Influence of Spark Plasma Sintering Parameters on the Microstructure and Room-Temperature Mechanical Properties of NiAl-28Cr-5.5Mo-0.5Zr Alloy
Received date: 2020-09-04
Revised date: 2021-04-25
Online published: 2021-05-20
Supported by
National Natural Science Foundation of China(91860122)
As a potential high-temperature structural material, the practical application of NiAl intermetallic compound is limited because of its low plasticity and fracture toughness at room temperature and poor strength at high temperature. Adding alloying elements and optimizing the preparation process are effective ways to improve the material's performance. In this study, NiAl-based alloys were prepared through spark plasma sintering using NiAl-28Cr-5.5Mo-0.5Zr (atom fraction, %) prealloyed powders. The influence of sintering temperature and holding time on the density, microstructure, and room-temperature compression properties of the sintered alloys was studied. The microstructures of the sintered alloys were investigated using SEM, and their room-temperature compression properties were tested using an electronic universal testing machine. It is shown that the influence of spark plasma sintering temperature on the density and room-temperature compression properties of sintered alloys is significant while that of the holding time is weaker. Under optimal sintering parameters, i.e., a sintering temperature of 1200oC, holding time of 3 min, and sintering pressure of 50 MPa, the yield strength, compressive strength, and plasticity strain of the sintered alloy were 1321.4 MPa, 2360 MPa, and 0.313, respectively. Additionally, the densification process of NiAl-28Cr-5.5Mo-0.5Zr alloy prepared by spark plasma sintering was studied.
Ze LIU , Hanwei NING , Zhangqian LIN , Dongjun WANG . Influence of Spark Plasma Sintering Parameters on the Microstructure and Room-Temperature Mechanical Properties of NiAl-28Cr-5.5Mo-0.5Zr Alloy[J]. Acta Metall Sin, 2021 , 57(12) : 1579 -1587 . DOI: 10.11900/0412.1961.2020.00346
| 1 | Gao H Y, He Y H, Shen P Z. Research status of FeAl intermetallics compound [J]. Mater. Rev., 2008, 22(7): 68 |
| 1 | 高海燕, 贺跃辉, 沈培智. FeAl金属间化合物研究现状 [J]. 材料导报, 2008, 22(7): 68 |
| 2 | Bochenek K, Basista M. Advances in processing of NiAl intermetallic alloys and composites for high temperature aerospace applications [J]. Prog. Aerosp. Sci., 2015, 79: 136 |
| 3 | Sun Y, Liu R Y, Zhang J S, et al. Progress in NiAl-based intermetallic compound research [J]. Mater. Rev., 2003, 17(7): 10 |
| 3 | 孙 岩, 刘瑞岩, 张俊善等. NiAl基金属间化合物的研究进展 [J]. 材料导报, 2003, 17(7): 10 |
| 4 | Chen L, Peng P, Zhan J P, et al. First-principles calculation on mechanical properties of B2-NiAl intermetallic compound with Fe addition [J]. Rare Met. Mater. Eng., 2010, 39: 229 |
