Research paper

Synergistic Effect Mechanism of Different Ions on the Electrochemical Corrosion Behavior of TC4 Titanium Alloy

  • ZHAO Pingping ,
  • SONG Yingwei ,
  • DONG Kaihui ,
  • HAN En-Hou
Expand
  • 1CAS Key Laboratory of Nuclear Materials and Safety Assessment, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    2Southern Marine Science and Engineering Guangdong Laboratory (Zhuhai), Zhuhai 519000, China
SONG Yingwei, professor, Tel: (024)23893115, E-mail: ywsong@imr.ac.cn

Received date: 2021-06-29

  Revised date: 2021-09-07

  Online published: 2021-11-29

Supported by

Innovation Group Project of Southern Marine Science and Engineering Guangdong Laboratory (Zhuhai)(311021013)

Abstract

Due to the compact passive film, titanium alloys exhibit excellent corrosion resistance. However, during practical applications, the passive film is inevitably damaged by aggressive ions. Among the common ions, F- is the most harmful to the passive film because of its high complexation with Ti. However, the destructiveness of F- varies with pH. Moreover, there are inhibitory ions that reduce the aggressiveness of F-. The acceleration effects of H+ and F- as well as the inhibition effect of Fe3+ on the corrosion behavior of TC4 alloy were examined in this work using electrochemical polarization curves measurements and electrochemical impedance spectroscopy (EIS). The results reveal that whereas H+ has slight destructive effect on the passive film, F- has a considerable aggressive effect. In particular, F- and H+ work synergistically to accelerate the corrosion of the TC4 alloy. The addition of Fe3+ can somewhat reduce corrosion of the TC4 alloy. This can be attributable to the fact that the faster cathodic reduction caused by Fe3+ moves the anodic curves from active-passive region to passive region. Meanwhile, F- is consumed by forming a compound with Fe3+, which mitigates the corrosive effect of F- on passive film.

Cite this article

ZHAO Pingping , SONG Yingwei , DONG Kaihui , HAN En-Hou . Synergistic Effect Mechanism of Different Ions on the Electrochemical Corrosion Behavior of TC4 Titanium Alloy[J]. Acta Metall Sin, 2023 , 59(7) : 939 -946 . DOI: 10.11900/0412.1961.2021.00266

