First-Principles Study on Free Energy and Elastic Properties of Disordered β-Ti1-xNbx Alloy: Comparison Between SQS and CPA
Received date: 2020-01-10
Revised date: 2020-02-24
Online published: 2020-04-28
Supported by
National Key Research and Development Program of China(2016YFB0701301);National Natural Science Foundation of China(91860107);National Basic Research Program of China(2014CB644001)
Elastic modulus is one of the key properties for the application of biomedical β titanium alloy as human bone replacement because the elastic modulus of the alloy has to match that of the bone so as to avoid the stress shielding effect. Alloying of Nb is commonly used in biomedical β titanium alloys. In the present work, the lattice parameter, free energy and elastic modulus of β-Ti1-xNbx alloy were investigated by using first-principles method based on density functional theory. The random distribution of Nb atoms in the alloy were described by using both special quasirandom structure (SQS) and the coherent potential approximation (CPA) techniques, in combination with first principles plane-wave pseudopotential (VASP) and exact muffin-tin orbital (EMTO) methods, respectively. The results showed that the lattice constants from both VASP-SQS and EMTO-CPA calculations increase linearly with Nb content x, while the influence of the local lattice distortion is negligible. The calculations of the free energies demonstrated that EMTO-CPA predicts reasonably the phase decomposition of β-Ti1-xNbx at relatively low temperature whereas VASP-SQS does not, which might be ascribed to the fact that the free energy depends strongly on the detailed SQS structures. The elastic constants C11 and C12 calculated by using EMTO-CPA and VASP-SQS without atomic relaxation increase with Nb content whereas C44 decreases. EMTO-CPA overestimates the elastic stability of β-Ti1-xNbx. At low Nb content, the local lattice distortion is abnormally large due to the lattice instability of the β-Ti1-xNbx, making the free energy and elastic constant against x from VASP-SQS calculations with atomic relaxation deviate significantly from the general trend.
Haijun ZHANG , Shi QIU , Zhimei SUN , Qingmiao HU , Rui YANG . First-Principles Study on Free Energy and Elastic Properties of Disordered β-Ti1-xNbx Alloy: Comparison Between SQS and CPA[J]. Acta Metall Sin, 2020 , 56(9) : 1304 -1312 . DOI: 10.11900/0412.1961.2020.00015
| [1] | Brunette D M, Tengvall P, Textor M, et al. Titanium in Medicine: Material Science, Surface Science, Engineering, Biological Responses and Medical Applications [M]. Berlin: Springer, 2001: 703 |
| [2] | Woodman J L, Jacobs J J, Galante J O, et al. Metal ion release from titanium-based prosthetic segmental replacements of long bones in baboons: A long-term study [J]. J. Orthop. Res., 1984, 1: 421 |
| [3] | Mohammadi S, Wictorin L, Ericson L E, et al. Cast titanium as implant material [J]. J. Mater. Sci.: Mater. Med., 1995, 6: 435 |
| [4] | Semlitsch M F, Weber H, Streicher R M, et al. Joint replacement components made of hot-forged and surface-treated Ti-6A1-7Nb alloy [J]. Biomaterials, 1992, 13: 781 |
| [5] | Bordji K, Jouzeau J Y, Mainard D, et al. Cytocompatibility of Ti-6A1-4V and Ti-5Al-2.5Fe alloys according to three surface treatments, using human fibroblasts and osteoblasts [J]. Biomaterials, 1996, 17: 929 |
| [6] | Yumoto S, Ohashi H, Nagai H, et al. Aluminum neurotoxicity in the rat brain [J]. Int. J. PIXE, 1992, 2: 493 |
| [7] | Rao S, Ushida T, Tateishi T, et al. Effect of Ti, Al, and V ions on the relative growth rate of fibroblasts (L929) and osteoblasts (MC3T3-E1) cells [J]. Biomed. Mater. Eng., 1996, 6: 79 |
| [8] | Walker P R, LeBlanc J, Sikorska M. Effects of aluminum and other cations on the structure of brain and liver chromatin [J]. Biochemistry, 1989, 28: 3911 |
| [9] | Sarkar B. Biological Aspects of Metals and Metal-Related Diseases [M]. New York: Raven Press, 1983: 209 |
