Research paper

Microstructure and Mechanical Properties of TiB2 Reinforced TiAl-Based Alloy Coatings Prepared by Laser Melting Deposition

  • Hu WANG ,
  • Lin ZHAO ,
  • Yun PENG ,
  • Xiaotao CAI ,
  • Zhiling TIAN
Expand
  • 1.Welding Research Institute, Central Iron & Steel Research Institute, Beijing 100081, China
    2.College of Materials Engineering, North China Institute of Aerospace Engineering, Langfang 065000, China

Received date: 2021-12-22

  Revised date: 2022-03-10

  Online published: 2022-04-22

Supported by

National Key Research and Development Program of China(2020YFE0200900)

Abstract

TiAl-based alloy coating produced by laser melting deposition exhibits excellent properties of high temperature and corrosion resistance and has a wide application potential across many fields. However, the wear resistance of the coating is poor, which limits its long-term usage in harsh and complex working environments. In this study, TiB2 reinforced TiAl-based alloy composite coatings are prepared by laser melting deposition to improve their wear resistance, and a theoretical reference for further exploring the applications of TiAl-based alloy composites in surface engineering is presented. TiAl-based alloy coatings with different TiB2 contents (0, 10%, 20%, 30%, mass fraction) were prepared on the surface of TC4 alloy using the laser melting deposition process. The effects of TiB2 content on the microstructure and mechanical properties of the coatings were systematically studied using XRD, OM, SEM, microhardness tester, indentation method, wear tester, and laser confocal microscope. Planar, columnar, and equiaxed crystal distributions were observed along the thickness direction from the bottom. With an increase in TiB2 content, the height of columnar crystal gradually decreased. TiB2/TiAl composite coatings are composed of a TiAl alloy matrix phase (γ + α2) and a TiB2 enhanced phase. Most of the directly added TiB2 particles do not melt, but the outer layer of the directly added TiB2 particles dissolves within the molten TiAl alloy, following which primary and secondary TiB2 are precipitated in situ. The primary TiB2 has a particle form and the secondary TiB2 has a needle or flake form. With the increase of TiB2 content from 0 to 10%, the matrix of the coating is noticeably refined, but an increase in TiB2 content (20% and 30%) do not produce further refinement. With the increase of TiB2 content from 0 to 30%, the surface hardness of the coating increases from 530.5 HV to 738.4 HV, the fracture toughness decreases from 7.75 MPa·m1/2 to 3.17 MPa·m1/2, the wear rate decreases from 3.98 mg/mm2 to 0.42 mg/mm2, and the wear degree and roughness of the wear surface also decrease. Furthermore, the wear mechanism of the coating without TiB2 is mainly microscopic cutting, supplemented by multiple plastic deformations. When the mass fraction of TiB2 is 10%, the wear mechanism of the coating is mainly microscopic cutting, supplemented by microscopic fracture. As the TiB2 content increases, the wear mechanism gradually turns to microscopic fracture. When the mass fraction of TiB2 is 30%, the wear mechanism of the coating is mainly microscopic fracture, supplemented by microscopic cutting.

Cite this article

Hu WANG , Lin ZHAO , Yun PENG , Xiaotao CAI , Zhiling TIAN . Microstructure and Mechanical Properties of TiB2 Reinforced TiAl-Based Alloy Coatings Prepared by Laser Melting Deposition[J]. Acta Metall Sin, 2023 , 59(2) : 226 -236 . DOI: 10.11900/0412.1961.2021.00577

