The Arc Physical Characteristics and Molten Pool Dynamic Behaviors in Conduction Plasma Arc Welding
Received date: 2020-07-06
Revised date: 2020-09-11
Online published: 2020-11-16
Supported by
Scientific Research Project of High Technology Ship in Ministry of Industry and Information Technology of China
Conduction plasma arc welding is widely used to weld thin stainless-steel plates in a liquefied natural gas carrier, in which high arc energy density can be achieved through the constraint effects of the constricting nozzle. However, the welding current is relatively low, such that a keyhole is not formed inside the molten pool in conduction plasma arc welding, causing significantly different arc physical characteristics and molten pool dynamic behaviors from those of keyhole plasma arc welding. In this study, a one-way coupled electrode-arc-molten pool model was developed, and spectral analysis, infrared thermography, and particle tracing methods were used to investigate the arc physical characteristics and molten pool dynamic behaviors in conduction plasma arc welding. In conduction plasma arc welding, numerical and experimental results show that plasma impinges on the surface and flows toward the edge of the molten pool. Two contrary convective eddies were found inside the molten pool. The counterclockwise eddy at the center of the molten pool is driven by arc pressure, Marangoni forces, and Lorentz forces, and the clockwise eddy at the rear part of the molten pool is driven by plasma shear stress, Marangoni forces, and buoyancy forces. Additionally, the maximum temperature of the molten pool in conduction plasma arc welding is higher than that in keyhole plasma arc welding due to higher arc energy density and weaker convection.
Zihan LI , Jianwen XIN , Xiao XIAO , Huan WANG , Xueming HUA , Dongsheng WU . The Arc Physical Characteristics and Molten Pool Dynamic Behaviors in Conduction Plasma Arc Welding[J]. Acta Metall Sin, 2021 , 57(5) : 693 -702 . DOI: 10.11900/0412.1961.2020.00237
| 1 | Liu Z M, Cui S L, Luo Z, et al. Plasma arc welding: Process variants and its recent developments of sensing, controlling and modeling [J]. J. Manuf. Process., 2016, 23: 315 |
| 2 | Westhoff R, Szekely J. A model of fluid, heat flow, and electromagnetic phenomena in a nontransferred arc plasma torch [J]. J. Appl. Phys., 1991, 70: 3455 |
| 3 | Yin F L, Hu S S, Zheng Z T, et al. Numerical analysis of arc in plasma arc welding [J]. Trans. China Weld. Inst., 2006, 27(8): 51 |
| 3 | 殷凤良, 胡绳荪, 郑振太等. 等离子弧焊电弧的数值模拟 [J]. 焊接学报, 2006, 27(8): 51 |
| 4 | Lancaster J F. The physics of welding [J]. Phys. Technol., 1984, 15: 73 |
| 5 | Wang X J, Wu C S, Chen M A. Numerical simulation of weld pool keyholing process in stationary plasma arc welding [J]. Acta Metall. Sin., 2010, 46: 984 |
| 5 | 王小杰, 武传松, 陈茂爱. 等离子弧定点焊熔池穿孔过程的数值分析 [J]. 金属学报, 2010, 46: 984 |
| 6 | Xu B, Jiang F, Chen S J, et al. Numerical analysis of plasma arc physical characteristics under additional constraint of keyhole [J]. Chin. Phys., 2018, 27B: 034701 |
| 7 | Wu D S, Tashiro S, Hua X M, et al. Analysis of the energy propagation in the keyhole plasma arc welding using a novel fully coupled plasma arc-keyhole-weld pool model [J]. Int. J. Heat Mass Transf., 2019, 141: 604 |
| 8 | Metcalfe J C, Quigley M B C. Heat transfer in plasma-arc welding [J]. Weld. J., 1975, 54: S99 |
| 9 | Evans D M, Huang D, McClure J C, et al. Arc efficiency of plasma arc welding [J]. Weld. J., 1998, 77: 53S |
| 10 | Tanaka M, Lowke J J. Predictions of weld pool profiles using plasma physics [J]. J. Phys, 2007, 40D: R1 |
| 11 | Arul S, Sellamuthu R. Application of a simplified simulation method to the determination of arc efficiency of gas tungsten arc welding (GTAW) and experimental validation [J]. Int. J. Comput. Mater. Sci. Surf. Eng., 2011, 4: 265 |
