Effect of Cu on In-Stent Restenosis and Corrosion Resistance of Ni-Ti Alloy
Received date: 2022-10-31
Revised date: 2022-12-07
Online published: 2023-01-16
Supported by
National Key Research and Development Program of China(2022YFC2406003);National Natural Science Foundation of China(81873918);National Natural Science Foundation of China(82272099);Natural Science Foundation of Liaoning Province(2021020399-JH2/103);Natural Science Foundation of Liaoning Province(2022-YGJC-34)
Ni-Ti alloys are used widely as a self-expanding vascular stent material because of their unique shape memory effect and superelasticity. However, after implantation, there is a risk of in-stent restenosis (ISR) because of insufficient endothelialization and coagulation problems. As a biological functional metal element, the proper addition of Cu endows vascular stent materials, such as stainless steel and cobalt-based alloys, with significant endothelialization promotion and anticoagulant effect, which can effectively inhibit the occurrence of ISR. Based on the alloying strategy, a biofunctional Ni-Ti-Cu alloy was prepared by adding the proper amount of Cu into medical Ni-Ti alloys. The inhibition effect of ISR and corrosion resistance of the Ni-Ti-Cu alloy were studied via OM, SEM, XRD, surface free energy test, electrochemical test, and in vitro cell experiment. Results showed that compared with the Ni-Ti alloy, the Ni-Ti-Cu alloy promoted the transformation of an equiaxed austenite grain structure to fine lath martensite, reduced the surface free energy, and improved corrosion resistance in simulated human blood. In addition, the extract of the Ni-Ti-Cu alloy could promote the proliferation, migration, and tube formation of human umbilical vein endothelial cells. Furthermore, compared with the Ni-Ti alloy, the Ni-Ti-Cu alloy decreased the blood coagulation rate, presenting better anticoagulation ability, which has an application potential for inhibiting the occurrence of ISR.
Key words: Ni-Ti alloy; Cu; in-stent restenosis; corrosion resistance
XU Linjie , LIU Hui , REN Ling , YANG Ke . Effect of Cu on In-Stent Restenosis and Corrosion Resistance of Ni-Ti Alloy[J]. Acta Metall Sin, 2023 , 59(4) : 577 -584 . DOI: 10.11900/0412.1961.2022.00553
| 1 | Hoh D J, Hoh B L, Amar A P, et al. Shape memory alloys: Metallurgy, biocompatibility, and biomechanics for neurosurgical applications [J]. Neurosurgery, 2009, 64: 199 |
| 2 | Robertson S W, Pelton A R, Ritchie R O. Mechanical fatigue and fracture of Nitinol [J]. Int. Mater. Rev., 2012, 57: 1 |
| 3 | Cockerill I, See C W, Young M L, et al. Designing better cardiovascular stent materials: A learning curve [J]. Adv. Funct. Mater., 2021, 31: 2005361 |
| 4 | Antherieu G, Connesson N, Payan Y, et al. NiTi based stent for the treatment of acute urinary retention due to benign prostatic hyperplasia: A preliminary study on NiTi wires and tubes under pure bending [J]. Comput. Methods Biomech. Biomed. Eng., 2014, 17: 190 |
| 5 | Tomita M, Saito S, Makimoto S, et al. Self-expandable metallic stenting as a bridge to surgery for malignant colorectal obstruction: Pooled analysis of 426 patients from two prospective multicenter series [J]. Surg. Endosc., 2019, 33: 499 |
| 6 | Maleckis K, Anttila E, Aylward P, et al. Nitinol stents in the femoropopliteal artery: A mechanical perspective on material, design, and performance [J]. Ann. Biomed. Eng., 2018, 46: 684 |
