Research paper

Influence of Pt-Al Coating on Hot Corrosion Resistance Behaviors of a Ni-Based Single-Crystal Superalloy

  • Di WANG ,
  • Dong WANG ,
  • Guang XIE ,
  • Li WANG ,
  • Jiasheng DONG ,
  • Lijia CHEN
Expand
  • 1.School of Materials Science and Engineering, Shenyang University of Technology, Shenyang 110870, China
    2.Shi -Changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
WANG Di, Tel: (024)23748876, E-mail: diwang@imr.ac.cn

Received date: 2020-07-09

  Revised date: 2020-08-12

  Online published: 2020-09-04

Supported by

National Key Research and Development Program of China(2016YFB0701403);National Science and Technology Major Project(2017-Ⅵ-0019-0091);National Natural Science Foundation of China(51771204)

Abstract

Pt-Al coating has been widely used in engine rotor blades because of its ability to improve the oxidation and hot corrosion resistance of Ni-based superalloys. However, the effect exerted by Pt on S and other refractory elements, as well as the rupture mechanisms, is under debate. To investigate the influence of Pt-Al coating on the corrosion resistance of single-crystal superalloy at high temperature, the hot corrosion test utilized Na2SO4 salt coated on the surface of the Pt-Al coating samples and the uncoated ones were carried out at 900oC, respectively. Using several techniques, such as XRD, SEM, EDS, and EPMA, the influence of Pt-Al coating on the hot corrosion behaviors of a Ni-based single-crystal superalloy was analyzed. Moreover, the hot corrosion kinetics, hot corrosion products, and microstructure evolution during the process were analyzed. The results reveal that the hot corrosion resistance of the substrate alloy was enhanced by Pt-Al coating. The hot corrosion rate of the Pt-Al coating sample was lower than that of the uncoated one. Thus, it can be inferred that Pt-Al coating exhibited better hot corrosion resistance. Pt prevented the diffusion of S into the β-(Ni, Pt)Al phase. The S atom was present at the oxide-metal interface, which reduced the hot corrosion rate of the substrate alloy. The presence of Pt in the β-(Ni, Pt)Al obstructed the great mass of Ta in the inter diffusion zone, which led to the diffusion of only a small quantity of Ta atoms into the oxide, and reduced the formation of Ta2O5. Finally, Pt-Al coating was also found to restrain to some extent the void formation at the oxide-metal interface.

Cite this article

Di WANG , Dong WANG , Guang XIE , Li WANG , Jiasheng DONG , Lijia CHEN . Influence of Pt-Al Coating on Hot Corrosion Resistance Behaviors of a Ni-Based Single-Crystal Superalloy[J]. Acta Metall Sin, 2021 , 57(6) : 780 -790 . DOI: 10.11900/0412.1961.2020.00246

