Overview

Recent Development of Nickel-Based Disc Alloys andCorresponding Cast-Wrought Processing Techniques

  • Beijiang ZHANG ,
  • Shuo HUANG ,
  • Wenyun ZHANG ,
  • Qiang TIAN ,
  • Shifu CHEN
Expand
  • High Temperature Materials Research Division, Central Iron & Steel Research Institute, Beijing 100081, China

Received date: 2019-03-22

  Revised date: 2019-06-24

  Online published: 2019-07-02

Supported by

Supported by National Science and Technology Major Project(2017-VI-0015-0087,2017-VI-0018-0090)

Abstract

The newly developed high-performance cast-wrought alloys have been widely applied in advanced turbine engines in recent years, particularly, served as turbine disc and compressor disc. The significant breakthrough has been made on the processing techniques for these highly alloyed disc alloys, including the triple-melting of the large-scale ingots with the diameter more than 500 mm, conversion of the large-scale ingot and the processing of fine-grained billets with the diameter more than 300 mm, customization of the microstructures and properties of disc forgings. The chemical compositions can be well controlled on vacuum arc remelting (VAR) ingots, including the ultra-low carbon content lower than 0.011%. The white spots and freckles have been found to be the primary defects on large-scale VAR ingots, which is triggered by the improper re-melting parameters. The metallurgical defects can be identified on fine-grained billets via supersonic inspection. The investigations have shown that the existence of the micro-duplex structure opens a window for the processing of these highly alloyed disc alloys with up to more than 60% mass fraction of precipitates. Via a multicycle thermal-mechanical processing technique, the hot working process of the disc alloys, can be achieved in a cost-effective way, and the un-recrystallized grains can also be eliminated efficiently. The above-mentioned techniques have greatly promoted the development and application of the high-performance disc alloys, such as GH4065, GH4720, GH4175 and GH4975, et al. These alloys can provide a promising solution of high reliability combined with low life cycle cost for military and commercial gas turbines. Nonetheless, in order to maximize the advantageous of cast-wrought disc alloys on reliability and cost-effective ratio, the comprehensive understanding about the prevention and identification of metallurgical defects, increase in the yield rate of materials during conversion, processing of fine-grained billets and dual-property disc forgings, is still needed.

Cite this article

Beijiang ZHANG , Shuo HUANG , Wenyun ZHANG , Qiang TIAN , Shifu CHEN . Recent Development of Nickel-Based Disc Alloys andCorresponding Cast-Wrought Processing Techniques[J]. Acta Metall Sin, 2019 , 55(9) : 1095 -1114 . DOI: 10.11900/0412.1961.2019.00078

