Overview

Present Status for Rolling TiAl Alloy Sheet

  • Yuyong CHEN ,
  • Yuan YE ,
  • Jianfei SUN
Expand
  • 1.School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001, China
    2.International Institute of Vanadium and Titanium, Panzhihua University, Panzhihua 617000, China
CHEN Yuyong, professor, Tel: (0451)86418802, E-mail: yychen@hit.edu.cn

Received date: 2021-10-15

  Revised date: 2022-03-22

  Online published: 2022-05-20

Supported by

National Nature Science Foundation of China(51434007);National Nature Science Foundation of China(51371064)

Abstract

TiAl alloy sheets are important strategic structural materials in aerospace and automotive industry because of their high strength-to-weight ratio and high service temperature. However, the preparation of TiAl alloy sheets is difficult, especially the rolling of large-size high-performance TiAl alloy sheets. The preparation process, size, microstructure, and mechanical properties of hot-rolling TiAl alloy sheets using ingot metallurgy, powder metallurgy, direct rolling, and roll bonding approaches in recent years were reviewed. The features and existing problems of the above processing routes were discussed. Meanwhile, some suggestions on rolling large-size TiAl alloy sheets and its future development were proposed.

Cite this article

Yuyong CHEN , Yuan YE , Jianfei SUN . Present Status for Rolling TiAl Alloy Sheet[J]. Acta Metall Sin, 2022 , 58(8) : 965 -978 . DOI: 10.11900/0412.1961.2021.00438

