Anisotropy of Stress Rupture Property of Ni Base Single Crystal Superalloy DD432
Received date: 2022-03-11
Revised date: 2022-06-01
Online published: 2022-06-06
Supported by
National Natural Science Foundation of China(51971214)
Ni base superalloys have been extensively used in advanced aeroengine. With the development of modern aviation industry, high demands are being placed on the comprehensive performance of Ni base superalloys at high temperatures. To meet this demand, numerous refractory alloy elements are added to Ni base superalloys. However, in this way, the temperature bearing capacity of the alloy is enhanced, while the microstructure stability is reduced. Therefore, some scholars proposed to develop single crystal blades with various orientations through the anisotropy of a single crystal alloy. The stress rupture anisotropies of a Ni base single crystal superalloy DD432 under 760oC, 810 MPa and 1000oC, 280 MPa have been investigated in this study. The stress rupture properties of Ni base single crystal superalloy DD432 that deviated from <001>, <011>, and <111> with certain degrees were measured. It is discovered that rafting does not occur in specimens with three orientations, and the stress rupture life anisotropy of specimens is visible at 760oC and 810 MPa. Furthermore, the stress rupture life of specimens with <111> orientation is the best, and as the orientation deviation degree increases, the stress rupture life gradually decreases. The stress rupture property of specimens with <001> orientation is lower than that of specimens with <111> orientation, and the stress rupture life increases with increasing orientation deviation degree. The creep resistance of specimens with <011> orientation is the lowest, and the stress rupture property is also enhanced as the orientation deviation degree increases. Rafting occurred in all the specimens with three orientations under the conditions of 1000oC and 280 MPa, and the stress rupture property anisotropy of specimens decreased, but still existed. The stress rupture property of specimens with <111> orientation was slightly better than that of specimens with <001> orientation, and the stress rupture property of specimens with <011> orientation was still the worst, although it improved. A difference still exists in the stress rupture life as the degree of orientation deviation changes. However, there is no visible linear tendency.
ZHANG Zixuan , YU Jinjiang , LIU Jinlai . Anisotropy of Stress Rupture Property of Ni Base Single Crystal Superalloy DD432[J]. Acta Metall Sin, 2023 , 59(12) : 1559 -1567 . DOI: 10.11900/0412.1961.2022.00108
| 1 | Jiang K H, Chen J W, Jing F L, et al. Thermomechanical fatigue on the nickel based single crystal superalloy DD6 with film cooling hole[J]. J. Aerosp. Power, 2019, 34: 980 |
| 蒋康河, 陈竞炜, 荆甫雷 等. 镍基单晶高温合金DD6气膜孔热机械疲劳试验[J]. 航空动力学报, 2019, 34: 980 | |
| 2 | Gell M, Duhl D N, Giamei A F. The development of single crystal superalloy turbine blades[A]. Superalloys[C]. Champion, PA: TMS, 1980: 205 |
| 3 | Sun X F, Jin T, Zhou Y Z, et al. Research progress of nickel-base single crystal superalloys[J]. Mater. China, 2012, 31(12): 1 |
| 孙晓峰, 金 涛, 周亦胄 等. 镍基单晶高温合金研究进展[J]. 中国材料进展, 2012, 31(12): 1 | |
| 4 | Gui Z L. Research status of anisotropy of Russian single crystal superalloys[J]. Aeronaut. Manufact. Eng., 1997, (1): 20 |
| 桂忠楼. 俄罗斯单晶高温合金各向异性的研究现状[J]. 航空制造工程, 1997, (1): 20 | |
| 5 | Rae C M F, Reed R C. Primary creep in single crystal superalloys: Origins, mechanisms and effects[J]. Acta Mater., 2007, 55: 1067 |
| 6 | Matan N, Cox D C, Carter P, et al. Creep of CMSX-4 superalloy single crystals: Effects of misorientation and temperature[J]. Acta Mater., 1999, 47: 1549 |
| 7 | Bai L. Creep behavior and constitutive modeling of single crystal nickel-base superalloys[D]. Beijing: Beihang University, 2010 |
| 白 露. 镍基单晶合金高温蠕变行为及其本构理论研究[D]. 北京: 北京航空航天大学, 2010 | |
| 8 | Yu J, Li J R, Han M, et al. Anisotropy of stress rupture properties of DD6 single crystal superalloy at 980oC/250 MPa near orientation [001][J]. J. Mater. Eng., 2012, (4): 1 |
