Dynamics Evolution and Mechanical Properties of the Erosion Process of Ag-CuO Contact Materials
Received date: 2021-11-18
Revised date: 2022-06-29
Online published: 2022-07-13
Supported by
National Natural Science Foundation of China(52007137);National Natural Science Foundation of China(51607132);China Postdoctoral Science Foundation(2021M702566);Shaanxi Provincial Education Department Special project(20JK0661)
Silver-copper oxide (Ag-CuO) materials are gaining more and more interest in the low voltage switches' field owing to their lower material transfer characteristics. However, with increasing arc erosion during the make-and-break operations, the CuO microstructure's dynamic evolution is complicated by the interaction of the convection-diffusion with the flow path. Therefore, tuning the microstructure to maximize the arc erosion properties of Ag-CuO contact materials using the dynamic model is crucial for their application in switches. In this study, three-dimensional models of Ag-CuO contacts were reconstructed by phase identification and microstructure analysis, using the microstructure characteristics of the Ag-45CuO (skeleton-restricted Ag-CuO) and Ag-20CuO (island-restricted Ag-CuO) contact materials. In parallel, the arc erosion dynamics of the microstructure evolution and skeleton reconstruction process were tracked and explored by employing computational fluid dynamics simulations. Experiment and simulation findings both indicate that the repetitive thermal effect can cause the formation of a cratered and smooth molten pool surface in island-restricted Ag-CuO and skeleton-restricted Ag-CuO, respectively. The local gap of skeleton-restricted Ag-CuO contact can function as the driving force to reconstruct the CuO skeleton, the newly formed CuO with an anisotropic microstructure, which can impede Ag's segregation and evaporation in the molten pool. The restructures of CuO are unimportant for the island-restricted Ag-CuO contact, and the continuous erosion impact of island CuO can render the contact invalid. Additionally, the CuO microstructure's effect on the mechanical properties of Ag-CuO contacts was examined by employing the local three-dimensional models, which were reconstructed using the visual recognition technology combined with the finite element approach. The findings exhibit that the skeleton CuO structure was less susceptible to stress and strain concentration at the molten pool surface compared with the island CuO structure, which can efficiently disperse the local effect force on the molten pool and can substantially enhance the Ag-CuO contact's erosion resistance.
Minjing MA , Yinhu QU , Zhe WANG , Jun WANG , Dan DU . Dynamics Evolution and Mechanical Properties of the Erosion Process of Ag-CuO Contact Materials[J]. Acta Metall Sin, 2022 , 58(10) : 1305 -1315 . DOI: 10.11900/0412.1961.2021.00498
| 1 | Lin Z J. Microstructure control and properties of Ag-SnO2 and Ag-Ni electrical contact materials [D]. Shenyang: Northeastern University, 2017 |
| 1 | 林智杰. Ag-SnO2和Ag-Ni电触头材料微结构调控与性能研究 [D]. 沈阳: 东北大学, 2017 |
| 2 | He X Q, Fu H D, Zhang H T, et al. Machine learning aided rapid discovery of high performance silver alloy electrical contact materials [J]. Acta Metall. Sin., 2022, 58: 816 |
| 2 | 何兴群, 付华栋, 张洪涛 等. 机器学习辅助高性能银合金电接触材料的快速发现 [J]. 金属学报, 2022, 58: 816 |
| 3 | Han Y, Wang H S, Cao Y D, et al. Mechanical and electrical properties of Cu-W composites with micro-oriented structures [J]. Acta Metall. Sin., 2021, 57: 1009 |
| 3 | 韩 颖, 王宏双, 曹云东 等. 微观定向结构Cu-W复合材料的力学与电学性能 [J]. 金属学报, 2021, 57: 1009 |
| 4 | Wu C P, Yi D Q, Wang W, et al. Influence of alloy components on arc erosion morphology of Ag/MeO electrical contact materials [J]. Trans. Nonferrous Met. Soc. China, 2016, 26: 185 |
| 5 | Wang B J, Saka N, Rabinowicz E. Static gap erosion of Ag-CdO electrodes [J]. IEEE. Trans. Compon., Hybrids, Manuf. Technol., 1991, 14: 374 |
| 6 | Li G J, Ma Y Y, Zhang X L, et al. Interface strengthening and fracture characteristics of the Ag-based contact materials reinforced with nanoporous SnO2 (Cu, CuO) phases [J]. Appl. Surf. Sci., 2021, 543: 148812 |
