Effects of Silicon on the Microstructure and Propertiesof Cast Duplex Stainless Steel with Ultra-HighChromium and High Carbon

  • Guiqin WANG ,
  • Qin WANG ,
  • Honglong CHE ,
  • Yajun LI ,
  • Mingkai LEI
Expand
  • Surface Engineering Laboratory, School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024, China

Received date: 2019-08-02

  Revised date: 2019-09-22

  Online published: 2019-11-06

Supported by

National Basic Research Program of China(2015CB057306);National Natural Science Foundation of China(U1508218)

Abstract

Duplex stainless steels have excellent corrosion resistance, but its insufficient wear resistance limits its application scope. Therefore, alloying of duplex stainless steels to form hard phases, such as carbides, becomes one of the important research directions to enhance their wear resistance keeping their good corrosion resistance. Specifically, carbides are considered as an ideal hard phase to strengthen Fe-Cr-C alloys, where their types, hardness, volume fraction, morphology, size, spacing and interconnecting feature are the important factors affecting the wear resistance of the alloys. It has been shown that, Si as an alloying addition can modify the carbide precipitates in type, phase morphology and distribution in Fe-Cr-C alloys, having an obvious influence on their wear and corrosion resistance as well as their mechanical properties. In this work, the microstructure and properties of two types of ultra-high chromium (40%, mass fraction) and high carbon (1.5%) duplex stainless steels with different concentrations of Si (0.46% and 1.36%) are investigated. The composition, as-cast microstructure and solidification process as well as the changes in the microstructure, phase structure after solution treatment were studied by chemical analysis, OM, SEM, EPMA and XRD. The mechanical properties including hardness, tensile strength, fracture toughness, corrosion resistance and wear resistance have been tested correspondingly. It is revealed that, both the two kinds of duplex stainless steels have a constitution of three phases in as-cast state, i.e. γ phase, σ phase and M23C6. During the solidification process of the steel with 0.46%Si, δ ferrite dendrite forms at the beginning, followed by eutectic (δ+M23C6), peritectic γ, and finally eutectic (γ+M23C6), in which the δ phase transformed into eutectoid (γ2+σ) in the subsequent cooling process. For the duplex stainless steel with 1.36%Si, the increase of δ ferrite amount is observed leading to obviously increased content of σ phase, the morphology of peritectic γ becomes intermittent and irregular shape, and no eutectic (γ+M23C6) forms. After solution treatment, the two kinds of steels are composed of ferrite, austenite and M23C6 type carbide. Note that, the volume fraction and continuity of α ferrite are promoted obviously by increasing Si content from 0.46% to 1.36%. The Si addition slightly improves the hardness, tensile strength and fracture toughness of the duplex stainless steel, while has little effect on the corrosion resistance and slightly reduces the wear resistance.

Cite this article

Guiqin WANG , Qin WANG , Honglong CHE , Yajun LI , Mingkai LEI . Effects of Silicon on the Microstructure and Propertiesof Cast Duplex Stainless Steel with Ultra-HighChromium and High Carbon[J]. Acta Metall Sin, 2020 , 56(3) : 278 -290 . DOI: 10.11900/0412.1961.2019.00259

