Effect of Post-Aging on Microstructure and Mechanical Properties of an Ultrafine-Grained 6061 Aluminum Alloy

  • LIU Manping ,
  • XUE Zhoulei ,
  • PENG Zhen ,
  • CHEN Yulin ,
  • DING Lipeng ,
  • JIA Zhihong
Expand
  • 1School of Materials Science and Engineering, Jiangsu University, Zhenjiang 212013, China
    2State Key Laboratory of Advanced Design and Manufacturing for Vehicle Body, Hunan University, Changsha 410082, China
    3Key Laboratory for Light-Weight Materials, Nanjing Tech University, Nanjing 211816, China
    4School of Materials Science and Engineering, Chongqing University, Chongqing 400030, China

Received date: 2021-06-02

  Revised date: 2022-04-18

  Online published: 2022-09-07

Supported by

National Natural Science Foundation of China(U1710124);National Natural Science Foundation of China(51871035);National Natural Science Foundation of China(52001159);Open Fund of the State Key Laboratory of Advanced Design and Manufacturing for Vehicle Body, Hunan University(32115014)

Abstract

Al-Mg-Si alloys are widely used in automotive body panels and parts of the engine owing to their low density, medium strength, high specific strength, good corrosion resistance and other characteristics. Currently, there are many studies on the precipitation behavior of undeformed Al-Mg-Si aluminum alloy, but there is a lack of research on the precipitation evolution and precipitation strengthening mechanism of ultra-fine grained 6061 aluminum alloy at different post-aging temperatures. In this study, the microstructure and mechanical properties of an ultrafine grain 6061 aluminum alloy produced by combining the equal channel angular pressing (ECAP) and post aging methods was comparatively evaluated via TEM, XRD, microhardness tests, and tensile tests. The results indicated that the average grain size of the alloy after two ECAP passes was refined to 210 nm. The average grain size of the alloy after the ECAP pass at 80oC and 20 min post aging was 278 nm; moreover, the fine needle β'', L phase, and Q' phase precipitates at nanoscale were dispersed in the matrix. Furthermore, the tensile and yield strengths were 514 and 483 MPa, respectively, while maintaining a remarkably uniform elongation of 15.1%. These results indicate that numerous dislocations introduced by ECAP in the matrix provide a location for the nucleation of the precipitate, which accelerates the precipitation kinetics during the post aging process. The high strength and toughness of the ECAP alloy after low temperature post aging can be attributed to the grain refinement strengthening, dislocation strengthening, and nanoprecipitation strengthening. Thus, the evolution of the aging precipitates during the ECAP and post aging alloy was analyzed.

Cite this article

LIU Manping , XUE Zhoulei , PENG Zhen , CHEN Yulin , DING Lipeng , JIA Zhihong . Effect of Post-Aging on Microstructure and Mechanical Properties of an Ultrafine-Grained 6061 Aluminum Alloy[J]. Acta Metall Sin, 2023 , 59(5) : 657 -667 . DOI: 10.11900/0412.1961.2021.00237

