Research paper

Degradation Mechanism on Corrosion Resistance of High Nb-Containing Zirconium Alloys in Oxygen-Containing Steam

  • HUANG Jiansong ,
  • PEI Wen ,
  • XU Shitong ,
  • BAI Yong ,
  • YAO Meiyi ,
  • HU Lijuan ,
  • XIE Yaoping ,
  • ZHOU Bangxin
Expand
  • Institute of Materials, Shanghai University, Shanghai 200072, China
YAO Meiyi, professor, Tel: (021)56338586, E-mail: yaomeiyi@shu.edu.cn

Received date: 2022-02-21

  Revised date: 2022-04-08

  Online published: 2022-05-30

Supported by

National Natural Science Foundation of China(51871141)

Abstract

In some water-cooled nuclear power reactors, a hydrogenation-deoxygenation device is generally not used to simplify the system and save space, which can increase dissolved oxygen (DO) concentration in primary loop water. The increase in DO concentration will inevitably affect the corrosion resistance of zirconium alloy cladding materials. In particular, DO will accelerate the corrosion of Nb-containing zirconium alloys, and the corrosion rate of zirconium alloys with high Nb content is sensitive to DO concentration. In exploring the deterioration mechanism of the corrosion resistance of high-Nb-containing zirconium alloys in oxygen-containing steam, the corrosion behavior of the Zr-0.75Sn-0.35Fe-0.15Cr-1.0Nb (mass fraction, %) alloy was studied in superheated steam through deoxygenation, with 300 μg/kg of DO and 1000 μg/kg of DO at 400oC and 10.3 MPa. The corrosion behavior was characterized by measuring the mass gain per unit area. SEM was used to observe the fracture morphology of the oxide film; TEM-EDS was used to observe and analyze the morphology, elemental distribution, and crystal structure of the alloy, second-phase particles (SPPs), and oxide film. The elemental distribution on the outer surface of the oxide film was analyzed by XPS, and the valence state of Nb was determined in accordance with the binding energy to analyze the influence of DO on the oxidation behavior of Nb in the oxide film. Results show that the corrosion resistance of the Zr-0.75Sn-0.35Fe-0.15Cr-1.0Nb alloy in superheated steam at 400oC deteriorates with the increase of DO concentration. The deterioration mechanism of the corrosion resistance of the alloy in oxygen-containing steam is proposed. On the one hand, DO accelerates the oxidation of Nb in the oxide film and promotes the conversion of Nb2+ to Nb5+. On the other hand, DO promotes the oxidation of SPPs to m-Nb2O5 (monoclinic) and amorphous phase, thereby promoting the initiation and growth of cracks. These newly generated cracks provide more channels for the diffusion of O2- and other oxidizing ions to accelerate the oxidation of SPPs near the cracks and the microstructural evolution of the oxide film, thereby accelerating the corrosion of the alloy.

Cite this article

HUANG Jiansong , PEI Wen , XU Shitong , BAI Yong , YAO Meiyi , HU Lijuan , XIE Yaoping , ZHOU Bangxin . Degradation Mechanism on Corrosion Resistance of High Nb-Containing Zirconium Alloys in Oxygen-Containing Steam[J]. Acta Metall Sin, 2024 , 60(4) : 509 -521 . DOI: 10.11900/0412.1961.2022.00066

