Mechanisms of Interfacial Reaction and Matrix Phase Transition in SiCf /Ti65 Composites
Received date: 2020-01-17
Revised date: 2020-03-05
Online published: 2020-04-22
Continuous silicon carbide (SiC) ?ber-reinforced titanium metal-matrix composites (TMCs) are potential candidates for high temperature application in jet engines because of their high specific strength and stiffness. However, severe interfacial reactions caused by high temperature manufacture and service have a detrimental effect on the mechanical properties of composites. Furthermore, the phase transition occurred in matrix at elevated temperature is unfavorable to the properties. In this work, the interfacial reaction, matrix phase transformation and thermal stability of SiCf /Ti65 composites were investigated. The composites were prepared by the combination of magnetron sputtering and hot isostatic pressing (HIP) method. Matrix-coated precursor wires prepared by sputtering were aligned, degased and encapsulated, then consolidated by HIP. And the densified composites were subjected to long-term thermal exposure at 650, 750, 800 and 900 ℃, respectively. Reaction products and element diffusion of SiCf /Ti65 composites in different conditions were studied. The results show that the elements diffuse and participate in both interfacial reaction and matrix phase transition during HIP and thermal exposure process. In the as-processed SiCf /Ti65 composites, TiC is the main product of interfacial reaction layer, and (Zr, Nb)5Si4 is the product of matrix phase transition. With the continuous consumption of C-coating layer in the process of thermal exposure, Ti5Si3 and (Zr, Nb)5Si4 form in the interfacial reaction layer, while Ti3(Al, Sn)C and TiC precipitate in the matrix. The results of thermal stability study indicate a parabolic correlation between interfacial reaction layer thickness and exposure time, and the activation energy of reaction layer growth estimated by Arrhenius equation is 93 kJ/mol. The interface of SiCf /Ti65 composites is stable below 650 ℃.
Chao WANG , Xu ZHANG , Yumin WANG , Qing YANG , Lina YANG , Guoxing ZHANG , Ying WU , Xu KONG , Rui YANG . Mechanisms of Interfacial Reaction and Matrix Phase Transition in SiCf /Ti65 Composites[J]. Acta Metall Sin, 2020 , 56(9) : 1275 -1285 . DOI: 10.11900/0412.1961.2020.00027
| [1] | Fan Z, Guo Z X, Cantor B. The kinetics and mechanism of interfacial reaction in sigma fibre-reinforced Ti MMCs [J]. Composites, 1997, 28A: 131 |
| [2] | Zhao G M, Yang Y Q, Zhang W, et al. Microstructure and grain growth of the matrix of SiCf/Ti-6Al-4V composites prepared by the consolidation of matrix-coated fibers in the β phase field [J]. Composites, 2013, 52B: 155 |
| [3] | Wang Y M, Zhang G X, Zhang X, et al. Advances in SiC fiber reinforced titanium matrix composites [J]. Acta Metall. Sin., 2016, 52: 1153 |
| [3] | (王玉敏, 张国兴, 张 旭等. 连续SiC纤维增强钛基复合材料研究进展 [J]. 金属学报, 2016, 52: 1153) |
| [4] | Baik K H, Grant P S. Chemical interaction between sigma 1140+ SiC fibre and Ti-6Al-4V [J]. Scr. Mater., 2001, 44: 607 |
| [5] | Yang Y Q, Ma Z J, Lü X H, et al. Studies on interface of SiCf /Ti-6Al-4V composites [J]. Rare Met. Mater. Eng., 2006, 35: 1516 |
| [6] | Boehlert C J, Majumdar B S, Krishnamurthy S, et al. Role of matrix microstructure on room-temperature tensile properties and fiber-strength utilization of an orthorhombic Ti-alloy-based composite [J]. Metall. Mater. Trans., 1997, 28A: 309 |
| [7] | Gundel D B, Miracle D B. The influence of interface structure and composition on the response of single-fiber SiC/Ti-6Al-4V composites to transverse tension [J]. Appl. Compos. Mater., 1998, 5: 95 |
| [8] | Xiao P. Study on interfacial property and residual stress of SiC fiber reinforced Ti-22Al-26Nb composites [D]. Graduate School of Chinese Academy of Science, 2010 |
| [8] | (肖 鹏. SiC纤维增强Ti-22Al-26Nb基复合材料的界面性能及残余应力研究 [D]. 中国科学院研究生院, 2010) |
| [9] | Zhang G X, Kang Q, Shi N L, et al. Kinetics and mechanism of interfacial reaction in a SiCf/Ti composite [J]. J. Mater. Sci. Technol., 2003, 19: 407 |