| 7 | Zhang Y, Wang X Y, Ma Z L, et al. A potential strategy for in-stent restenosis: Inhibition of migration and proliferation of vascular smooth muscle cells by Cu ion [J]. Mater. Sci. Eng., 2020, C115: 111090 |
| 8 | Ahmed R A. Electrochemical properties of Ni47Ti49Co4 shape memory alloy in artificial urine for urological implant [J]. Ind. Eng. Chem. Res., 2015, 54: 8397 |
| 9 | Shen Y, Wang G X, Chen L, et al. Investigation of surface endothelialization on biomedical nitinol (NiTi) alloy: Effects of surface micropatterning combined with plasma nanocoatings [J]. Acta Biomater., 2009, 5: 3593 |
| 10 | Boodagh P, Guo D J, Nagiah N, et al. Evaluation of electrospun PLLA/PEGDMA polymer coatings for vascular stent material [J]. J. Biomater. Sci. Polym. Ed., 2016, 27: 1086 |
| 11 | Lih E, Jung J W, Joung Y K, et al. Synergistic effect of anti-platelet and anti-inflammation of drug-coated Co-Cr substrates for prevention of initial in-stent restenosis [J]. Colloids Surf., 2016, 140B: 353 |
| 12 | Yang D Y, Lu X Y, Hong Y, et al. The molecular mechanism for effects of TiN coating on NiTi alloy on endothelial cell function [J]. Biomaterials, 2014, 35: 6195 |
| 13 | Zhao Y, Wang Z, Bai L, et al. Regulation of endothelial functionality through direct and immunomodulatory effects by Ni-Ti-O nanospindles on NiTi alloy [J]. Mater. Sci. Eng., 2021, C123: 112007 |
| 14 | Kim H J, Moon M W, Lee K R, et al. Mechanical stability of the diamond-like carbon film on nitinol vascular stents under cyclic loading [J]. Thin Solid Films, 2008, 517: 1146 |
| 15 | Yelkarasi C, Recek N, Kazmanli K, et al. Biocompatibility and mechanical stability of nanopatterned titanium films on stainless steel vascular stents [J]. Int. J. Mol. Sci., 2022, 23: 4595 |
| 16 | Ren L, Xu L, Feng J W, et al. In vitro study of role of trace amount of Cu release from Cu-bearing stainless steel targeting for reduction of in-stent restenosis [J]. J. Mater. Sci.: Mater. Med., 2012, 23: 1235 |
| 17 | Jin S J, Qi X, Wang T M, et al. In vitro study of stimulation effect on endothelialization by a copper bearing cobalt alloy [J]. J. Biomed. Mater. Res., 2018, 106A: 561 |
| 18 | Gil F J, Planell J A. Effect of copper addition on the superelastic behavior of Ni-Ti shape memory alloys for orthodontic applications [J]. J. Biomed. Mater. Res., 1999, 48: 682 |
| 19 | Gil F J, Solano E, Pe?a J, et al. Microstructural, mechanical and citotoxicity evaluation of different NiTi and NiTiCu shape memory alloys [J]. J. Mater. Sci.: Mater. Med., 2004, 15: 1181 |
| 20 | Phukaoluan A, Khantachawana A, Kaewtatip P, et al. Property improvement of TiNi by Cu addition for orthodontics applications [J]. Appl. Mech. Mater., 2011, 87: 95 |
| 21 | Colombo S, Cannizzo C, Gariboldi F, et al. Electrical resistance and deformation during the stress-assisted two-way memory effect in Ni45Ti50Cu5 alloy [J]. J. Alloys Compd., 2006, 422: 313 |
| 22 | Sakuma T, Hosogi M, Okabe N, et al. Effect of copper content on superelasticity characteristics in Ti-Ni and Ti-Ni-Cu alloy wires [J]. Mater. Trans., 2002, 43: 828 |
| 23 | Vokoun D, ?ittner P, Stalmans R. Study of the effect of curing treatment in fabrication of SMA/polymer composites on deformational behavior of NiTi-5at.%Cu SMA wires [J]. Scr. Mater., 2003, 48: 623 |
| 24 | Li H F, Qiu K J, Zhou F Y, et al. Design and development of novel antibacterial Ti-Ni-Cu shape memory alloys for biomedical application [J]. Sci. Rep., 2016, 6: 37475 |
