Effect of Ce on the Microstructure, High-Temperature Tensile Properties, and Fracture Mode of Strip Casting Non-Oriented 6.5%Si Electrical Steel
Received date: 2021-03-23
Revised date: 2021-07-29
Online published: 2021-11-22
Supported by
National Natural Science Foundation of China(51801221)
Non-oriented 6.5%Si electrical steel exhibits excellent high-frequency magnetic properties, such as low iron loss and near-zero magnetostriction. Moreover, the high Si content causes poor deformability due to the solution strengthening effect of Si and the resulting ordering transformations, delaying the commercial application. Strip casting is a near-net forming technology that directly produces thin strips from the melt and reduces the required rolling deformation for the fabrication of thin sheets. This technology could be a viable option for industrializing the production of non-oriented 6.5%Si electrical steel. Despite this, even in the strip casting process, this brittle material is prone to edge cracks. Thus, improving the intrinsic plasticity of strip casting non-oriented 6.5%Si electrical steel is necessary through chemical modification to eliminate the deforming defects. The effect of Ce on the ordered phase of the solidification microstructure, high-temperature tensile properties, and fracture mode of strip casting non-oriented 6.5%Si electrical steel was investigated in this work. The results showed that the addition of Ce introduced high-melting Ce2O2.5S and Ce4O4S3 during strip casting, which promoted heterogeneous nucleation and refined the solidification microstructure of the as-cast strip. The presence of Ce did not affect the ordering condition of the as-cast strip. In decreasing order, the tensile temperatures corresponding to the ordered degree of the as-cast strip were 650, 400, and 800oC. With the tensile temperature increasing, the yield and tensile strengths of the as-cast strip decreased, whereas the elongation gradually increased. When the tensile temperature exceeded 500oC, the purification and microstructure refining effects of Ce improved grain-boundary cohesion and prevented intergranular cracking. Moreover, the occurrences of dynamic recovery and recrystallization eventually made the as-cast strip doped with Ce fractured by dimples, leading to a considerably enhanced tensile ductility. According to the findings, the rare-earth treatment should be considered as an effective method for increasing the ductility of strip casting non-oriented 6.5%Si electrical steel.
Min LI , Haoze LI , Jijie WANG , Yingche MA , Kui LIU . Effect of Ce on the Microstructure, High-Temperature Tensile Properties, and Fracture Mode of Strip Casting Non-Oriented 6.5%Si Electrical Steel[J]. Acta Metall Sin, 2022 , 58(5) : 637 -648 . DOI: 10.11900/0412.1961.2021.00115
| 1 | Yao Y C, Sha Y H, Liu J L, et al. Texture and magnetic properties of rolled Fe-6.5wt.% Si thin sheets [J]. J. Electron. Mater., 2014, 43: 121 |
| 2 | Tanaka Y, Takada Y, Abe M, et al. Magnetic properties of 6.5%Si-Fe sheet and its applications [J]. J. Magn. Magn. Mater., 1990, 83: 375 |
| 3 | Abe M, Takada Y, Murakami T, et al. Magnetic properties of commercially produced Fe-6.5wt% Si sheet [J]. J. Mater. Eng., 1989, 11: 109 |
| 4 | Phway T P P, Moses A J. Magnetostriction trend of non-oriented 6.5% Si-Fe [J]. J. Magn. Magn. Mater., 2008, 320: e611 |
| 5 | Viala B, Degauque J, Fagot M, et al. Study of the brittle behaviour of annealed Fe-6.5wt% Si ribbons produced by planar flow casting [J]. Mater. Sci. Eng., 1996, A212: 62 |
| 6 | Ouyang G Y, Chen X, Liang Y F, et al. Review of Fe-6.5 wt%Si high silicon steel—A promising soft magnetic material for sub-kHz application [J]. J. Magn. Magn. Mater., 2019, 481: 234 |
| 7 | Li C S, Yang C L, Cai G J, et al. Ordered phases and microhardness of Fe-6.5%Si steel sheet after hot rolling and annealing [J]. Mater. Sci. Eng., 2016, A650: 84 |
| 8 | Li R, Shen Q, Zhang L M, et al. Magnetic properties of high silicon iron sheet fabricated by direct powder rolling [J]. J. Magn. Magn. Mater., 2004, 281: 135 |
| 9 | Fu H D, Zhang Z H, Jiang Y B, et al. Improvement of magnetic properties of an Fe-6.5wt.% Si alloy by directional solidification [J]. Mater. Lett., 2011, 65: 1416 |
| 10 | Xie J X, Fu H D, Zhang Z H, et al. Deformation twinning feature and its effects on significant enhancement of tensile ductility in columnar-grained Fe-6.5wt.%Si alloy at intermediate temperatures [J]. Intermetallics, 2012, 23: 20 |