| 4 | 陈 律, 彭 平, 湛建平等. Fe对NiAl力学性能影响的第一原理计算 [J]. 稀有金属材料与工程, 2010, 39: 229 |
| 5 | Guo J T, Ren W L, Zhou J. Progress in research on alloying effects in NiAl intermetallic alloys [J]. Acta Metall. Sin., 2002, 38: 667 |
| 5 | 郭建亭, 任维丽, 周 健. NiAl合金化研究进展 [J]. 金属学报, 2002, 38: 667 |
| 6 | Leng W X, Tian W H. Precipitation hardening of NiAl(Fe) intermetallic compounds in Ni-Al-Fe system [J]. Rare Met. Mater. Eng., 2010, 39: 460 |
| 6 | 冷文秀, 田文怀. Ni-Al-Fe系中NiAl(Fe)金属间化合物的析出强化 [J]. 稀有金属材料与工程, 2010, 39: 460 |
| 7 | Chen L. First-principles study on mechanical properties of B2-NiAl intermetallic compound with P microalloying [J]. Rare Met. Mater. Eng., 2012, 41(suppl.2): 290 |
| 7 | 陈 律. 微量P对NiAl力学性能影响的理论研究 [J]. 稀有金属材料与工程, 2012, 41(): 290 |
| 8 | Hu X L, Luo Y, Zhao R X, et al. Effect of P on mechanical properties of NiAl intermetallics [J]. J. Civil Aviat. Univ. China, 2016, 34(6): 61 |
| 8 | 胡雪兰, 罗 阳, 赵若汐等. 磷对NiAl弹性模量和韧塑性影响的第一原理研究 [J]. 中国民航大学学报, 2016, 34(6): 61 |
| 9 | Johnson D R, Chen X F, Oliver B F, et al. Processing and mechanical properties of in-situ composites from the NiAl-Cr and the NiAl-(Cr, Mo) eutectic systems [J]. Intermetallics, 1995, 3: 99 |
| 10 | Yuan C, Zhou L Z, Li G S, et al. Characteristics of a NiAl eutectic alloy JJ-3 with excellent properties [J]. Acta Metall. Sin., 2013, 49: 1347 |
| 10 | 袁 超, 周兰章, 李谷松等. 高性能NiAl共晶合金JJ-3 [J]. 金属学报, 2013, 49: 1347 |
| 11 | Sheng L Y, Zhang W, Lai S, et al. Microstructure and mechanical properties of Laves phase strengthening NiAl base composite fabricated by rapid solidification [J]. Acta Metall. Sin., 2013, 49: 1318 |
| 11 | 盛立远, 章 炜, 赖 琛等. 快速凝固制备Laves相增强NiAl基复合材料的微观组织及力学性能 [J]. 金属学报, 2013, 49: 1318 |
| 12 | Sun J, Ma S N, Qi Y H. Microstructure and mechanical properties of rapidly solidified NiAl-Cr(Mo)-Zr alloy [J]. J. Liaoning Inst. Univ. Technol. (Nat. Sci. Ed.), 2013, 33: 367 |
| 12 | 孙 静, 马胜男, 齐义辉. 快速凝固NiAl-Cr(Mo)-Zr合金的显微组织与力学性能 [J]. 辽宁工业大学学报(自然科学版), 2013, 33: 367 |
| 13 | Xiao S W. High temperature tensile properties and brittle-to-ductile transition of directionally solidified NiAl-15Cr alloy [J]. Mater. Mech. Eng., 2010, 34(5): 60 |
| 13 | 肖思文. 定向凝固NiAl-15Cr合金的高温拉伸性能和韧脆转变条件 [J]. 机械工程材料, 2010, 34(5): 60 |
| 14 | Sun Y, Lin P, Yuan S J. A novel method for fabricating NiAl alloy sheet components using laminated Ni/Al foils [J]. Mater. Sci. Eng., 2019, A754: 428 |
| 15 | Cui C Y, Guo J T. Investigation on microstructure and mechanical property of NiAl-28Cr-5Mo-1Hf alloy [J]. Acta Metall. Sin., 1999, 35: 477 |
| 15 | 崔传勇, 郭建亭. NiAl-28Cr-5Mo-1Hf多相金属间化合物的显微组织及力学性能研究 [J]. 金属学报, 1999, 35: 477 |
| 16 | Ning H W, Wang D J, Wang B, et al. Investigations on the NiAl-Cr(Mo) eutectic alloy with optimized microstructure and improved room-temperature compressive properties [J]. Mater. Sci. Eng., 2021, A813: 141138 |
