Microstructure and Wear Resistance of Ni-Based WC Coating by Ultra-High Speed Laser Cladding
Received date: 2020-01-21
Revised date: 2020-06-21
Online published: 2020-07-14
Supported by
National Key Research and Development Program of China(2018YFB2002000);Tianjin Natural Science Foundation(19JCQNJC03800)
Steel materials are highly sourced construction materials owing to their robust mechanical properties, and they are widely used in the construction industry for building bridges, tunnels, skyscrapers, towers, ship-metal parts, and other industrial metal applications. However, as steel has poor surface wear resistance, parts are susceptible to failure due to friction damage. To improve the surface wear resistance of steel materials, Ni-based WC coating was prepared by ultra-high-speed laser cladding. Using low-speed laser cladding as a reference, the surface morphology, microstructure, and wear resistance of ultra-high-speed laser cladding of Ni-based WC coatings were studied using SEM, EDS, and XRD, respectively. Experimental results revealed that the Ni-based WC coating prepared by ultra-high-speed laser cladding exhibited better surface quality compared with that prepared by low-speed laser cladding. Comparatively, ultra-high-speed laser cladding requires a smaller heat input and a faster cooling rate. However, the dilution rate of the coating is significantly reduced. In addition, ultra-high-speed laser cladding significantly reduces thermal damage in the WC coating; it inhibits the precipitation of carbides and formation of porosities and promotes the uniform distribution of the WC in the coating, thereby significantly reducing stress localization in the coating and also inhibits crack nucleation in the coating. Because of the reduction of porosities, cracks, and other surface defects in the coating and uniform distribution of WC particles, the Ni-based WC coating prepared by ultra-high-speed laser cladding possesses better wear resistance than that prepared by low-speed laser cladding, and the wear mechanism is abrasion.
Yu ZHANG , Liyan LOU , Qinglong XU , Yan LI , Changjiu LI , Chengxin LI . Microstructure and Wear Resistance of Ni-Based WC Coating by Ultra-High Speed Laser Cladding[J]. Acta Metall Sin, 2020 , 56(11) : 1530 -1540 . DOI: 10.11900/0412.1961.2020.00033
| [1] | Liu Q, Lin N M, Zou J J, et al. Recent developments in improving tribological behaviors of iron and steel via surface texturing [J]. Surf. Technol., 2016, 45(5): 41 |
| [1] | (刘 强, 林乃明, 邹娇娟等. 改善钢铁材料摩擦学行为的表面织构研究现状 [J]. 表面技术, 2016, 45(5): 41) |
| [2] | Zhang Q. Manual on Wear of Metals and Wear Resistance of Metallic Materials [M]. Beijing: Metallurgical Industry Press, 1991: 22 |
| [2] | (张 清. 金属磨损和金属耐磨材料手册 [M]. 北京: 冶金工业出版社, 1991: 22) |
| [3] | Zhao M H, Liu A G, Guo M H. Research on WC reinforced metal matrix composite [J]. Weld. Joining, 2006, (11): 26 |
| [3] | (赵敏海, 刘爱国, 郭面焕. WC颗粒增强耐磨材料的研究现状 [J]. 焊接, 2006, (11): 26) |
| [4] | Wu P, Zhou C Z, Tang X N. Wear characteristics of Ni-base alloy and Ni/WC coatings by laser cladding [J]. Acta Metall. Sin., 2002, 38: 1257 |
| [4] | (吴 萍, 周昌炽, 唐西南. 激光熔覆镍基合金和Ni/WC涂层的磨损特性 [J]. 金属学报, 2002, 38: 1257) |
| [5] | Wang K M, Lei Y P, Fu H G, et al. Effect of power on microstructure and hardness of laser cladding Ni-based WC coating [J]. Rare Met. Mater. Eng., 2017, 46: 3474 |
| [5] | (王开明, 雷永平, 符寒光等. 功率对激光熔覆Ni基WC涂层组织与硬度的影响 [J]. 稀有金属材料与工程, 2017, 46: 3474) |