References

[1] ReedR C. The Superalloys: Fundamentals and Applications [M]. Cambridge: Cambridge University Press, 2006: 236
[2] DonachieM J, DonachieS J. Superalloys: A Technical Guide [M]. 2nd Ed., Ohio: ASM International, 2002: 120
[3] ShiC X, ZhongZ Y. Forty years of superalloy R & D in China [J]. Acta Metall. Sin., 1997, 33: 1
[3] 师昌绪, 仲增墉. 中国高温合金40年 [J]. 金属学报, 1997, 33: 1
[4] JiangH F. Requirements and forecast of turbine disk materials [J]. Gas Turb. Exp. Res., 2002, 15(4): 1
[4] 江和甫. 对涡轮盘材料的需求及展望 [J]. 燃气涡轮试验与研究, 2002, 15(4): 1)
[5] WangX D, WangH C. Improved development superalloys, promote the aero-engine development [A]. The Thirteenth Session of the Annual China Superalloys Conference [C]. Beijing: Metallurgical Industry Press, 2015: 3
[5] (王旭东, 王海川. 改进发展高温合金, 推动航空发动机研制 [A]. 第十三届中国高温合金年会论文集 [C]. 北京: 冶金工业出版社, 2015: 3)
[6] SimsC T, StoloffN S, HagelW C. Superalloys II—High Temperature Materials for Aerospace and Industrial Power [M]. New York: John Wiley & Sons, 1987: 32
[7] DevauxA, GeorgesE, HéritierP. Development of new C&W superalloys for high temperature disk applications [J]. Adv. Mater. Res., 2011, 278: 405
[8] High Temperature Material Branch of the Chinese Society for Metals. China Superalloys Handbook (Volume One) [M]. Beijing: China Standards Press, 2012: 891
[8] (中国金属学会高温材料分会. 中国高温合金手册/上卷: 变形高温合金 焊接用高温合金丝 [M]. 北京: 中国标准出版社, 2012: 891)
[9] WilliamsJ C, Starke JrE A. Progress in structural materials for aerospace systems [J]. Acta Mater., 2003, 51: 5775
[10] FangB, JiZ, LiuM, , et al. Study on constitutive relationships and processing maps for FGH96 alloy during two-pass hot deformation [J]. Mater. Sci. Eng., 2014, A590: 255
[11] CarterJ L W, KuperM W, UchicM D, , et al. Characterization of localized deformation near grain boundaries of superalloy René-104 at elevated temperature [J]. Mater. Sci. Eng., 2014, A605: 127
[12] FindleyK O, SaxenaA. Low cycle fatigue in René 88DT at 650 ℃: Crack nucleation mechanisms and modeling [J]. Metall. Mater. Trans., 2006, 37A: 1469
[13] ViswanathanG B, SarosiP M, HenryM F, , et al. Investigation of creep deformation mechanisms at intermediate temperatures in René 88 DT [J]. Acta Mater., 2005, 53: 3041
[14] HuangQ Y, LiH K. Superalloy [M]. Beijing: Metallurgical Industry Press, 2000: 385
[14] 黄乾尧, 李汉康. 高温合金 [M]. 北京: 冶金工业出版社, 2000: 385)
[15] DeckerR F. The evolution of wrought age-hardenable superalloys [J]. JOM, 2006, 58(9): 32
[16] PreliF R, FurrerD. Lessons learned from the development, application and advancement of alloy 718 [A]. 8th International Symposium on Superalloy 718 and Derivatives [C]. Pittsburgh: TMS, 2014: 3
[17] HayesR W, UnocicR R, NasrollahzadehM. Creep deformation of allvac 718Plus [J]. Metall. Mater. Trans., 2015, 46A: 218
[18] LiuY C, ZhangH J, GuoQ Y, , et al. Microstructure evolution of Inconel 718 superalloy during hot working and its recent development tendency [J]. Acta Metall. Sin., 2018, 54: 1653
[18] 刘永长, 张宏军, 郭倩颖等. Inconel 718变形高温合金热加工组织演变与发展趋势 [J]. 金属学报, 2018, 54: 1653
[19] DevauxA, PicquéB, GervaisM F, , et al. AD730TM—A new nickel-based superalloy for high temperature engine rotative parts [A]. Superalloys 2012 [C]. Warrendale, PA: TMS, 2012: 911
[20] CrozetC, DevauxA, ForestierR, , et al. Effect of ingot size on microstructure and properties of the new advanced AD730TM superalloy [A]. Superalloys 2016 [C]. Warrendale, PA: TMS, 2016: 437
