for hypersonic space vehicles, for instance. Extensive studies on alloying and hot mechanical processes have been conducted to control the microstructure and then enhance the inherent ductility of TiAl alloys. Alloying is considered as an effective method to stabilize softening phases or refine grains to optimize microstructural homogeneity and hot workability. Thus, β-solidifying γ-TiAl alloys represented by Ti-(40-45)Al-(2-8)Nb-(1-8)(Cr, Mn, V, Mo)-(0-0.5)(B, C) (atomic fraction, %) alloys were designed. Nb and Mo are added as β-phase stabilizers. Meanwhile, B, C, and Y serve as grain refiners, and they are added to increase the hot workability. However, multiple phases, precipitation, and corresponding phase transformations are introduced, leading to complex flow localization and deformation incompatibility. Therefore, considerable effort has been exerted on thermo-mechanical processing to improve the microstructural homogeneity of these alloys. The interaction among work hardening, recovery, recrystallization, and multiphase transformation under different deformation conditions easily aggravates flow localization and deformation incompatibility, which are inadequately studied. Therefore, a comprehensive understanding of the deformation behavior among multiphase β-solidifying γ-TiAl alloys is necessary. In this work, the uniaxial hot compressions of the β-solidifying γ-TiAl alloys with the nominal compositions of Ti-44Al-5Nb-1Mo and Ti-44Al-5Nb-1Mo-2V-0.2B were conducted. The microstructure of the alloys under different temperatures and strain rates was contrastively studied using SEM-BSE and TEM. The effects of V and B on the microstructural evolutions and deformation mechanisms were analyzed. The results indicated that the addition of V and B contributed considerable differences in microstructure and thermal mechanical sensibility. The Ti-44Al-5Nb-1Mo-2V-0.2B alloy showed high-temperature deformation ability. The deflection of residual lamellae and the formation of shear bands were the main deformation mechanisms, and a nearly lamellar microstructure with a nonuniform grain size was easily generated at 1250oC for the Ti-44Al-5Nb-1Mo alloy. On the contrary, for the Ti-44Al-5Nb-1Mo-2V-0.2B alloy, the deformation-induced lamellae decomposition of lamellar (α/γ) (L(α/γ) for short)→α + γ + β/B2 and γα and the spheroidization or dynamic recrystallization of α and B2 grains could be promoted with the increase of deformation temperatures and decrease of strain rates. Consequently, the microstructural homogeneity was greatly improved. Furthermore, specific deformation conditions of the microstructural control, including a nearly full lamellar and nearly duplex microstructure, were presented in this work.

Cite this article

LI Tianrui , XU Yuqian , WU Wenping , GAN Wenxuan , YANG Yong , LIU Guohuai , WANG Zhaodong . Effects of V and B on the Microstructure Evolution and Deformation Mechanisms of Ti-44Al-5Nb-1Mo Alloys[J]. Acta Metall Sin, 2024 , 60(5) : 650 -660 . DOI: 10.11900/0412.1961.2022.00557

