Effects of Alloying Elements on the Adsorption of Oxygen on V(110) Surfaces: A First-Principles Study
Received date: 2019-12-02
Revised date: 2020-01-06
Online published: 2020-04-09
Supported by
National Natural Science Foundation of China(11975213);National Research Project on the Development of Magnetically Confined Fusion Energy(2017YFE0300304);National Research Project on the Development of Magnetically Confined Fusion Energy(2018YFE0313100)
The oxygen adsorption behavior of V(110) surfaces and the alloying effects of Al, Ti, Cr are calculated using first-principles method. Then the surface phase diagrams for oxygen adsorption on binary V alloy surfaces are constructed combining with thermodynamics formalism. The microscopic mechanisms for oxidation of V alloy surfaces are analyzed. The calculated results of surface energies indicate that Al and Ti are preferable to be segregated on V(110) surfaces, while Cr is not. The oxygen adsorption behavior indicates that Al and Ti are favored to be oxidized on V(110) surfaces, while Cr is not. In this work, the microscopic oxidation mechanisms of V alloy surfaces have been successfully used to explain the experimental results of oxidation behavior. Moreover, the selective oxidation behavior of V-Al alloys has been predicted, and it would provide guidance for the fabrication of oxide tritium permeation barrier.
Xiang GAO , Guikai ZHANG , Xin XIANG , Lizhu LUO , Xiaolin WANG . Effects of Alloying Elements on the Adsorption of Oxygen on V(110) Surfaces: A First-Principles Study[J]. Acta Metall Sin, 2020 , 56(6) : 919 -928 . DOI: 10.11900/0412.1961.2019.00411
| [1] | Muroga T, Chen J M, Chernov V M, et al. Present status of vanadium alloys for fusion applications [J]. J. Nucl. Mater., 2014, 455: 263 |
| [2] | Dolan M D, Kellam M E, McLennan K G, et al. Hydrogen transport properties of several vanadium-based binary alloys [J]. Int. J. Hydrogen Energy, 2013, 38: 9794 |
| [3] | Xiang X, Zhang G K, Wang X L, et al. Review on preparation techniques of FeAl/Al2O3 composite tritium permeation barriers [J]. Rare Met. Mater. Eng., 2016, 45: 522 |
| [3] | 向 鑫, 张桂凯, 汪小琳等. FeAl/Al2O3复合阻氚涂层制备技术的研究进展 [J]. 稀有金属材料与工程, 2016, 45: 522 |
| [4] | Zhang G K, Li J, Chen C A, et al. Tritium permeation barrier-aluminized coating prepared by Al-plating and subsequent oxidation process [J]. J. Nucl. Mater., 2011, 417: 1245 |
| [5] | Sasaki T, Yakou T. Features of intermetallic compounds in aluminized steels formed using aluminum foil [J]. Surf. Coat. Technol., 2006, 201: 2131 |
| [6] | Aiello A, Ciampichetti A, Benamati G. An overview on tritium permeation barrier development for WCLL blanket concept [J]. J. Nucl. Mater., 2004, 329-333: 1398 |
| [7] | Wulf S E, Krauss W, Konys J. Comparison of coating processes in the development of aluminum-based barriers for blanket applications [J]. Fusion Eng. Des., 2014, 89: 2368 |
| [8] | Han S L, Li H L, Wang S M, et al. Influence of silicon on hot-dip aluminizing process and subsequent oxidation for preparing hydrogen/tritium permeation barrier [J]. Int. J. Hydrogen Energy, 2010, 35: 2689 |
| [9] | Yang H G, Zhan Q, Zhao W W, et al. Study of an iron-aluminide and alumina tritium barrier coating [J]. J. Nucl. Mater., 2011, 417: 1237 |
| [10] | Zhang G K, Li J, Chen C A, et al. A new preparing method and performances of FeAl/Al2O3 tritium permeation barrier [J]. Rare Met. Mater. Eng., 2011, 40: 1120 |
| [10] | 张桂凯,李 炬, 陈长安等. FeAl/Al2O3阻氚层的制备新方法与性能 [J]. 稀有金属材料与工程, 2011, 40: 1120 |
| [11] | Peng X X. Fabrication and characterization of V-Al/Al2O3 tritium permeation barrier on V-5Cr-5Ti alloy substrate [D]. Mianyang: China Academy of Engineering Physics, China, 2016 |
| [11] | 彭雪星. V-5Cr-5Ti表面V-Al/Al2O3阻氚涂层的制备及性能研究 [D]. 绵阳: 中国工程物理研究院, 2016 |
| [12] | Wagner C. Theoretical analysis of the diffusion processes determining the oxidation rate of alloys [J]. J. Electrochem. Soc., 1952, 99: 369 |
