Plastic Deformation Behavior and Fracture Mechanism of Rare Earth H13 Steel Based on In Situ TEM Tensile Study
Received date: 2020-05-06
Revised date: 2020-08-26
Online published: 2020-09-01
Supported by
National Key Research and Development Program of China(2016YFB0300900);National Natural Science Foundation of China-Liaoning Joint Fund(U1708251)
Fatigue failure caused by crack propagation is one of the main failure modes of H13 die steel. Because H13 die steel is mainly used under operational conditions involving high-pressure cycling or high friction, its crack initiation and propagation behavior play a critical role in fatigue failure. However, to the best of the authors' knowledge, few reports on the direct observation of deformation and crack propagation behavior of H13 die steel exist, which limits the understanding of the fracture mechanism of H13 die steel. In this work, an in situ TEM tensile study combined with post-mortem EBSD analysis was employed to investigate the microstructure evolution and crack propagation behavior of rare earth (RE) H13 steel. Results indicate that the stress concentration at the grain boundaries and coarse granular inclusions in the tensile specimen were the main sources of crack initiation. After crack initiation and during the tensile process, many cracks converged into the main crack. The main crack propagated along the direction perpendicular to the tensile direction, exhibiting zigzag-shaped features. The stress distribution in the area near a crack in a specimen was heterogeneous; the length fraction of V1/V2 inter-variant boundaries in the relatively high-stress area increased from 56.5% to 58.8% compared with the relatively low-stress area, and the length fraction of V1/V3&V5 inter-variant boundaries increased from 16.3% to 21.6%. The increase in the length fraction of V1/V2 inter-variant boundaries indicated an increase in the twin martensite fraction, which effectively relieved the stress concentration at the grain boundaries and reduced crack initiation. During the tensile process, the austenite retained at the grain boundaries underwent stress-induced phase transformation and was partially transformed into V1/V2 and V1/V3&V5 variant pairs. The dislocation propagation in martensite contributed to dislocation pile-up at high-angle grain boundaries and carbide precipitation. Moreover, the dislocation pile-up at the high-angle grain boundaries promoted the stress-induced phase transformation of the retained austenite.
Jian ZHU , Zhihao ZHANG , Jianxin XIE . Plastic Deformation Behavior and Fracture Mechanism of Rare Earth H13 Steel Based on In Situ TEM Tensile Study[J]. Acta Metall Sin, 2020 , 56(12) : 1592 -1604 . DOI: 10.11900/0412.1961.2020.00141
| [1] | Klob?ar D, Tu?ek J, Taljat B. Thermal fatigue of materials for die-casting tooling [J]. Mater. Sci. Eng., 2008, A472: 198 |
| [2] | Zhou Q C, Wu X C, Shi N N, et al. Microstructure evolution and kinetic analysis of DM hot-work die steels during tempering [J]. Mater. Sci. Eng., 2011, A528: 5696 |
| [3] | Srivastava A, Joshi V, Shivpuri R, et al. A multi-layer coating architecture to reduce heat checking of die surfaces [J]. Surf. Coat. Technol., 2003, 163-164: 631 |
| [4] | Zhang M L, Xing S M, Xin Q, et al. Abnormal failure analysis of H13 punches in steel squeeze casting process [J]. J. Iron Steel Res. Int., 2008, 15: 47 |
| [5] | Sj?str? J, Bergstr?m J. Thermal fatigue in hot-working tools [J]. Scand. J. Metall., 2005, 34: 221 |
| [6] | Delagnes D, Réza?-Aria F, Levaillant C. Influence of testing and tempering temperatures on fatigue behaviour, life and crack initiation mechanisms in a 5%Cr martensitic steel [J]. Procedia Eng., 2010, 2: 427 |
