Grain Structure and Metallurgical Defects Regulation of Selective Laser Melted René 88DT Superalloy
Received date: 2020-05-06
Revised date: 2020-09-10
Online published: 2020-11-23
Supported by
Fundamental Research Funds for the Central Universities(FRF-TP-18-092A1)
Columnar grain and hot crack restrict the performance of laser melting deposited René 88DT superalloy when applied to turbine disks, requiring equiaxed grain to improve the fatigue property. Selective laser melting can fabricate material with low composition segregation, reduced defects, and equiaxed or near-equiaxed grains due to the fast cooling rate and vastly varied local heat flow direction during processing. In this study, a selective laser melted René 88DT was fabricated under variable processing parameters. The formation mechanism and control methods of grain structure and metallurgical defects were investigated. Results showed that changing the processing parameters can affect the preferred growth direction of crystal; thus, affecting the grain morphology and size. Processed with low heat input and 67° scan vectors rotation between deposited layers, cellular dendrites with different orientations grow competitively with each other, leading to the formation of near-equiaxed grains. The cellular dendrites can grow epitaxially across multiple deposited layers due to high heat input and 0° scan vector rotation, forming columnar grains. The columnar grains with a relatively low aspect ratio can be fabricated with 90° scan vectors rotation. However, anisotropy exists between the two orthogonal scanning directions due to the shielding effect of metal vapor dust. The primary defects in specimens are solidification cracks along grain boundaries caused by remelting of low-melting-point eutectic. Specimens with equiaxed grains showed much better ability in preventing solidification cracks from propagation than that with columnar grains. The defect density in the columnar grains is about 21 times higher than the equiaxed grains. Suitable processing conditions for selective laser melted René 88DT superalloys are low heat input and 67° scan vectors rotation based on the forming quality and service conditions.
Jian LIU , Qin PENG , Jianxin XIE . Grain Structure and Metallurgical Defects Regulation of Selective Laser Melted René 88DT Superalloy[J]. Acta Metall Sin, 2021 , 57(2) : 191 -204 . DOI: 10.11900/0412.1961.2020.00143
| 1 | Reed R C. The Superalloys: Fundamentals and Applications [M]. Cambridge: Cambridge University Press, 2006: 256 |
| 2 | Shi C X, Zhong Z Y. Development and innovation of superalloy in China [J]. Acta Metall. Sin., 2010, 46: 1281 |
| 2 | 师昌绪, 仲增墉. 我国高温合金的发展与创新 [J]. 金属学报, 2010, 46: 1281 |
| 3 | Zhang G Q, Zhang Y W, Zheng L, et al. Research progress in powder metallurgy superalloys and manufacturing technologies for aero-engine application [J]. Acta Metall. Sin., 2019, 55: 1133 |
| 3 | 张国庆, 张义文, 郑 亮等. 航空发动机用粉末高温合金及制备技术研究进展 [J]. 金属学报, 2019, 55: 1133 |
| 4 | Mao J, Chang K M, Yang W H, et al. Cooling precipitation and strengthening study in powder metallurgy superalloy Rene88DT [J]. Mater. Sci. Eng., 2002, A332: 318 |
| 5 | Hu D Y, Wang T, Ma Q H, et al. Effect of inclusions on low cycle fatigue lifetime in a powder metallurgy nickel-based superalloy FGH96 [J]. Int. J. Fatigue, 2019, 118: 237 |
| 6 | Shi Y, Yang D D, Yang X G, et al. The effect of inclusion factors on fatigue life and fracture-mechanics-based life method for a P/M superalloy at elevated temperature [J]. Int. J. Fatigue, 2020, 131: 105365 |
| 7 | Ning Y Q, Zhou C, Liang H Q, et al. Abnormal flow behavior and necklace microstructure of powder metallurgy superalloys with previous particle boundaries (PPBs) [J]. Mater. Sci. Eng., 2016, A652: 84 |
| 8 | Benjamin J S, Larson J M. Powder metallurgy techniques applied to superalloys [J]. J. Aircr., 1977, 14: 613 |
| 9 | Chlebus E, Gruber K, Ku?nicka B, et al. Effect of heat treatment on the microstructure and mechanical properties of Inconel 718 processed by selective laser melting [J]. Mater. Sci. Eng., 2015, A639: 647 |
| 10 | Jia Q B, Gu D D. Selective laser melting additive manufacturing of Inconel 718 superalloy parts: Densification, microstructure and properties [J]. J. Alloys Compd., 2014, 585: 713 |
