Phase-Field Simulation of the Interaction Between Pore and Grain Boundary

  • Zhengyang SUN ,
  • Yutian WANG ,
  • Wenbo LIU
Expand
  • 1 School of Nuclear Science and Technology, Xi'an Jiaotong University, Xi'an 710049, China
    2 Shaanxi Key Laboratory of Advanced Nuclear Energy and Technology, Shaanxi Engineering Research Center of Advanced Nuclear Energy, Xi'an Jiaotong University, Xi'an 710049, China
    3 School of Mechanical Engineering, Xi'an Jiaotong University, Xi'an 710049, China

Received date: 2020-04-16

  Revised date: 2020-06-04

  Online published: 2020-06-10

Supported by

NSAF Joint Fund(U1830124);National Natural Science Foundation of China(11705137);China Postdoctoral Science Foundation(2019M663738);State Key Laboratory of New Ceramic and Fine Processing Tsinghua University(KF201713)

Abstract

The grain boundary (GB) and average grain size considerably affect the properties of materials, such as the fracture strength, dielectric constant, and thermal conductivity. For instance, when subjected to irradiation at 1750 ℃, the swelling of the UO2 pellets and the release of fission gas from them decrease significantly with the increasing average grain size. However, several second-phase particles, such as pores, are inevitably introduced into a material during the solid-phase sintering or neutron radiation processes. Therefore, studying the interaction between the pores and GBs is considerably important. In this study, a phase-field model of the interaction between the pores and GBs is developed. Subsequently, the free-energy density function was modified, where the diffusion coefficient was incorporated in the tensor form. In addition, the selection of the phenomenological parameters, such as the coefficient in the free-energy density function of the phase-field model, was analyzed, and the influencing factors of interface energy and interface width were discussed. The phase-field model simulation results of the interaction between the pores and GBs show that the curvature of GB was the major driving force associated with the movement of GB and that pores resisted the movement of GB. Accordingly, the pores moved together with the GBs when the maximum pinning force exerted by the pores was larger than the driving force produced by the curvature of GB; however, the pores and GBs separated in the opposite case, during which the GB moved much faster than pores. The results of the phase-field simulation of the grain growth of the pore-containing UO2 show that the grain growth speed decreases with the increasing porosity. The average grain size of UO2 is a power function of time, the exponent of which increases with the increasing porosity.

Cite this article

Zhengyang SUN , Yutian WANG , Wenbo LIU . Phase-Field Simulation of the Interaction Between Pore and Grain Boundary[J]. Acta Metall Sin, 2020 , 56(12) : 1643 -1653 . DOI: 10.11900/0412.1961.2020.00120