| [7] | Meng C, Zhou H, Tong X, et al. Comparison of thermal fatigue behaviour and microstructure of different hot work tool steels processed by biomimetic couple laser remelting process [J]. Mater. Sci. Technol., 2013, 29: 496 |
| [8] | Oliver E C, Withers P J, Daymond M R, et al. Neutron-diffraction study of stress-induced martensitic transformation in TRIP steel [J]. Appl. Phys., 2002, 74A: S1143 |
| [9] | Frommeyer G, Brüx U, Neumann P. Supra-ductile and high-strength manganese-TRIP/TWIP steels for high energy absorption purposes [J]. ISIJ Int., 2003, 43: 438 |
| [10] | Van Slycken J, Verleysen P, Degrieck J, et al. High-strain-rate behavior of low-alloy multiphase aluminum- and silicon-based transformation-induced plasticity steels [J]. Metall. Mater. Trans., 2006, 37A: 1527 |
| [11] | Dong H, Cao W Q, Shi J, et al. Microstructure and performance control technology of the 3rd generation auto sheet steels [J]. Iron Steel, 2011, 46(6): 1 |
| [11] | (董 瀚, 曹文全, 时 捷等. 第3代汽车钢的组织与性能调控技术 [J]. 钢铁, 2011, 46(6): 1) |
| [12] | Cai Z H, Ding H, Misra R D K, et al. Austenite stability and deformation behavior in a cold-rolled transformation-induced plasticity steel with medium manganese content [J]. Acta Mater., 2015, 84: 229 |
| [13] | Wang R M, Liu J L, Song Y J. Progress and applications of in situ transmission electron microscopy [J]. Physics, 2015, 44: 96 |
| [13] | (王荣明, 刘家龙, 宋源军. 原位透射电子显微学进展及应用 [J]. 物理, 2015, 44: 96) |
| [14] | Mompiou F, Caillard D, Legros M, et al. In situ TEM observations of reverse dislocation motion upon unloading in tensile-deformed UFG aluminium [J]. Acta Mater., 2012, 60: 3402 |
| [15] | Voisin T, Krywopusk N M, Mompiou F, et al. Precipitation strengthening in nanostructured AZ31B magnesium thin films characterized by nano-indentation, STEM/EDS, HRTEM, and in situ TEM tensile testing [J]. Acta Mater., 2017, 138: 174 |
| [16] | Legros M, Gianola D S, Hemker K J. In situ TEM observations of fast grain-boundary motion in stressed nanocrystalline aluminum films [J]. Acta Mater., 2008, 56: 3380 |
| [17] | Manchuraju S, Kroeger A, Somsen C, et al. Pseudoelastic deformation and size effects during in situ transmission electron microscopy tensile testing of NiTi [J]. Acta Mater., 2012, 60: 2770 |
| [18] | Yao T T, Du K, Wang H L, et al. In situ scanning and transmission electron microscopy investigation on plastic deformation in a metastable β titanium alloy [J]. Acta Mater., 2017, 133: 21 |
| [19] | Zárubová N, Gemperlová J, Gemperle A, et al. In situ TEM observation of stress-induced martensitic transformations and twinning processes in CuAlNi single crystals [J]. Acta Mater., 2010, 58: 5109 |
| [20] | Zhong Y, Xiao F R, Zhang J W, et al. In situ TEM study of the effect of M/A films at grain boundaries on crack propagation in an ultra-fine acicular ferrite pipeline steel [J]. Acta Mater., 2006, 54: 435 |
| [21] | Beausir B, Fressengeas C, Gurao N P, et al. Spatial correlation in grain misorientation distribution [J]. Acta Mater., 2009, 57: 5382 |
| [22] | Stormvinter A, Miyamoto G, Furuhara T, et al. Effect of carbon content on variant pairing of martensite in Fe-C alloy [J]. Acta Mater., 2012, 60: 7265 |
| [23] | Takayama N, Miyamoto G, Furuhara T. Effects of transformation temperature on variant pairing of bainitic ferrite in low carbon steel [J]. Acta Mater., 2012, 60: 2387 |
| [24] | Wang X L. Study on welding physical metallurgy behavior of high performance offshore engineering steel [D]. Beijing: University of Science and Technology Beijing, 2018 |
| [24] | (王学林. 高性能海洋工程用钢焊接物理冶金行为研究 [D]. 北京: 北京科技大学, 2018) |
| [25] | Wang X L, Wang Z Q, Dong L L, et al. New insights into the mechanism of cooling rate on the impact toughness of coarse grained heat affected zone from the aspect of variant selection [J]. Mater. Sci. Eng., 2017, A704: 448 |
