Research paper

Effect of Heat Treatment Temperature on Microstructure and Mechanical Properties of Ti0.5Zr1.5NbTa0.5Sn0.2 High-Entropy Alloy

  • Linzhi HAN ,
  • Juan MU ,
  • Yongkang ZHOU ,
  • Zhengwang ZHU ,
  • Haifeng ZHANG
Expand
  • 1.Key Laboratory for Anisotropy and Texture of Materials, Ministry of Education, School of Materials Science and Engineering, Northeastern University, Shenyang 110819, China
    2.Shi -changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
MU Juan, associate professor, Tel: (024)83691568, E-mail: muj@atm.neu.edu.cn

Received date: 2021-12-13

  Revised date: 2022-04-12

  Online published: 2022-06-13

Supported by

National Natural Science Foundation of China(51771049);National Natural Science Foundation of China(51790484);National Key Laboratory Foundation of Science and Technology on Materials under Shock and Impact(JCKYS20-20602005)

Abstract

Refractory high-entropy alloys (RHEAs) have great application potential in extreme conditions due to their outstanding high-temperature properties. However, several issues, such as high density, poor room temperature plasticity, and high cost limit their practical application. A new Ti0.5Zr1.5NbTa0.5Sn0.2 (molar ratio) RHEA with a medium density of approximately 8.0 g/cm3 was prepared to address the aforementioned issues; the effects of heat treatment temperature on the alloy's microstructure and mechanical properties were systematically examined. The findings indicate that as-cast Ti0.5Zr1.5NbTa0.5Sn0.2 RHEA contains Zr-rich and Ta-rich bcc phases and lath-like Zr5Sn3 intermetallics in the crystal. The volume fraction of the Ta-rich bcc phase gradually decreases with the increase in heat treatment temperature, and Zr5Sn3 intermetallic first increases and then decreases. The sample presents a near single-phase bcc structure when the heat treatment temperature is 1400oC. A series of samples have good compressive plastic deformation ability under quasi-static conditions, and the alloy's yield strength increased gradually with an increasing heat treatment temperature. The sample's yield strength quenched at 1400oC is as high as 1749 MPa. The alloy showed strain rate strengthening effect under dynamic loading, and the yield strength significantly increased. The sample's yield strength quenched at 1400oC reaches 2750 MPa; however, the plastic deformation ability is reduced. The reason why the strength increases with the heat treatment temperature is that the 9.8% average atomic size difference results in a significant solid solution strengthening effect.

Cite this article

Linzhi HAN , Juan MU , Yongkang ZHOU , Zhengwang ZHU , Haifeng ZHANG . Effect of Heat Treatment Temperature on Microstructure and Mechanical Properties of Ti0.5Zr1.5NbTa0.5Sn0.2 High-Entropy Alloy[J]. Acta Metall Sin, 2022 , 58(9) : 1159 -1168 . DOI: 10.11900/0412.1961.2021.00551

