Local Structure-Property Correlation of Fe-Based Amorphous Alloys: Based on Minor Alloying Research
Received date: 2020-04-09
Revised date: 2020-07-08
Online published: 2020-07-31
Supported by
National Key Research and Development Program of China(2016YFB1100103);Natural Science Foundation for Young Scientists of Jiangsu Province(BK20180985);Natural Science Foundation in Higher Education of Jiangsu Province(18KJB430011)
Fe-based amorphous alloys are well known for their excellent soft magnetic and mechanical properties such as high saturation magnetization (Bs), very low coercive force (Hc), high magnetic permeability (μ), low core loss, and high strength, and they are suitable for application as transformer-core materials and have potential applications as structural materials. The minor addition of early transition metal (ETM) such as Zr, Nb, Mo, Hf, Ta, or W can effectively improve the glass-forming abilities, thermal stability, soft magnetic and mechanical properties of Fe-based metallic glasses. The beneficial effects of the minor addition on the glass-forming ability can generally be classified into three aspects: (1) it favors the formation of the unique atomic dense configurations with small free volumes, strong liquid behavior, and high viscosity, which are significantly different from those for conventional metallic glasses; (2) it makes the melts energetically closer to the crystalline state than other metallic melts due to their high packing density in conjunction with a tendency to develop short-range order; (3) it makes the melts more viscous, which leads to slow crystallization kinetics. Despite these advantages, the fundamental theory about the mechanism of the minor addition of ETM in glass formation and properties tailoring is yet to be fully established. In this study, a "cluster plus glue atom" local structure model has been proposed to explore the local structure-property correlation of metallic glasses. The accessibility of calorimetric glass transition (Tg), glass-forming ability, thermal glass stability, and the mechanical properties of metallic glasses are explained in terms of the intra- and inter-atomic cluster correlations in the amorphous structures. Based on the local structure model, the Tg and its composition dependence micro-hardness and strength have been attributed to the inter-cluster correlation, and the enhancement of intra-cluster correlation due to minor alloying would contribute to the enhanced thermal glass stability. The experimental results were verified by alloying the Fe-B-based glassy alloy with Si and alloying the Fe-B-Si-based glassy alloy with ETMs (Zr, Hf, Nb, or Ta) and rare-earth metals (Y, Ce, Pr, Nd, Sm, Gd, or Dy). The experimental results correspond well with theoretical analysis. This study provides a novel understanding of the local structure-property correlation and minor alloying beneficial effects on amorphous alloys.
Yaoxiang GENG , Yingmin WANG . Local Structure-Property Correlation of Fe-Based Amorphous Alloys: Based on Minor Alloying Research[J]. Acta Metall Sin, 2020 , 56(11) : 1558 -1568 . DOI: 10.11900/0412.1961.2020.00112
| [1] | Liu C T, White C L, Horton J A. Effect of boron on grain-boundaries in Ni3Al [J]. Acta Metall., 1985, 33: 213 |
| [2] | Nishizawa T. Thermodynamics of micro-alloying [J]. Mater. Trans., 2001, 42: 2027 |
| [3] | Greer A L. Grain refinement of alloys by inoculation of melts [J]. Phil. Trans. Roy. Soc. Lond., 2003, 361A: 479 |
| [4] | Wang W H. Roles of minor additions in formation and properties of bulk metallic glasses [J]. Prog. Mater. Sci., 2007, 52: 540 |
| [5] | Lu Z P, Liu C T. Role of minor alloying additions in formation of bulk metallic glasses: A review [J]. J. Mater. Sci., 2004, 39: 3965 |