| [10] | Lü X H, Yang Y Q, Huang B, et al. Reaction diffusion in continuous SiC fiber reinforced Ti matrix composite [J]. Trans. Nonferrous Met. Soc. China, 2007, 17: 27 |
| [11] | Sandhu S, Tsakiropoulos P, Wood M J, et al. Interfacial studies in titanium aluminide/SiCf composites [J]. Key Eng. Mater., 1997, 127-131: 671 |
| [12] | Zhang S M, Wang M J, Wen M, et al. Interfacial reactions and matrix microstructure evolution in SiCf/Ti composites dominated by primary structure of Ti matrix [J]. Ceram. Int., 2019, 45: 17767 |
| [13] | Yang Y Q, Lu X H, Luo X, et al. Kinetics of interfacial reaction in SiCf/Ti6Al4V composites [J]. Mater. Sci. Forum, 2007, 546-549: 1627 |
| [14] | Naka M, Feng J C, Schuster J C. Phase reaction and diffusion path of the SiC/Ti system [J]. Metall. Mater. Trans., 1997, 28A: 1385 |
| [15] | Yue K, Liu J R, Zhang H J, et al. Precipitates and alloying elements distribution in near α titanium alloy Ti65 [J]. J. Mater. Sci. Technol., 2020, 36: 91 |
| [16] | Wang Q J, Liu J R, Yang R. High temperature titanium alloys: Status and perspective [J]. J. Aerona. Mater., 2014, 34(4): 1 |
| [16] | (王清江, 刘建荣, 杨 锐. 高温钛合金的现状与前景 [J]. 航空材料学报, 2014, 34(4): 1) |
| [17] | Subramanian P R, Krishnamurthy S, Keller S T, et al. Processing of continuously reinforced Ti-alloy metal matrix composites (MMC) by magnetron sputtering [J]. Mater. Sci. Eng., 1998, A244: 1 |
| [18] | Martineau P, Lahaye M, Pailler R, et al. SiC filament/titanium matrix composites regarded as model composites: Part 1 Filament microanalysis and strength characterization [J]. J. Mater. Sci., 1984, 19: 2731 |
| [19] | Wu M, Zhang K, Huang H, et al. Interfacial reactions in SiCf/C/Ti17 composites dominated by texture of carbon coatings [J]. Carbon, 2017, 124: 238 |
| [20] | Ning X J, Pirouz P, Lagerlof K P D, et al. The structure of carbon in chemically vapor deposited SiC monofilaments [J]. J. Mater. Res., 1990, 5: 2865 |
| [21] | Das G. A study of the reaction zone in an SiC fiber-reinforced titanium alloy composite [J]. Metall. Mater. Trans., 1990, 21A: 1571 |
| [22] | Martineau P, Pailler R, Lahaye M, et al. SiC filament/titanium matrix composites regarded as model composites: Part 2 Fibre/matrix chemical interactions at high temperatures [J]. J. Mater. Sci., 1984, 19: 2749 |
| [23] | Lü X H, Yang Y Q, Ma Z J, et al. Kinetics and mechanism of interfacial reaction in SCS-6 SiC continuous fiber-reinforced Ti-Al intermetallic matrix composites [J]. Trans. Nonferrous Met. Soc. China, 2006, 16: 77 |
| [24] | Lü X H, Yang Y Q, Ma Z J, et al. The formation sequence of interfacial reaction products and diffusion path in SiC/Ti6Al4V composite [J]. Rare Met. Mater. Eng., 2007, 36: 1162 |
| [25] | Rudy E. Part V, materials laboratory [R]. Tech. Rep. AFML-TR-65-2, Wright-Patterson Air Force Base, OH, 1969 |
| [26] | Morozumi S, Endo M, Kikuchi M, et al. Bonding mechanism between silicon carbide and thin foils of reactive metals [J]. J. Mater. Sci., 1985, 20: 3976 |
| [27] | Hall I W, Ni C Y. Thermal stability of an SCS-6/Ti-22Al-23Nb composite [J]. Mater. Sci. Eng., 1995, A192-193: 987 |
| [28] | Zhang X, Wang Y M, Lei J F, et al. The interfacial thermal stability and element diffusion mechanism of SiCf/TC17 composite [J]. Acta Metall. Sin., 2012, 48: 1306 |
| [28] | (张 旭, 王玉敏, 雷家峰等. SiCf/TC17复合材料界面热稳定性及元素扩散机理 [J]. 金属学报, 2012, 48: 1306) |
| [29] | Yang J M, Jeng S M. Interfacial reactions in titanium-matrix composites [J]. JOM, 1989, 41(11): 56 |
| [30] | Lü X H. Study on the interfacial diffusion behaviors of SiC continuous fiber reinforced Ti-matrix composites [D]. Xi'an: Northwestern Polytechnical University, 2006 |
| [30] | (吕祥鸿. SiC连续纤维增强Ti基复合材料的界面扩散行为研究 [D]. 西安: 西北工业大学, 2006) |
| [31] | Kong X, Wang Y M, Zhang X, et al. Thermal stability of SiCf /Ti60 composites [J]. Rare Met. Mater. Eng., 2017, 46(S1): 71 |
| [31] | (孔 旭, 王玉敏, 张 旭等. SiCf/Ti60复合材料的热稳定性 [J]. 稀有金属材料与工程, 2017, 46(S1): 71) |
/
| 〈 |
|
〉 |