Effect of Partial Recrystallization Annealing on Magnetic Properties and Mechanical Properties of Non-Oriented Silicon Steel

  • Lei YU ,
  • Haiwen LUO
Expand
  • School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing, Beijing 100083, China

Received date: 2019-09-25

  Revised date: 2019-11-04

  Online published: 2019-11-13

Abstract

With the rapid development of high-speed motors, traditional non-oriented silicon steel is difficult to meet its strength requirements. High strength enables resistance to deformation and fatigue fracture induced by centrifugal force. In this work, Nb element is added to traditional non-oriented silicon steel to improve its strength without greatly sacrificing good magnetism. The previous research on Nb-containing high strength non-oriented silicon steel showed that the annealing at high temperature led to good magnetic properties but poor mechanical properties. In order to improve the strength of the steel, the annealing temperature was decreased to make part of the dislocation structure retained in the cold rolled material. The influences of annealing below 900 ℃ on the microstructures, texture, magnetic and mechanical properties of cold rolled Nb-alloyed non-oriented electrical steel were investigated in this work. The increase of annealing temperature promoted recovery at 700~750 ℃ and led to a partial recrystallization with higher fraction at 800~850 ℃; meanwhile, α texture component was enhanced but γ texture suppressed with the increasing temperature. In contrast, the annealing at 900 ℃ resulted in a complete recrystallization, stronger γ but weaker α texture component. Higher annealing temperature produced lower strength and higher ductility as expected, due to dislocations annihilated by recovery and recrystallization, which also led to lower high-frequency iron loss. The value of magnetic induction B50 corresponds well with the intensity of α texture in the annealed steel, and reaches the maximum value at 850 ℃ due to the most intense α texture formed, at which the best combination of mechanical and magnetic properties is also achieved, including the value of magnetic flux B50 (1.572 T), high-frequency iron loss P1.0/400 (33.26 W/kg) and yield strength about 600 MPa, the latter is attributed to the multiple strengthening mechanisms including dislocation, precipitation and grain refinement strengthening.

Cite this article

Lei YU , Haiwen LUO . Effect of Partial Recrystallization Annealing on Magnetic Properties and Mechanical Properties of Non-Oriented Silicon Steel[J]. Acta Metall Sin, 2020 , 56(3) : 291 -300 . DOI: 10.11900/0412.1961.2019.00314