| [10] | Sumner D R, Galante J O. Determinants of stress shielding: Design versus materials versus interface [J]. Clin. Orthop. Relat. Res., 1992, 274: 202 |
| [11] | Engh C A, Bobyn J D. The influence of stem size and extent of porous coating on femoral bone resorption after primary cementless hip arthroplasty [J]. Clin. Orthop. Relat. Res., 1988, 231: 7 |
| [12] | Wang K. The use of titanium for medical applications in the USA [J]. Mater. Sci. Eng., 1996, A213: 134 |
| [13] | Huiskes R, Weinans H, Van Rietbergen B. The relationship between stress shielding and bone resorption around total hip stems and the effects of flexible materials [J]. Clin. Orthop. Relat. Res., 1992, 274: 124 |
| [14] | Khan M A, Williams R L, Williams D M. In-vitro corrosion and wear of titanium alloys in the biological environment [J]. Biomaterials, 1996, 17: 2117 |
| [15] | Kuroda D, Niinomi M, Morinaga M, et al. Design and mechanical properties of new β type titanium alloys for implant materials [J]. Mater. Sci. Eng., 1998, A243: 244 |
| [16] | Tane M, Akita S, Nakano T, et al. Peculiar elastic behavior of Ti-Nb-Ta-Zr single crystals [J]. Acta Mater., 2008, 56: 2586 |
| [17] | Zhang M H, Yu Z T, Zhou L, et al. Biocompatibility evaluation of β-type titanium alloys [J]. Rare Met. Mater. Eng., 2007, 36: 1815 |
| [17] | (张明华, 于振涛, 周 廉等. β型钛合金材料的生物相容性评价 [J]. 稀有金属材料与工程, 2007, 36: 1815) |
| [18] | Song Y, Xu D S, Yang R, et al. Theoretical study of the effects of alloying elements on the strength and modulus of β-type bio-titanium alloys [J]. Mater. Sci. Eng., 1999, A260: 269. |
| [19] | Sun J, Yao Q, Xing H, et al. Elastic properties of β, α'' and ω metastable phases in Ti-Nb alloy from first-principles [J]. J. Phys. Condens. Matter, 2007, 19: 486215 |
| [20] | Ikehata H, Nagasako N, Furuta T, et al. First-principles calculations for development of low elastic modulus Ti alloys [J]. Phys. Rev., 2004, 70B: 174113 |
| [21] | Gutiérrez Moreno J J, Papageorgiou D G, Evangelakis G A, et al. An abinitio study of the structural and mechanical alterations of Ti-Nb alloys [J]. J. Appl. Phys., 2018, 124: 245102 |
| [22] | Gutiérrez Moreno J J, Bonisch M, Panagiotopoulos N T, et al. Ab-initio and experimental study of phase stability of Ti-Nb alloys [J]. J. Alloys Compd., 2017, 696: 481 |
| [23] | Dai J H, Song Y, Li W, et al. Influence of alloying elements Nb, Zr, Sn, and oxygen on structural stability and elastic properties of the Ti2448 alloy [J]. Phys. Rev., 2014, 89B: 014103 |
| [24] | Zhou W C, Sahara R, Tsuchiya K. First-principles study of the phase stability and elastic properties of Ti-X alloys (X=Mo, Nb, Al, Sn, Zr, Fe, Co, and O) [J]. J. Alloys Compd., 2017, 727: 579 |
| [25] | Zunger A, Wei S H, Ferreira L G, et al. Special quasirandom structures [J]. Phys. Rev. Lett., 1990, 65: 353 |
| [26] | Wei S H, Ferreira L G, Bernard J E, alel. Electronic properties of random alloys: Special quasirandom structures [J]. Phys. Rev., 1990, 42B: 9622 |
| [27] | Soven P. Coherent-potential model of substitutional disordered alloys [J]. Phys. Rev., 1967, 156: 809 |
| [28] | Gyorffy B L. Coherent-potential approximation for a nonoverlapping-muffin-tin-potential model of random substitutional alloys [J]. Phys. Rev., 1972, 5B: 2382 |
| [29] | Zhang S Z, Cui H, Li M M, et al. First-principles study of phase stability and elastic properties of binary Ti-xTM (TM=V, Cr, Nb, Mo) and ternary Ti-15TM-yAl alloys [J]. Mater. Des., 2016, 110: 80 |
| [30] | Hu Q M, Li S J, Hao Y L, et al. Phase stability and elastic modulus of Ti alloys containing Nb, Zr, and/or Sn from first-principles calculations [J]. Appl. Phys. Lett., 2008, 93: 121902 |
| [31] | Zhao Y F, Fu Y C, Hu Q M, et al. First-principles investigations of lattice parameters, bulk moduli and phase stabilities of Ti1-xVxand Ti1-xNbx alloys [J]. Acta Metall. Sin., 2009, 45: 1042 |
