Quantitative Crystallographic Characterization of Boundaries in Ferrite-Bainite/Martensite Dual-Phase Steels
Received date: 2019-11-22
Revised date: 2019-12-23
Online published: 2020-01-03
Supported by
National Key Research and Development Program of China(2017YFB0304900)
In this study, two dual-phase steels with different ferrite-bainite/martensite ratios were obtained by rolling in two-phase region and setting the relaxation time after rolling. The tested steel with smaller ferrite content obtained higher yield strength and tensile strength, greater total elongation and lower ductile-brittle transition temperature; while the steel with higher ferrite content obtained higher uniform elongation and lower yield strength ratio. The EBSD characterization of the two steels shows that for the ferrite-ferrite boundaries and ferrite-bainite/martensite boundaries, if the interface has a large overall misorientation angle, it usually has a large cleavage plane misorientation angle and large slip plane misorientation angle; but for the variant-variant boundaries within bainite or martensite, if the interface has a large overall misorientation angle, it usually has a large cleavage plane misorientation angle, but not necessarily has a large slip plane misorientation angle, and this phenomenon is more significant in martensite microstructure. The ductility of dual-phase steel is not only affected by the proportion of the two phases, but also influenced by the grain refinement of the two phases. Therefore, in order to improve the comprehensive mechanical properties of the dual phase steel, it is necessary to refine the dual phase microstructure from the view of effective slip unit and the effective cleavage unit.
Key words: dual-phase steel; microstructure; grain boundary; misorientation; grain refinement
Xiucheng LI , Mingyu SUN , Jingxiao ZHAO , Xuelin WANG , Chengjia SHANG . Quantitative Crystallographic Characterization of Boundaries in Ferrite-Bainite/Martensite Dual-Phase Steels[J]. Acta Metall Sin, 2020 , 56(4) : 653 -660 . DOI: 10.11900/0412.1961.2019.00398
| [1] | Xia D X, Wang X L, Li X C, et al. Properties and microstructure of thirdgeneration X90 pipeline steel [J]. Acta Metall. Sin., 2013, 49: 271 |
| [1] | 夏佃秀, 王学林, 李秀程等. X90级别第三代管线钢的力学性能与组织特征 [J]. 金属学报, 2013, 49: 271 |
| [2] | Nie W J, Shang C J, Guan H L, et al. Control of microstructures of ferrite/bainite (F/B) dual-phase steels and analysis of their resistance to deformation behavior [J]. Acta Metall. Sin., 2012, 48: 298 |
| [2] | 聂文金, 尚成嘉, 关海龙等. 铁素体/贝氏体(F/B)双相钢组织调控及其抗变形行为分析 [J]. 金属学报, 2012, 48: 298 |
| [3] | Meng D L, Kang Y L, Zheng X F, et al. Effect of two-stage controlled cooling on the microstructure and properties of Mo-containing X80 high-deformability pipeline steel [J]. J. Univ. Sci. Technol. Beijing, 2011, 33: 834 |
| [3] | 孟德亮, 康永林, 郑晓飞等. 两阶段控制冷却工艺对含钼X80抗大变形管线钢组织与性能的影响 [J]. 北京科技大学学报, 2011, 33: 834 |
| [4] | Zhou C, Yan L, Zhang P, et al. Microstructure and mechanical properties of EH47 high strength brittle crack arrest steel for container ship [J]. Trans. Mater. Heat Treat., 2017, 38(8): 83 |
| [4] | 周 成, 严 玲, 张 鹏等. 集装箱船用EH47高止裂钢的组织和性能 [J]. 材料热处理学报, 2017, 38(8): 83 |
| [5] | Ishikawa N, Endo S, Kondo J. High performance UOE linepipes [J]. JFE Technol. Rep., 2006, 12: 15 |
| [6] | Jiao D T, Cai Q W, Wu H B. Effects of cooling process after rolling on microstructure and yield ratio of high-strain pipeline steel X80 [J]. Acta Metall. Sin., 2009, 45: 1111 |
| [6] | 焦多田, 蔡庆伍, 武会宾. 轧后冷却制度对X80级抗大变形管线钢组织和屈强比的影响 [J]. 金属学报, 2009, 45: 1111 |
| [7] | Hanamura T, Yin F, Nagai K. Ductile-brittle transition temperature of ultrafine ferrite/cementite microstructure in a low carbon steel controlled by effective grain size [J]. ISIJ Int., 2004, 44: 610 |
| [8] | Morito S, Huang X, Furuhara T, et al. The morphology and crystallography of lath martensite in alloy steels [J]. Acta Mater., 2006, 54: 5323 |
| [9] | Kitahara H, Ueji R, Tsuji N, et al. Crystallographic features of lath martensite in low-carbon steel [J]. Acta Mater., 2006, 54: 1279 |
| [10] | Lambert-Perlade A, Gourgues A F, Pineau A. Austenite to bainite phase transformation in the heat-affected zone of a high strength low alloy steel [J]. Acta Mater., 2004, 52: 2337 |