References

1 Chen T K, Shun T T, Yeh J W, et al. Nanostructured nitride films of multi-element high-entropy alloys by reactive DC sputtering [J]. Surf. Coat. Technol., 2004, 188-189: 193
2 Yeh J W, Lin S J, Chin T S, et al. Formation of simple crystal structures in Cu-Co-Ni-Cr-Al-Fe-Ti-V alloys with multiprincipal metallic elements [J]. Metall. Mater. Trans., 2004, 35A: 2533
3 Yeh J W, Chen S K, Lin S J, et al. Nanostructured high-entropy alloys with multiple principal elements: novel alloy design concepts and outcomes [J]. Adv. Eng. Mater., 2004, 6: 299
4 Miracle D B, Senkov O N. A critical review of high entropy alloys and related concepts [J]. Acta Mater., 2017, 122: 448
5 Senkov O N, Wilks G B, Scott J M, et al. Mechanical properties of Nb25Mo25Ta25W25 and V20Nb20Mo20Ta20W20 refractory high entropy alloys [J]. Intermetallics, 2011, 19: 698
6 Zou Y, Maiti S, Steurer W, et al. Size-dependent plasticity in an Nb25Mo25Ta25W25 refractory high-entropy alloy [J]. Acta Mater., 2014, 65: 85
7 Chen J, Zhou X Y, Wang W L, et al. A review on fundamental of high entropy alloys with promising high-temperature properties [J]. J. Alloys Compd., 2018, 760: 15
8 Chen G, Luo T, Shen S C, et al. Research progress in refractory high-entropy alloys [J]. Mater. Rep., 2021, 35: 17064
8 陈 刚, 罗 涛, 沈书成 等. 难熔高熵合金的研究进展 [J]. 材料导报, 2021, 35: 17064
9 Senkov O N, Miracle D B, Chaput K J, et al. Development and exploration of refractory high entropy alloys—A review [J]. J. Mater. Res., 2018, 33: 3092
10 Li T X, Lu Y P, Cao Z Q, et al. Opportunity and challenge of refractory high-entropy alloys in the field of reactor structural materials [J]. Acta Metall. Sin., 2021, 57: 42
10 李天昕, 卢一平, 曹志强 等. 难熔高熵合金在反应堆结构材料领域的机遇与挑战 [J]. 金属学报, 2021, 57: 42
11 Yang S F, Wen J N, Mo J, et al. Microstructure and strengthening mechanisms in FCC-structured single-phase TiC-CoCrFeCuNiAl0.3 HEACs with deformation twinning [J]. Mater. Sci. Eng., 2021, A814: 141215
12 Yang S F, Zhang Y, Yan X, et al. Deformation twins and interface characteristics of nano-Al2O3 reinforced Al0.4FeCrCo1.5NiTi0.3 high entropy alloy composites [J]. Mater. Chem. Phys., 2018, 210: 240
13 An Z B, Mao S C, Liu Y N, et al. A novel HfNbTaTiV high-entropy alloy of superior mechanical properties designed on the principle of maximum lattice distortion [J]. J. Mater. Sci. Technol., 2021, 79: 109
14 Hu Y M, Liu X D, Guo N N, et al. Microstructure and mechanical properties of NbZrTi and NbHfZrTi alloys [J]. Rare Met, 2019, 38: 840
15 Hu M l, Song W D, Duan D B, et al. Dynamic behavior and microstructure characterization of TaNbHfZrTi high-entropy alloy at a wide range of strain rates and temperatures [J]. Int. J. Mech. Sci., 2020, 182: 105738
16 Dirras G, Lilensten L, Djemia P, et al. Elastic and plastic properties of as-cast equimolar TiHfZrTaNb high-entropy alloy [J]. Mater. Sci. Eng., 2016, A654: 30
17 Senkov O N, Scott J M, Senkova S V, et al. Microstructure and room temperature properties of a high-entropy TaNbHfZrTi alloy [J]. J. Alloys Compd., 2011, 509: 6043
18 Senkov O N, Semiatin S L. Microstructure and properties of a refractory high-entropy alloy after cold working [J]. J. Alloys Compd., 2015, 649: 1110
19 Wang R X, Tang Y, Li S, et al. Novel metastable engineering in single-phase high-entropy alloy [J]. Mater. Des., 2019, 162: 256.
20 Senkov O N, Woodward C, Miracle D B. Microstructure and properties of aluminum-containing refractory high-entropy alloys [J]. JOM, 2014, 66: 2030
21 Voyiadjis G Z, Abed F H. Microstructural based models for bcc and fcc metals with temperature and strain rate dependency [J]. Mech. Mater., 2005, 37: 355
22 Chen H H, Zhang X F, Liu C, et al. Research progress on impact deformation behavior of high-entropy alloys [J]. Explos. Shock Waves, 2021, 41: 041402
22 陈海华, 张先锋, 刘 闯 等. 高熵合金冲击变形行为研究进展 [J]. 爆炸与冲击, 2021, 41: 041402
23 Dirras G, Couque H, Lilensten L, et al. Mechanical behavior and microstructure of Ti20Hf20Zr20Ta20Nb20 high-entropy alloy loaded under quasi-static and dynamic compression conditions [J]. Mater. Charact., 2016, 111: 106
24 Zhang Z R, Zhang H, Tang Y, et al. Microstructure, mechanical properties and energetic characteristics of a novel high-entropy alloy HfZrTiTa0.53 [J]. Mater. Des., 2017, 133: 435
25 Takeuchi A, Inoue A. Classification of bulk metallic glasses by atomic size difference, heat of mixing and period of constituent elements and its application to characterization of the main alloying element [J]. Mater. Trans., 2005, 46: 2817
26 Wu Y D, Si J J, Lin D Y, et al. Phase stability and mechanical properties of AlHfNbTiZr high-entropy alloys [J]. Mater. Sci. Eng., 2018, A724: 249
27 Yu Q, Chen Y J, Fang Y. Heterogeneity in chemical distribution and its impact in high-entropy alloys [J]. Acta Metall. Sin., 2021, 57: 393
27 余 倩, 陈雨洁, 方 研. 高熵合金中的元素分布规律及其作用 [J]. 金属学报, 2021, 57: 393
28 Zhang Y, Zhou Y J, Lin J P, et al. Solid-solution phase formation rules for multi-component alloys [J]. Adv. Eng. Mater., 2008, 10: 534.
29 Wen C, Mo W W, Tian Y W, et al. Research progress on solid solution strengthening of high entropy alloys [J]. Mater. Rep., 2021, 35: 17081
29 文 成, 莫湾湾, 田玉琬 等. 高熵合金固溶强化问题的研究进展 [J]. 材料导报, 2021, 35: 17081
30 Yang Y, He Q F. Lattice distortion in high-entropy alloys [J]. Acta Metall. Sin., 2021, 57: 385
30 杨 勇, 赫全锋. 高熵合金中的晶格畸变 [J]. 金属学报, 2021, 57: 385
Outlines

/