| 7 | Chen S Y, Wang J, Yuan Z, et al. Microstructure and arc erosion behaviors of Ag-CuO contact material prepared by selective laser melting [J]. J. Alloys Compd., 2021, 860: 158494 |
| 8 | Han X L, Wang Z, Li G J, et al. Interfacial thermal stress relief in Ag-SnO2 composites by in situ formation of CuO nanoparticles additive on SnO2 [J]. Ceram. Int., 2022, 48: 16638 |
| 9 | Tao Q Y, Zhou X L, Zhou Y H, et al. Contact resistance and arc erosion morphology of AgCuO electrical contact material [J]. Rare Met. Mater. Eng., 2015, 44: 1219 |
| 9 | 陶麒鹦, 周晓龙, 周允红 等. Ag-CuO电触头材料的接触电阻及电弧侵蚀形貌分析 [J]. 稀有金属材料与工程, 2015, 44: 1219 |
| 10 | Wang Z, Wang Y P. Impact of convection-diffusion and flow-path interactions on the dynamic evolution of microstructure: Arc erosion behavior of Ag-SnO2 contact materials [J]. J. Alloys Compd., 2019, 774: 1046 |
| 11 | Zhang J F, Sun X J, Tong H, et al. Mechanism investigation on effects of glass composition on Ag/Si contact for crystalline silicon solar cells [J]. J. Mater. Sci.: Mater. Electron., 2021, 32: 6778 |
| 12 | Liu S T, Sun Q Y, Wang J B, et al. Exploration of the influence mechanism of La doping on the arc erosion resistance of Ag/SnO2 contact materials by a laser-simulated arc [J]. J. Mater. Eng. Perform., 2021, 30: 7577 |
| 13 | Wu Q, Xu G F, Yuan M, et al. Influence of operation numbers on arc erosion of Ag/CuO electrical contact material [J]. J. Mater. Sci.: Mater. Electron., 2020, 31: 2497 |
| 14 | Zhou X, Cui X L, Chen M, et al. Evaporation erosion of contacts under static arc by gas dynamics and molten pool simulation [J]. IEEE. Trans. Plasma Sci., 2015, 43: 4149 |
| 15 | Wang Y L, Liang S H, Li Z B. Experiment and simulation analysis of surface structure for CuW contact after arc erosion [J]. Mater. Sci. Technol., 2015, 31: 243 |
| 16 | Wang J, Kang Y Q, Wang C. Microstructure and vacuum arc characteristics of CuO skeletal structure Ag-CuO contact materials [J]. J. Alloys Compd., 2016, 686: 702 |
| 17 | dos Santos J F, Staron P, Fischer T, et al. Understanding precipitate evolution during friction stir welding of Al-Zn-Mg-Cu alloy through in-situ measurement coupled with simulation [J]. Acta Mater., 2018, 148: 163 |
| 18 | Wang Z, Wang X, Tong Y G, et al. Impact of structure and flow-path on in situ synthesis of AlN: Dynamic microstructural evolution of Al-AlN-Si materials [J]. Sci. China Mater., 2018, 61: 948 |
| 19 | Duan C X, Yu Y, Yang P F, et al. Engineering new defects in MIL-100 (Fe) via a mixed-ligand approach to effect enhanced volatile organic compound adsorption capacity [J]. Ind. Eng. Chem. Res., 2020, 59: 774 |
| 20 | Wang Z, Zhang Y J, Jiang S, et al. The red deer antler: Bioinspired design of an Al-Si composite with a fenestrated network-particle structure [J]. J. Materiomics, 2020, 6: 545 |
| 21 | Davis J R. Metals Handbook [M]. 2nd Ed., Materials Park, Ohio: ASM International, 1998: 415 |
| 22 | Lyon R N. Liquid-Metals Handbook [M]. 2nd Ed., Washington: U. S. Government Printing Office, 1952: 38 |
| 23 | Ayyar A, Chawla N. Microstructure-based modeling of crack growth in particle reinforced composites [J]. Compos. Sci. Technol., 2006, 66: 1980 |
| 24 | Wu Y, Yang L H, Xu T F, et al. Combined effect of rarefaction and effective viscosity on micro-elasto-aerodynamic lubrication performance of gas microbearings [J]. Micromachines, 2019, 10: 657 |
| 25 | Ding J X, Tian W B, Wang D D, et al. Corrosion and degradation mechanism of Ag/Ti3AlC2 composites under dynamic electric arc discharge [J]. Corros. Sci., 2019, 156: 147 |
| 26 | Zhang X H, Zhang Y, Tian B H, et al. Arc erosion behavior of the Al2O3-Cu/(W, Cr) electrical contacts [J]. Composites, 2019, 160B: 110 |
| 27 | Li H Y, Li P, Wang J, et al. Microstructure and properties of AgSnO2 contact materials prepared by cold spray [J]. Rare Met. Mater. Eng., 2017, 46: 3858 |
| 27 | 李海燕, 李 鹏, 王 军 等. 冷喷涂AgSnO2触点涂层的组织与性能 [J]. 稀有金属材料与工程, 2017, 46: 3858 |
| 28 | Ding J X, Tian W B, Wang D D, et al. Arc erosion and degradation mechanism of Ag/Ti2AlC composite [J]. Acta Metall. Sin., 2019, 55: 627 |
| 28 | 丁健翔, 田无边, 汪丹丹 等. Ag/Ti2AlC复合材料的电弧侵蚀及退化机理 [J]. 金属学报, 2019, 55: 627 |
/
| 〈 |
|
〉 |