Macrosegregation Mechanism of Primary Silicon Phase in Cast Hypereutectic Al-Si Alloys Under Alternating Electropulsing

  • ZHANG Limin ,
  • LI Ning ,
  • ZHU Longfei ,
  • YIN Pengfei ,
  • WANG Jianyuan ,
  • WU Hongjing
Expand
  • 1MOE Key Laboratory of Material Physics and Chemistry Under Extraordinary, School of Physical Science and Technology, Northwestern Polytechnical University, Xi'an 710072, China
    2School of Materials Science and Engineering, Taiyuan University of Science and Technology, Taiyuan 030024, China
    3College of Science, Sichuan Agricultural University, Ya'an 625014, China

Received date: 2021-11-08

  Revised date: 2022-03-20

  Online published: 2022-05-07

Supported by

National Natural Science Foundation of China(52074227);National Natural Science Foundation of China(51801186);National Natural Science Foundation of China(52130405);Key Re-search and Development Program of Shaanxi Province(2020ZDLGY13-03)

Abstract

Controlling the macrosegregation induced by electropulsing is of high commercial importance. This study investigates the macrosegregation of the primary Si phase in casting Al-Si hypereutectic alloys via the different solidification stages and components of alloys treated with electropulsing. Experimental results show that a serious gradient macrosegregation of the primary Si phase occurs, and four types of primary Si regions are formed: coarse plate-like, refined plate-like, and fine polygon primary Si, as well as a eutectic structure. The wider the solidification temperature range, the more serious the macrosegregation. A near-eutectic structure occurs at the center of ingots when the solidification temperature range exceeds a certain threshold. With an increasing current density of electropulsing, the segregation degree of primary Si increases initially and then decreases for different Al-Si hypereutectic alloys, but the current density with regard to the most serious segregation is closely related to the Si content. Furthermore, it is proved that the migration behavior of primary Si particles plays an important role in macrosegregation. A special casting experiment under the condition of limited heat flux along the radial direction was performed to clarify the macrosegregation mechanism of primary Si under electropulsing. After nucleation during the solidification process, the primary Si particles move to the front of the solid-liquid interface due to secondary flow in bulk liquid and then are easily captured due to the electromagnetic repulsive force or its component. The force flow in the bulk liquid and mush zone and the secondary flow in front of the solid-liquid interface make obvious solute redistribution and promote the growth of the primary Si phase, which is maintained until the solute concentration in the bulk liquid approaches the eutectic composition.

Cite this article

ZHANG Limin , LI Ning , ZHU Longfei , YIN Pengfei , WANG Jianyuan , WU Hongjing . Macrosegregation Mechanism of Primary Silicon Phase in Cast Hypereutectic Al-Si Alloys Under Alternating Electropulsing[J]. Acta Metall Sin, 2023 , 59(12) : 1624 -1632 . DOI: 10.11900/0412.1961.2021.00480