References

1 Kesler M S, Goyel S, Ebrahimi F, et al. Effect of microstructural parameters on the mechanical behavior of TiAlNb(Cr, Mo) alloys with γ + σ microstructure at ambient temperature[J]. J. Alloys Compd., 2017, 695: 2672
2 Zhou H T, Kong F T, Wang X P, et al. High strength in high Nb containing TiAl alloy sheet with fine duplex microstructure produced by hot pack rolling[J]. J. Alloys Compd., 2017, 695: 3495
3 Yue H Y, Chen Y Y, Wang X P, et al. Effect of beam current on microstructure, phase, grain characteristic and mechanical properties of Ti-47Al-2Cr-2Nb alloy fabricated by selective electron beam melting[J]. J. Alloys Compd., 2018, 750: 617
4 Yang J, Xiao S, Zhang Q K, et al. In-situ synthesis of Ti-Al intermetallic compounds coating on Ti alloy by magnetron sputtering deposition followed by vacuum annealing[J]. Vacuum, 2020, 172: 109060
5 Kurzina I A, Kozlov E V, Sharkeev Y P, et al. Influence of ion implantation on nanoscale intermetallic-phase formation in Ti-Al, Ni-Al and Ni-Ti systems[J]. Surf. Coat. Technol., 2007, 201: 8463
6 Zhao Y C, Liu K. Effect of CeO2 and Y2O3 on tribological properties of Ti-Al/WC cermet composite coatings[J]. Lubr. Eng., 2019, 44(7): 78
6 赵运才, 刘 克. CeO2和Y2O3对Ti-Al/WC金属陶瓷复合涂层摩擦学性能的影响[J]. 润滑与密封, 2019, 44(7): 78
7 Burkov A A, Chigrin P G. Synthesis of Ti-Al intermetallic coatings via electrospark deposition in a mixture of Ti and Al granules technique[J]. Surf. Coat. Technol., 2020, 387: 125550.
8 Chang Z X, Wang W X, Ge Y Q, et al. Microstructure and mechanical properties of Ni-Cr-Si-B-Fe composite coating fabricated through laser additive manufacturing[J]. J. Alloys Compd., 2018, 747: 401
9 Carrullo J C Z, Falcón J C P, Borrás V A. Influence of process parameters and initial microstructure on the oxidation resistance of Ti48Al2Cr2Nb coating obtained by laser metal deposition[J]. Surf. Coat. Technol., 2019, 358: 114
10 Cheng J, Zhu S Y, Qiao Z H, et al. Recent advances of the tribology research of TiAl based intermetallics[J]. Tribology, 2015, 35: 342
10 程 军, 朱圣宇, 乔竹辉 等. TiAl基金属间化合物的摩擦学研究进展[J]. 摩擦学学报, 2015, 35: 342
11 He X, Song R G, Kong D J. Effects of TiC on the microstructure and properties of TiC/TiAl composite coating prepared by laser cladding[J]. Opt. Laser Technol., 2019, 112: 339
12 Cheng J, Yu Y, Fu L C, et al. Effect of TiB2 on dry-sliding tribological properties of TiAl intermetallics[J]. Tribol. Int., 2013, 62: 91
13 Schubert W D, Neumeister H, Kinger G, et al. Hardness to toughness relationship of fine-grained WC-Co hardmetals[J]. Int. J. Refract. Met. Hard Mater., 1998, 16: 133
14 Witusiewicz V T, Bondar A A, Hecht U, et al. The Al-B-Nb-Ti system: V. Thermodynamic description of the ternary system Al-B-Ti[J]. J. Alloys Compd., 2009, 474: 86
15 Larson D J, Liu C T, Miller M K. Boron solubility and boride compositions in α2 + γ titanium aluminides[J]. Intermetallics, 1997, 5: 411
16 Hyman M E, McCullough C, Levi C G, et al. Evolution of boride morphologies in TiAl-B alloys[J]. Metall. Trans., 1991, 22A: 1647
17 Li P T. The growth mechanisms and control of TiB2 and LaB6 in-situ synthesized in Al melts[D]. Jinan: Shandong University, 2013
17 李鹏廷. 铝溶体中原位生成TiB2与LaB6的生长机制及控制[D]. 济南: 山东大学, 2013
18 Witusiewicz V T, Bondar A A, Hecht U, et al. The Al-B-Nb-Ti system: III. Thermodynamic re-evaluation of the constituent binary system Al-Ti[J]. J. Alloys Compd., 2008, 465: 64
19 Zhang L, Su Y Q, Yang H M, et al. As-cast structure refinement of Ti-46Al alloy by hafnium and boron additions[J]. China Foundry, 2009, 6: 115
20 Han J C, Xiao S L, Tian J, et al. Grain refinement by trace TiB2 addition in conventional cast TiAl-based alloy[J]. Mater. Charact., 2015, 106: 112
21 Yang G Y, Liu Y, Wang Y, et al. Effects of trace B and Y elements on microstructures of cast Ti-Al-Nb-W alloy[J]. Chin. J. Nonferrous Met., 2011, 21: 777
21 杨广宇, 刘 咏, 王 岩 等. 微量B和Y对铸造Ti-Al-Nb-W合金显微组织的影响[J]. 中国有色金属学报, 2011, 21: 777
22 Goodarzi D M, Pekkarinen J, Salminen A. Analysis of laser cladding process parameter influence on the clad bead geometry[J]. Weld. World, 2017, 61: 883
23 Kurz W, Bezen?on C, G?umann M. Columnar to equiaxed transition in solidification processing[J]. Sci. Technol. Adv. Mater., 2001, 2: 185
24 Rong L, Huang J, Li Z G, et al. Microstructure and property of laser cladding Ni-based alloy coating reinforced by WC particles[J]. China Surf. Eng., 2010, 23(6): 40
24 戎 磊, 黄 坚, 李铸国 等. 激光熔覆WC颗粒增强Ni基合金涂层的组织与性能[J]. 中国表面工程, 2010, 23(6): 40
25 Ritchie R O. The conflicts between strength and toughness[J]. Nat. Mater., 2011, 10: 817
26 Rabinowicz E, Dunn L A, Russell P G. A study of abrasive wear under three-body conditions[J]. Wear, 1961, 4: 345
27 Moore M A, King F S. Abrasive wear of brittle solids[J]. Wear, 1980, 60: 123
28 Lu N. The three-dimension evaluation system establishment and detection method research of casting surface roughness[D]. Harbin: Harbin University of Science and Technology, 2014
28 卢 男. 铸造表面粗糙度三维评价体系建立及检测方法研究[D]. 哈尔滨: 哈尔滨理工大学, 2014
Outlines

/