Research paper

Microstructure Evolution and Mechanical Properties of Ti-44Al-5Nb-1Mo-2V-0.2B Alloys in the Cross Hot-Pack Rolling Process

  • WANG Xiuqi ,
  • LI Tianrui ,
  • LIU Guohuai ,
  • GUO Ruiqi ,
  • WANG Zhaodong
Expand
  • 1 State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819, China
    2 School of Metallurgical Engineering, Anhui University of Technology, Maanshan 243000, China
LIU Guohuai, associate professor, Tel: (024)83686739, E-mail: liugh@ral.neu.edu.cn

Received date: 2022-05-18

  Revised date: 2022-08-06

  Online published: 2022-09-02

Supported by

National Natural Science Foundation of China(52071065);Fundamental Research Funds for the Central Universities(N2007007)

Abstract

TiAl alloys are highly promising for high-temperature structural applications in the aerospace and automotive industries because of their low density, excellent high-temperature strength, and resistance to creep and oxidation. Nevertheless, low-temperature brittleness and poor deformability are the main factors severely restricting the widespread application of TiAl alloys. The process of β-solidifying γ-TiAl alloys results in alloys that consist primarily of α2, γ, and B2 phases, and have superior hot workability. Further thermomechanical treatments are applied to achieve a fine microstructure and enhance the inherent ductility of γ-TiAl alloys. In this work, Ti-44Al-5Nb-1Mo-2V-0.2B alloy sheet with ultrahigh plasticity at 800oC was achieved by cross hot-pack rolling (CHPR) and one-step annealing processes. SEM, EBSD, TEM, and tensile methods were used to investigate the hot deformation behavior, and the effects of different rolling processes and heat treatments on the microstructural evolution and mechanical properties of the alloy. The results show that the CHPR sheet had a more highly uniform deformation microstructure along the thickness direction and sheet plane compared with that of a unidirectional hot-pack rolled (UHPR) sheet, which consisted of residual lamellar colonies and equiaxed γ, α2, and B2 grains at colony boundaries. The size of the residual lamellar colonies was significantly smaller and the content was lower in the CHPR sheet compared with the UHPR sheet. This was due to a large number of broken residual lamellae and complete recrystallization under the combined action of a bidirectional shear force and compressive stress during the CHPR process. The high-temperature flow-softening mechanisms of TiAl alloy in the CHPR process mainly included bending and kinked lamellae, β/B2 coordinated deformation, phase-transformation decomposition of α2/γ lamellar, and dynamic recrystallization induced by primary and secondary twinning. To achieve further grain refinement, subsequent annealing of the CHPR-processed TiAl alloy was performed at 1200-1340oC. A multiphase equiaxed microstructure with fine lamellar colonies was obtained at 1200oC and a nearly complete lamellar microstructure was obtained at 1340oC. Moreover, the room-temperature and high-temperature tensile properties of UHPR and CHPR sheets in the horizontal and vertical directions were compared with samples annealed at 1200oC. The tensile properties of the CHPR sheets were more uniform in both directions. The multiphase equiaxed microstructure obtained in the CHPR alloy annealed at 1200oC had the best strength-plasticity balance with a tensile strength of 624 MPa (515 MPa) and elongation of 1.32% (107.0%) at room temperature (800oC). According to the fracture behavior, the fracture mode of these alloy sheets was translamellar or cleavage fracture at room temperature. Conversely, the fracture mode changed to ductile fracture at 800oC, and the failure mechanism was mainly via microhole coupling. The fractures in the annealed sheets (1200oC) had small and deep dimples, indicating optimal tensile elongation. The uniform and fine lamellar structure and equiaxed microstructure can hinder crack propagation and achieve enhanced mechanical properties.

Cite this article

WANG Xiuqi , LI Tianrui , LIU Guohuai , GUO Ruiqi , WANG Zhaodong . Microstructure Evolution and Mechanical Properties of Ti-44Al-5Nb-1Mo-2V-0.2B Alloys in the Cross Hot-Pack Rolling Process[J]. Acta Metall Sin, 2024 , 60(1) : 95 -106 . DOI: 10.11900/0412.1961.2022.00247