References

1 Miller W S, Zhuang L, Bottema J, et al. Recent development in aluminium alloys for the automotive industry[J]. Mater. Sci. Eng., 2000, A280: 37
2 Liu M P, Chen J, Lin Y J, et al. Microstructure, mechanical properties and wear resistance of an Al-Mg-Si alloy produced by equal channel angular pressing[J]. Prog. Nat. Sci. Mater. Int., 2020, 30: 485
3 Ding L P, Jia Z H, Nie J F, et al. The structural and compositional evolution of precipitates in Al-Mg-Si-Cu alloy[J]. Acta Mater., 2018, 145: 437
4 Chen J, Pan Q L, Yu X H, et al. Effect of annealing treatment on microstructure and fatigue crack growth behavior of Al-Zn-Mg-Sc-Zr alloy[J]. J. Cent. South Univ., 2018, 25: 961
5 Feng L, Pan Q L, Wei L L, et al. Through-thickness inhomogeneity of localized corrosion in 7050-T7451 Al alloy thick plate[J]. J. Cent. South Univ., 2015, 22: 2423
6 Liu M P, Wu Z J, Yang R, et al. DSC analyses of static and dynamic precipitation of an Al-Mg-Si-Cu aluminum alloy[J]. Prog. Nat. Sci. Mater. Int., 2015, 25: 153
7 Duan Z C, Chinh N Q, Xu C, et al. Developing processing routes for the equal-channel angular pressing of age-hardenable aluminum alloys[J]. Metall. Mater. Trans., 2010, 41A: 802
8 Wang B F, Sun J Y, Zou J D, et al. Mechanical responses, texture and microstructural evolution of high purity aluminum deformed by equal channel angular pressing[J]. J. Cent. South Univ., 2015, 22: 3698
9 Liu M P, Xie X F, Zhang Z Y, et al. Deformation-induced solid-state amorphization in a nanostructured Al-Mg alloy processed by high pressure torsion[J]. Mater. Sci. Forum, 2015, 817: 627
10 Liu C H, Li X L, Wang S H, et al. A tuning nano-precipitation approach for achieving enhanced strength and good ductility in Al alloys[J]. Mater. Des., 2014, 54: 144
11 Li K, Béché A, Song M, et al. Atomistic structure of Cu-containing β'' precipitates in an Al-Mg-Si-Cu alloy[J]. Scr. Mater., 2014, 75: 86
12 Cerri E, Leo P. Influence of severe plastic deformation on aging of Al-Mg-Si alloys[J]. Mater. Sci. Eng., 2005, A410-411: 226
13 Kim W J, Kim J K, Park T Y, et al. Enhancement of strength and superplasticity in a 6061 Al alloy processed by equal-channel-angular-pressing[J]. Metall. Mater. Trans., 2002, 33A: 3155
14 Hockauf K, Meyer L W, Hockauf M, et al. Improvement of strength and ductility for a 6056 aluminum alloy achieved by a combination of equal-channel angular pressing and aging treatment[J]. J. Mater. Sci., 2010, 45: 4754
15 Roven H J, Liu M P, Werenskiold J C. Dynamic precipitation during severe plastic deformation of an Al-Mg-Si aluminium alloy[J]. Mater. Sci. Eng., 2008, A483-484: 54
16 Hockauf M, Meyer L W, Zillmann B, et al. Simultaneous improvement of strength and ductility of Al-Mg-Si alloys by combining equal-channel angular extrusion with subsequent high-temperature short-time aging[J]. Mater. Sci. Eng., 2009, A503: 167
17 Liu Y F, Wang F, Cao Y, et al. Unique defect evolution during the plastic deformation of a metal matrix composite[J]. Scr. Mater., 2019, 162: 316
18 Zhu S Q, Shih H C, Cui X Y, et al. Design of solute clustering during thermomechanical processing of AA6016 Al-Mg-Si alloy[J]. Acta Mater., 2021, 203: 116455
19 Li P, Lin Q, Zhou Y F, et al. TEM analysis of microstructure evolution process of pure tungsten under high pressure torsion[J]. Acta Metall. Sin., 2019, 55: 521
  李 萍, 林 泉, 周玉峰 等. 纯W高压扭转显微组织演化过程TEM分析[J]. 金属学报, 2019, 55: 521
20 Jiang J W, Liu M P, Liu Y, et al. Microstructure and mechanical properties of 6013 aluminium alloy processed by a combination of ECAP and preaging treatment[J]. Mater. Sci. Forum, 2017, 877: 437
21 Jia Z H, Ding L P, Cao L F, et al. The influence of composition on the clustering and precipitation behavior of Al-Mg-Si-Cu alloys[J]. Metall. Mater. Trans., 2017, 48A: 459
22 Marioara C D, Andersen S J, R?yset J, et al. Improving thermal stability in Cu-containing Al-Mg-Si alloys by precipitate optimization[J]. Metall. Mater. Trans., 2014, 45A: 2938
