New Development of Research on Casting of Bulk Amorphous Alloys
Received date: 2020-10-20
Revised date: 2020-12-24
Online published: 2021-01-19
Supported by
National Natural Science Foundation of China(52071278);National Key Research and Development Program of China(2018YFA0703603)
Bulk amorphous alloys possess a metastable structure, which is difficult to process and manufacture into components or parts by conventional forging or welding. Instead, components or parts from bulk amorphous alloys can be fabricated by vacuum casting with the fluidity of bulk amorphous-alloy melts. Based on the casting forming of bulk amorphous alloys, this paper briefly introduces the fluidity and filling ability of bulk amorphous-alloy melts. In addition, the technical methods and applications of vacuum die casting, vacuum suction casting, gravity casting in a water-cooled copper crucible, and phase-change refrigeration casting are also mentioned. The theoretical problems and technical bottlenecks to be resolved in the forming process of bulk amorphous alloys are then discussed. Finally, the engineering application prospects of bulk amorphous alloys are suggested.
Riping LIU , Mingzhen MA , Xinyu ZHANG . New Development of Research on Casting of Bulk Amorphous Alloys[J]. Acta Metall Sin, 2021 , 57(4) : 515 -528 . DOI: 10.11900/0412.1961.2020.00414
| 1 | Wang W H, Luo P. The dynamic behavior hidden in the long time scale of metallic glasses and its effect on the properties [J]. Acta Metall. Sin., 2018, 54: 1479 |
| 1 | 汪卫华, 罗 鹏. 金属玻璃中隐藏在长时间尺度下的动力学行为及其对性能的影响 [J]. 金属学报, 2018, 54: 1479 |
| 2 | Inoue A, Takeuchi A. Recent development and application products of bulk glassy alloys [J]. Acta Mater., 2011, 59: 2243 |
| 3 | Tian H F, Qiao J W, Yang H J, et al. The corrosion behavior of in-situ Zr-based metallic glass matrix composites in different corrosive media [J]. Appl. Surf. Sci., 2016, 363: 37 |
| 4 | Li B, Sun W C, Qi H N, et al. Effects of Ag substitution for Fe on glass-forming ability, crystallization kinetics, and mechanical properties of Ni-free Zr-Cu-Al-Fe bulk metallic glasses [J]. J. Alloys Compd., 2020, 827: 154385 |
| 5 | Jin Z S, Yang Y J, Zhang Z P, et al. Effect of Hf substitution Cu on glass-forming ability, mechanical properties and corrosion resistance of Ni-free Zr-Ti-Cu-Al bulk metallic glasses [J]. J. Alloys Compd., 2019, 806: 668 |
| 6 | Kramer J. Noconducting modification of metals [J]. Annln Phys., 1934, 19: 37 |
| 7 | Brenner A, Couch D E, Williams E K. Electrodeposition of alloys of phosphorus with nickel or cobalt [J]. J. Res. Natl. Bur. Srtand., 1950, 44: 109 |
| 8 | Buckel W, Hilsch R. Einflu? der kondensation bei tiefen temperaturen auf den elektrischen widerstand und die supraleitung für verschiedene metalle [J]. Z. Phys., 1954, 138: 109 |
| 9 | Turnbull D, Cohen M H. Concerning reconstructive transformation and formation of glass [J]. J. Chem. Phys., 1958, 29: 1049 |
| 10 | Chen H S, Turnbull D. Evidence of a glass-liquid transition in a gold-germanium-silicon alloy [J]. J. Chem. Phys., 1968, 48: 2560 |
| 11 | Klement W K, Willens P H, Duwez P. Non-crystalline structure in solidified gold-silicon alloys [J]. Nature, 1960, 187: 869 |
| 12 | Inoue A, Kohinata M, Tasi A P, et al. Mg-Ni-La amorphous alloys with a wide supercooled liquid region [J]. Mater Trans. JIM, 1989, 30: 378 |
| 13 | Inoue A, Zhang T, Masumoto T. Al-La-Ni amorphous alloys with a wide supercooled liquid region [J]. Mater. Trans. JIM, 1989, 30: 965 |
| 14 | Peker A, Johnson W L. A highly processable metallic glass: Zr41.2Ti13.8Cu12.5Ni10.0Be22.8 [J]. Appl. Phys. Lett., 1993, 63: 2342 |