| [13] | Wang G, Gleeson B, Douglass D L. An extension of Wagner's analysis of competing scale formation [J]. Oxid. Met., 1991, 35: 317 |
| [14] | Keller J G, Douglass D L. The high-temperature oxidation behavior of vanadium-aluminum alloys [J]. Oxid. Met., 1991, 36: 439 |
| [15] | Liang Y J, Che Y C. Handbook of Inorganic Materials Thermodynamics [M]. Shenyang: Northeast University Press, 1993: 45 |
| [15] | 梁英教, 车荫昌. 无机物热力学数据手册 [M]. 沈阳: 东北大学出版社, 1993: 45 |
| [16] | Xu C H, Gao W, Gong H. Oxidation behaviour of FeAl intermetallics. The effects of Y and/or Zr on isothermal oxidation kinetics [J]. Intermetallics, 2000, 8: 769 |
| [17] | Young D J, Naumenko D, Wessel E, et al. Effect of Zr additions on the oxidation kinetics of FeCrAlY alloys in low and high pO2 gases [J]. Metall. Mater. Trans., 2011, 42A: 1173 |
| [18] | Schmiedgen M, Graat P C J, Baretzky B, et al. The initial stages of oxidation of γ-TiAl: An X-ray photoelectron study [J]. Thin Solid Films, 2002, 415: 114 |
| [19] | Zhao L L, Lin J P, Zhang L Q, et al. Initial stages of oxidation of Ti45Al7Nb0.4Y alloy at 900 ℃ in air [J]. J. Mater. Res., 2010, 25: 1204 |
| [20] | Liu S Y, Liu S Y, Li D J, et al. Ab initio atomistic thermodynamics study on the oxidation mechanism of binary and ternary alloy surfaces [J]. J. Chem. Phys., 2015, 142: 064705 |
| [21] | Liu S Y, Shang J X, Wang F H, et al. Ab initio study of surface self-segregation effect on the adsorption of oxygen on the γ-TiAl (111) surface [J]. Phys. Rev., 2009, 79B: 075419 |
| [22] | Wang L, Shang J X, Wang F H, et al. Oxygen adsorption on γ-TiAl surfaces and the related surface phase diagrams: A density-functional theory study [J]. Acta Mater., 2013, 61: 1726 |
| [23] | Gong L, Su Q L, Deng H Q, et al. The stability and diffusion properties of foreign impurity atoms on the surface and in the bulk of vanadium: A first-principles study [J]. Comput. Mater. Sci., 2014, 81: 191 |
| [24] | Zhang X M, Li Y F, He Q L, et al. Investigation of the interstitial oxygen behaviors in vanadium alloy: A first-principles study [J]. Curr. Appl. Phys., 2018, 18: 183 |
| [25] | Vanderbilt D. Soft self-consistent pseudopotentials in a generalized eigenvalue formalism [J]. Phys. Rev., 1990, 41B: 7892(R) |
| [26] | Perdew J P, Wang Y. Accurate and simple analytic representation of the electron-gas correlation energy [J]. Phys. Rev., 1992, 45B: 13244 |
| [27] | Monkhorst H J, Pack J D. Special points for Brillouin-zone integrations [J]. Phys. Rev., 1976, 13B: 5188 |
| [28] | Fischer T H, Almlof J. General methods for geometry and wave function optimization [J]. J. Phys. Chem., 1992, 96: 9768 |
| [29] | Rochana P, Lee K, Wilcox J. Nitrogen adsorption, dissociation, and subsurface diffusion on the vanadium (110) surface: A DFT study for the nitrogen-selective catalytic membrane application [J]. J. Phys. Chem., 2014, 118C: 4238 |
| [30] | Kittel C. Introduction to Solid State Physics [M]. 7th Ed., New York: Wiley, 1996: 1 |
| [31] | Chohan U K, Koehler S P K, Jimenez-Melero E. Incipient FeO(111) monolayer formation during O-adsorption on Fe(110) surface [J]. Comput. Mater. Sci., 2017, 134: 109 |
| [32] | Fujiwara M, Natesan K, Satou M, et al. Effects of doping elements on oxidation properties of V-Cr-Ti type alloys in several environments [J]. J. Nucl. Mater., 2002, 307-311: 601 |
| [33] | Fujiwara M, Takanashi K, Satou M, et al. Influence of Cr, Ti concentrations on oxidation and corrosion resistance of V-Cr-Ti type alloys [J]. J. Nucl. Mater., 2004, 329-333: 452 |
| [34] | Natesan K, Uz M. Oxidation performance of V-Cr-Ti alloys [J]. Fusion Eng. Des., 2000, 51-52: 145 |
| [35] | Natesan K, Soppet W K. Effect of oxygen and oxidation on tensile properties of V-5Cr-5Ti alloy [J]. J. Nucl. Mater., 1996, 233-237: 482 |
| [36] | Maurice V, Despert G, Zanna S, et al. XPS study of the initial stages of oxidation of α2-Ti3Al and γ-TiAl intermetallic alloys [J]. Acta Mater., 2007, 55: 3315 |
/
| 〈 |
|
〉 |