| [6] | Xu D H, Duan G, Johnson W L. Unusual glass-forming ability of bulk amorphous alloys based on ordinary metal copper [J]. Phys. Rev. Lett., 2004, 92: 245504 |
| [7] | Ponnambalam V, Poon S J, Shiflet Gary J. Fe-based bulk metallic glasses with diameter thickness larger than one centimeter [J]. J. Mater. Res., 2004, 19: 1320 |
| [8] | Egami T. Magnetic amorphous alloys: Physics and technological applications [J]. Rep. Prog. Phys., 1984, 47: 1601 |
| [9] | Hasegawa R. Amorphous magnetic materials—A history [J]. J. Magn. Magn. Mater., 1991, 100: 1 |
| [10] | McHenry M E, Willard M A, Laughlin D E. Amorphous and nanocrystalline materials for applications as soft magnets [J]. Prog. Mater. Sci., 1999, 44: 291 |
| [11] | Suryanarayana C, Inoue A. Iron-based bulk metallic glasses [J]. Int. Mater. Rev., 2013, 58: 131 |
| [12] | Sadoc J F, Wagner C N J. Structure of Metallic Glasses [M]. Berlin, Heidelberg, New York, Tokyo: Springer-Verlag, 1983: 78 |
| [13] | Steeb S, Lamparter P. Structure of binary metallic glasses [J]. J. Non-Cryst. Solids, 1993, 156-158: 24 |
| [14] | Hasegawa R, Ray R. Iron-boron metallic glasses [J]. J. Appl. Phys., 1978, 49: 4174 |
| [15] | Sánchez F H, Zhang Y D, Budnick J I. Short-range order in a partially crystallized Fe0.86B0.14 amorphous alloy: A comparison between spin-echo NMR and M?ssbauer-effect studies [J]. Phys. Rev., 1988, 38B: 8508 |
| [16] | Chien C L, Hasegawa R. M?ssbauer study of glassy alloys (Fe-Mo)80B20 [J]. J. Appl. Phys., 1978, 49: 1721 |
| [17] | Polk D E. The structure of glassy metallic alloys [J]. Acta Metall., 1972, 20: 485 |
| [18] | Gu X J, Poon S J, Shiflet G J, et al. Ductility improvement of amorphous steels: Roles of shear modulus and electronic structure [J]. Acta Metall., 2008, 56: 88 |
| [19] | Xia J H, Qiang J B, Wang Y M, et al. Ternary bulk metallic glasses formed by minor alloying of Cu8Zr5 icosahedron [J]. Appl. Phys. Lett., 2006, 88: 101907 |
| [20] | Wang Y M, Wang Q, Zhao J J, et al. Ni-Ta binary bulk metallic glasses [J]. Scr. Mater., 2010, 63: 178 |
| [21] | Yuan L, Pang C, Wang Y M, et al. Understanding the Ni-Nb-Zr BMG composition from a binary eutectic Ni-Nb icosahedral cluster [J]. Intermetallics, 2010, 18: 1800 |
| [22] | Dong C, Wang Q, Qiang J B, et al. From clusters to phase diagrams: Composition rules of quasicrystals and bulk metallic glasses [J]. J. Phys., 2007, 40D: R273 |
| [23] | Wang Z R, Qiang J B, Wang Y M, et al. Composition design procedures of Ti-based bulk metallic glasses using the cluster-plus-glue-atom model [J]. Acta Mater., 2016, 111: 366 |
| [24] | Cheng Y Q, Ma E. Atomic-level structure and structure-property relationship in metallic glasses [J]. Prog. Mater. Sci., 2011, 56: 379 |
| [25] | Sheng H W, Luo W K, Alamgir F M, et al. Atomic packing and short-to-medium-range order in metallic glasses [J]. Nature, 2006, 439: 419 |
| [26] | Stillinger F H. Relaxation and flow mechanisms in "fragile" glass-forming liquids [J]. J. Chem. Phys., 1988, 89: 6461 |
| [27] | Ediger M D. Spatially heterogeneous dynamics in supercooled liquids [J]. Annu. Rev. Phys. Chem., 2000, 51: 99 |
| [28] | Tanaka H. Two-order-parameter model of the liquid-glass transition. II. Structural relaxation and dynamic heterogeneity [J]. J. Non-Cryst. Solids, 2005, 351: 3385 |
| [29] | Geng Y X, Wang Y M, Wang Z R, et al. Formation and structure-property correlation of new bulk Fe-B-Si-Hf metallic glasses [J]. Mater. Des., 2016, 106: 69 |
| [30] | Kelton K F. Crystal nucleation in liquids and glasses [J]. Solid State Phys., 1991, 45: 75 |
| [31] | Spaepen F. A structural model for the solid-liquid interface in monatomic systems [J]. Acta Metall., 1975, 23: 729 |
