Overview

Research Progress of Cold Spray in Institute of Metal Research, Chinese Academy of Sciences

  • XIONG Tianying ,
  • WANG Jiqiang
Expand
  • Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
WANG Jiqiang, professor, Tel: (024)23971743, E-mail: jqwang11s@imr.ac.cn

Received date: 2022-10-31

  Revised date: 2022-12-23

  Online published: 2023-01-03

Supported by

National Natural Science Foundation of China(52271078);National Natural Science Foundation of China(51801217);National Natural Science Foundation of China(51671205)

Abstract

Owing to low spraying temperature and high particle velocity, cold spray is a rapidly developing solid-material deposition technology that has broad application prospects in areas of metal coating preparation, additive manufacturing, and component repair. The Institute of Metal Research, Chinese Academy of Sciences, has conducted extensive research on cold spray, including the exploration of bonding mechanism, strategies and methods of tailoring microstructures and properties of deposits, and application of the cold spray technology. This paper systematically introduces the research progress of cold spray by the Institute of Metal Research, Chinese Academy of Sciences.

Cite this article

XIONG Tianying , WANG Jiqiang . Research Progress of Cold Spray in Institute of Metal Research, Chinese Academy of Sciences[J]. Acta Metall Sin, 2023 , 59(4) : 537 -546 . DOI: 10.11900/0412.1961.2022.00552

