Effects of Stacking Fault Energy on the Deformation Mechanisms and Mechanical Properties of Face-Centered Cubic Metals
Received date: 2022-10-27
Revised date: 2023-01-16
Online published: 2023-02-17
Supported by
National Natural Science Foundation of China(52130002);National Natural Science Foundation of China(51901230)
Stacking fault energy (SFE) can play a crucial role in plastic deformation and damage mechanisms of face-centered cubic (fcc) metals. This study mainly summarized the following results: (1) With the reduction of SFE, the slip mode of fcc metals gradually changes from a facile cross-slip wavy mode to a planar mode until deformation twinning occurs; (2) The concept of effective SFE is applied to investigate the variation of SFE with dislocation density in the fcc metals, with the increase in dislocation density, the effective SFE increases; (3) The reduction of SFE is not the only factor determining the formation of deformation twins in fcc metals. In terms of calculating the competition between simulated slipping and twinning using the first principles, the critical criterion for forming deformation twinning in fcc metals was established; (4) The fatigue dislocation configuration of high-, medium-, and low-SFE fcc metals were analyzed and the judgment conditions for forming regular persistent slip bands (PSBs) are proposed; (5) With the increase in Al content, the SFE of Cu-Al alloy decreases, resulting in a simultaneous increasing trend in the tensile strength and the uniform elongation due to the increasing planar slip degree; (6) The exponential strain-hardening model can accurately describe the tensile strain-hardening process of Cu-Al alloys. The quantitative relationship among yield strength, tensile strength, and uniform elongation of Cu-Al alloy with different alloy compositions and microstructure states was successfully predicted; (7) With the increase in Al content, the fatigue strength of Cu-Al alloy is improved. Increasing Al content at the same strain amplitude will enhance its low-cycle fatigue life. Based on the experimental results above, it is shown that the alloy composition affects the deformation and damage mechanisms, and the evolution process of microscopic defects (dislocations, twins) in fcc metals and alloys. Thus, it drastically affects the tensile and fatigue properties of the fcc metals and alloys. These results provide experimental evidence and a theoretical basis for improving the mechanical properties and service reliability of fcc metals and alloys via alloy designing.
Key words: face-centered cubic metal; stacking fault energy; slip; twinning; strength; plasticity; fatigue strength
ZHANG Zhefeng , LI Keqiang , CAI Tuo , LI Peng , ZHANG Zhenjun , LIU Rui , YANG Jinbo , ZHANG Peng . Effects of Stacking Fault Energy on the Deformation Mechanisms and Mechanical Properties of Face-Centered Cubic Metals[J]. Acta Metall Sin, 2023 , 59(4) : 467 -477 . DOI: 10.11900/0412.1961.2022.00548
| 1 | Pan J S, Tong J M, Tian M B. Fundamentals of Materials Science [M]. Beijing: Tsinghua University Press, 2011: 1 |
| 潘金生, 仝健民, 田民波. 材料科学基础 [M]. 北京: 清华大学出版社, 2011: 1 | |
| 2 | Anderson P M, Hirth J P, Lothe J. Theory of Dislocations [M]. 3rd Ed., Cambridge: Cambridge University Press, 2017: 1 |
| 3 | Wang Z R. Cyclic deformation response of planar-slip materials and a new criterion for the wavy-to-planar-slip transition [J]. Philos. Mag., 2004, 84: 351 |
| 4 | Luká? P, Klesnil M. Cyclic stress-strain response and fatigue life of metals in low amplitude region [J]. Mater. Sci. Eng., 1973, 11: 345 |
| 5 | Mughrabi H. On the current understanding of strain gradient plasticity [J]. Mater. Sci. Eng., 2004, A387-389: 209 |
| 6 | de Campos M F. Selected values for the stacking fault energy of face centered cubic metals [J]. Mater. Sci. Forum, 2008, 591-593: 708 |
| 7 | Dillamore I L, Smallman R E, Roberts W T. A determination of the stacking-fault energy of some pure F.C.C. metals [J]. Philos. Mag., 1964, 9: 517 |
| 8 | Cockayne D J H, Jenkins M L, Ray I L F. The measurement of stacking-fault energies of pure face-centred cubic metals [J]. Philos. Mag., 1971, 24: 1383 |