References

1 Yang R. Advances and challenges of TiAl base alloys [J]. Acta Metall. Sin., 2015, 51: 129
  杨 锐. 钛铝金属间化合物的进展与挑战 [J]. 金属学报, 2015, 51: 129
2 Kim Y W, Kim S L. Advances in gammalloy materials-processes-application technology: Successes, dilemmas, and future [J]. JOM, 2018, 70: 553
3 Wu X H. Review of alloy and process development of TiAl alloys [J]. Intermetallics, 2006, 14: 1114
4 Dimiduk D M. Gamma titanium aluminide alloys—An assessment within the competition of aerospace structural materials [J]. Mater. Sci. Eng., 1999, A263: 281
5 Habel U, Heutling F, Kunze C, et al. Forged intermetallic γ-TiAl based alloy low pressure turbine blade in the geared turbofan [A]. Proceedings of the 13th World Conference on Titanium [C]. Hoboken: Wliey, 2016: 1223
6 Liu G H, Wang Z D, Fu T L, et al. Study on the microstructure, phase transition and hardness for the TiAl-Nb alloy design during directional solidification [J]. J. Alloys Compd., 2015, 650: 45
7 Appel F, Clemens H, Fischer F D. Modeling concepts for intermetallic titanium aluminides [J]. Prog. Mater. Sci., 2016, 81: 55
8 Jin Y G, Wang J N, Yang J, et al. Microstructure refinement of cast TiAl alloys by β solidification [J]. Scr. Mater., 2004, 51: 113
9 Li T R, Liu G H, Xu M, et al. Microstructures and high temperature tensile properties of Ti-43Al-4Nb-1.5Mo alloy in the canned forging and heat treatment process [J]. Acta Metall. Sin., 2017, 53: 1055
  李天瑞, 刘国怀, 徐 莽 等. Ti-43Al-4Nb-1.5Mo合金包套锻造与热处理过程的微观组织及高温拉伸性能 [J]. 金属学报, 2017, 53: 1055
10 Niu H Z, Kong F T, Xiao S L, et al. Effect of pack rolling on microstructures and tensile properties of as-forged Ti-44Al-6V-3Nb-0.3Y alloy [J]. Intermetallics, 2012, 21: 97
11 Clemens H, Chladil H F, Wallgram W, et al. In and ex situ investigations of the β-phase in a Nb and Mo containing γ-TiAl based alloy [J]. Intermetallics, 2008, 16: 827
12 Clemens H, Wallgram W, Kremmer S, et al. Design of novel β-solidifying TiAl alloys with adjustable β/B2-phase fraction and excellent hot-workability [J]. Adv. Eng. Mater., 2008, 10: 707
13 Tetsui T, Shindo K, Kobayashi S, et al. Strengthening a high-strength TiAl alloy by hot-forging [J]. Intermetallics, 2003, 11: 299
14 Li T R, Liu G H, Xu M, et al. High temperature deformation and control of homogeneous microstructure during hot pack rolling of Ti-44Al-5Nb-(Mo, V, B) alloys: The impact on mechanical properties [J]. Mater. Sci. Eng., 2019, A751: 1
15 Zhang W J, Lorenz U, Appel F. Recovery, recrystallization and phase transformations during thermomechanical processing and treatment of TiAl-based alloys [J]. Acta Mater., 2000, 48: 2803
16 Niu H Z, Kong F T, Chen Y Y, et al. Low-temperature superplasticity of forged Ti-43Al-4Nb-2Mo-0.5B alloy [J]. J. Alloys Compd., 2012, 543: 19
17 Imayev V M, Salishchev G A, Shagiev M R, et al. Low-temperature superplasticity of submicrocrystalline Ti-48Al-2Nb-2Cr alloy produced by multiple forging [J]. Scr. Mater., 1998, 40: 183
18 Janschek P. Wrought TiAl blades [J]. Mater. Today: Proc., 2015, 2(): S92
19 Paul J D H, Lorenz U, Oehring M, et al. Up-scaling the size of TiAl components made via ingot metallurgy [J]. Intermetallics, 2013, 32: 318
20 Tang B, Cheng L, Kou H C, et al. Hot forging design and microstructure evolution of a high Nb containing TiAl alloy [J]. Intermetallics, 2015, 58: 7
21 Zeng S W, Zhao A M, Luo L, et al. Development of β-solidifying γ-TiAl alloys sheet [J]. Mater. Lett., 2017, 198: 31
22 Davim J P. Modern Manufacturing Engineering [M]. Cham: Springer, 2015: 41
23 Zhi C C, Ma L F, Huang Q X, et al. Effect of cross rolling on the edge microstructure and formability of AZ31B magnesium alloy [J]. Rare Met. Mater. Eng., 2018, 47: 1555
  支晨琛, 马立峰, 黄庆学 等. 交叉轧制对AZ31B镁合金边部组织及成形性的影响 [J]. 稀有金属材料与工程, 2018, 47: 1555