| [6] | Rong L, Huang J, Li Z G, et al. Microstructure and property of laser cladding Ni-based alloy coating reinforced by WC particles [J]. China Surf. Eng., 2010, 23(6): 40 |
| [6] | (戎 磊, 黄 坚, 李铸国等. 激光熔覆WC颗粒增强Ni基合金涂层的组织与性能 [J]. 中国表面工程, 2010, 23(6): 40) |
| [7] | Si S H, Yuan X M, Xu K, et al. Effect of laser power on microstructures and wear properties of WCP/Ni metal ceramics coating [J]. J. Chin. Soc. Corros. Prot., 2004, 24: 183 |
| [7] | (斯松华, 袁晓敏, 徐 锟等. 激光功率对激光熔覆WCP/Ni基金属陶瓷涂层的组织与磨损性能的影响 [J]. 中国腐蚀与防护学报, 2004, 24: 183) |
| [8] | Stewart D A, Shipway P H, McCartney D G. Influence of heat treatment on the abrasive wear behaviour of HVOF sprayed WC-Co coatings [J]. Surf. Coat. Technol., 1998, 105: 13 |
| [9] | Shu D, Li Z G, Zhang K, et al. In situ synthesized high volume fraction WC reinforced Ni-based coating by laser cladding [J]. Mater. Lett., 2017, 195: 178 |
| [10] | Liu F R, Gao Q, Gao P D, et al. Cracking analysis of WC reinforced composites coating by laser cladding [J]. J. Mater. Eng., 2003, (5): 37 |
| [10] | (刘富荣, 高 谦, 高登攀等. 激光熔覆WC增强复合涂层开裂行为分析 [J]. 材料工程, 2003, (5): 37) |
| [11] | Ma Q S, Li Y J, Wang J, et al. Investigation on cored-eutectic structure in Ni60/WC composite coatings fabricated by wide-band laser cladding [J]. J. Alloys Compd., 2015, 645: 151 |
| [12] | Leunda J, Sanz C, Soriano C. Laser cladding strategies for producing WC reinforced NiCr coatings inside twin barrels [J]. Surf. Coat. Technol., 2016, 307: 720 |
| [13] | Schopphoven T, Gasser A, Backes G. EHLA: Extreme high-speed laser material deposition [J]. Laser Tech. J., 2017, 14: 45 |
| [14] | Kelbassa I, Gasser A, Meiners W, et al. High speed LAM [A]. International Photonics and Optoelectronics Meetings [C]. Washington: OSA Technical Digest, 2012: 3386 |
| [15] | Li L Q, Shen F M, Zhou Y D, et al. Comparative study of stainless steel AISI 431 coatings prepared by extreme-high-speed and conventional laser cladding [J]. J. Laser Appl., 2019, 31: 042009 |
| [16] | Cui G, Han B, Cui N, et al. Effects of scanning speed on microstructure and properties of laser cladding Ni-based WC alloy coating [J]. China Surf. Eng., 2014, 27(4): 82 |
| [16] | (崔 岗, 韩 彬, 崔 娜等. 扫描速度对激光熔覆Ni基WC合金涂层组织与性能的影响 [J]. 中国表面工程, 2014, 27(4): 82) |
| [17] | Song L J, Zeng G C, Xiao H, et al. Repair of 304 stainless steel by laser cladding with 316L stainless steel powders followed by laser surface alloying with WC powders [J]. J. Manuf. Processes, 2016, 24: 116 |
| [18] | Schopphoven T, Gasser A, Wissenbach K, et al. Investigations on ultra-high-speed laser material deposition as alternative for hard chrome plating and thermal spraying [J]. J. Laser Appl., 2016, 28: 022501 |
| [19] | Li L Q, Shen F M, Zhou Y D, et al. Comparison of microstructure and corrosion resistance of 431 stainless steel coatings prepared by extreme high-speed laser cladding and conventional laser cladding [J]. Chin. J. Laser., 2019, 46: 1002010 |
| [19] | (李俐群, 申发明, 周远东等. 超高速激光熔覆与常规激光熔覆431不锈钢涂层微观组织和耐蚀性的对比 [J]. 中国激光, 2019, 46: 1002010) |
| [20] | Tantai F L, Tian H F, Chen F, et al. Discussion on application of high-speed laser cladding on 27SiMn hydraulic support column [J]. New Technol. New Process, 2019, (3): 52 |
| [20] | (澹台凡亮, 田洪芳, 陈 峰等. 高速激光熔覆在27SiMn液压支架立柱上的应用探讨 [J]. 新技术新工艺, 2019, (3): 52) |
| [21] | Jing Z J, Zhou H, Zhang P, et al. Effect of thermal fatigue on the wear resistance of graphite cast iron with bionic units processed by laser cladding WC [J]. Appl. Surf. Sci., 2013, 271: 329 |