| [11] | Karthikeyan T, Dash M K, Ravikirana K, et al. Effect of prior-austenite grain refinement on microstructure, mechanical properties and thermal embrittlement of 9Cr-1Mo-0.1C steel [J]. J. Nucl. Mater., 2017, 494: 260 |
| [12] | Miao C L, Shang C J, Zhang G D, et al. Recrystallization and strain accumulation behaviors of high Nb-bearing line pipe steel in plate and strip rolling [J]. Mater. Sci. Eng., 2010, A527: 4985 |
| [13] | Miao C L, Shang C J, Zurob H S, et al. Recrystallization, precipitation behaviors, and refinement of austenite grains in high Mn, high Nb steel [J]. Metall. Mater. Trans., 2012, 43A: 665 |
| [14] | Bouyne E, Flower H M, Lindley T C, et al. Use of EBSD technique to examine microstructure and cracking in a bainitic steel [J]. Scr. Mater., 1998, 39: 295 |
| [15] | Wang C F, Wang M Q, Shi J, et al. Effect of microstructural refinement on the toughness of low carbon martensitic steel [J]. Scr. Mater., 2008, 58: 492 |
| [16] | Tomita Y, Okabayashi K. Effect of microstructure on strength and toughness of heat-treated low alloy structural steels [J]. Metall. Trans., 1986, 17A: 1203 |
| [17] | Morito S, Yoshida H, Maki T, et al. Effect of block size on the strength of lath martensite in low carbon steels [J]. Mater. Sci. Eng., 2006, A438-440: 237 |
| [18] | Kim M C, Oh Y J, Hong J H. Characterization of boundaries and determination of effective grain size in Mn-Mo-Ni low alloy steel from the view of misorientation [J]. Scr. Mater., 2000, 43: 205 |
| [19] | Hwang B, Kim Y G, Lee S, et al. Effective grain size and Charpy impact properties of high-toughness X70 pipeline steels [J]. Metall. Mater. Trans., 2005, 36A: 2107 |
| [20] | Miao C L, Shang C J, Wang X M, et al. Microstructure and toughness of HAZ in X80 pipeline steel with high Nb content [J]. Acta Metall. Sin., 2010, 46: 541 |
| [20] | 缪成亮, 尚成嘉, 王学敏等. 高Nb X80管线钢焊接热影响区显微组织与韧性 [J]. 金属学报, 2010, 46: 541 |
| [21] | Lambert A, Garat X, Sturel T, et al. Application of acoustic emission to the study of cleavage fracture mechanism in a HSLA steel [J]. Scr. Mater., 2000, 43: 161 |
| [22] | You Y, Shang C J, Nie W J, et al. Investigation on the microstructure and toughness of coarse grained heat affected zone in X-100 multi-phase pipeline steel with high Nb content [J]. Mater. Sci. Eng., 2012, A558: 692 |
| [23] | Li X D, Ma X P, Subramanian S V, et al. Influence of prior austenite grain size on martensite-austenite constituent and toughness in the heat affected zone of 700 MPa high strength linepipe steel [J]. Mater. Sci. Eng., 2014, A616: 141 |
| [24] | Gourgues A F, Flower H M, Lindley T C. Electron backscattering diffraction study of acicular ferrite, bainite, and martensite steel microstructures [J]. Mater. Sci. Technol., 2000, 16: 26 |
| [25] | Morris J W, Lee C S, Guo Z. The Nature and consequences of coherent transformations in steel [J]. ISIJ Int., 2003, 43: 410 |
| [26] | Ghosh A, Kundu S, Chakrabarti D. Effect of crystallographic texture on the cleavage fracture mechanism and effective grain size of ferritic steel [J]. Scr. Mater., 2014, 81: 8 |
| [27] | Guo Z, Lee C S, Morris J W. On coherent transformations in steel [J]. Acta Mater., 2004, 52: 5511 |
| [28] | Wang X L, Ma X P, Wang Z Q, et al. Carbon microalloying effect of base material on variant selection in coarse grained heat affected zone of X80 pipeline steel [J]. Mater. Charact., 2019, 149: 26 |
| [29] | Stormvinter A, Miyamoto G, Furuhara T, et al. Effect of carbon content on variant pairing of martensite in Fe-C alloys [J]. Acta Mater., 2012, 60: 7265 |
| [30] | Kaneshita T, Miyamoto G, Furuhara T. Variant selection in grain boundary nucleation of bainite in Fe-2Mn-C alloys [J]. Acta Mater., 2017, 127: 368 |
| [31] | Morris J W. Stronger, tougher steels [J]. Science, 2008, 320: 1022 |
| [32] | Gui H, Gao X X, Bai Y, et al. Variant selection of bainite on the surface of allotriomorphic ferrite in a low carbon steel [J]. Mater. Charact., 2012, 67: 34 |
| [33] | Liu D S, Luo M, Cheng B G, et al. Microstructural evolution and ductile-to-brittle transition in a low-carbon MnCrMoNiCu heavy plate steel [J]. Metall. Mater. Tran., 2018, 49A: 4918 |
| [34] | Liu S L, Li X C, Guo H, et al. Selective role of bainitic lath boundary in influencing slip systems and consequent deformation mechanisms and delamination in high-strength low-alloy steel [J]. Philos. Mag., 2018, 98: 934 |
/
| 〈 |
|
〉 |