23 Man J, Jing L, Jie S G. The effects of Cu addition on the microstructure and thermal stability of an Al-Mg-Si alloy[J]. J. Alloys Compd., 2007, 437: 146
24 Liu M P, Wei J T, Li Y C, et al. Dynamic aging behavior and mechanical properties of an Al-Mg-Si aluminium alloy induced by equal channel angular pressing[J]. Chin. J. Mater. Res., 2016, 30: 721
  刘满平, 韦江涛, 李毅超 等. 等通道转角挤压Al-Mg-Si铝合金的动态时效特性和力学性能[J]. 材料研究学报, 2016, 30: 721
25 Jiang T H, Liu M P, Xie X F, et al. Grain boundary structure of Al-Mg alloys processed by high pressure torsion[J]. Chin. J. Mater. Res., 2014, 28: 371
  蒋婷慧, 刘满平, 谢学锋 等. 高压扭转大塑性变形Al-Mg合金中的晶界结构[J]. 材料研究学报, 2014, 28: 371
26 Dobatkin S V. On the increase of thermal stability of ultrafine grained materials obtained by severe plastic deformation[J]. Mater. Sci. Forum, 2003, 426-432: 2699
27 Wang Z X, Li H, Miao F F, et al. Improving the strength and ductility of Al-Mg-Si-Cu alloys by a novel thermo-mechanical treatment[J]. Mater. Sci. Eng., 2014, A607: 313
28 Starink M J, Wang S C. A model for the yield strength of overaged Al-Zn-Mg-Cu alloys[J]. Acta Mater., 2003, 51: 5131
29 Dunstan D J, Bushby A J. Grain size dependence of the strength of metals: The Hall-Petch effect does not scale as the inverse square root of grain size[J]. Int. J. Plast., 2014, 53: 56
30 Gubicza J, Chinh N Q, Krállics G, et al. Microstructure of ultrafine-grained fcc metals produced by severe plastic deformation[J]. Curr. Appl. Phys., 2006, 6: 194
31 Gutierrez-Urrutia I, Mu?oz-Morris M A, Morris D G. Recovery of deformation substructure and coarsening of particles on annealing severely plastically deformed Al-Mg-Si alloy and analysis of strengthening mechanisms[J]. J. Mater. Res., 2006, 21: 329
32 Mu?oz-Morris M A, Oca C G, Morris D G. Mechanical behaviour of dilute Al-Mg alloy processed by equal channel angular pressing[J]. Scr. Mater., 2003, 48: 213
33 Deschamps A, Brechet Y. Influence of predeformation and ageing of an Al-Zn-Mg alloy—II. Modeling of precipitation kinetics and yield stress[J]. Acta Mater., 1999, 47: 293
34 Moreno-Valle E C, Sabirov I, Perez-Prado M T, et al. Effect of the grain refinement via severe plastic deformation on strength properties and deformation behavior of an Al6061 alloy at room and cryogenic temperatures[J]. Mater. Lett., 2011, 65: 2917
35 Wang B B, Liu Y D, Xue P, et al. Prepration and mechanical properties of ultrafine-grained 6061 Al-alloy by friction stir process[J]. Chin. J. Mater. Res., 2021, 35: 321
  王贝贝, 刘沿东, 薛 鹏 等. 超细晶6061铝合金的搅拌摩擦制备和性能[J]. 材料研究学报, 2021, 35: 321
36 Sha G, Tugcu K, Liao X Z, et al. Strength, grain refinement and solute nanostructures of an Al-Mg-Si alloy (AA6060) processed by high-pressure torsion[J]. Acta Mater., 2014, 63: 169
37 Nurislamova G, Sauvage X, Murashkin M, et al. Nanostructure and related mechanical properties of an Al-Mg-Si alloy processed by severe plastic deformation[J]. Philos. Mag. Lett., 2008, 88: 459
38 Mohamed I F, Lee S, Edalati K, et al. Aging behavior of Al 6061 alloy processed by high-pressure torsion and subsequent aging[J]. Metall. Mater. Trans., 2015, 46A: 2664
39 Rao P N, Singh D, Brokmeier H G, et al. Effect of ageing on tensile behavior of ultrafine grained Al 6061 alloy[J]. Mater. Sci. Eng., 2015, A641: 391
40 Majchrowicz K, Pakie?a Z, Chrominski W, et al. Enhanced strength and electrical conductivity of ultrafine-grained Al-Mg-Si alloy processed by hydrostatic extrusion[J]. Mater. Charact., 2018, 135: 104
41 Rezaei M R, Toroghinejad M R, Ashrafizadeh F. Effects of ARB and ageing processes on mechanical properties and microstructure of 6061 aluminum alloy[J]. J. Mater. Process. Technol., 2011, 211: 1184
42 Gu Y, Chen J H, Liu C H, et al. Effect of pre-deformation on age- hardening and microstructure in Al-Mg-Si-Cu alloy[J]. Acta Metall. Sin., 2015, 51: 1400
  顾 媛, 陈江华, 刘春辉 等. 预变形对Al-Mg-Si-Cu合金时效硬化和显微结构的影响[J]. 金属学报, 2015, 51: 1400
Outlines

/