| [31] | (赵宇飞, 符跃春, 胡青苗等. Ti1-xVx及Ti1-xNbx合金晶格参数、体模量及相稳定性的第一原理研究 [J]. 金属学报, 2009, 45: 1042) |
| [32] | Vitos L. Computational Quantum Mechanics for Materials Engineers: The EMTO Method and Applications [M]. London: Springer, 2007: 247 |
| [33] | Perdew J P, Burke K, Ernzerhof M. Generalized gradient approximation made simple [J]. Phys. Rev. Lett., 1996, 77: 3865 |
| [34] | Girifalco L A, Weizer V G. Application of the Morse potential function to cubic metals [J]. Phys. Rev., 1959, 114: 687 |
| [35] | Kresse G, Hafner J. Ab initio molecular dynamics for liquid metals [J]. Phys. Rev., 1993, 47B: 558 |
| [36] | Kresse G, Furthmüller J. Efficient iterative schemes for ab initio total-energy calculations using a plane-wave basis set [J]. Phys. Rev., 1996, 54B: 11169 |
| [37] | Kresse G, Furthmüller J. Efficiency of ab-initio total energy calculations for metals and semiconductors using a plane-wave basis set [J]. Comput. Mater. Sci., 1996, 6: 15 |
| [38] | Bl?chl P E. Projector augmented-wave method [J]. Phys. Rev., 1994, 50B: 17953 |
| [39] | Van de Walle A, Tiwary P, De Jong M, et al. Efficient stochastic generation of special quasirandom structures [J]. Calphad, 2013, 42: 13 |
| [40] | Birch F. Finite elastic strain of cubic crystals [J]. Phys. Rev., 1947, 71: 809 |
| [41] | Von Pezold J, Dick A, Friák M, et al. Generation and performance of special quasirandom structures for studying the elastic properties of random alloys: Application to Al-Ti [J]. Phys. Rev., 2010, 81: 094203 |
| [42] | Tasnádi F, Odén M, Abrikosov I A. Ab initio elastic tensor of cubic Ti0.5Al0.5N alloys: Dependence of elastic constants on size and shape of the supercell model and their convergence [J]. Phys. Rev., 2012, 85B: 144112 |
| [43] | Holec D, Tasnádi F, Wagner P, et al. Macroscopic elastic properties of textured ZrN-AlN polycrystalline aggregates: From ab initio calculations to grain-scale interactions [J]. Phys. Rev., 2014, 90B: 184106 |
| [44] | Hariharan Y, Janawadkar M P, Radhakrishnan T S, et al. Structure property correlations in superconducting Ti-Nb alloys [J]. Pramana, 1986, 26: 513 |
| [45] | Kim H Y, Ikehara Y, Kim J I, et al. Martensitic transformation, shape memory effect and superelasticity of Ti-Nb binary alloys [J]. Acta Mater., 2006, 54: 2419 |
| [46] | Dobromyslov A V, Elkin V A. Martensitic transformation and metastable β-phase in binary titanium alloys with d-metals of 4-6 periods [J]. Scr. Mater., 2001, 44: 905 |
| [47] | Tian L Y, Hu Q M, Yang R, et al. Elastic constants of random solid solutions by SQS and CPA approaches: The case of fcc Ti-Al [J]. J. Phys. Condens. Matter, 2015, 27: 315702 |
| [48] | Tian L Y, Ye L H, Hu Q M, et al. CPA descriptions of random Cu-Au alloys in comparison with SQS approach [J]. Comput. Mater. Sci., 2017, 128: 302 |
| [49] | Ye L H, Wang H, Zhou G, et al. Phase stability of TiAl-X (X=V, Nb, Ta, Cr, Mo, W, and Mn) alloys [J]. J. Alloys Compd., 2020, 819: 153291 |
| [50] | Hao Y L, Wang H L, Li T, et al. Superelasticity and tunable thermal expansion across a wide temperature range [J]. J. Mater. Sci. Technol., 2016, 32: 705 |
| [51] | Wang H L, Hao Y L, He S Y, et al. Elastically confined martensitic transformation at the nano-scale in a multifunctional titanium alloy [J]. Acta Mater., 2017, 135: 330 |
| [52] | Reid C N, Routbort J L, Maynard R A. Elastic constants of Ti-40at.% Nb at 298 °K [J]. J. Appl. Phys., 1973, 44: 1398 |
| [53] | Hermann R, Hermann H, Calin M, et al. Elastic constants of single crystalline β-Ti70Nb30 [J]. Scr. Mater., 2012, 66: 198 |
| [54] | Jeong H W, Yoo Y S, Lee Y T, et al. Elastic softening behavior of Ti-Nb single crystal near martensitic transformation temperature [J]. J. Appl. Phys., 2010, 108: 063515 |
| [55] | Born M. On the stability of crystal lattices. I [J]. Math. Proc. Cambridge Philos. Soc., 1940, 36: 160 |
/
| 〈 |
|
〉 |