References

1 Cao Y L, Wang S W, Xiong W B, et al. Features and application analysis of the small modular reactors[J]. Nucl. Electron. Detect. Technol., 2014, 34: 801
  曹亚丽, 王韶伟, 熊文彬 等. 小型模块化反应堆特性及应用分析[J]. 核电子学与探测术, 2014, 34: 801
2 Bradhurst D H, Shirvington P J, Heuer P M. The effects of radiation and oxygen on the aqueous oxidation of zirconium and its alloys at 290oC[J]. J. Nucl. Mater., 1973, 46: 53
3 Motta A T, Comstock R J, Count A. Corrosion of zirconium alloys used for nuclear fuel cladding[J]. Annu. Rev. Mater. Res., 2015, 45: 311
4 Kumar M K, Aggarwal S, Beniwal D, et al. Localized oxidation of zirconium alloys in high temperature and pressure oxidizing environments of nuclear reactors[J]. Mater. Corros., 2014, 65: 244
5 Cox B. Some thoughts on the mechanisms of in-reactor corrosion of zirconium alloys[J]. J. Nucl. Mater., 2005, 336: 331
6 Jeong Y H, Park S Y, Lee M H, et al. Out-of-pile and in-pile performance of advanced zirconium alloys (HANA) for high burn-up fuel[J]. J. Nucl. Sci. Mater., 2006, 43: 977
7 Zhou B X, Yao M Y, Li Z K, et al. Optimization of N18 zirconium alloy for fuel cladding of water reactors[J]. J. Mater. Sci. Technol., 2012, 28: 606
8 Liu J Z. Structure Nuclear Materials[M]. Beijing: Chemical Industry Press, 2007: 56
  刘建章. 核结构材料[M]. 北京: 化学工业出版社, 2007: 56
9 Kim Y S, Kim S K, Bang J G, et al. Effects of Sn and Nb on massive hydriding kinetics of Zr ± XSn ± YNb alloy[J]. J. Nucl. Mater., 2000, 279: 335
10 Kim H G, Yong H J, Kim T H. Effect of isothermal annealing on the corrosion behavior of Zr-xNb alloys[J]. J. Nucl. Mater., 2004, 326: 125
11 Dai J X, Gong Z M, Xu S T, et al. In situ study on the initial oxidation behavior of zirconium alloys with near-ambient pressure XPS[J]. Acta Phys. Chim. Sin., 2022, 38: 76
  戴久翔, 龚忠苗, 徐诗彤 等. 锆合金初始氧化行为的原位近常压XPS研究[J]. 物理化学学报, 2022, 38: 76
12 Jeong Y H, Kim H G, Kim D J, et al. Influence of Nb content in the α-matrix on the corrosion behavior of Zr-xNb binary alloys[J]. J. Nucl. Mater., 2003, 323: 72
13 Wang B Y, Zhou B X, Wang Z, et al. Corrosion resistance of Zr-0.72Sn-0.32Fe-0.14Cr-xNb alloys in 500oC superheated steam[J]. Acta. Metall. Sin., 2015, 51: 1545
  王波阳, 周邦新, 王 桢 等. Zr-0.72Sn-0.32Fe-0.14Cr-xNb合金在500℃过热蒸汽中的耐腐蚀性能[J]. 金属学报, 2015, 51: 1545
14 Wu Y, Chen B, Lin X D, et al. Corrosion behavior of 90Nb-10Zr alloy in 500oC superheated steam[J]. Rare. Met. Mater. Eng., 2021, 50: 4437
  吴 悦, 陈 兵, 林晓冬 等. 90Nb-10Zr合金在500℃过热蒸气中的腐蚀行为[J]. 稀有金属材料与工程, 2021, 50: 4437
15 Yao M Y, Zhou B X. Mechanism of the accelerated corrosion of Zr-Nb alloys in lithiated water from the viewpoint of β-Nb oxidation[J]. J. Shanghai Univ.: Nat. Sci. Ed., 2020, 26: 681
  姚美意, 周邦新. 从β-Nb氧化角度探究Zr-Nb系锆合金在LiOH水溶液中腐蚀加速的机理[J]. 上海大学学报(自然科学版), 2020, 26: 681
16 Xu S T, Huang J S, Pei W, et al. Effect of oxygen content in 400oC superheated steam on the corrosion resistance of Zr-xSn-0.35Fe-0.15Cr-0.15Nb alloys[J]. Corros. Sci., 2022, 198: 110135
17 Kumar M K, Aggarwal S, Kain V, et al. Effect of dissolved oxygen on oxidation and hydrogen pick up behaviour—Zircaloy vs Zr-Nb alloys[J]. Nucl. Eng. Des., 2010, 240: 985
18 Wei T G, Lin J K, Long C S, et al. Effect of dissolved oxygen in steam on the corrosion behaviors of zirconium alloys[J]. Acta. Metall. Sin., 2016, 52: 209
  韦天国, 林建康, 龙冲生 等. 蒸汽中的溶解氧对锆合金腐蚀行为的影响[J]. 金属学报, 2016, 52: 209
19 Liu Q D, Zhang H, Zeng Q F, et al. Pre-transition corrosion behavior of SZA-4 and ZIRLO alloys in dissolved oxygen aqueous condition at 360oC[J]. J. Mech. Eng. 2019, 55(8): 88
  刘庆冬, 张 浩, 曾奇锋 等. SZA-4和ZIRLO锆合金在360℃含氧水环境中的腐蚀行为[J]. 机械工程学报, 2019, 55(8): 88
20 Qin W, Nam C, Li H L, et al. Tetragonal phase stability in ZrO2 film formed on zirconium alloys and its effects on corrosion resistance[J]. Acta Mater., 2007, 55: 1695
21 Olsson C O A, Landolt D. Atmospheric oxidation of a Nb-Zr alloy studied with XPS[J]. Corros. Sci., 2004, 46: 213
22 Hauffe K. Oxidation of Metal.[M]. New York: Plenum Press, 1965: 176
23 Li M S. High Temperature Corrosion of Metal[M]. Beijing: Metallurgical Industry Press, 2001: 55
  李美栓. 金属的高温腐蚀[M]. 北京: 冶金工业出版社, 2001: 55
24 Li T F. High Temperature Oxidation and Thermal Corrosion in Metals[M]. Beijing: Chemical Industry Press, 2003: 18
  李铁藩. 金属高温氧化和热腐蚀.[M]. 北京: 化学工业出版社, 2003: 18
25 Cao X X, Yao M Y, Peng J C, et al. Corrosion behavior of Zr(Fe x, Cr1- x)2 alloys in 400oC superheated steam[J]. Acta Metall. Sin, 2011, 47: 882
  曹潇潇, 姚美意, 彭建超 等. Zr(Fe x, Cr1- x)2合金在400℃过热蒸汽中的腐蚀行为[J]. 金属学报, 2011, 47: 882
26 Yang W D. Reactor Materials Science.[M]. 2nd Ed., Beijing: Atomic Energy Press, 2006: 123
  杨文斗. 反应堆材料学[M]. 第二版, 北京: 原子能出版社, 2006: 123
27 Zhou B X, Li Q, Yao M Y, et al. Microstructure of oxide films formed on zircaloy-4[J]. Corros. Prot., 2009, 30: 589
  周邦新, 李 强, 姚美意 等. Zr-4合金氧化膜的显微组织研究[J]. 腐蚀与防护, 2009, 30: 589
28 Liu W Q, Li Q, Zhou B X, et al. Effect of heat treatment on the corrosion resistance for new zirconium-based alloy[J]. Nucl. Power Eng., 2005, 26: 249
  刘文庆, 李 强, 周邦新 等. 热处理制度对N18新锆合金耐腐蚀性能的影响[J]. 核动力工程, 2005, 26: 249
Outlines

/