References

1 Wu Y, Wang S J, Li H, et al. A new technique to modify hypereutectic Al-24%Si alloys by a Si-P master alloy[J]. J. Alloys Compd., 2009, 477: 139
2 Feng H K, Yu S R, Li Y L, et al. Effect of ultrasonic treatment on microstructures of hypereutectic Al-Si alloy[J]. J. Mater. Process. Technol., 2008, 208: 330
3 Zhang Y H, Ye C Y, Xu Y Y, et al. Influence of growth velocity on the separation of primary silicon in solidified Al-Si hypereutectic alloy driven by a pulsed electric current[J]. Metals, 2017, 7: 184
4 Hernández F C R, Sokolowski J H. Comparison among chemical and electromagnetic stirring and vibration melt treatments for Al-Si hypereutectic alloys[J]. J. Alloys Compd., 2006, 426: 205
5 R?biger D, Zhang Y H, Galindo V, et al. The relevance of melt convection to grain refinement in Al-Si alloys solidified under the impact of electric currents[J]. Acta Mater., 2014, 79: 327
6 Li N, Zhang R, Zhang L M, et al. Study on grain refinement mechanism of hypoeutectic Al-7%Si alloy under low voltage alternating current pulse[J]. Acta Metall. Sin., 2017, 53: 192
  李 宁, 张 蓉, 张利民 等. 低压交流电脉冲下Al-7%Si合金晶粒细化机理研究[J]. 金属学报, 2017, 53: 192
7 Zhang L M, Liu H N, Li N, et al. The relevance of forced melt flow to grain refinement in pure aluminum under a low-frequency alternating current pulse[J]. J. Mater. Res., 2016, 31: 396
8 Wang T M, Zhu J, Kang H J, et al. In situ synchrotron X-ray imaging on morphological evolution of dendrites in Sn-Bi hypoeutectic alloy under electric currents[J]. Appl. Phys., 2014, 117A: 1059
9 Zhang X F, Qin R S. Electric current-driven migration of electrically neutral particles in liquids[J]. Appl. Phys. Lett., 2014, 104: 114106
10 Zhang Y H, Xu Y Y, Ye C Y, et al. Relevance of electrical current distribution to the forced flow and grain refinement in solidified Al-Si hypoeutectic alloy[J]. Sci. Rep., 2018, 8: 3242
11 Chen Z X, Ding H S, Chen R R, et al. Microstructural evolution and mechanism of solidified TiAl alloy applied electric current pulse[J]. Acta Metall. Sin., 2019, 55: 611
  陈占兴, 丁宏升, 陈瑞润 等. 脉冲电流作用下TiAl合金凝固组织演变及形成机理[J]. 金属学报, 2019, 55: 611
12 Zhang Y H, Song C J, Zhu L, et al. Influence of electric-current pulse treatment on the formation of regular eutectic morphology in an Al-Si eutectic alloy[J]. Metall. Mater. Trans., 2011, 42B: 604
13 Li F, Regel L L, Wilcox W R. The influence of electric current pulses on the microstructure of the MnBi/Bi eutectic[J]. J. Cryst. Growth, 2001, 223: 251
14 Flemings M C, Mehrabian R, Nereo G E. Macrosegregation: Part II[J]. Trans. Met. Soc. AIME, 1968, 242: 41
15 Beckermann C. Modelling of macrosegregation: Applications and future needs[J]. Int. Mater. Rev., 2002, 47: 243
16 Jie J C, Zou Q C, Sun J L, et al. Separation mechanism of the primary Si phase from the hypereutectic Al-Si alloy using a rotating magnetic field during solidification[J]. Acta Mater., 2014, 72: 57
17 Zimmermann G, Weiss A, Mbaya Z. Effect of forced melt flow on microstructure evolution in AlSi7Mg0.6 alloy during directional solidification[J]. Mater. Sci. Eng., 2005, A413-414: 236
18 Noeppel A, Ciobanas A, Wang X D, et al. Influence of forced/natural convection on segregation during the directional solidification of Al-based binary alloys[J]. Metall. Mater. Trans., 2010, 41B: 193
19 Zhang Y H, Miao X C, Shen Z Y, et al. Macro segregation formation mechanism of the primary silicon phase in directionally solidified Al-Si hypereutectic alloys under the impact of electric currents[J]. Acta Mater., 2015, 97: 357