| 9 | Stobbs W M, Sworn C H. The weak beam technique as applied to the determination of the stacking-fault energy of copper [J]. Philos. Mag., 1971, 24: 1365 |
| 10 | Reed R P, Schramm R E. Relationship between stacking-fault energy and X-ray measurements of stacking-fault probability and microstrain [J]. J. Appl. Phys., 1974, 45: 4705 |
| 11 | Murr L E. Interfacial Phenomena in Metals and Alloys [M]. Reading: Addison-Wesley, 1975: 1 |
| 12 | Müllner P, Ferreira P J. On the energy of terminated stacking faults [J]. Philos. Mag. Lett., 1996, 73: 289 |
| 13 | Pierce D T, Jiménez J A, Bentley J, et al. The influence of manganese content on the stacking fault and austenite/ε-martensite interfacial energies in Fe-Mn-(Al-Si) steels investigated by experiment and theory [J]. Acta Mater., 2014, 68: 238 |
| 14 | Curtze S, Kuokkala V T, Oikari A, et al. Thermodynamic modeling of the stacking fault energy of austenitic steels [J]. Acta Mater., 2011, 59: 1068 |
| 15 | Li K Q. Atomistic simulation of the micromechanisms of plastic deformation in face-centered cubic metals [D]. Shenyang: University of Science and Technology of China (Institute of Metal Research, Chinese Academy of Sciences), 2020 |
| 李克强. 面心立方金属塑性变形微观机制的原子模拟研究 [D]. 沈阳: 中国科学技术大学(中国科学院金属研究所), 2020 | |
| 16 | Li K Q, Zhang Z J, Li L L, et al. Effective stacking fault energy in face-centered cubic metals [J]. Acta Metall. Sin. (Engl. Lett.), 2018, 31: 873 |
| 17 | Gray III G T, Kaschner G C, Mason T A, et al. The influence of interstitial content, temperature, and strain rate on deformation twin formation [A]. Advances in Twinning. Proceedings International Symposium [C]. 1999 TMS Annual Meeting, 1999: 157 |
| 18 | Chen M W, Ma E, Hemker K J, et al. Deformation twinning in nanocrystalline aluminum [J]. Science, 2003, 300: 1275 |
| 19 | Wu X L, Zhu Y T. Inverse grain-size effect on twinning in nanocrystalline Ni [J]. Phys. Rev. Lett., 2008, 101: 025503 |
| 20 | Meyers M A, V?hringer O, Lubarda V A. The onset of twinning in metals: A constitutive description [J]. Acta Mater., 2001, 49: 4025 |
| 21 | Rogers H C, Reed-Hill R E, Hirth J P. Deformation Twinning [M]. New York: Gordon and Breach Science Publishers, 1964: 1 |
| 22 | Tadmor E B, Bernstein N. A first-principles measure for the twinnability of FCC metals [J]. J. Mech. Phys. Solids, 2004, 52: 2507 |
| 23 | Asaro R J, Suresh S. Mechanistic models for the activation volume and rate sensitivity in metals with nanocrystalline grains and nano-scale twins [J]. Acta Mater., 2005, 53: 3369 |
| 24 | Cai T, Zhang Z J, Zhang P, et al. Competition between slip and twinning in face-centered cubic metals [J]. J. Appl. Phys., 2014, 116: 163512 |
| 25 | Cai T. Computation and simulation for deformation mechanisms of face-centered cubic metals and alloys [D]. Shenyang: Institute of Metal Research, Chinese Academy of Sciences, 2016 |
| 蔡 拓. 面心立方金属及合金变形机制计算模拟 [D]. 沈阳: 中国科学院金属研究所, 2016 | |
| 26 | Wei X M, Zhang J M, Xu K W. Generalized stacking fault energy in FCC metals with MEAM [J]. Appl. Surf. Sci., 2007, 254: 1489 |
| 27 | Mughrabi H. The cyclic hardening and saturation behaviour of copper single crystals [J]. Mater. Sci. Eng., 1978, 33: 207 |
| 28 | Winter A T. A model for the fatigue of copper at low plastic strain amplitudes [J]. Philos. Mag., 1974, 30: 719 |
| 29 | Li P. Study on the cyclic deformation behavior of face-centered cubic crystals [D]. Shenyang: Institute of Metal Research, Chinese Academy of Sciences, 2009 |
| 李 鹏. 面心立方晶体循环变形行为研究 [D]. 沈阳: 中国科学院金属研究所, 2009 | |
| 30 | Woods P J. Low-amplitude fatigue of copper and copper-5 at.% aluminium single crystals [J]. Philos. Mag., 1973, 28: 155 |
| 31 | Wu X M, Wang Z G, Li G Y. Cyclic deformation and strain burst behavior of Cu-7at.%Al and Cu-16at.%Al single crystals with different orientations [J]. Mater. Sci. Eng., 2001, A314: 39 |
| 32 | Zhang Z F, Wang Z G. Grain boundary effects on cyclic deformation and fatigue damage [J]. Prog. Mater. Sci., 2008, 53: 1025 |
| 33 | Qu S, Zhang P, Wu S D, et al. Twin boundaries: Strong or weak? [J]. Scr. Mater., 2008, 59: 1131 |
| 34 | Zhang P, Zhang Z J, Li L L, et al. Twin boundary: Stronger or weaker interface to resist fatigue cracking [J]. Scr. Mater., 2012, 66: 854 |