| 17 | Bai L, Ge C C, Shen W P. Spark plasma sintering technology [J]. Powder Metall. Technol., 2007, 25: 217 |
| 17 | 白 玲, 葛昌纯, 沈卫平. 放电等离子烧结技术 [J]. 粉末冶金技术, 2007, 25: 217 |
| 18 | Liang Y C, Guo J T, Sheng L Y, et al. Effects of rare earth element Gd On the microstructure and mechanical properties of NiAl-Cr(Mo)-Hf eutectic alloy [J]. Acta Metall. Sin., 2010, 46: 528 |
| 18 | 梁永纯, 郭建亭, 盛立远等. 稀土元素Gd对NiAl-Cr(Mo)-Hf共晶合金的组织和压缩性能的影响 [J]. 金属学报, 2010, 46: 528 |
| 19 | Guo J T. Research progress of intermetallic NiAl alloys [J]. J. Cent. South Univ. (Sci. Technol.), 2007, 38: 1013 |
| 19 | 郭建亭. 金属间化合物NiAl的研究进展 [J]. 中南大学学报(自然科学版), 2007, 38: 1013 |
| 20 | Sheng L Y, Zhang W, Guo J T, et al. Microstructure and mechanical properties of Hf and Ho doped NiAl-Cr(Mo) near eutectic alloy prepared by suction casting [J]. Mater. Charact., 2009, 60: 1311 |
| 21 | Sheng L Y, Zhang W, Guo J T, et al. Microstructure evolution and mechanical properties' improvement of NiAl-Cr(Mo)-Hf eutectic alloy during suction casting and subsequent HIP treatment [J]. Intermetallics, 2009, 17: 1115 |
| 22 | Sheng L Y, Guo J T, Ye H Q. Microstructure and mechanical properties of NiAl-Cr(Mo)/Nb eutectic alloy prepared by injection-casting [J]. Mater. Des., 2009, 30: 964 |
| 23 | Hao F C, Cui Z Q, Wang W X. Effects of spark plasma sintering temperature on microstructure and mechanical properties of ZK61 magnesium alloy [J]. Trans. Mater. Heat Treat., 2017, 38(3): 34 |
| 23 | 郝峰晨, 崔泽琴, 王文先. 放电等离子烧结温度对ZK61镁合金组织及力学性能的影响 [J]. 材料热处理学报, 2017, 38(3): 34 |
| 24 | Li X X, Yang C, Lu H Z, et al. Correlation between atomic diffusivity and densification mechanism during spark plasma sintering of titanium alloy powders [J]. J. Alloys Compd., 2019, 787: 112 |
| 25 | Liu R F, Wang W X, Chen H S, et al. Densification of pure magnesium by spark plasma sintering-discussion of sintering mechanism [J]. Adv. Powder Technol., 2019, 30: 2649 |
| 26 | Song X Y, Liu X M, Zhang J X. Mechanism of conductive powder microstructure evolution in the process of SPS [J]. Sci. China, 2005, 48E: 459 |
| 26 | 宋晓艳, 刘雪梅, 张久兴. SPS过程中导电粉体的显微组织演变规律及机理 [J]. 中国科学, 2005, 35E: 459 |
| 27 | Yao L, Chi Y S, Zhao Z K. Influence of the sintering pressure on Al90Mn9Ce1 alloy SPS densification [J]. J. Changchun Univ. Technol. (Nat. Sci. Ed.), 2009, 30: 121 |
| 27 | 姚 露, 迟元顺, 赵占奎. 烧结压力对Al90Mn9Ce1合金SPS致密化的影响 [J]. 长春工业大学学报(自然科学版), 2009, 30: 121 |
| 28 | Kang S J L. Sintering: Densification, Grain Growth and Microstructure [M]. Oxford: Elsevier Butterworth-Heinemann, 2005: 674 |
| 29 | Huai K W, Guo J T, Du X H, et al. Microstructure and mechanical properties of NiAl-Cr(Mo)/Hf alloy prepared by injection casting[J]. Mater. Des., 2007, 28: 1940 |
/
| 〈 |
|
〉 |