| [32] | Kauzmann W. The nature of the glassy state and the behavior of liquids at low temperatures [J]. Chem. Rev., 1948, 43: 219 |
| [33] | Schuh C A, Hufnagel T C, Ramamurty U. Mechanical behavior of amorphous alloys [J]. Acta Mater., 2007, 55: 4067 |
| [34] | Gao F M, He J L, Wu E D, et al. Hardness of covalent crystals [J]. Phys. Rev. Lett., 2003, 91: 015502 |
| [35] | Wang W H. The elastic properties, elastic models and elastic perspectives of metallic glasses [J]. Prog. Mater. Sci., 2012, 57: 487 |
| [36] | Gaskell P H. Models for the structure of amorphous metals [A]. Beck H, Güntherodt H J. |
| [36] | Glassy Metal II. Topics in Applied Physics [M]. Berlin, Heidelberg: Springer-Verlag, 1983: 5 |
| [37] | Hasegawa R, Ray R. Iron-boron metallic glasses [J]. J. Appl. Phys., 1978, 49: 4174 |
| [38] | Geng Y X, Wang Y M, Qiang J B, et al. Composition formulas of Fe-B binary amorphous alloys [J]. J. Non-Cryst. Solids, 2016, 432: 453 |
| [39] | Carini J P, Basak S, Nagel S R, et al. The thermoelectric power of the metallic glass Ca0.8Al0.2 [J]. Phys. Lett., 1981, 81A: 525 |
| [40] | de Boer F R, Boom R, Mattens W C M, et al. Cohesion in Metals [M]. Amsterdam: North-Holland Publishing Co., 1989: 217 |
| [41] | Luborsky F E, Reeve J, Davies H A, et al. Effect of Fe-B-Si composition on maximum thickness for casting amorphous metals [J]. IEEE Trans. Magn., 1982, 18: 1385 |
| [42] | Gale W F, Totemeier T C. Smithells Metals Reference Book [M]. Oxford: Butterworth-Heinemann, 1992: 108 |
| [43] | Geng Y X, Wang Y M, Qiang J B, et al. Composition design and optimization of Fe-B-Si-Nb bulk amorphous alloys [J]. Acta Metall. Sin., 2016, 52: 1459 |
| [43] | (耿遥祥, 王英敏, 羌建兵等. Fe-B-Si-Nb块体非晶合金的成分设计与优化 [J]. 金属学报, 2016, 52: 1459) |
| [44] | Geng Y X, Wang Y M, Qiang J B, et al. Fe-B-Si-Zr soft magnetic bulk glassy alloys [J]. Intemetallics, 2015, 67: 138 |
| [45] | Geng Y X, Han K M, Wang Y M, et al. Composition design of Fe-B-Si-Ta bulk amorphous alloys based on cluster + glue atom model [J]. Acta Metall. Sin., 2015, 51: 1017 |
| [45] | (耿遥祥, 韩凯明, 王英敏等. 基于团簇+连接原子模型的Fe-B-Si-Ta块体非晶合金的成分设计 [J]. 金属学报, 2015, 51: 1017) |
| [46] | Chang H W, Huang Y C, Chang C W, et al. Soft magnetic properties and glass formability of Y-Fe-B-M bulk metals (M=Al, Hf, Nb, Ta, and Ti) [J]. J. Alloys Compd., 2009, 472: 166 |
| [47] | Li J W, Estévez D, Jiang K M, et al. Electronic-structure origin of the glass-forming ability and magnetic properties in Fe-RE-B-Nb bulk metallic glasses [J]. J. Alloys Compd., 2014, 617: 332 |
| [48] | Zhang W, Jia X J, Li Y H, et al. Effects of Mo addition on thermal stability and magnetic properties of a ferromagnetic Fe75P10C10B5 metallic glass [J]. J. Appl. Phys., 2014, 115: 17A768 |
| [49] | Lu Z P, Liu C T, Thompson J R, et al. Structural amorphous steels [J]. Phys. Rev. Lett., 2004, 92: 245503 |
| [50] | Gao S F, Qiu J L, Yu P, et al. Fe-based bulk metallic glasses: Brittle or ductile? [J]. Appl. Phys. Lett., 2014, 105: 161901 |
| [51] | Cheung T L, Shek C H. Thermal and mechanical properties of Cu-Zr-Al bulk metallic glasses [J]. J. Alloys Compd., 2007, 434-435: 71 |
| [52] | Duan G, Lind M L, De Blauwe K, et al. Thermal and elastic properties of Cu-Zr-Be bulk metallic glass forming alloys [J]. Appl. Phys. Lett., 2007, 90: 211901 |
| [53] | Zhang T, Men H, Pang S J, et al. Effects of a minor addition of Si and/or Sn on formation and mechanical properties of Cu-Zr-Ti bulk metallic glass [J]. Mater. Sci. Eng., 2007, A449-451: 295 |
| [54] | Li Y H, Zhang W, Dong C, et al. Formation and mechanical properties of Zr-Ni-Al glassy alloys with high glass-forming ability [J]. Intermetallics, 2010, 18: 1851 |
/
| 〈 |
|
〉 |