| 11 | Liang Y J, Cheng X, Wang H M. A new microsegregation model for rapid solidification multicomponent alloys and its application to single-crystal nickel-base superalloys of laser rapid directional solidification [J]. Acta Mater., 2016, 118: 17 |
| 12 | Zhao X M, Lin X, Chen J. The effect of hot isostatic pressing on crack healing, microstructure, mechanical properties of Rene88DT superalloy prepared by laser solid forming [J]. Mater. Sci. Eng., 2009, A504: 129 |
| 13 | Zhao X M, Chen J, He F, et al. The cracking mechanism of Rene88DT superalloy by laser rapid forming [J]. Rare Met. Mater. Eng., 2007, 36: 216 |
| 13 | 赵晓明, 陈 静, 何 飞等. 激光快速成形Rene88DT高温合金开裂机理研究 [J]. 稀有金属材料与工程, 2007, 36: 216 |
| 14 | Li N, Kong H P, Du B R, et al. Analysis of microstructure and defects of FGH96 superalloy manufactured by laser rapid prototyping [J]. Fail. Anal. Prev., 2016, 11: 124 |
| 14 | 李 楠, 孔焕平, 杜博睿等. 激光快速成型FGH96高温合金的显微组织及缺陷分析 [J]. 失效分析与预防, 2016, 11: 124 |
| 15 | Zhang H Y, Zhang A F, He B, et al. Investigation on the microstructure and segregation of superalloy FGH96 by direct laser forming [J]. Appl. Mech. Mater., 2014, 464: 58 |
| 16 | Wen S, Dong A P, Lu Y L, et al. Finite element simulation of the temperature field and residual stress in GH536 superalloy treated by selective laser melting [J]. Acta Metall. Sin., 2018, 54: 393 |
| 16 | 文 舒, 董安平, 陆燕玲等. GH536高温合金选区激光熔化温度场和残余应力的有限元模拟 [J]. 金属学报, 2018, 54: 393 |
| 17 | Wu H Y, Zhang D, Yang B B, et al. Microstructural evolution and defect formation in a powder metallurgy nickel-based superalloy processed by selective laser melting [J]. J. Mater. Sci. Technol., 2020, 36: 7 |
| 18 | Sames W J, List F A, Pannala S, et al. The metallurgy and processing science of metal additive manufacturing [J]. Int. Mater. Rev., 2016, 61: 315 |
| 19 | Huang W D. The research progress of 3D printing technology [J]. J. New Ind., 2016, 6(3): 53 |
| 19 | 黄卫东. 材料3D打印技术的研究进展 [J]. 新型工业化, 2016, 6(3): 53 |
| 20 | Yang H O, Zhao Y F, Xu J J, et al. As-deposited microstructures of Rene88DT nickel-base superalloy by laser solid forming [J]. J. Netshape Form. Eng., 2019, 11(4): 9 |
| 20 | 杨海欧, 赵宇凡, 许建军等. 激光立体成形Rene88DT镍基高温合金沉积态组织研究 [J]. 精密成形工程, 2019, 11(4): 9 |
| 21 | Liu S, Zhang X, Yu H X, et al. Effect of laser melting deposition process on microstructure and property for FGH96 [J]. Aeronaut. Manuf. Technol., 2019, 62(1-2): 72 |
| 21 | 刘 帅, 张 雪, 于海鑫等. FGH96激光熔化沉积成形过程对组织与性能的影响 [J]. 航空制造技术, 2019, 62(1-2): 72 |
| 22 | Guo J T, Zhou L Z, Qin X Z. Phase transformations and their mechanisms in Fe- and Ni-base superalloys [J]. Chin. J. Nonferrous Met., 2011, 21: 476 |
| 22 | 郭建亭, 周兰章, 秦学智. 铁基和镍基高温合金的相变规律与机理 [J]. 中国有色金属学报, 2011, 21: 476 |
| 23 | Amato K N, Gaytan S M, Murr L E, et al. Microstructures and mechanical behavior of Inconel 718 fabricated by selective laser melting [J]. Acta Mater., 2012, 60: 2229 |
| 24 | Carter L N, Martin C, Withers P J, et al. The influence of the laser scan strategy on grain structure and cracking behaviour in SLM powder-bed fabricated nickel superalloy [J]. J. Alloys Compd., 2014, 615: 338 |
| 25 | Ladewig A, Schlick G, Fisser M, et al. Influence of the shielding gas flow on the removal of process by-products in the selective laser melting process [J]. Addit. Manuf., 2016, 10: 1 |
| 26 | Wang H M. Materials?? fundamental issues of laser additive manufacturing for high-performance large metallic component [J]. Acta Aeronaut. Astronaut. Sin., 2014, 35: 2690 |
| 26 | 王华明. 高性能大型金属构件激光增材制造: 若干材料基础问题 [J]. 航空学报, 2014, 35: 2690 |
| 27 | Tin S, Pollock T M. Stabilization of thermosolutal convective instabilities in Ni-based single-crystal superalloys: Carbide precipitation and rayleigh numbers [J]. Metall. Mater. Trans., 2003, 34A: 1953 |
| 28 | Zhong M L, Sun H Q, Liu W J, et al. Boundary liquation and interface cracking characterization in laser deposition of Inconel 738 on directionally solidified Ni-based superalloy [J]. Scr. Mater., 2005, 53: 159 |
| 29 | Zhang J, Li S, Wei Q S, et al. Cracking behavior and inhibiting process of Inconel 625 alloy formed by selective laser melting [J]. Chin. J. Rare Met., 2015, 39: 961 |
| 29 | 张 洁, 李 帅, 魏青松等. 激光选区熔化Inconel 625合金开裂行为及抑制研究 [J]. 稀有金属, 2015, 39: 961 |
| 30 | ?am G, Ko?ak M. Progress in joining of advanced materials [J]. Int. Mater. Rev., 1998, 43: 1 |
| 31 | Yang J, Huang W D, Chen J, et al. Residual stress on laser rapid forming metal part [J]. Appl. Laser, 2004, 24: 5 |
| 31 | 杨 健, 黄卫东, 陈 静等. 激光快速成形金属零件的残余应力 [J]. 应用激光, 2004, 24: 5 |
/
| 〈 |
|
〉 |