References

[1] Liang T, Kang X H, Hu X Q, et al. Investigation on heat treatment of a duplex stainless steel for nuclear power plant impeller [J]. Acta Metall. Sin., 2011, 47: 921
[1] 梁 田, 康秀红, 胡小强等. 核电叶轮用双相不锈钢热处理工艺研究 [J]. 金属学报, 2011, 47: 921
[2] Guha P, Clark C A. Properties and applications of high chromium duplex stainless steels [A]. Proceedings of Conference on Duplex Stainless Steel [C]. Ohio: American Society for Metals, 1983: 355
[3] Atkinson R F, King R W. The properties and applications of two cast duplex stainless steels [A]. Proceedings of Conference on Duplex Stainless Steel [C]. Ohio: American Society for Metals, 1983: 399
[4] Dwars A, Emmel A. Funktionale oberfl?chen auf duplex‐stahl durch laserfeinbeschichten [J]. Materialwiss. Werkstofftech., 2008, 39: 511
[5] Dwars A, Prechtl W, Schr?pfer J, et al. Legierungstechnische M?glichkeiten zur Erh?hung der Korrosionsbest?ndigkeit verschlei?best?ndiger Duplex-St?hle [J]. Mater. Corros., 1995, 46: 674
[6] Tabrett C P, Sare I R, Gomashchi M R. Microstructure-property relationships in high chromium white iron alloys [J]. Int. Mater. Rev., 1996, 41: 59
[7] Wang J L, Sun X W, Zhang H C. Effect of alloys element on abrasive resistance of high chromium cast iron [J]. Hot Work. Technol., 2016, 45(20): 42
[7] 王建玲, 孙秀伟, 张洪潮. 合金元素对高铬铸铁耐磨性能的影响 [J]. 热加工工艺, 1996, 45(20): 42
[8] Liang G Y, Su J Y. The effect of rare earth elements on the growth of eutectic carbides in white cast irons containing chromium [J]. Cast Met., 1992, 4: 83
[9] Wu H Q, Sasaguri N, Matsubara Y, et al. Solidification of multi-alloyed white cast iron: Type and morphology of carbides [J]. AFS Trans., 1996, 104: 103
[10] Dupin P, Schissler J M. Influence of addition of silicon, molybdenum, vanadium, and tungsten upon the structural evolution of the as-cast state of a high-cromium cast iron (20% Cr, 2.6% C) [J]. AFS Trans., 1984, 92: 355
[11] Fulcher J K, Kosel T H, Fiore N F. The effect of carbide volume fraction on the low stress abrasion resistance of high Cr-Mo white cast irons [J]. Wear, 1983, 84: 31
[12] Gahr K H Z, Eldis G T. Abrasive wear of white cast irons [J]. Wear, 1980, 64: 175
[13] Charles J. Super duplex stainless steels: Structure and properties [A]. Duplex Stainless Steel '91 [C]. Les Ulis: Les Editions de Physique, 1991: 3
[14] Sch?n C G, Sinatora A. Simulation of solidification paths in high chromium white cast irons for wear applications [J]. Calphad, 1998, 22: 437
[15] Jacuinde A B, Rainforth W M. The wear behaviour of high-chromium white cast irons as a function of silicon and mischmetal content [J]. Wear, 2001, 250: 449
[16] Lai J P, Pan Q L, Peng H J, et al. Effects of Si on the microstructures and mechanical properties of high-chromium cast iron [J]. J. Mater. Eng. Perform., 2016, 25: 4617
[17] Lai J P, Pan Q L, Sun Y W, et al. Effect of Si content on the microstructure and wear resistance of high chromium cast iron [J]. ISIJ Int., 2018, 58: 1532
[18] Powell G, Randle V. The effect of Si on the relationship between orientation and carbide morphology in high chromium white irons [J]. J. Mater. Sci., 1997, 32: 561
[19] Laird G, Powell G L F. Solidification and solid-state transformation mechanisms in Si alloyed high-chromium white cast irons [J]. Metall. Trans., 1993, 24A: 981
[20] Shen J, Zhou Q D. Solidification behaviour of boron-bearing high-chromium cast iron and the modification mechanism of silicon [J]. Cast Met., 1988, 1: 79
[21] Michalska J, Sozańska M. Qualitative and quantitative analysis of σ and χ phases in 2205 duplex stainless steel [J]. Mater. Charact., 2006, 56: 355
[22] Knyazeva M, Pohl M. Duplex steels. Part II: Carbides and nitrides [J]. Metallogr. Microstruct. Anal., 2013, 2: 343
[23] Hsieh C C, Wu W T. Phase transformation of δσ in multipass heat-affected and fusion zones of dissimilar stainless steels [J]. Met. Mater. Int., 2011, 17: 375
[24] Chen J Y, Yang Z Y, Yang W, et al. Characteristic of phase σ precipitation and its effects on behavior in duplex stainless steel [J]. J. Iron Steel Res. Int., 2006, 18(8): 1
[24] 陈嘉砚, 杨卓越, 杨 武等. 双相不锈钢中σ相的形成特点及其对性能的影响 [J]. 钢铁研究学报, 2006, 18(8): 1
[25] Liu F X. σ phase precipitation and its effect on mechanical properties of S32205 duplex stainless steel [J]. Iron Steel, 2010, 45(7): 62
[25] 刘复兴. S32205双相不锈钢中σ相的析出及其对力学性能的影响 [J]. 钢铁, 2010, 45(7): 62
[26] Montemor M F, Ferreira M G S, Hakiki N E, et al. Chemical composition and electronic structure of the oxide films formed on 316L stainless steel and nickel based alloys in high temperature aqueous environments [J]. Corros. Sci., 2000, 42: 1635
[27] Rivlin V G. Critical review of constitution of carbon-chromium-iron and carbon-iron-manganese systems [J]. Int. Mater. Rev., 1984, 29: 299
[28] Cui T H, Zhu L Y, He J Z, et al. Effect of Si content on microstructure and properties of DP600 hot rolled dual phase steel [J]. T. Mater. Heat Treat., 2015, 36(9): 103
[28] 崔田灏, 周乐育, 何建中等. Si含量对DP-600级别热轧双相钢组织及性能的影响 [J]. 材料热处理学报, 2015, 36(9): 103
[29] Guo H X, Zhang J M, Xia S L. Analysis on abnormal structure in color metallography of as-cast duplex stainless steel [J]. Phys. Test. Chem. Anal. Phys. Test., 2014, 50(4): 273
[29] 郭海霞, 张金民, 夏申林. 铸态双相不锈钢彩色金相异常组织分析 [J]. 理化检验-物理分册, 2014, 50(4): 273
[30] Wu J. Duplex Stainless Steel [M]. Beijing: Metallurgical Industry Press, 1999: 31
[30] 吴 玖. 双相不锈钢 [M]. 北京: 冶金工业出版社, 1999: 31
[31] Lin D Y, Chang T C, Liu G L. Effect of Si contents on the growth behavior of σ phase in USU 309L stainless steel [J]. Scr. Mater., 2003, 49: 855
[32] ?Norstr?m L, Pettersson S, Nordin S. σ-phase embrittlement in some ferritic-austenitic stainless steels [J]. Mater. Sci. Eng. Technol., 1981, 12: 229
[33] Svensson L E, Gretoft B, Ulander B, et al. Fe-Cr-C hardfacing alloys for high-temperature applications [J]. J. Mater. Sci., 1986, 21: 1015
[34] Chang C M, Lin C M, Hsieh C C, et al. Micro-structural characteristics of Fe-40wt%Cr-xC hardfacing alloys with [1.0-4.0wt%] carbon content [J]. J. Alloys Compd., 2009, 487: 83
[35] Wang B C. Material Corrosion and Protection [M]. Beijing: Peking University Press, 2012: 246
[35] 王保成. 材料腐蚀与防护 [M]. 北京: 北京大学出版社, 2012: 246
Outlines

/