| [26] | Bachmann F, Hielscher R, Schaeben H. Texture analysis with MTEX-free and open source software toolbox [J]. Solid State Phenom., 2010, 160: 63 |
| [27] | Nyyss?nen T, Peura P, Kuokkala V T. Crystallography, morphology, and martensite transformation of prior austenite in intercritically annealed high-aluminum steel [J]. Metall. Mater. Trans., 2018, 49A: 6426 |
| [28] | Chen Q Z, Chu W Y, Wang B Y, et al. In situ TEM observations of nucleation and bluntness of nano cracks in thin crystals of 310 stainless steel [J]. Acta Metall. Mater., 1995, 43: 4371 |
| [29] | Zhang Y, Chu W Y, Wang Y B, et al. TEM observation of brittle microcrack nucleation of intermetallic compounds [J]. Sci. China, 1994, 24A: 551 |
| [29] | (张 跃, 褚武扬, 王燕斌等. 金属间化合物脆性微裂纹形核的TEM观察 [J]. 中国科学, 1994, 24A: 551) |
| [30] | Gao K W, Chen Q Z, Chu W Y, et al. Nucleation and propagation of microcracks in nanoscale cleavage [J]. Sci. China, 1994, 24A: 993 |
| [30] | (高克玮, 陈奇志, 褚武扬等. 纳米级解理微裂纹的形核和扩展 [J]. 中国科学, 1994, 24A: 993) |
| [31] | Chen Q Z, Chu W Y, Xiao J M. In situ observation and study of nucleation of ductile microcracks [J]. Sci. China, 1994, 24A: 291 |
| [31] | (陈奇志, 褚武扬, 肖纪美. 韧断微裂纹形核的原位观察与研究 [J]. 中国科学, 1994, 24A: 291) |
| [32] | Huang W K, Kong F Y. Microstructure and mechanical property of cold drawn high strength 00Cr18Ni10N stainless steel wire [J]. Acta Metall. Sin., 2009, 45: 275 |
| [32] | (黄文克, 孔凡亚. 冷拔高强00Cr18Ni10N不锈钢丝显微组织与力学性能 [J]. 金属学报, 2009, 45: 275) |
| [33] | Choi H, Lee S, Lee J, et al. Characterization of fracture in medium Mn steel [J]. Mater. Sci. Eng., 2017, A687: 200 |
| [34] | Li H F, Wang S G, Zhang P, et al. Crack propagation mechanisms of AISI 4340 steels with different strength and toughness [J]. Mater. Sci. Eng., 2018, A729: 130 |
| [35] | Lubarda V A, Schneider M S, Kalantar D H, et al. Void growth by dislocation emission [J]. Acta Mater., 2004, 52: 1397 |
| [36] | Li S C, Zhu G M, Kang Y L. Effect of substructure on mechanical properties and fracture behavior of lath martensite in 0.1C-1.1Si-1.7Mn steel [J]. J. Alloys Compd., 2016, 675: 104 |
| [37] | Guo Z, Sha W, Vaumousse D. Microstructural evolution in a PH13-8 stainless steel after ageing [J]. Acta Mater., 2003, 51: 101 |
| [38] | Wang X L, Wang Z Q, Ma X P, et al. Analysis of impact toughness scatter in simulated coarse-grained HAZ of E550 grade offshore engineering steel from the aspect of crystallographic structure [J]. Mater. Charact., 2018, 140: 312 |
| [39] | Morito S, Tanaka H, Konishi R, et al. The morphology and crystallography of lath martensite in Fe-C alloys [J]. Acta Mater., 2003, 51: 1789 |
| [40] | Rancel L, Gómez M, Medina S F, et al. Measurement of bainite packet size and its influence on cleavage fracture in a medium carbon bainitic steel [J]. Mater. Sci. Eng., 2011, A530: 21 |
| [41] | Morito S, Saito H, Ogawa T. Effect of austenite grain size on the morphology and crystallography of lath martensite in low carbon steels [J]. ISIJ Int., 2005, 45: 91 |
| [42] | Morris J W, Lee C S, Guo Z. The nature and consequences of coherent transformations in steel [J]. ISIJ Int., 2003, 43: 410 |
| [43] | Wang J L, Madsen G K H, Drautz R. Grain boundaries in bcc-Fe: A density-functional theory and tight-binding study [J]. Modell. Simul. Mater. Sci. Eng., 2018, 26: 025008 |
| [44] | Lambert-Perlade A, Gourgues A F, Pineau A. Austenite to bainite phase transformation in the heat-affected zone of a high strength low alloy steel [J]. Acta Mater., 2004, 52: 2337 |
| [45] | Wang S H, Li J, Ge X, et al. Microstructural evolution and work hardening behavior of Fe-19Mn alloy containing duplex austenite and ε-martensite [J]. Acta Metall. Sin., 2020, 56: 311 |
| [45] | (王世宏, 李 健, 葛 昕等. γ/ε双相Fe-19Mn合金在拉伸变形过程中的组织演变和加工硬化行为 [J]. 金属学报, 2020, 56: 311) |
/
| 〈 |
|
〉 |