References

1 Appel F, Clemens H, Fischer F D. Modeling concepts for intermetallic titanium aluminides [J]. Prog. Mater. Sci., 2016, 81: 55
2 Zhang W J, Reddy B V, Deevi S C. Physical properties of TiAl-base alloys [J]. Scr. Mater., 2001, 45: 645
3 Das G, Kestler H, Clemens H, et al. Sheet gamma TiAl: Status and opportunities [J]. JOM, 2004, 56(11): 42
4 Chen Y Y, Kong F T, Cui N. Preparation and microstructural analysis of TiAl alloy sheet [J]. Mater. China, 2015, 34: 379
4 陈玉勇, 孔凡涛, 崔 宁. TiAl合金板材的制备与组织分析 [J]. 中国材料进展, 2015, 34: 379
5 Lin J P, Chen G L. Development of TiAl intermetallic based compound [J]. Mater. China, 2009, 28(1): 31
5 林均品, 陈国良. TiAl基金属间化合物的发展 [J]. 中国材料进展, 2009, 28(1): 31
6 Zhang D M, Chen G Q, Han J C, et al. Research on gamma TiAl-based alloy sheet fabricated by EB-PVD [J]. J. Aeronaut. Mater., 2006, 26(4): 35
6 章德铭, 陈贵清, 韩杰才 等. EB-PVD制备γ-TiAl基合金薄板的研究 [J]. 航空材料学报, 2006, 26(4): 35
7 Liu J P, Su Y Q, Luo L S, et al. Fabrication of wavy γ-TiAl based sheet with foil metallurgy [J]. Trans. Nonferrous Met. Soc. China, 2012, 22: 72
8 Rivard J D K, Blue C A, Ott R D, et al. Advanced manufacturing technologies utilising high density infrared radiant heating [J]. Surf. Eng., 2004, 20: 220
9 Chen Y Y, Yue H Y, Wang X P, et al. Selective electron beam melting of TiAl alloy: Microstructure evolution, phase transformation and microhardness [J]. Mater. Charact., 2018, 142: 584
10 Yue H Y, Chen Y Y, Wang X P, et al. Effect of beam current on microstructure, phase, grain characteristic and mechanical properties of Ti-47Al-2Cr-2Nb alloy fabricated by selective electron beam melting [J]. J. Alloys Compd., 2018, 750: 617
11 Chen Y Y, Yue H Y, Wang X P. Microstructure, texture and tensile property as a function of scanning speed of Ti-47Al-2Cr-2Nb alloy fabricated by selective electron beam melting [J]. Mater. Sci. Eng., 2018, A713: 195
12 Yue H Y, Chen Y Y, Wang X P, et al. Microstructure, texture and tensile properties of Ti-47Al-2Cr-2Nb alloy produced by selective electron beam melting [J]. J. Alloys Compd., 2018, 766: 450
13 Tomita M, Noguchi Y. Miti program on high temperature intermetallics [J]. Trans. Nonferrous Met. Soc. China, 1999, 9(): 346
14 Semiatin S L, Seetharaman V. Deformation and microstructure development during hot-pack rolling of a near-gamma titanium aluminide alloy [J]. Metall. Mater. Trans., 1995, 26A: 371
15 Clemens H, Kestler H. Processing and applications of intermetallic γ‐TiAl‐based alloys [J]. Adv. Eng. Mater., 2000, 2: 551
16 Zhang G C. TiAl intermetallic sheet isothermal rolling equipment and technology [J]. Titanium Alloy. Inf., 1996, (1): 7
16 张功才. TiAl金属间化合物薄板的等温轧制设备及其工艺 [J]. 钛合金信息, 1996, (1): 7
17 Cui X P. Microstructure and mechanical properties of micro-laminated TiB2-TiAl composite sheets prepared by roll bonding and reaction annealing [D]. Harbin: Harbin Institute of Technology, 2012
17 崔喜平. 轧制及反应退火制备微叠层TiB2-TiAl复合材料板组织与性能 [D]. 哈尔滨: 哈尔滨工业大学, 2012
18 Clemens H, Glatz W, Eberhardt N, et al. Processing, properties and applications of gamma titanium aluminide sheet and foil materials [J]. MRS Online Proc. Lib., 1996, 460: 29
19 Zhou H T, Kong F T, Wang X P, et al. High strength in high Nb containing TiAl alloy sheet with fine duplex microstructure produced by hot pack rolling [J]. J. Alloys Compd., 2017, 695: 3495
20 Zhou H T, Kong F T, Wu K, et al. Hot pack rolling nearly lamellar Ti-44Al-8Nb-(W, B, Y) alloy with different rolling reductions: Lamellar colonies evolution and tensile properties [J]. Mater. Des., 2017, 121: 202
21 Liu H W. Hot working, structure and properties of (γ + α2 + B2) multiphase TiAl alloy [D]. Qinhuangdao: Yanshan University, 2017
21 刘宏武. (γ + α2 + B2)三相TiAl合金热加工特性及组织性能研究 [D]. 秦皇岛: 燕山大学, 2017
22 Zhang Y, Wang X P, Kong F T, et al. A high-performance β-stabilized Ti-43Al-9V-0.2Y alloy sheet with a nano-scaled antiphase domain [J]. Mater. Lett., 2018, 214: 182
23 Zhang Y, Wang X P, Kong F T, et al. A high-performance β-solidifying TiAl alloy sheet: Multi-type lamellar microstructure and phase transformation [J]. Mater. Charact., 2018, 138: 136