| 15 | Mukherjee S, Schroers J, Zhou Z, et al. Viscosity and specific volume of bulk metallic glass-forming alloys and their correlation with glass forming ability [J]. Acta Mater., 2004, 52: 3689 |
| 16 | Saini S, Srivastava A P, Neogy S. The effect of Ag addition on the crystallization kinetics and glass forming ability of Zr-(CuAg)-Al bulk metallic glass [J]. J. Alloys Compd., 2019, 772: 961 |
| 17 | Yang Y J, Cheng B Y, Jin Z S, et al. Crystallization kinetics and mechanical properties of Zr56Cu24Al9Ni7-xTi4Agx (x=0, 1, 3, 5, and 7) metallic glasses [J]. J. Alloys Compd., 2020, 816: 152589 |
| 18 | Rahvard M M, Tamizifar M, Ali Boutorabi S M. The effect of Ag addition on the non-isothermal crystallization kinetics and fragility of Zr56Co28Al16 bulk metallic glass [J]. J. Non-Cryst. Solids, 2018, 481: 74 |
| 19 | Wang Z, Ketov S V, Chen C L, et al. Nucleation and thermal stability of an icosahedral nanophase during the early crystallization stage in Zr-Co-Cu-Al metallic glasses [J]. Acta Mater., 2017, 132: 298 |
| 20 | Wang W H. The elastic properties, elastic models and elastic perspectives of metallic glasses [J]. Prog. Mater. Sci., 2012, 57: 487 |
| 21 | Dandana W, Hajlaoui K. Effect of hydrogen addition on the mechanical properties of Zr-based metallic glass [J]. J. Alloys Compd., 2018, 742: 563 |
| 22 | Bian Z, He G, Chen G L. Investigation of shear bands under compressive testing for Zr-base bulk metallic glasses containing nanocrystals [J]. Scr. Mater., 2002, 46: 407 |
| 23 | Zan Y, Wang W H, Greer A L. Making metallic glasses plastic by control of residual stress [J]. Nat. Mater., 2006, 5: 857 |
| 24 | Ma D Q, Jiao W T, Zhang Y F, et al. Strong work-hardening behavior induced by the solid solution strengthening of dendrites in TiZr-based bulk metallic glass matrix composites [J]. J. Alloys Compd., 2015, 624: 9 |
| 25 | Hilke S, R?sner H, Geissler D, et al. The influence of deformation on the medium-range order of a Zr-based bulk metallic glass characterized by variable resolution fluctuation electron microscopy [J]. Acta Mater., 2019, 171: 275 |
| 26 | Fu J, Zhu Y H, Zheng C, et al. Effect of laser shock peening on the compressive deformation and plastic behavior of Zr-based bulk metallic glass [J]. Opt. Lasers Eng., 2016, 86: 53 |
| 27 | Ma D Q, Li J, Zhang Y F, et al. Effect of compositional tailoring on the glass-forming ability and mechanical properties of TiZr-based bulk metallic glass matrix composites [J]. Mater. Sci. Eng., 2014, A612: 310 |
| 28 | Zhong H, Chen J, Dai L Y, et al. Effect of counterpart material on the tribological properties of Zr-based bulk metallic glass under relatively heavy loads [J]. Wear, 2016, 346-347: 22 |
| 29 | Zhong H, Chen J, Dai L Y, et al. Tribological behaviors of Zr-based bulk metallic glass versus Zr-based bulk metallic glass under relative heavy loads [J]. Intermetallics, 2015, 65: 88 |
| 30 | Yue Y, Wang R, Ma D Q, et al. Fatigue behavior of a Zr-based bulk metallic glass under uniaxial tension-tension and three-point bending loading mode [J]. Intermetallics, 2015, 60: 86 |
| 31 | Telford M. The case for bulk metallic glass [J]. Mater. Today, 2004, 7: 36 |
| 32 | Johnson W L. Fundamental aspects of bulk metallic glass formation in multicomponent alloys [J]. Mater. Sci. Forum., 1996, 225: 35 |
| 33 | Wang W H. The nature and properties of amorphous matter [J]. Prog. Phys., 2013, 33: 177 |
| 33 | 汪卫华. 非晶态物质的本质和特性 [J]. 物理学进展, 2013, 33: 177 |
| 34 | Yang Y J, Liu W C, Guo D, et al. Research progress in casting forming of bulk amorphous alloy [J]. Spec. Cast. Nonferrous Alloys, 2017, 37: 1354 |