References

[1] Sha Y H, Sun C, Zhang F, et al. Strong cube recrystallization texture in silicon steel by twin-roll casting process [J]. Acta Mater., 2014, 76: 106
[2] Zhang N, Yang P, Mao W M. Through process texture evolution of new thin-gauge non-oriented electrical steels with high permeability [J]. J. Magn. Magn. Mater., 2016, 397: 125
[3] Gong J, Luo H W. Progress on the research of high-strength non-oriented silicon steel sheets in traction motors of hybrid/electrical vehicles [J]. J. Mater. Eng., 2015, 43(6): 102
[3] 龚 坚, 罗海文. 新能源汽车驱动电机用高强度无取向硅钢片的研究与进展 [J]. 材料工程, 2015, 43(6): 102
[4] Pan Z D, Xiang L, Zhang C, et al. Development of high-strength non-oriented electrical steel by TSCR [J]. Iron Steel Van. Tit., 2013, 34(4): 78
[4] 潘振东, 项 利, 张 晨等. TSCR 试制高强度无取向电工钢 [J]. 钢铁钒钛, 2013, 34(4): 78
[5] Wang Y Q, Zhang X M, He Z, et al. Effect of copper precipitates on mechanical and magnetic properties of Cu-bearing non-oriented electrical steel processed by twin-roll strip casting [J]. Mater. Sci. Eng., 2017, A703: 340
[6] Lu Y K, Zu G Q, Luo L, et al. Investigation of microstructure and properties of strip-cast 4.5 wt% Si non-oriented electrical steel by different rolling processes [J]. J. Magn. Magn. Mater., 2019, 497: 165975
[7] Tanaka I, Yashiki H, Iwamoto S, et al. Development of high strength electrical steel SXRC of resource-saving design [J]. J. Iron Steel Res. Int., 2011, 6: 15
[8] Liu B, Song X L, Zhu R Q, et al. Effect of niobium on goss texture evolution of low temperature orientation silicon steel [J]. Trans. Mater. Heat Treat., 2017, 38(11): 71
[8] 刘 彪, 宋新莉, 朱瑞琪等. Nb对低温取向硅钢高斯织构演变的影响 [J]. 材料热处理学报, 2017, 38(11): 71
[9] Huang J, Luo H W. Influence of annealing process on microstructures, mechanical and magnetic properties of Nb-containing high-strength non-oriented silicon steel [J]. Acta Metall. Sin., 2018, 54: 377
[9] 黄 俊, 罗海文. 退火工艺对含Nb高强无取向硅钢组织及性能的影响 [J]. 金属学报, 2018, 54: 377
[10] Honda A, Senda K, Sadahiro K. Electrical steel for motors of electric and hybrid vehicles [J]. Kawasaki Steel Tech. Rep., 2002, 34: 85
[11] Goldschmidt H J. The constitution of the iron-niobium-silicon system [J]. J. Iron Steel Inst., 1960, 194: 169
[12] Raghavan V, Ghosh G. The Fe-Nb-Si (iron-niobium-silicon) system [J]. Trans. Indian Inst. Met., 1984, 37: 421
[13] Raghavan V. Phase Diagrams of Ternary Iron Alloys [M]. Metals Park, Ohio: ASM International, 1987: 226
[14] Singh B N, Gupta K P. Laves and μ phases in the Nb-Fe-Si and Nb-Co-Si systems [J]. Metall. Trans., 1972, 3: 1427
[15] Wang D, Yang S Y, Yang M J, et al. Experimental investigation of phase equilibria in the Fe-Nb-Si ternary system [J]. J. Alloys Compd., 2014, 605: 183
[16] Muraki M, Toge T, Sakata K, et al. Formation mechanism of {111} recrystallization texture in ferritic steels [J]. Tetsu Hagané, 1999, 85: 751
[16] 村木 峰男, 峠 哲雄, 坂田 敬, 待って. フェライト鋼の{111}再結晶集合組織生成機構の-考察. 鉄と鋼, 1999, 85: 751
[17] Park J T, Szpunar J A. Evolution of recrystallization texture in nonoriented electrical steels [J]. Acta Mater., 2003, 51: 3037
[18] Hutchinson W B. Development of textures in recrystallization [J]. Met. Sci., 1974, 8: 185
[19] Park J T, Szpunar J A. Texture development during grain growth in nonoriented electrical steels [J]. ISIJ Int., 2005, 45: 743
[20] Jenkins K, Lindenmo M. Precipitates in electrical steels [J]. J. Magn. Magn. Mater., 2008, 320: 2423
[21] Li M, Xiao Y D, Wang W, et al. Effect of annealing parameter on microstructure and magnetic properties of cold rolled non-oriented electrical steel [J]. Trans. Nonferrous Met. Soc. China, 2007, 17: 74
[22] Zhao Y H, Zhu G H, Wang L T, et al. Effect of annealing temperature on properties of thin specification non-oriented electric steel [J]. Metall. Funct. Mater., 2012, 19(2): 22
[22] 赵亚慧, 朱国辉, 王立涛等. 退火温度对CSP生产薄规格无取向电工钢性能的影响 [J]. 金属功能材料, 2012, 19(2): 22
[23] Yang F, Xiong C G, Xiang L, et al. Effect of annealing time on microstructure of non-oriented electrical steel 50W600 [J]. Hot Work. Technol., 2015, 44: 208
[23] 杨 帆, 熊晨光, 项 利等. 退火时间对无取向电工钢50W600组织的影响 [J]. 热加工工艺, 2015, 44: 208
[24] Zhang N, Yang P, Mao W N. {001}<120>-{113}<361> recrystallization textures induced by initial {001} grains and related microstructure evolution in heavily rolled electrical steel [J]. Mater. Charact., 2016, 119: 225
[25] Sidor J J, Verbeken K, Gomes E, et al. Through process texture evolution and magnetic properties of high Si non-oriented electrical steels [J]. Mater. Charact., 2012, 71: 49
[26] Zu G Q, Zhang X M, Zhao J W, et al. Analysis of {411}<148> recrystallisation texture in twin-roll strip casting of 4.5 wt% Si non-oriented electrical steel [J]. Mater. Lett., 2016, 180: 63
[27] He B B, Hu B, Yen H W, et al. High dislocation density-induced large ductility in deformed and partitioned steels [J]. Science, 2017, 357: 1029
[28] Ungár T, Gubicza J, Ribárik G, et al. Crystallite size distribution and dislocation structure determined by diffraction profile analysis: principles and practical application to cubic and hexagonal crystals [J]. J. Appl. Crystallogr., 2001, 34: 298
[29] Shintani T, Murata Y. Evaluation of the dislocation density and dislocation character in cold rolled type 304 steel determined by profile analysis of X-ray diffraction [J]. Acta Mater., 2011, 59: 4314
[30] Ungár T, Tichy G. The effect of dislocation contrast on X-ray line profiles in untextured polycrystals [J]. Phys. Status Sol., 1999, 171A: 425
[31] Yin F, Hanamura T, Umezawa O, et al. Phosphorus-induced dislocation structure variation in the warm-rolled ultrafine-grained low-carbon steels [J]. Mater. Sci. Eng., 2003, A354: 31
[32] Ungár T, Borbély A. The effect of dislocation contrast on X-ray line broadening: A new approach to line profile analysis [J]. Appl. Phys. Lett., 1996, 69: 3173
[33] Kunieda T, Nakai M, Murata Y, et al. Estimation of the system free energy of martensite phase in an Fe-Cr-C ternary alloy [J]. ISIJ Int., 2005, 45: 1909
[34] Gladman T. The Physical Metallurgy of Microalloyed Steels [M]. London: Maney Pub, 1997: 40
[35] Pickering F B. Physical Metallurgy and the Design of Steels [M]. London: Applied Science Publishers, 1978: 63
Outlines

/