| 25 | Pun D K, Berzins D W. Corrosion behavior of shape memory, superelastic, and nonsuperelastic nickel-titanium-based orthodontic wires at various temperatures [J]. Dent. Mater., 2008, 24: 221 |
| 26 | Cheng F T, Lo K H, Man H C. An electrochemical study of the crevice corrosion resistance of NiTi in Hanks' solution [J]. J. Alloys Compd., 2007, 437: 322 |
| 27 | Kassab E, Neelakantan L, Frotscher M, et al. Effect of ternary element addition on the corrosion behaviour of NiTi shape memory alloys [J]. Mater. Corros., 2014, 65: 18 |
| 28 | Dos Reis Barros C D, Da Cunha Ponciano Gomes J A. Influence of Cu addition and autoclave sterilization on corrosion resistance and biocompatibility of NiTi for orthodontics applications [J]. Mater. Res., 2021, 24: 20200369 |
| 29 | Rondelli G, Vicentini B. Effect of copper on the localized corrosion resistance of Ni-Ti shape memory alloy [J]. Biomaterials, 2002, 23: 639 |
| 30 | Craciunescu C, Hamdy A S. The effect of copper alloying element on the corrosion characteristics of Ti-Ni and ternary Ni-Ti-Cu meltspun shape memory alloy ribbons in 0.9% NaCl solution [J]. Int. J. Electrochem. Sci., 2013, 8: 10320 |
| 31 | Zhang X Y, Zhao Y H, Gao W W, et al. Study of TiCuN/ZrN multilayer coatings with adjustable combination properties deposited on TiCu alloy [J]. Vacuum, 2022, 202: 111202 |
| 32 | Toker S M, Canadinc D, Maier H J, et al. Evaluation of passive oxide layer formation-biocompatibility relationship in NiTi shape memory alloys: Geometry and body location dependency [J]. Mater. Sci. Eng., 2014, C36: 118 |
| 33 | Zhao J. Study on biological functions of Cu-bearing stainless steel for urethral system [D]. Shenyang: Institute of Metal Research, Chinese Academy of Sciences, 2017 |
| 赵 静. 含铜不锈钢在泌尿系统中的生物医学功能研究 [D]. 沈阳: 中国科学院金属研究所, 2017 | |
| 34 | Yang H J, Yang K, Zhang B C. Study of in vitro anticoagulant property of the La added medical 316L stainless steel [J]. Acta Metall. Sin., 2006, 42: 959 |
| 杨化娟, 杨 柯, 张炳春. 含La医用316L不锈钢的体外抗凝血性能研究 [J]. 金属学报, 2006, 42: 959 | |
| 35 | Yu X X, Hong Z, Jiang H W, et al. Surface wettability of water and blood on diversified nanocone‐shaped ZnO films modified with n‐dodecyl mercaptan [J]. Surf. Interface Anal., 2022, 54: 1211 |
| 36 | Qiu P, Gao P P, Wang S Y, et al. Study on corrosion behavior of the selective laser melted NiTi alloy with superior tensile property and shape memory effect [J]. Corros. Sci., 2020, 175: 108891 |
| 37 | Brice?o J, Romeu A, Espinar E, et al. Influence of the microstructure on electrochemical corrosion and nickel release in NiTi orthodontic archwires [J]. Mater. Sci. Eng., 2013, C33: 4989 |
| 38 | Marattukalam J J, Singh A K, Datta S, et al. Microstructure and corrosion behavior of laser processed NiTi alloy [J]. Mater. Sci. Eng., 2015, C57: 309 |
| 39 | Liu H, Zhang X Y, Jin S J, et al. Effect of copper-doped titanium nitride coating on angiogenesis [J]. Mater. Lett., 2020, 269: 127634 |
| 40 | Jin S J, Qi X, Zhang B, et al. Evaluation of promoting effect of a novel Cu-bearing metal stent on endothelialization process from in vitro and in vivo studies [J]. Sci. Rep., 2017, 7: 17394 |
| 41 | Hong Z, Yu X X, Jiang H W, et al. Influence of surface morphology and surface free energy on the anticoagulant properties of nanocone‐shaped ZnO films [J]. J. Appl. Polym. Sci., 2022, 139: 52005 |
/
| 〈 |
|
〉 |