References

[1] Rahaman M N. Ceramic Processing and Sintering [M]. New York: Marcel Dekker, 1995: 540
[2] Turnbull J A. The effect of grain size on the swelling and gas release properties of UO2 during irradiation [J]. J. Nucl. Mater., 1974, 50: 62
[3] Ahmed K, Tonks M, Zhang Y F, et al. Particle-grain boundary interactions: A phase field study [J]. Comput. Mater. Sci., 2017, 134: 25
[4] Zhao Y, Zhang H Y, Wei H, et al. A phase field study for scaling rules of grain coarsening in polycrystalline system containing second-phase particles [J]. Acta Metall. Sin., 2013, 49: 981
[4] (赵 彦, 张洪宇, 韦 华等. 相场法研究含第二相颗粒多晶体系的晶粒粗化标度律 [J]. 金属学报, 2013, 49: 981)
[5] Zhou G Z, Wang Y X, Chen Z. Phase-field method simulation of the effect of hard particles with different shapes on two-phase grain growth [J]. Acta Metall. Sin., 2012, 48: 227
[5] (周广钊, 王永欣, 陈 铮. 相场法模拟不同形状的硬质颗粒对两相晶粒长大的影响 [J]. 金属学报, 2012, 48: 227)
[6] Gao Y J, Zhang H L, Jin X, et al. Phase-field simulation of two-phase grain growth with hard particles [J]. Acta Metall. Sin., 2009, 45: 1190
[6] (高英俊, 张海林, 金 星等. 相场方法研究硬质颗粒钉扎的两相晶粒长大过程 [J]. 金属学报, 2009, 45: 1190)
[7] Ahmed K, Yablinsky C A, Schulte A, et al. Phase field modeling of the effect of porosity on grain growth kinetics in polycrystalline ceramics [J]. Model. Simul. Mater. Sci. Eng., 2013, 21: 065005
[8] Moelans N, Blanpain B, Wollants P. Pinning effect of second-phase particles on grain growth in polycrystalline films studied by 3-D phase field simulations [J]. Acta Mater., 2007, 55: 2173
[9] Moelans N, Blanpain B, Wollants P. A phase field model for the simulation of grain growth in materials containing finely dispersed incoherent second-phase particles [J]. Acta Mater., 2005, 53: 1771
[10] Chang K, Feng W M, Chen L Q. Effect of second-phase particle morphology on grain growth kinetics [J]. Acta Mater., 2009, 57: 5229
[11] H?tzer J, Rehn V, Rheinheimer W, et al. Phase-field study of pore-grain boundary interaction [J]. J. Ceram. Soc. Jpn., 2016, 124: 329
[12] Kundin J, Sohaib H, Schiedung R, et al. Phase-field modelling of pores and precipitates in polycrystalline systems [J]. Model. Simul. Mater. Sci. Eng., 2018, 26: 065003
[13] Nichols F A. Theory of grain growth in porous compacts [J]. J. Appl. Phys., 1966, 37: 4599
[14] Brook R J. Pore-grain boundary interactions and grain growth [J]. J. Am. Ceram. Soc., 1969, 52: 56
[15] Riedel H, Svoboda J. A theoretical study of grain growth in porous solids during sintering [J]. Acta Metall. Mater., 1993, 41: 1929
[16] Petrishcheva E, Renner J. Two-dimensional analysis of pore drag and drop [J]. Acta Mater., 2005, 53: 2793
[17] Klinger L, Rabkin E, Shvindlerman L S, et al. Grain growth in porous two-dimensional nanocrystalline materials [J]. J. Mater. Sci., 2008, 43: 5068
[18] Fan D, Chen L Q. Computer simulation of grain growth using a continuum field model [J]. Acta Mater., 1997, 45: 611
[19] Moelans N, Blanpain B, Wollants P. An introduction to phase-field modeling of microstructure evolution [J]. Calphad, 2008, 32: 268
[20] Krivilyov M D, Mesarovic S D, Sekulic D P. Phase-field model of interface migration and powder consolidation in additive manufacturing of metals [J]. J. Mater. Sci., 2017, 52: 4155
[21] Lin M Z, Zhang R J, Fang W, et al. Phase field simulation of sintering process in biphasic porous material [J]. Acta Metall. Sin., 2012, 48: 1207
[21] (刘明治, 张瑞杰, 方 伟等. 相场法模拟两相多孔组织烧结 [J]. 金属学报, 2012, 48: 1207)
[22] Chen Y, Kang X H, Xiao N M, et al. Phase field modelling of grain growth in polycrystalline material [J]. Acta Phys. Sin., 2009, 58: 124
[22] (陈 云, 康秀红, 肖纳敏等. 多晶材料晶粒生长粗化过程的相场方法模拟 [J]. 物理学报, 2009, 58: 124)
[23] Jing X N, Ni Y, He L H, et al. 2-D phase-field simulation of pore evolution in sintering ceramics [J]. J. Inorg. Mater., 2002, 17: 1078
[23] (景晓宁, 倪 勇, 何陵辉等. 陶瓷烧结过程孔隙演化的二维相场模拟 [J]. 无机材料学报, 2002, 17: 1078)
[24] Deng J. A phase field model of sintering with direction-dependent diffusion [J]. Mater. Trans., 2012, 53: 385
[25] Sun Z Y, Yang C, Liu W B. Phase-field simulations of the sintering process of uranium dioxide [J]. Acta Metall. Sin., 2020, 56: 1295
[25] (孙正阳, 杨 超, 柳文波. UO2烧结过程的相场模拟 [J]. 金属学报, 2020, 56: 1295)
[26] Lu D, Jiang P, Xu Z Z. Solid State Physics [M]. 2nd Ed., Shanghai: Shanghai Scientific and Technical Publishers, 2010: 364
[26] (陆 栋, 蒋 平, 徐至中. 固体物理学 [M]. 第2版. 上海: 上海科学技术出版社, 2010: 364)
[27] Chen L Q, Fan D N. Computer simulation model for coupled grain growth and Ostwald ripening—Application to Al2O3-ZrO2 two-phase systems [J]. J. Am. Ceram. Soc., 1996, 79: 1163
[28] Cahn J W. On spinodal decomposition [J]. Acta Metall., 1961, 9: 795
[29] Moelans N, Blanpain B, Wollants P. Quantitative analysis of grain boundary properties in a generalized phase field model for grain growth in anisotropic systems [J]. Phys. Rev., 2008, 78B: 024113
[30] Hsueh C H, Evans A G, Coble R L. Microstructure development during final/intermediate stage sintering—I. Pore/grain boundary separation [J]. Acta Metall., 1982, 30: 1269
[31] Ahmed K, Allen T, El-Azab A. Phase field modeling for grain growth in porous solids [J]. J. Mater. Sci., 2016, 51: 1261
[32] Ahmed K, Pakarinen J, Allen T, et al. Phase field simulation of grain growth in porous uranium dioxide [J]. J. Nucl. Mater., 2014, 446: 90
Outlines

/