| [22] | Paul C P, Alemohammad H, Toyserkani E, et al. Cladding of WC-12Co on low carbon steel using a pulsed Nd:YAG laser [J]. Mater. Sci. Eng., 2007, A464: 170 |
| [23] | Lee C, Park H, Yoo J, et al. Residual stress and crack initiation in laser clad composite layer with Co-based alloy and WC+NiCr [J]. Appl. Surf. Sci., 2015, 345: 286 |
| [24] | Kadolkar P B, Watkins T R, de Hosson J T M, et al. State of residual stress in laser-deposited ceramic composite coatings on aluminum alloys [J]. Acta Mater., 2007, 55: 1203 |
| [25] | Jendrzejewski R, ?liwiński G, Krawczuk M, et al. Temperature and stress fields induced during laser cladding [J]. Comput. Struct., 2004, 82: 653 |
| [26] | Zhou S F, Zeng X Y, Hu Q W, et al. Analysis of crack behavior for Ni-based WC composite coatings by laser cladding and crack-free realization [J]. Appl. Surf. Sci., 2008, 255: 1646 |
| [27] | Zhou S F, Huang Y J, Zeng X Y. A study of Ni-based WC composite coatings by laser induction hybrid rapid cladding with elliptical spot [J]. Appl. Surf. Sci., 2008, 254: 3110 |
| [28] | LU Y S, Guo C S, Ma T S, et al. Technical Manual of Mechanical Manufacturing Process Materials [M]. Beijing: China Machine Press, 1993: 477 |
| [28] | (陆燕荪, 郭春生, 马铁山等. 机械制造工艺材料技术手册-下册 [M]. 北京: 机械工业出版社, 1993: 477) |
| [29] | Bowie O L. Analysis of an infinite plate containing radial cracks originating at the boundary of an internal circular hole [J]. J. Math. Phys., 1956, 35: 60 |
| [30] | Alam M M, Kaplan A F H, Tuominen J, et al. Analysis of the stress raising action of flaws in laser clad deposits [J]. Mater. Des., 2013, 46: 328 |
| [31] | Shen F M, Tao W, Li L Q, et al. Effect of microstructure on the corrosion resistance of coatings by extreme high speed laser cladding [J]. Appl. Surf. Sci., 2020, 517: 146085 |
| [32] | Chen H H, Xu C Y, Chen J, et al. Microstructure and phase transformation of WC/Ni60B laser cladding coatings during dry sliding wear [J]. Wear, 2008, 264: 487 |
| [33] | Suh N P. An overview of the delamination theory of wear [J]. Wear, 1977, 44: 1 |
| [34] | Suh N P. New theories of wear and their implications for tool materials [J]. Wear, 1980, 62: 1 |
| [35] | Dong X, Jahanmir S, Ives L K. Wear transition diagram for silicon carbide [J]. Tribol. Int., 1995, 28: 559 |
| [36] | Sun N, Shan H Y, Zhou H, et al. Friction and wear behaviors of compacted graphite iron with different biomimetic units fabricated by laser cladding [J]. Appl. Surf. Sci., 2012, 258: 7699 |
| [37] | Wu C F, Ma M X, Liu W J, et al. Study on wear resistance of laser cladding Fe-based composite coatings reinforced by in-situ multiple carbide particles [J]. Acta Metall. Sin., 2009, 45: 1013 |
| [37] | (吴朝锋, 马明星, 刘文今等. 激光原位制备复合碳化物颗粒增强铁基复合涂层及其耐磨性的研究 [J]. 金属学报, 2009, 45: 1013) |
| [38] | Wan M Q, Shi J, Lei L, et al. A comparative study of the microstructure, mechanical properties and corrosion resistance of Ni- or Fe- based composite coatings by laser cladding [J]. J. Mater. Eng. Perform., 2018, 27: 2844 |
| [39] | Zhu S M, Zhang Y D. The microstructure and wear-resistant properties of laser cladding Ni-Based WC alloy on Q345 steel surface [J]. Appl. Mech. Mater., 2014, 556-562: 189 |
| [40] | Wu X W, Zeng X Y, Zhu B D, et al. Heat damage of laser clad Ni-based WC coating [J]. Acta Metall. Sin., 1997, 33: 1282 |
| [40] | (吴新伟, 曾晓雁, 朱蓓蒂等. 镍基WC金属陶瓷激光熔覆涂层的熔化烧损规律 [J]. 金属学报, 1997, 33: 1282) |
/
| 〈 |
|
〉 |