References

1 Swad?ba R, Hetmańczyk M, Wiedermann J, et al. Microstructure degradation of simple, Pt- and Pt + Pd-modified aluminide coatings on CMSX-4 superalloy under cyclic oxidation conditions [J]. Surf. Coat. Technol., 2013, 215: 16
2 Rehman A, Bidabadi M H S, Liang Y, et al. Hot corrosion behaviour of yttrium and aluminium modified wear resistance coating alloy in mixed sulphate at 900oC [J]. Corros. Sci., 2020, 165: 108369
3 Liu Y D, Sun J, Pei Z L, et al. Oxidation and hot corrosion behavior of NiCrAlYSi+NiAl/cBN abrasive coating [J]. Corros. Sci., 2020, 167: 108486
4 Montero X, Ishida A, Mei?ner T M, et al. Effect of surface treatment and crystal orientation on hot corrosion of a Ni-based single-crystal superalloy [J]. Corros. Sci., 2020, 166: 108472
5 Ye L Y, Chen H F, Yang G, et al. Oxidation behavior of Hf-modified platinum aluminide coatings during thermal cycling [J]. Prog. Nat. Sci.: Mater. Int., 2018, 28: 34
6 Jiang C Y, Yang Y F, Zhang Z Y, et al. A Zr-doped single-phase Pt-modified aluminide coating and the enhanced hot corrosion resistance [J]. Corros. Sci., 2018, 133: 406
7 Yang Y F, Liu Z L, Ren P, et al. Hot corrosion behavior of Pt+Hf co-modified NiAl coating in the mixed salt of Na2SO4-NaCl at 900oC [J]. Corros. Sci., 2020, 167: 108527
8 Yang Y F, Jiang C Y, Zhang Z Y, et al. Hot corrosion behaviour of single-phase platinum-modified aluminide coatings: Effect of Pt content and pre-oxidation [J]. Corros. Sci., 2017, 127: 82
9 Li M S. High Temperature Corrosion of Metals [M]. Beijing: Metallurgical Industry Pressure, 2001: 1
9 李美栓. 金属的高温腐蚀 [M]. 北京: 冶金工业出版社, 2001: 1
10 Simms N J, Encinas-Oropesa A, Nicholls J R. Hot corrosion of coated and uncoated single crystal gas turbine materials [J]. Mater. Corros., 2008, 59: 476
11 Goebel J A, Pettit F S. Na2SO4-induced accelerated oxidation (hot corrosion) of nickel [J]. Metall. Trans., 1970, 1: 1943
12 Potgieter J H, Maledi N B. High temperature corrosion resistance of Pt-based superalloys in 0.2% SO2-N2 Gas [J]. Open Mater. Sci. J., 2014, 8: 18
13 Zhang Y, Lee W Y, Haynes J A, et al. Synthesis and cyclic oxidation behavior of a (Ni, Pt)Al coating on a desulfurized Ni-base superalloy [J]. Metall. Mater. Trans., 1999, 30A: 2679
14 Lehnert G, Meinhardt H W. A new protective coating for nickel alloys [J]. Electrodeposit. Surf. Treat., 1973, 1: 189
15 Yu C T, Liu H, Ullah A, et al. High-temperature performance of (Ni, Pt)Al coatings on second-generation Ni-base single-crystal superalloy at 1100oC: Effect of excess S impurities [J]. Corros. Sci., 2019, 159: 108115
16 Das D K. Microstructure and high temperature oxidation behavior of Pt-modified aluminide bond coats on Ni-base superalloys [J]. Prog. Mater. Sci., 2013, 58: 151
17 Wang R L, Gong X Y, Peng H, et al. Interdiffusion behavior between NiAlHf coating and Ni-based single crystal superalloy with different crystal orientations [J]. Appl. Surf. Sci., 2015, 326: 124
18 Chang J X, Wang D, Liu T, et al. Role of tantalum in the hot corrosion of a Ni-base single crystal superalloy [J]. Corros. Sci., 2015, 98: 585
19 Chang J X, Wang D, Zhang G, et al. Interaction of Ta and Cr on Type-I hot corrosion resistance of single crystal Ni-base superalloys [J]. Corros. Sci., 2017, 117: 35
20 Zhu R Z, Zuo Y, Guo M J. An approach to mechanism of internal sulphidation-internal oxidation during hot corrosion of Ni-base alloy [J]. Acta Metall. Sin., 1985, 21: A451
20 朱日彰, 左 禹, 郭曼玖. 镍基高温合金热腐蚀过程中内硫化-内氧化机制的探讨 [J]. 金属学报, 1985, 21: A451
21 Haynes J A, Zhang Y, Lee Y W, et al. Effects of platinum additions and sulfur impurities on the microstructure and scale adhesion behavior of single-phase CVD aluminide bond coatings [A]. Elevated Temperature Coatings: Science and Technology Ⅲ [C]. Warrendale, PA: TMS, 1999: 185
22 Grabkee H J, Kurbatov G, Schmutzler H J. Segregation beneath oxide scales [J]. Oxid. Met., 1995, 43: 97
23 Hou P Y, Priimak K. Interfacial segregation, pore formation, and scale adhesion on NiAl alloys [J]. Oxid. Met., 2005, 63: 113
24 Hou P Y, Izumi T, Gleeson B. Sulfur segregation at Al2O3/γ-Ni+γ'-Ni3Al interfaces: Effects of Pt, Cr and Hf additions [J]. Oxid. Met., 2009, 72: 109
25 Jiang C, Besser M F, Sordelet D J, et al. A combined first-principles and experimental study of the lattice site preference of Pt in B2 NiAl [J]. Acta Mater., 2005, 53: 2101
26 Hou P Y, McCarty K F. Surface and interface segregation in β-NiAl with and without Pt addition [J]. Scr. Mater., 2006, 54: 937
27 Rivoaland L, Maurice V, Josso P, et al. The effect of sulfur segregation on the adherence of the thermally-grown oxide on NiAl—I: Sulfur segregation on the metallic surface of NiAl(001) single-crystals and at NiAl(001)/Al2O3 interfaces [J]. Oxid. Met., 2003, 60: 137
28 Barin I, translated by Cheng N L, Niu S T, Xu G Y, et al. Thermochemical Data of Pure Substances [M]. Beijing: Science Press, 2003: 67
28 Barin I著, 程乃良, 牛四通, 徐桂英等译. 纯物质热化学数据手册 [M]. 北京: 科学出版社, 2003: 67
29 Cadoret Y, Bacos M P, Josso P, et al. Effect of Pt additions on the sulfur segregation, void formation and oxide scale growth of cast nickel aluminides [J]. Mater. Sci. Forum, 2004, 461-464: 247
30 Gururajan M P, Abinandanan T A. Mean field theory of point defects in β-NiAl [J]. Intermetallics, 2000, 8: 759
31 Pint B A, Wright I G, Lee W Y, et al. Substrate and bond coat compositions: Factors affecting alumina scale adhesion [J]. Mater. Sci. Eng., 1998, A245: 201
32 Carling K M, Carter E A. Effects of segregating elements on the adhesive strength and structure of the α-Al2O3/β-NiAl interface [J]. Acta Mater., 2007, 55: 2791
33 Dickey E C, Pint B A, Alexander K B, et al. Oxidation behavior of platinum-aluminum alloys and the effect of Zr doping [J]. J. Mater. Res., 1999, 14: 4531
Outlines

/