| 35 | Zhang Z J. Study on the effect of delamination energy on strength-plasticity matching and fatigue behavior of single-phase copper-zinc alloy [D]. Shenyang: University of Chinese Academy of Sciences (Institute of Metal Research, Chinese Academy of Sciences), 2013 |
| 张振军. 层错能对单相铜锌合金强度塑性匹配及疲劳行为影响研究 [D]. 沈阳: 中国科学院大学(中国科学院金属研究所), 2013 | |
| 36 | Zhang Z J, Zhang P, Li L L, et al. Fatigue cracking at twin boundaries: Effects of crystallographic orientation and stacking fault energy [J]. Acta Mater., 2012, 60: 3113 |
| 37 | Liu R. Study on tensile and fatigue properties of copper-aluminum alloy [D]. Shenyang: University of Chinese Academy of Sciences (Institute of Metal Research, Chinese Academy of Sciences), 2018 |
| 刘 睿. 铜铝合金拉伸与疲劳性能研究 [D]. 沈阳: 中国科学院大学(中国科学院金属研究所), 2018 | |
| 38 | An X H, Wu S D, Wang Z G, et al. Significance of stacking fault energy in bulk nanostructured materials: Insights from Cu and its binary alloys as model systems [J]. Prog. Mater. Sci., 2019, 101: 1 |
| 39 | Yang H K, Tian Y Z, Zhang Z F. Revealing the mechanical properties and microstructure evolutions of Fe-22Mn-0.6C-(x)Al TWIP steels via Al alloying control [J]. Mater. Sci. Eng., 2018, A731: 61 |
| 40 | Sun S J, Tian Y Z, Lin H R, et al. Enhanced strength and ductility of bulk CoCrFeMnNi high entropy alloy having fully recrystallized ultrafine-grained structure [J]. Mater. Des., 2017, 133: 122 |
| 41 | Zhang Z F, Shao C W, Wang B, et al. Tensile and fatigue properties and deformation mechanisms of twinning-induced plasticity steels [J]. Acta Metall. Sin., 2020, 56: 476 |
| 张哲峰, 邵琛玮, 王 斌 等. 孪生诱发塑性钢拉伸与疲劳性能及变形机制 [J]. 金属学报, 2020, 56: 476 | |
| 42 | Zhang Z J, Qu Z, Xu L, et al. A general physics-based hardening law for single phase metals [J]. Acta Mater., 2022, 231: 117877 |
| 43 | Zhang Z J, Qu Z, Xu L, et al. Relationship between strength and uniform elongation of metals based on an exponential hardening law [J]. Acta Mater., 2022, 231: 117866 |
| 44 | Liu R, Zhang Z J, Zhang P, et al. Extremely-low-cycle fatigue behaviors of Cu and Cu-Al alloys: Damage mechanisms and life prediction [J]. Acta Mater., 2015, 83: 341 |
| 45 | Liu R, Zhang Z J, Li L L, et al. Microscopic mechanisms contributing to the synchronous improvement of strength and plasticity (SISP) for TWIP copper alloys [J]. Sci. Rep., 2015, 5: 9550 |
| 46 | An X H, Wu S D, Wang Z G, et al. Enhanced cyclic deformation responses of ultrafine-grained Cu and nanocrystalline Cu-Al alloys [J]. Acta Mater., 2014, 74: 200 |
| 47 | Liu R, Tian Y Z, Zhang Z J, et al. Exploring the fatigue strength improvement of Cu-Al alloys [J]. Acta Mater., 2018, 144: 613 |
| 48 | Pang J C, Li S X, Wang Z G, et al. General relation between tensile strength and fatigue strength of metallic materials [J]. Mater. Sci. Eng., 2013, A564: 331 |
| 49 | Han D, Zhang Y J, Li X W. A crucial impact of short-range ordering on the cyclic deformation and damage behavior of face-centered cubic alloys: A case study on Cu-Mn alloys [J]. Acta Mater., 2021, 205: 116559 |
| 50 | Zhang Y J, Han D, Li X W. Improving the stress-controlled fatigue life of low solid-solution hardening Ni-Cr alloys by enhancing short range ordering degree [J]. Int. J. Fatigue, 2021, 149: 106266 |
| 51 | Wu Y, Zhang F, Yuan X Y, et al. Short-range ordering and its effects on mechanical properties of high-entropy alloys [J]. J. Mater. Sci. Technol., 2021, 62: 214 |
| 52 | George E P, Curtin W A, Tasan C C. High entropy alloys: A focused review of mechanical properties and deformation mechanisms [J]. Acta Mater., 2020, 188: 435 |
| 53 | Yan J X, Zhang Z J, Zhang P, et al. Design and optimization of the composition and mechanical properties for non-equiatomic CoCrNi medium-entropy alloys [J]. J Mater. Sci. Technol., 2023, 139: 232 |
| 54 | Zhang P, Zhang Z F. Getting tougher in ultracold [J]. Science, 2022, 378: 947 |
| 55 | Liu D, Yu Q, Kabra S, et al. Exceptional fracture toughness of CrCoNi-based medium- and high-entropy alloys at 20 kelvin [J]. Science, 2022, 378: 978 |
| 56 | Hu Q M, Yang R. The endless search for better alloys [J]. Science, 2022, 378: 26 |
/
| 〈 |
|
〉 |