| 11 | Fu H D, Zhang Z H, Jiang Y B, et al. Applying the grain orientation dependence of deformation twinning to improve the deformation properties of an Fe-6.5wt%Si alloy [J]. J. Alloys Compd., 2016, 689: 307 |
| 12 | Haiji H, Okada K, Hiratani T, et al. Magnetic properties and workability of 6.5%Si steel sheet [J]. J. Magn. Magn. Mater., 1996, 160: 109 |
| 13 | Yamaji T, Abe M, Takada Y, et al. Magnetic properties and workability of 6.5% silicon steel sheet manufactured in continuous CVD siliconizing line [J]. J. Magn. Magn. Mater., 1994, 133: 187 |
| 14 | Matsushita T, Nakayama K, Fukase H, et al. Development and commercialization of twin roll strip caster [J]. IHI Eng. Rev., 2009, 42: 1 |
| 15 | Zapuskalov N. Comparison of continuous strip casting with conventional technology [J]. ISIJ Int., 2003, 43: 1115 |
| 16 | Ge S, Isac M, Guthrie R I L. Progress in strip casting technologies for steel; technical developments [J]. ISIJ Int., 2013, 53: 729 |
| 17 | Ge S, Isac M, Guthrie R I L. Progress of strip casting technology for steel; historical developments [J]. ISIJ Int., 2012, 52: 2109 |
| 18 | Liu H T, Liu Z Y, Sun Y, et al. Development of λ-fiber recrystallization texture and magnetic property in Fe-6.5wt% Si thin sheet produced by strip casting and warm rolling method [J]. Mater. Lett., 2013, 91: 150 |
| 19 | Li H Z, Liu H T, Liu Z Y, et al. Microstructure, texture evolution and magnetic properties of strip-casting non-oriented 6.5 wt.% Si electrical steel doped with cerium [J]. Mater. Charact., 2015, 103: 101 |
| 20 | Li H Z, Liu H T, Liu Z Y, et al. Characterization of microstructure, texture and magnetic properties in twin-roll casting high silicon non-oriented electrical steel [J]. Mater. Charact., 2014, 88: 1 |
| 21 | Liu H T, Li H Z, Li H L, et al. Effects of rolling temperature on microstructure, texture, formability and magnetic properties in strip casting Fe-6.5 wt% Si non-oriented electrical steel [J]. J. Magn. Magn. Mater., 2015, 391: 65 |
| 22 | Li H Z, Liu Z Y. Tensile properties of strip casting 6.5 wt% Si steel at elevated temperatures [J]. Mater. Sci. Eng., 2015, A639: 412 |
| 23 | Li H Z, Liu H T, Wang X L, et al. Effect of cerium on the as-cast microstructure and tensile ductility of the twin-roll casting Fe-6.5wt% Si alloy [J]. Mater. Lett., 2016, 165: 5 |
| 24 | Liu H T, Liu Z Y, Qiu Y Q, et al. Characterization of the solidification structure and texture development of ferritic stainless steel produced by twin-roll strip casting [J]. Mater. Charact., 2009, 60: 79 |
| 25 | Spinelli J E, Tosetti J P, Santos C A, et al. Microstructure and solidification thermal parameters in thin strip continuous casting of a stainless steel [J]. J. Mater. Process. Technol., 2004, 150: 255 |
| 26 | Takatani H, Gandin C A, Rappaz M. EBSD characterisation and modelling of columnar dendritic grains growing in the presence of fluid flow [J]. Acta Mater., 2000, 48: 675 |
| 27 | Waudby P E. Rare earth additions to steel [J]. Int. Met. Rev., 1978, 23: 74 |
| 28 | Chen X, Li Y X. Fracture toughness improvement of austempered high silicon steel by titanium, vanadium and rare earth elements modification [J]. Mater. Sci. Eng., 2007, A444: 298 |
| 29 | Bramfitt B L. The effect of carbide and nitride additions on the heterogeneous nucleation behavior of liquid iron [J]. Metall. Trans., 1970, 1: 1987 |
| 30 | Ouyang G Y, Macziewski C R, Jensen B, et al. Effects of solidification cooling rates on microstructures and physical properties of Fe-6.5% Si alloys [J]. Acta Mater., 2021, 205: 116575 |
| 31 | Cai G J, Yang Y, Huang Y R, et al. The significance of Ce on hot compression deformation and mechanical behavior of Fe-6.9 wt%Si alloy: Decrease of order degree and transformation of dislocations [J]. Mater. Charact., 2020, 163: 110220 |
| 32 | Shi X J, Liang Y F, Liu B B, et al. Warm deformation behavior and work-softening mechanism of Fe-6.5wt.%Si alloy [J]. J. Iron Steel Res. Int., 2020, 27: 342 |
| 33 | Jung H, Kim J. Influence of cooling rate on iron loss behavior in 6.5wt% grain-oriented silicon steel [J]. J. Magn. Magn. Mater., 2014, 353: 76 |
| 34 | Yu X, Zhang Z H, Xie J X. Microstructure, ordered structure and warm tensile ductility of Fe-6.5% Si alloy with various Ce content [J]. Acta Metall. Sin., 2017, 53: 927 |
| 34 | 于 宣, 张志豪, 谢建新. 不同Ce含量Fe- 6.5%Si合金的组织、有序结构和中温拉伸塑性 [J]. 金属学报, 2017, 53: 927 |
/
| 〈 |
|
〉 |