References

1 Assadi H, G?rtner F, Stoltenhoff T, et al. Bonding mechanism in cold gas spraying [J]. Acta Mater., 2003, 51: 4379
2 Assadi H, Kreye H, G?rtner F, et al. Cold spraying—A materials perspective [J]. Acta Mater., 2016, 116: 382
3 Huang W, Xue Z L, Liu X, et al. Preparation and friction-wear property of plasma-sprayed CoCrAlTaY-Al2O3 coating [J]. Chin. J. Rare Met., 2021, 45: 836
  黄 文, 薛召露, 刘 侠 等. 等离子喷涂CoCrAlTaY-Al2O3涂层的制备及高温摩擦磨损性能研究 [J]. 稀有金属, 2021, 45: 836
4 Fu W, Wu S G, Chen Q Y, et al. Microstructure and properties of high velocity oxygen fuel sprayed WC-Co-Ni coatings [J]. Chin. J. Rare Met., 2021, 45: 673
  富 伟, 巫顺根, 陈清宇 等. 超音速火焰喷涂WC-Co-Ni涂层结构和性能研究 [J]. 稀有金属, 2021, 45: 673
5 Alkimov A P, Kosarev V F, Papyrin A N. A method of cold gas-dynamic spraying [J]. Doklady Akademii Nauk Sssr, 1990, 315: 1062
6 Ma G L, Cui X Y, Shen Y F, et al. Influence of substrate mechanical properties on deposition behaviour of 316L stainless steel powder [J]. Acta Metall. Sin., 2016, 52: 1610
  马广璐, 崔新宇, 沈艳芳 等. 基体材料力学性能对316L不锈钢颗粒沉积行为的影响 [J]. 金属学报, 2016, 52: 1610
7 Ma G L, Kong L Y, Li T F, et al. Microstructure of copper particle deposited on aluminum by cold spray [J]. Rare Met. Mater. Eng., 2018, 47: 1166
  马广璐, 孔令艳, 李铁藩 等. 冷喷涂单颗粒铜在铝基体上的显微结构研究 [J]. 稀有金属材料与工程, 2018, 47: 1166
8 Zhao Z P, Tang J R, Du H, et al. In-situ chemical interaction in cold-sprayed Zn/Cu composite coating [J]. Mater. Lett., 2018, 228: 246
9 Liu H H, Tariq N U H, Ren Y P, et al. Beneficial role of the continuous powder oxide film in establishing chemical bonding at cold sprayed Al coating/PEEK substrate interface [J]. Appl. Surf. Sci., 2022, 601: 154234
10 Ren Y P, Tariq N U H, Liu H H, et al. Study of microstructural and mechanical anisotropy of 7075 Al deposits fabricated by cold spray additive manufacturing [J]. Mater. Des., 2021, 212: 110271
11 Liu H H, Ren Y P, Li T F, et al. Pores in cold sprayed deposits and their control methods [J]. Mater. Prot., 2022, 55(1): 1
  刘晗珲, 任宇鹏, 李铁藩 等. 冷喷涂沉积层中的孔隙及其控制措施 [J]. 材料保护, 2022, 55(1): 1
12 Ren Y P, Qiu X, Liu H H, et al. Application of heat treatment in cold spraying additive manufacturing [J]. Therm. Spray Technol., 2020, 12(3): 1
  任宇鹏, 邱 翔, 刘晗珲 等. 热处理在冷喷涂增材制造中的应用 [J]. 热喷涂技术, 2020, 12(3): 1
13 Tang J R, Zhao Z P, Li N, et al. Influence of feedstock powder on microstructure and mechanical properties of Ta cold spray depositions [J]. Surf. Coat. Technol., 2019, 377: 124903
14 Wang J Q, Cui X Y, Xiong T Y. Research progress of cold sprayed metal matrix composite coatings and materials [J]. China Surf. Eng., 2020, 33(4): 51
  王吉强, 崔新宇, 熊天英. 冷喷涂金属基复合涂层及材料研究进展 [J]. 中国表面工程, 2020, 33(4): 51
15 Qiu X, Tariq N U H, Qi L, et al. Effects of dissimilar alumina particulates on microstructure and properties of cold-sprayed alumina/A380 composite coatings [J]. Acta Metall. Sin. (Engl. Lett.), 2019, 32: 1449
16 Qiu X, Tariq N U H, Wang J Q, et al. Microstructure, microhardness and tribological behavior of Al2O3 reinforced A380 aluminum alloy composite coatings prepared by cold spray technique [J]. Surf. Coat. Technol., 2018, 350: 391
17 Qiu X, Tariq N U H, Qi L, et al. A hybrid approach to improve microstructure and mechanical properties of cold spray additively manufactured A380 aluminum composites [J]. Mater. Sci. Eng., 2020, A772: 138828
18 Qiu X, Tariq NH, Qi L, et al. Influence of particulate morphology on microstructure and tribological properties of cold sprayed A380/Al2O3 composite coatings [J]. J. Mater. Sci. Technol., 2020, 44: 9
19 Bray M, Cockburn A, O'Neill W. The laser-assisted cold spray process and deposit characterisation [J]. Surf. Coat. Technol., 2009, 203: 2851
20 Qiu X, Wang J Q, Tariq N H, et al. Effect of heat treatment on microstructure and mechanical properties of A380 aluminum alloy deposited by cold spray [J]. J. Thermal Spray Technol., 2017, 26: 1898
21 Qiu X, Tariq N U H, Qi L, et al. In-situ Sip/A380 alloy Nano/Micro composite formation through cold spray additive manufacturing and subsequent hot rolling treatment: Microstructure and mechanical properties [J]. J. Alloys Compd., 2019, 780: 597
22 Tariq N H, Gyansah L, Qiu X, et al. Thermo-mechanical post-treatment: A strategic approach to improve microstructure and mechanical properties of cold spray additively manufactured composites [J]. Mater. Des., 2018, 156: 287