| 喻 健, 李嘉荣, 韩 梅 等. 近[001]取向DD6单晶高温合金980℃/250 MPa持久性能各向异性研究[J]. 材料工程, 2012, (4): 1 | |
| 9 | Hu B, Li S S, Pei Y L, et al. Influence of small misorientation from <111> on creep properties of a Ni-based single crystal superalloy[J]. Acta Metall. Sin., 2019, 55: 1204 |
| 胡 斌, 李树索, 裴延玲 等. <111>取向小角偏离对一种镍基单晶高温合金蠕变性能的影响[J]. 金属学报, 2019, 55: 1204 | |
| 10 | Xu J H, Li L F, Liu X G, et al. Thermal-stress coupling effect on microstructure evolution of a fourth-generation nickel-based single-crystal superalloy at 1100oC[J]. Acta Metall. Sin., 2021, 57: 205 |
| 徐静辉, 李龙飞, 刘心刚 等. 热力耦合对一种第四代镍基单晶高温合金1100℃蠕变组织演变的影响[J]. 金属学报, 2021, 57: 205 | |
| 11 | Han G M. Investigation of anisotropic stress rupture, creep and thermo-mechanical fatigue properties of SRR99 alloy[D]. Shenyang: Institute of Metal Research, Chinese Academy of Sciences, 2010 |
| 韩国明. SRR99合金持久蠕变各向异性行为及热机械疲劳性能的研究article-title>[D]. 沈阳: 中国科学院金属研究所, 2010 | |
| 12 | Liu J L. Tensile property and stress rupture property and microstructure evolution of a nickel base single crystal superalloy[D]. Shenyang: Institute of Metal Research, Chinese Academy of Sciences, 2002 |
| 刘金来. 一种镍基单晶高温合金的拉伸、持久性能及组织演化[D]. 沈阳: 中国科学院金属研究所, 2002 | |
| 13 | Knowles D M, Chen Q Z. Superlattice stacking fault formation and twinning during creep in γ/γ' single crystal superalloy CMSX-4[J]. Mater. Sci. Eng., 2003, A340: 88 |
| 14 | Sui T X, Shi D Q, Wang X P, et al. Analysis on the stress rupture properties' anisotropy of single crystal superalloy[J]. J. Aerosp. Power, 2021, 36: 1286 |
| 隋天校, 石多奇, 王相平 等. 单晶高温合金持久性能各向异性分析[J]. 航空动力学报, 2021, 36: 1286 | |
| 15 | Rae C M F, Matan N, Reed R C. The role of stacking fault shear in the primary creep of [001]-oriented single crystal superalloys at 750oC and 750 MPa[J]. Mater. Sci. Eng., 2001, A300: 125 |
| 16 | Rae C M F, Matan N, Cox D C, et al. On the primary creep of CMSX-4 superalloy single crystals[J]. Metall. Mater. Trans., 2000, 31A: 2219 |
| 17 | Peng Z, Glatzel U, Link T, et al. Change of phase morpholigies during creep of CMSX-4 at 1253 K[J]. Scr. Mater., 1996, 34: 221 |
| 18 | Caron P, Ohta Y, Nakagawa Y G, et al. Creep deformation anisotropy in single crystal superalloys[A]. Superalloys[C]. Warrendale, PA: TMS, 1988: 215 |
| 19 | Sass V, Feller-Kniepmeier M. Orientation dependence of dislocation structures and deformation mechanisms in creep deformed CMSX-4 single crystals[J]. Mater. Sci. Eng., 1998, A245: 19 |
| 20 | Feller-Kniepmeier M, Kuttner T. [011] creep in a single crystal nickel base superalloy at 1033 K[J]. Acta Metall. Mater., 1994, 42: 3167 |
| 21 | Kakehi K. Influence of secondary precipitates and crystallographic orientation on the strength of single crystals of a Ni-based superalloy[J]. Metall. Mater. Trans., 1999, 30A: 1249 |
| 22 | Liu J L, Jin T, Sun X F, et al. Anisotropy of stress rupture properties of a Ni base single crystal superalloy at two temperatures[J]. Mater. Sci. Eng., 2008, A479: 277 |
| 23 | Mackay R A, Maier R D. The influence of orientation on the stress rupture properties of nickel-base superalloy single crystals[J]. Metall. Trans., 1982, 13A: 1747 |
| 24 | Wang X G, Liu J L, Jin T, et al. Creep deformation related to dislocations cutting the γ' phase of a Ni-base single crystal superalloy[J]. Mater. Sci. Eng., 2015, A626: 406 |
| 25 | Yan H J, Tian S G, Zhu X J, et al. Stacking fault energies of single crystal nickel-based superalloy and its influence on creep mechanism[J]. J. Mater. Eng., 2018, 46(10): 87 |
| 闫化锦, 田素贵, 朱新杰 等. 单晶镍基合金的层错能及其对蠕变机制的影响[J]. 材料工程, 2018, 46(10): 87 | |
| 26 | Link T, Epishin A, Fedelich B. Inhomogeneity of misfit stresses in nickel-base superalloys: Effect on propagation of matrix dislocation loops[J]. Philos. Mag., 2009, 89: 1141 |
| 27 | Field R D, Pollock T M, Murphy W H. The development of γ/γ' interfacial dislocation networks during creep in Ni-base superalloys[A]. Superalloys 1988[C]. Champaign: The Minerals, Metals & Materials Society (TMS), 1992: 557 |
/
| 〈 |
|
〉 |