| 12 | Van A N, Tashiro S, Van H B, et al. Experimental investigation on the weld pool formation process in plasma keyhole arc welding [J]. J. Phys., 2018, 51D: 015204 |
| 13 | Feng C, Qin G L, Meng X M, et al. Defect evolution of 409L stainless steel in high-speed TIG welding [J]. Mater. Manuf. Process., 2020, 35: 179 |
| 14 | Van A N, Tashiro S, Tanaka M. Undercut formation mechanism in keyhole plasma arc welding [J]. Weld. J., 2019, 98: 202 |
| 15 | Wu C S, Meng X M, Chen J, et al. Progress in numerical simulation of thermal processes and weld pool behaviors in fusion welding [J]. J. Mech. Eng., 2018, 54(2): 1 |
| 15 | 武传松, 孟祥萌, 陈 姬等. 熔焊热过程与熔池行为数值模拟的研究进展 [J]. 机械工程学报, 2018, 54(2): 1 |
| 16 | Wu C S, Wang L, Ren W J, et al. Plasma arc welding: Process, sensing, control and modeling [J]. J. Manuf. Process., 2014, 16: 74 |
| 17 | Song Y L, Li J Y. Thermo-equilibrium in welding arc plasma [J]. Trans. China Weld. Inst., 1994, 15: 138 |
| 17 | 宋永伦, 李俊岳. 焊接电弧等离子体的平衡性质 [J]. 焊接学报, 1994, 15: 138 |
| 18 | Wang A Y, He J P, Wang X X, et al. Distribution characteristics and parameters effects of MPLW arc [J]. Trans. China. Weld. Inst., 2017, 38(8): 77 |
| 18 | 王昂洋, 何建萍, 王晓霞等. 微束等离子弧焊电弧温度场的分布特征及参数影响 [J]. 焊接学报, 2017, 38(8): 77 |
| 19 | Zhang J N, He J P, Wang X X, et al. Multi-field coupling of arc in micro-plasma arc welding [J]. Trans. China. Weld. Inst., 2018, 39(6): 13 |
| 19 | 张济楠, 何建萍, 王晓霞等. 微束等离子弧焊电弧多物理场耦合 [J]. 焊接学报, 2018, 39(6): 13 |
| 20 | Sakai P R, Lima M S F, Fanton L, et al. Comparison of mechanical and microstructural characteristics in maraging 300 steel welded by three different processes: LASER, PLASMA and TIG [J]. Proc. Eng., 2015, 114: 291 |
| 21 | Jian X X, Wu C S, Zhang G K, et al. A unified 3D model for an interaction mechanism of the plasma arc, weld pool and keyhole in plasma arc welding [J]. J. Phys., 2015, 48D: 465504 |
| 22 | Pan J J, Hu S S, Yang L J, et al. Numerical analysis of the heat transfer and material flow during keyhole plasma arc welding using a fully coupled tungsten-plasma-anode model [J]. Acta Mater., 2016, 118: 221 |
| 23 | Li Y, Wang L, Wu C S. Simulation of keyhole plasma arc welding with electro-magneto-thermo-hydrodynamic interactions [J]. Int. J. Adv. Manuf. Technol., 2019, 101: 2497 |
| 24 | Xin J W, Wu D S, Li F, et al. Influence mechanisms of keyhole on the arc characteristics in plasma arc welding [J]. J. Mech. Eng., 2020, 56(20): 82 |
| 24 | 忻建文, 吴东升, 李 芳等. 等离子弧焊匙孔对电弧物理特性影响规律的研究 [J]. 机械工程学报, 2020, 56(20): 82 |
| 25 | Wu D S, Hua X M, Ye D J, et al. Understanding of humping formation and suppression mechanisms using the numerical simulation [J]. Int. J. Heat Mass Transf., 2017, 104: 634 |
| 26 | Li T Q, Wu C S, Chen J. Transient variation of arc heat flux and pressure distribution on keyhole wall in PAW [J]. Weld. World, 2016, 60: 363 |
| 27 | Wu D S, Van A N, Tashiro S, et al. Elucidation of the weld pool convection and keyhole formation mechanism in the keyhole plasma arc welding [J]. Int. J. Heat Mass Transf., 2019, 131: 920 |
| 28 | Huang Y, Li F, Zhang Y L, et al. Spectral analysis of the dynamic behavior of a welding arc during pulsed gas metal arc welding of AA5083 aluminum alloy with ER5183 wire [J]. IEEE Trans. Plasma Sci., 2019, 47: 5078 |
| 29 | Poueyo-Verwaerde A, Dabezies B, Fabbro R. Thermal coupling inside the keyhole during welding process [A]. Proceedings SPIE 2207, Laser Materials Processing: Industrial and Microelectronics Applications [C]. Vienna, Austria: SPIE, 1994: 176 |
| 30 | Mao Z W, Zhong Q F, Zhou S L, et al. Numerical analysis of influence of nozzle diameter on plasma arc welding [J]. Hot Work. Technol., 2016, 45: 200 |
| 30 | 毛志伟, 钟庆飞, 周少玲等. 喷嘴孔径对等离子弧焊影响的数值分析 [J]. 热加工工艺, 2016, 45: 200 |
/
| 〈 |
|
〉 |