References

1 Chen Y Y, Ye Y, Sun J F. Present status for rolling TiAl alloy sheet[J]. Acta Metall. Sin., 2022, 58: 965
  陈玉勇, 叶 园, 孙剑飞. TiAl合金板材轧制研究现状[J]. 金属学报, 2022, 58: 965
2 Yang R. Advances and challenges of TiAl base alloys[J]. Acta Metall. Sin., 2015, 51: 129
  杨 锐. 钛铝金属间化合物的进展与挑战[J]. 金属学报, 2015, 51: 129
3 Huang X, Li Z X, Huang H. Recent development of new high-temperature titanium alloys for high thrust-weight ratio aero-engines[J]. Mater. China, 2011, 30(6): 21
  黄 旭, 李臻熙, 黄 浩. 高推重比航空发动机用新型高温钛合金研究进展[J]. 中国材料进展, 2011, 30(6): 21
4 Zeng S W, Zhao A M, Luo L, et al. Development of β-solidifying γ-TiAl alloys sheet[J]. Mater. Lett., 2017, 198: 31
5 Xu M, Liu G H, Li T R, et al. Microstructure characteristics of Ti-43Al alloy during twin-roll strip casting and heat treatment[J]. Trans. Nonferrous Met. Soc. China, 2019, 29: 1017
6 Li T R, Liu G H, Xu M, et al. Effects of hot-pack rolling process on microstructure, high-temperature tensile properties, and deformation mechanisms in hot-pack rolled thin Ti-44Al-5Nb-(Mo, V, B) sheets[J]. Mater. Sci. Eng., 2019, A764: 138197
7 Guo J M, Liang J L, Li H, et al. Research progress on preparation technology of titanium aluminum alloy and its intermetallic compounds[J]. Multipurp. Util. Miner. Resour., 2022, (3): 1
  郭佳明, 梁精龙, 李 慧 等. 钛铝合金及其金属间化合物制备工艺研究进展[J]. 矿产综合利用, 2022, (3): 1
8 Kim Y W. Microstructural evolution and mechanical properties of a forged gamma titanium aluminide alloy[J]. Acta Metall. Mater., 1992, 40: 1121
9 Jiang H T, Zeng S W, Zhao A M, et al. Hot deformation behavior of β phase containing γ-TiAl alloy[J]. Mater. Sci. Eng., 2016, A661: 160
10 Wang Q, Chen R R, Yang Y H, et al. Effects of lamellar spacing on microstructural stability and creep properties in β-solidifying γ-TiAl alloy by directional solidification[J]. Mater. Sci. Eng., 2018, A711: 508
11 Niu H Z, Gao T X, Sun Q Q, et al. Prior particle boundaries and microstructural homogenization of a β-solidifying γ-TiAl alloy fabricated from prealloyed powder[J]. Mater. Sci. Eng., 2018, A737: 151
12 Han J C, Dong J, Zhang S Z, et al. Microstructure evolution and tensile properties of conventional cast TiAl-based alloy with trace Ni addition[J]. Mater. Sci. Eng., 2018, A715: 41
13 Ye T, Song L, Liang Y F, et al. Precipitation behavior of ωo phase and texture evolution of a forged Ti-45Al-8.5Nb-(W, B, Y) alloy during creep[J]. Mater. Charact., 2018, 136: 41
14 Guo B Q, Aranas C, Foul A, et al. Effect of multipass deformation at elevated temperatures on the flow behavior and microstructural evolution in Ti-6Al-4V[J]. Mater. Sci. Eng., 2018, A729: 119
15 Schnabel J E, Bargmann S, Paul J D H, et al. Work hardening and recovery in fully lamellar TiAl: Relative activity of deformation systems[J]. Philos. Mag., 2019, 99: 148
16 Gu X, Jiang S D, Cao F Y, et al. A β-solidifying TiAl alloy reinforced with ultra-fine Y-rich precipitates[J]. Scr. Mater., 2021, 192: 55
17 Niu H Z, Kong F T, Xiao S L, et al. Effect of pack rolling on microstructures and tensile properties of as-forged Ti-44Al-6V-3Nb-0.3Y alloy[J]. Intermetallics, 2012, 21: 97
18 Zhao E T, Niu H Z, Zhang S Z, et al. Microstructural control and mechanical properties of a β-solidified γ-TiAl alloy Ti-46Al-2Nb-1.5V-1Mo-Y[J]. Mater. Sci. Eng., 2017, A701: 1
19 Zhang J H, Huang B Y, Zhou K C, et al. Pack rolling of TiAl based alloy[J]. Chin. J. Nonferrous Met., 2001, 11: 1055
  张俊红, 黄伯云, 周科朝 等. 包套轧制制备TiAl基合金板材[J]. 中国有色金属学报, 2001, 11: 1055
20 Ouadah O, Merad G, Abdelkader H S. Effect of co-alloying elements on the structural stability, elastic, ductility and thermodynamic properties of TiAl intermetallic compound[J]. Solid State Commun., 2021, 337: 114438
21 Yang R, Rahman K M, Rakhymberdiyev A N, et al. Mechanical behaviour of Ti-Nb-Hf alloys[J]. Mater. Sci. Eng., 2019, A740-741: 398
22 Ding H S, Zhang H L, Wang Q, et al. Effect of Y2O3 particles on the fracture toughness of directionally solidified TiAl-based alloys[J]. Mater. Sci. Eng., 2017, A703: 108
23 Niu H Z, Tong R L, Chen X J, et al. Rapid decomposition of lamellar microstructure and enhanced hot workability of an as-cast triphase Ti-45Al-6Nb-1Mo alloy via one-step alpha-extrusion & annealing[J]. Mater. Sci. Eng., 2021, A801: 140438
24 Lapin J, Pelachová T, Bajana O. High temperature deformation behaviour and microstructure of cast in-situ TiAl matrix composite reinforced with carbide particles[J]. J. Alloys Compd., 2019, 797: 754
25 Jin Y G, Wang J N, Yang J, et al. Microstructure refinement of cast TiAl alloys by β solidification[J]. Scr. Mater., 2004, 51: 113
26 Lapin J, ?tamborská M, Pelachová T, et al. Fracture behaviour of cast in-situ TiAl matrix composite reinforced with carbide particles[J]. Mater. Sci. Eng., 2018, A721: 1
27 Jiang H T, Tian S W, Guo W Q, et al. Hot deformation behavior and deformation mechanism of two TiAl-Mo alloys during hot compression[J]. Mater. Sci. Eng., 2018, A719: 104
28 Song L, Wang L, Oehring M, et al. Evidence for deformation twinning of the D019-α2 phase in a high Nb containing TiAl alloy[J]. Intermetallics, 2019, 109: 91
Outlines

/