20 Li J Y, Ni P, Wang L, et al. Influence of direct electric current on solidification process of Al-Si alloy[J]. Mater. Sci. Semicond. Process., 2017, 61: 79
21 Ban C Y, Han Y, Ba Q X, et al. Influence of pulse electric current on solidification structures of Al-Si alloys[J]. Mater. Sci. Forum, 2007, 546-549: 723
22 Zhang B W, Ren Z M, Zhong Y B, et al. Theoretical analysis on electromagnetic separation of inclusions from molten metal only by current[J]. J. Baotou Univ. Iron Steel Technol., 2002, 21: 228
  张邦文, 任忠鸣, 钟云波 等. 金属液单电流电磁净化的理论分析[J]. 包头钢铁学院学报, 2002, 21: 228
23 Du C M. The effect of current on inclusion and bubble in molten steel[D]. Shenyang: Northeastern University, 2013
  杜传明. 电流对钢液中气泡和夹杂物的影响[D]. 沈阳: 东北大学, 2013
24 Qin R S, Bhowmik A. Computational thermodynamics in electric current metallurgy[J]. Mater. Sci. Technol., 2015, 31: 1560
25 Wang X L, Guo J D, Wang Y M, et al. Segregation of lead in Cu-Zn alloy under electric current pulses[J]. Appl. Phys. Lett., 2006, 89: 061910
26 Zhang X F, Lu W J, Qin R S. Removal of MnS inclusions in molten steel using electropulsing[J]. Scr. Mater., 2013, 69: 453
27 Zhang L M, Zhang R, Li N, et al. Evolution of solidification structure of hypereutectic Al-Si alloy under a novel low-voltage alternating current pulse[J]. J. Iron Steel Res. Int., 2012, 19(suppl.): 355
28 Zhang L M, Zhang R, Chen W J, et al. Effect of a novel low-voltage alternating current pulse on solidification structure of Al-7Si-0.52Mg alloy[J]. Adv. Mater. Res., 2012, 482-484: 1431
29 Murray J L, McAlister A J. Massalski T B. Binary Alloy Phase Diagrams, Vol. I[M]. 2nd Ed., ASM International, 1996: 211
30 Mao W M, Li S S, Zhao A M, et al. Effect of electromagnetic stirring on the distribution of primary silicon in hypereutectic Al-Si alloys[J]. Acta Metall. Sin., 2001, 37: 781
  毛卫民, 李树索, 赵爱民 等. 电磁搅拌对过共晶Al-Si合金初生Si分布的影响[J]. 金属学报, 2001, 37: 781
31 Taniguchi S, Brimacombe J K. Application of pinch force to the separation of inclusion particles from liquid steel[J]. ISIJ Int., 1994, 34: 722
32 Zhang X F, Yan L G. Regulating the non-metallic inclusions by pulsed electric current in molten metal[J]. Acta Metall. Sin., 2020, 56: 257
  张新房, 闫龙格. 脉冲电流调控金属熔体中的非金属夹杂物[J]. 金属学报, 2020, 56: 257
33 Nikrityuk P A, Eckert K, Grundmann R, et al. An impact of a low voltage steady electrical current on the solidification of a binary metal alloy: A numerical study[J]. Steel Res. Int., 2007, 78: 402
34 Bojarevi?s V, Shcherbinin E V. Azimuthal rotation in the axisymmetric meridional flow due to an electric-current source[J]. J. Fluid Mech., 1983, 126: 413
35 Schmitz J, Hallstedt B, Brillo J, et al. Density and thermal expansion of liquid Al-Si alloys[J]. J. Mater. Sci., 2012, 47: 3706
36 Yu W Z, Ma W H, Zheng Z, et al. Effects of melt viscosity on enrichment and separation of primary silicon from Al-Si melt[J]. Trans. Nonferrous Met. Soc. China, 2017, 27: 467
37 Yin M Z. Effect of centrifugal casting on microstructures and properties of hypereutectic Al-20wt.%Si alloy[D]. Changchun: Jilin University, 2014
  尹茂振. 离心铸造对过共晶Al-20wt.%Si合金组织及性能的影响[D]. 长春: 吉林大学, 2014
38 Li X, Fautrelle Y, Ren Z M. Influence of thermoelectric effects on the solid-liquid interface shape and cellular morphology in the mushy zone during the directional solidification of Al-Cu alloys under a magnetic field[J]. Acta Mater., 2007, 55: 3803
Outlines

/