24 Gao S B, Liang Y F, Ye T, et al. In-situ control of microstructure and mechanical properties during hot rolling of high-Nb TiAl alloy [J]. Materialia, 2018, 1: 229
25 Liu F X, He Y H, Liu Y, et al. Present status and future prospects for PM TiAl-based alloy sheet [J]. Rare Met. Mater. Eng., 2005, 34: 169
25 刘峰晓, 贺跃辉, 刘 咏 等. 粉末冶金制备TiAl基合金板材的研究现状及趋势 [J]. 稀有金属材料与工程, 2005, 34: 169
26 Yang F, Kong F T, Chen Y Y, et al. Manufacture and present status of TiAl alloy sheet [J]. J. Mater. Eng., 2010, (5): 96
26 杨 非, 孔凡涛, 陈玉勇 等. TiAl合金板材的制备及研究现状 [J]. 材料工程, 2010, (5): 96
27 Xu L, Bai C G, Wang G, et al. Manufacturing of γ-TiAl sheet by hot packed rolling of powder metallurgy preform [J]. Titanium Ind. Prog., 2011, 28(5): 17
27 徐 磊, 柏春光, 王 刚 等. 包覆热轧制备粉末冶金TiAl合金板材及热加工行为研究 [J]. 钛工业进展, 2011, 28(5): 17
28 Liu Y, Liang X P, Liu B, et al. Investigations on processing powder metallurgical high-Nb TiAl alloy sheets [J]. Intermetallics, 2014, 55: 80
29 Li H Z, Qi Y L, Liang X P, et al. Microstructure and high temperature mechanical properties of powder metallurgical Ti-45Al-7Nb-0.3W alloy sheets [J]. Mater. Des., 2016, 106: 90
30 Zhang D D. Preparation of powder TiAl alloy sheet and study on microstructure and properties [D]. Harbin: Harbin Institute of Technology, 2020
30 张冬冬. 粉末TiAl合金板材的制备及其组织性能研究 [D]. 哈尔滨: 哈尔滨工业大学, 2020
31 Matsuo M. Developments in processing technology of gamma titanium aluminides for potential application to airframe structures [J]. ISIJ Int., 1991, 31: 1212
32 Hanamura T, Hashimoto K. Improvement of microstructure and mechanical properties in TiB2-doped TiAl alloy by direct sheet casting [J]. Mater. Trans. JIM, 1998, 39: 724
33 Shen Z Z. The Investigation of manufacturing, microstructure, properties of high Nb-TiAl alloy sheet [D]. Beijing: University of Science and Technology Beijing, 2016
33 沈正章. 高Nb-TiAl合金板材制备及组织性能研究 [D]. 北京: 北京科技大学, 2016
34 Zeng S W. Research on hot deformation and oxidation behavior of TiAl containing Nb, Mo [D]. Beijing: University of Science and Technology Beijing, 2016
34 曾尚武. 含铌、钼TiAl合金热变形及氧化行为研究 [D]. 北京: 北京科技大学, 2016
35 Chen L. Study on microstructure optimization and creep properties of TiAl alloy containing β stable element [D]. Beijing: University of Science and Technology Beijing, 2021
35 陈 林. 含β稳定元素TiAl合金组织优化及其蠕变性能研究 [D]. 北京: 北京科技大学, 2021
36 Li T R, Liu G H, Xu M, et al. High temperature deformation and control of homogeneous microstructure during hot pack rolling of Ti-44Al-5Nb-(Mo, V, B) alloys: The impact on mechanical properties [J]. Mater. Sci. Eng., 2019, A751: 1
37 Luo J G, Acoff V L. Processing gamma-based TiAl sheet materials by cyclic cold roll bonding and annealing of elemental titanium and aluminum foils [J]. Mater. Sci. Eng., 2006, A433: 334
38 Zhang R G, Acoff V L. Processing sheet materials by accumulative roll bonding and reaction annealing from Ti/Al/Nb elemental foils [J]. Mater. Sci. Eng., 2007, A463: 67
39 Chaudhari G P, Acoff V L. Titanium aluminide sheets made using roll bonding and reaction annealing [J]. Intermetallics, 2010, 18: 472
40 Kong F T, Chen Y Y. Preparation of γ-TiAl/TC4 composite sheet and its microstructure and properties [J]. Rare Met. Mater. Eng., 2009, 38: 1484
40 孔凡涛, 陈玉勇. γ-TiAl/TC4复合板材的制备及组织性能研究 [J]. 稀有金属材料与工程, 2009, 38: 1484
41 Bian Z W. Study of process of rolling and heat treatment on multilaminated Ti-B4C/Al sheets [D] Harbin: Harbin Institute of Technology, 2010
41 边卓伟. 多层Ti-(B4C/Al)板轧制和热处理工艺研究 [D]. 哈尔滨: 哈尔滨工业大学, 2010
42 Wang Y. Microstructure and mechanical properties of titanium aluminide composite sheet prepared by roll bonding and reactive annealing [D]. Harbin: Harbin Institute of Technology, 2011
42 王 银. 叠轧及热处理制备钛铝基复合材料板的微观组织与性能 [D]. 哈尔滨: 哈尔滨工业大学, 2011
43 Sun W, Yang F, Kong F T, et al. Interface characteristics of Ti6Al4V-TiAl metal-intermetallic laminate (MIL) composites prepared by a novel hot-pack rolling [J]. Mater Charact., 2018, 144: 173
44 Ren L B, Wang J, Wang H W, et al. A method for preparing titanium alloy sheet by roll bonding using steel plate can [P]. Chin Pat, 201110104578.8, 2011
44 任连宝, 王 俭, 王红武 等. 一种钢板包覆叠轧制备钛合金薄板的方法 [P]. 中国专利, 201110104578.8, 2011)
Outlines

/