24 Kim D G, Lee K M, Lee J S, et al. Evolution of microstructures and textures in magnesium AZ31 alloys deformed by normal and cross-roll rolling [J]. Mater. Lett., 2012, 75: 122
25 Chino Y, Sassa K, Kamiya A, et al. Enhanced formability at elevated temperature of a cross-rolled magnesium alloy sheet [J]. Mater. Sci. Eng., 2006, A441: 349
26 Fan C H, Zheng D S, Chen X H, et al. Effect of large strain cross rolling on microstructure and properties of Al-Li alloy plates with high magnesium content [J]. Trans. Nonferrous Met. Soc. China, 2019, 29: 263
27 Liu D K, Huang G S, Gong G L, et al. Influence of different rolling routes on mechanical anisotropy and formability of commercially pure titanium sheet [J]. Trans. Nonferrous Met. Soc. China, 2017, 27: 1306
28 Chen W, Wang H D, Lin Y C, et al. The dynamic responses of lamellar and equiaxed near β-Ti alloys subjected to multi-pass cross rolling [J]. J. Mater. Sci. Technol., 2020, 43: 220
29 Chen W, Lv Y P, Wang H D, et al. On the {10 1 ˉ 1} twin-accommodated mechanisms in equiaxed near β-Ti alloys operating by unidirectional and cross rolling [J]. Mater. Sci. Eng., 2020, A769: 138516
30 Wang D Z, Ji Y X, Wu Z Z. Effects of cross rolling on texture, mechanical properties and anisotropy of pure Mo plates [J]. Trans. Nonferrous Met. Soc. China, 2020, 30: 2170
31 Zhu J L, Liu S F, Cao Y, et al. Effect of cross rolling cycle on the deformed and recrystallized gradient in high-purity tantalum plate [J]. Acta Metall. Sin., 2019, 55: 1019
  祝佳林, 刘施峰, 曹 宇 等. 交叉轧制周期对高纯Ta板变形及再结晶梯度的影响 [J]. 金属学报, 2019, 55: 1019
32 Fan H Y, Liu S F, Li L J, et al. Largely alleviating the orientation dependence by sequentially changing strain paths [J]. Mater. Des., 2016, 97: 464
33 Liu S F, Fan H Y, Deng C, et al. Through-thickness texture in clock-rolled tantalum plate [J]. Int. J. Refract. Met. Hard Mater., 2015, 48: 194
34 Cerreta E, Mahajan S. Formation of deformation twins in TiAl [J]. Acta Mater., 2001, 49: 3803
35 Hu D, Jiang H. Martensite in a TiAl alloy quenched from beta phase field [J]. Intermetallics, 2015, 56: 87
36 Wan Z P, Sun Y, Hu L X, et al. Experimental study and numerical simulation of dynamic recrystallization behavior of TiAl-based alloy [J]. Mater. Des., 2017, 122: 11
37 Niu H Z, Tong R L, Chen X J, et al. Rapid decomposition of lamellar microstructure and enhanced hot workability of an as-cast triphase Ti-45Al-6Nb-1Mo alloy via one-step alpha-extrusion & annealing [J]. Mater. Sci. Eng., 2021, A801: 140438
38 Li T R, Liu G H, Xu M, et al. Effects of hot-pack rolling process on microstructure, high-temperature tensile properties, and deformation mechanisms in hot-pack rolled thin Ti-44Al-5Nb-(Mo, V, B) sheets [J]. Mater. Sci. Eng., 2019, A764: 138197
39 Liu X F, Liu D, Liu R C, et al. Microstructure and tensile properties of Ti-43.5Al-4Nb-1Mo-0.1B alloy processed by hot canned extrusion [J]. Acta Metall. Sin., 2020, 56: 979
  刘先锋, 刘 冬, 刘仁慈 等. Ti-43.5Al-4Nb-1Mo-0.1B合金的包套热挤压组织与拉伸性能 [J]. 金属学报, 2020, 56: 979
40 Han J C, Dong J, Zhang S Z, et al. Microstructure evolution and tensile properties of conventional cast TiAl-based alloy with trace Ni addition [J]. Mater. Sci. Eng., 2018, A715: 41
41 Liang X P, Liu Y, Li H Z, et al. An investigation on microstructural and mechanical properties of powder metallurgical TiAl alloy during hot pack-rolling [J]. Mater. Sci. Eng., 2014, A619: 265
42 Zhou H T, Kong F T, Wu K, et al. Hot pack rolling nearly lamellar Ti-44Al-8Nb-(W, B, Y) alloy with different rolling reductions: Lamellar colonies evolution and tensile properties [J]. Mater. Des., 2017, 121: 202
43 Huang Z W, Lin J P, Zhao Z X, et al. Fatigue response of a grain refined TiAl alloy Ti-44Al-5Nb-1W-1B with varied surface quality and thermal exposure history [J]. Intermetallics, 2017, 85: 1
Outlines

/