| 34 | 杨玉婧, 刘文超, 郭 栋等. 块体非晶合金铸造成形的研究现状 [J]. 特种铸造及有色合金, 2017, 37: 1354 |
| 35 | Wu S F. New breakthrough in research and industrialization of amorphous materials in Dongguan EONTEC. Co., Ltd. [EB/OL]. Science and technology media network, (2015-01-27). |
| 35 | 吴少芳. 宜安科技非晶材料研究与产业化获新突破[EB/OL]. 科技传媒网, (2015-01-27). |
| 36 | Ma M Z, Zong H T, Wang H Y, et al. The fluidity and molding ability of glass-forming Zr-based alloy melt [J]. Sci. China, 2008, 51G: 438 |
| 37 | Ma M Z, Liu R P, Ma D Q, et al. Flowability testing method and device for zirconium base block amorphous alloy melt [P]. Chin Pat, 201310083859.9, 2015马明臻, 刘日平, 马德强等. 锆基块体非晶合金熔体流动性测试方法及其装置 [P]. 中国专利, 201310083859.9, 2015) |
| 38 | Ma D Q, Ma X Z, Zhang H Y, et al. Evaluation of casting fluidity and filling capacity of Zr-based amorphous metal melts [J]. J. Iron Steel Res. Int., 2018, 25: 1163 |
| 39 | Hofmann D C, Roberts S N. Microgravity metal processing: From undercooled liquids to bulk metallic glasses [J]. NPJ Microgravity, 2015, 1: 15003 |
| 40 | Ramasamy P, Szabo A, Borzel S, et al. High pressure die casting of Fe-based metallic glass [J]. Sci. Rep., 2016, 6: 35258 |
| 41 | Liu L H, Zhang T, Liu Z Y, et al. Near-net forming complex shaped Zr-based bulk metallic glasses by high pressure die casting [J]. Materials, 2018, 11: 2338 |
| 42 | Liu L H, Zhang T, Liu Z Y, et al. Abnormal increase of glass forming ability under rising mold temperature in high pressure die casting [J]. Mater. Lett., 2019, 247: 215 |
| 43 | Inoue A, Nakamura T, Nishiyama N, et al. Mg-Cu-Y bulk amorphous alloys with high tensile strength produced by a high-pressure die casting method [J]. Mater. Trans. JIM, 1992, 33: 937 |
| 44 | Laws K J, Gun B, Ferry M. Effect of die-casting parameters on the production of high quality bulk metallic glass samples [J]. Mater. Sci. Eng., 2006, A425: 114 |
| 45 | Inoue A, Nakamura T, Sugita T, et al. Bulky La-Al-TM (TM = transition metal) amorphous alloys with high tensile strength produced by a high-pressure die casting method [J]. Mater. Trans. JIM, 1993, 34: 351 |
| 46 | Hofmann D C, Polit-Casillas R, Roberts S N, et al. Castable bulk metallic glass strain wave gears: Towards decreasing the cost of high-performance robotics [J]. Sci. Rep., 2016, 6: 37773 |
| 47 | Ma M Z, Liu R P, Zhang X Y, et al. Casting method of zirconium-based bulk amorphous alloy casting [P]. Chin Pat, 201210367027.5, 2014 |
| 47 | 马明臻, 刘日平, 张新宇等. 一种锆基块体非晶合金铸件的铸造成形方法 [P]. 中国专利, 201210367027.5, 2014) |
| 48 | Wang W K, Zhan Z J. Method for phase change refrigeration to induce material controlled coagulation [P]. Chin Pat, 200410079097.6, 2009 |
| 48 | 王文魁, 战再吉. 相变致冷诱发凝固控制材料组织的方法 [P]. 中国专利, 200410079097.6, 2009) |
| 49 | Li P J, Liu X S, Pan L L, et al. Manufacture of die casting equipment for Zr based bulk metallic glass and its industrialization progress [A]. Special Issue of 2016 Annual Meeting of Special Casting & Nonferrous Alloy [C]. Nantong: Chinese Society of Mechanical Engineering, Chinese Society of Ordnance Engineering, 2016: 254 |
| 49 | 李培杰, 刘相尚, 潘玲玲等. 锆基非晶合金的压铸设备的开发及产业化进展 [A]. 2016年(第八届)中国压铸、挤压铸造、半固态加工年会 [C]. 南通: 中国机械工程学会, 中国兵工学会, 2016: 254 |
| 50 | Zhang F L. Amorphous alloy diecasting equipment and amorphous alloy diecasting process [P]. Chin Pat, 201110421420.3, 2015 |
| 50 | 张法亮. 非晶合金压铸设备及非晶合金压铸工艺 [P]. 中国专利, 201110421420.3, 2015) |
| 51 | Science and Technology Media Network/Today's Headlines. Yi'an Dongguan EONTEC Co., Ltd. benefits continuously, and the first liquid metal die casting machine in China comes out [EB/OL].(2016-11-30). |
| 51 | 科技传媒网/今日头条. 宜安科技利好不断, 参股公司国内首台液态金属压铸机问世[EB/OL]. (2016-11-30). |
/
| 〈 |
|
〉 |