23 Tariq N U H, Gyansah L, Qiu X, et al. Achieving strength-ductility synergy in cold spray additively manufactured Al/B4C composites through a hybrid post-deposition treatment [J]. J. Mater. Sci. Technol., 2019, 35: 1053
24 Tao Y S, Xiong T Y, Sun C, et al. Effect of α-Al2O3 on the properties of cold sprayed Al/α-Al2O3 composite coatings on AZ91D magnesium alloy [J]. Appl. Surf. Sci., 2009, 256: 261
25 Tao Y S, Xiong T Y, Sun C, et al. Microstructure and corrosion performance of a cold sprayed aluminium coating on AZ91D magnesium alloy [J]. Corros. Sci., 2010, 52: 3191
26 Zhao Z P, Tang J R, Tariq N H, et al. Microstructure and corrosion behavior of cold-sprayed Zn-Al composite coating [J]. Coatings, 2020, 10: 931
27 Wang J Q, Kong L Y, Li T F, et al. Oxidation behavior of thermal barrier coatings with a TiAl3 bond coat on γ-TiAl Alloy [J]. J. Therm. Spray Technol., 2015, 24: 467
28 Wang J Q, Kong L Y, Li T F, et al. Microstructure evolution of cold-sprayed Al-Si alloy coatings on γ-TiAl during heat treatment [J]. J. Therm. Spray Technol., 2015, 24: 1071
29 Wang J Q, Kong L Y, Wu J, et al. Microstructure evolution and oxidation resistance of silicon-aluminizing coating on γ-TiAl alloy [J]. Appl. Surf. Sci., 2015, 356: 827
30 Huang J, Zhao F, Cui X Y, et al. Long-term oxidation behavior of silicon-aluminizing coating with an in-situ formed Ti5Si3 diffusion barrier on γ-TiAl alloy [J]. Appl. Surf. Sci., 2022, 582: 152444
31 Liu H H, Tariq N U H, Ren Y P, et al. Effect of accelerating gas temperature on microstructure and properties of cold sprayed Al coating on polyether ether ketone (PEEK) [J]. Surf. Coat. Technol., 2022, 429: 127972
32 Liu H H, Tariq N U H, Ren Y P, et al. Influence of Al2O3 content on microstructure, electrical conductivity and adhesion strength of cold sprayed Al-Al2O3 coatings on PEEK substrate [J]. Surf. Coat. Technol., 2022, 446: 128752
33 Tariq N H, Gyansah L, Wang J Q, et al. Cold spray additive manufacturing: A viable strategy to fabricate thick B4C/Al composite coatings for neutron shielding applications [J]. Surf. Coat. Technol., 2018, 339: 224
34 Zhao L J, Tariq N U H, Ren Y P, et al. Effect of particle size on ceramic particle content in cold sprayed Al-based metal matrix composite coating [J]. J. Therm. Spray Technol., 2022, 31: 2505
35 Tang J R, Zhao Z P, Cui X Y, et al. Microstructure and bioactivity of a cold sprayed rough/porous Ta coating on Ti6Al4V substrate [J]. Sci. China Technol. Sci., 2020, 63: 731
36 Tang J R, Liu H Y, Guo M X, et al. Enhanced spreading, migration and osteodifferentiation of HBMSCs on macroporous CS-Ta—A biocompatible macroporous coating for hard tissue repair [J]. Mater. Sci. Eng., 2021, C129: 112411
37 Tang J R, Zhao Z P, Liu H S, et al. A novel bioactive Ta/hydroxyapatite composite coating fabricated by cold spraying [J]. Mater. Lett., 2019, 250: 197
38 Zhao Z P, Tariq N U H, Tang J R, et al. Microstructural evolutions and mechanical characteristics of Ti/steel clad plates fabricated through cold spray additive manufacturing followed by hot-rolling and annealing [J]. Mater. Des., 2020, 185: 108249
39 Zhao Z P, Tang J R, Tariq N U H, et al. Effect of rolling temperature on microstructure and mechanical properties of Ti/steel clad plates fabricated by cold spraying and hot-rolling [J]. Mater. Sci. Eng., 2020, A795: 139982
40 Zhao Z P, Tariq N U H, Tang J R, et al. Influence of annealing on the microstructure and mechanical properties of Ti/steel clad plates fabricated via cold spray additive manufacturing and hot-rolling [J]. Mater. Sci. Eng., 2020, A775: 138968
41 Ren Y P, Tariq N U H, Liu H H, et al. An innovative and flexible approach to fabricate Mg/Al composite plates: Cold spraying and hot rolling post-treatment [J]. Mater. Sci. Eng., 2022, A849: 143515
42 Ren Y P, Tariq N H, Liu H H, et al. Unraveling the effects of hot rolling on microstructure and mechanical properties of cold sprayed Mg/Al clad plates [J]. Mater. Today Commun., 2022, 33: 104553
43 Tang J R, Tariq N U H, Zhao Z P, et al. Microstructure and mechanical properties of Ti-Ta composites prepared through cold spray additive manufacturing [J]. Acta Metall. Sin. (Engl. Lett.), 2022, 35: 1465
Outlines

/