References

1 Yan M Q, Chen L Q, Yang P, et al. Effect of hot deformation parameters on the evolution of microstructure and texture of β phase in TC18 titanium alloy [J]. Acta Metall. Sin., 2021, 57: 880
  颜孟奇, 陈立全, 杨 平 等. 热变形参数对TC18钛合金β相组织及织构演变规律的影响 [J]. 金属学报, 2021, 57: 880
2 Xu X, Liang W P, Miao Q, et al. Effect of ZrN modified layer on friction and wear properties of TA18 titanium alloy [J]. Surf. Technol., 2021, 50(5): 133
  许 肖, 梁文萍, 缪 强 等. ZrN改性层对TA18钛合金摩擦磨损性能的影响 [J]. 表面技术, 2021, 50(5): 133
3 Dong J J, Fan J, Zhang H B, et al. Electrochemical performance of passive film pormed on Ti-Al-Nb-Zr alloy in simulated deep sea environments [J]. Acta Metall. Sin. (Engl. Lett.), 2020, 33: 595
4 Wang Y H, Li X, Alexandrov I V, et al. Impact of equal channel angular pressing on mechanical behavior and corrosion resistance of hot-rolled Ti-2Fe-0.1B alloy [J]. Materials (Basel), 2020, 13: 5117
5 Zhao P P, Song Y W, Dong K H, et al. Effect of passive film on the galvanic corrosion of titanium alloy Ti60 coupled to copper alloy H62 [J]. Mater. Corros., 2019, 70: 1745
6 Hu C Y, Lo S L, Kuan W H, et al. Treatment of high fluoride-content wastewater by continuous electrocoagulation-flotation system with bipolar aluminum electrodes [J]. Sep. Purif. Technol., 2008, 60: 1
7 Zhang C W, Fu T L, Chen H Y, et al. Research progress on crevice corrosion, plasma nitriding and surface nanocrystallization of titanium alloys [J]. Surf. Technol., 2019, 48(11): 114
  张乘玮, 付天琳, 陈涵悦 等. 钛合金缝隙腐蚀、离子渗氮与表面纳米化的研究进展 [J]. 表面技术, 2019, 48(11): 114
8 Pang J J, Blackwood D J. Corrosion of titanium alloys in high temperature near anaerobic seawater [J]. Corros. Sci., 2016, 105: 17
9 Amrutha M S, Fasmin F, Ramanathan S. Effect of HF concentration on anodic dissolution of titanium [J]. J. Electrochem. Soc., 2017, 164: H188
10 Wang Z B, Hu H X, Liu C B, et al. The effect of fluoride ions on the corrosion behavior of pure titanium in 0.05 M sulfuric acid [J]. Electrochim. Acta, 2014, 135: 526
11 Robin A, Meirelis J P. Influence of fluoride concentration and pH on corrosion behavior of titanium in artificial saliva [J]. J. Appl. Electrochem., 2007, 37: 511
12 Noel J J. The electrochemistry of titanium corrosion [D]. Winnipeg: University of Manitoba, 2000
13 Levy M. Anodic behavior of titanium and commercial alloys in sulfuric acid [J]. Corrosion, 1967, 23: 236
14 Cobb J R, Uhlig H H. Resistance of titanium to sulfuric and hydrochloric acids inhibited by ferric and cupric ions [J]. J. Electrochem. Soc., 1952, 99: 13
15 Stern M. The mechanism of passivating-type inhibitors [J]. J. Electrochem. Soc., 1958, 105: 638
16 Liu Y, Schaller R F, Asselin E. Effect of Fe(III) and Cu(II) on the passivation of Ti-2 in acidic chloride solutions [J]. J. Electrochem. Soc., 2019, 166: C76
17 Zhao P P, Song Y W, Shi L J, et al. Destruction of few fluorides to passive film of Ti-6Al-4V alloy under oxygen deficiency crevice conditions [J]. J. Mater. Sci., 2021, 56: 3510
18 Zhao P P, Song Y W, Dong K H, et al. Corrosion behavior of dual-phase Ti-6Al-4V alloys: A discussion on the impact of element Fe [J]. J. Alloys Compd., 2021, 858: 157708
19 Geng L, Qiao G Y, Gu K K. The effect of fluoride on electrochemical corrosion of the dental pure titanium before and after adhesion of Streptococcus mutans [J]. Shanghai J. Stomatol., 2016, 25: 150
  耿 黎, 乔广艳, 顾凯凯. 氟对变形链球菌黏附前后纯钛表面腐蚀性能的影响 [J]. 上海口腔医学, 2016, 25: 150
20 Wang Z B. Study of the critical fluoride concentration for the corrosion of pure titanium and its protective measurements in desulfurized wet flue gas environment [D]. Shenyang: University of Chinese Academy of Sciences, 2017
  王政彬. 脱硫湿烟气环境下纯钛腐蚀的临界氟离子浓度现象及防护措施研究 [D]. 沈阳: 中国科学院大学, 2017
21 Bar?o V, Mathew M T, Assun??o W, et al. Stability of cp-Ti and Ti-6Al-4V alloy for dental implants as a function of saliva pH—An electrochemical study [J]. Clin. Oral Implants Res., 2012, 23: 1055
22 Li X F, Wu X F, Liu S W, et al. Effects of fluorine on photocatalysis [J]. Chin. J Catal., 2020, 41: 1451
23 Huang H H. Effects of fluoride concentration and elastic tensile strain on the corrosion resistance of commercially pure titanium [J]. Biomaterials, 2002, 23: 59
24 Yue G K, Zhao L M, Olvera O G, et al. Speciation of the H2SO4-Fe2(SO4)3-FeSO4-H2O system and development of an expression to predict the redox potential of the Fe3+/Fe2+ couple up to 150oC [J]. Hydrometallurgy, 2014, 147-148: 196
25 Liang Y J, Che Y C. Handbook of Thermodynamics of Inogranic Substances [M]. Shenyang: Northeastern University Press, 1993: 616
  梁英教, 车荫昌. 无机物热力学数据手册 [M]. 沈阳: 东北大学出版社, 1993: 616
Outlines

/