[21] HeaneyJ A, LasondeM L, PowellA M, , et al. Development of a new cast and wrought alloy (René 65) for high temperature disk applications [A]. 8th International Symposium on Superalloy 718 and Derivatives [C]. Pittsburgh: TMS, 2014: 67
[22] ReedR C, MotturaA, CruddenD J. Alloys-by-design: Towards optimization of compositions of nickel-based superalloys [A]. Superalloys 2016 [C]. Warrendale, PA: TMS, 2016: 15
[23] ShiC X, ZhongZ Y. Development and innovation of superalloy in China [J]. Acta Metall. Sin., 2010, 46: 1281
[23] 师昌绪, 仲增墉. 我国高温合金的发展与创新 [J]. 金属学报, 2010, 46: 1281
[24] LongZ D, ZhuangJ Y, DengB, , et al. A new method to improve the hot workability of high strength Ni-based superalloys [J]. Acta Metall. Sin., 1999, 35: 1211
[24] 龙正东, 庄景云, 邓 波等. 一种提高高强化高温合金热加工性能的新方法 [J]. 金属学报, 1999, 35: 1211
[25] ZhongZ Y, ZhuangJ Y. Development of several important problems on producing technologies of wrought superalloy [J]. J. Iron Steel Res., 2003, 15: 1
[25] 仲增墉, 庄景云. 变形高温合金生产工艺中几个重要问题的研究和进展 [J]. 钢铁研究学报, 2003, 15: 1
[26] DongJ X, LiL H, LiH Y, , et al. Effect of extent of homogenization on the hot deformation recrystallization of superalloy ingot in cogging process [J]. Acta Metall. Sin., 2015, 51: 1207
[26] 董建新, 李林翰, 李浩宇等. 高温合金铸锭均匀化程度对开坯热变形的再结晶影响 [J]. 金属学报, 2015, 51: 1207
[27] DuJ H, ZhaoG P, DengQ, , et al. Development of wrought superalloy in China [J]. J. Aeron. Mater., 2016, 36(3): 27
[27] 杜金辉, 赵光普, 邓 群等. 中国变形高温合金研制进展 [J]. 航空材料学报, 2016, 36(3): 27)
[28] ZhangB J, ZhaoG P, ZhangW Y, , et al. Investigation of high performance disc alloy GH4065 and associated advanced processing techniques [J]. Acta Metall. Sin., 2015, 51: 1227
[28] 张北江, 赵光普, 张文云等. 高性能涡轮盘材料GH4065及其先进制备技术研究 [J]. 金属学报, 2015, 51: 1227
[29] ZhangB J, ZhaoG P, ZhangW Y, , et al. Deformation mechanisms and microstructural evolution of γ+γ' duplex aggregates generated during thermomechanical processing of nickel-base superalloys [A]. Superalloys 2016 [C]. Warrendale, PA: TMS, 2016: 487
[30] Van Den AvyleJ A, BrooksJ A, PowellA C. Reducing defects in remelting processes for high-performance alloys [J]. JOM, 1998, 50(3): 22
[31] AuburtinP, WangT, CockcroftS L, , et al. Freckle formation and freckle criterion in superalloy castings [J]. Metall. Mater. Trans., 2000, 31B: 801
[32] WangZ X, HuangS, ZhangB J, , et al. Study on freckle of a high-alloyed GH4065 Nickel base wrought superalloy [J]. Acta Metall. Sin., 2019, 55: 417
[32] 王资兴, 黄 烁, 张北江等. 高合金化GH4065镍基变形高温合金点状偏析研究 [J]. 金属学报, 2019, 55: 417
[33] GenereuxP D, BorgC A. Characterization of freckles in a high strength wrought nickel superalloy [A]. Superalloys 2000 [C]. Warrendale, PA: TMS, 2000: 19
[34] CharpagneM A, CharpagneM A, BillotT, , et al. Heteroepitaxial recrystallization observed in René 65TM and Udimet 720TM: A new recrystallization mechanism possibly occurring in all low lattice mismatch γ-γ' superalloys? [A]. Superalloys 2016 [C]. Warrendale, PA: TMS, 2016: 417
[35] AndrewW, AudeL, AudeL, , et al. Thermal stability of cast and wrought alloy Rene 65 [A]. Superalloys 2016 [C]. Warrendale, PA: TMS, 2016: 793
[36] WlodekS T, KellyM, AldenD A. The structure of René 88 DT [A]. Superalloys 1996 [C]. Warrendale, PA: TMS, 1996: 129
[37] BryantD J, McIntoshD G. The manufacture and evaluation of a large turbine disc in cast and wrought alloy 720Li [A]. Superalloys 1996 [C]. Warrendale, PA: TMS, 1996: 713
[38] ZhangB J, ZhaoG P, JiaoL Y, , et al. Influence of hot working process on microstructures of superalloy GH4586 [J]. Acta Metall. Sin., 2005, 41: 351
[38] 张北江, 赵光普, 焦兰英等. 热加工工艺对GH4586合金微观组织的影响 [J]. 金属学报, 2005, 41: 351
[39] ZhangB J, ZhaoG P, XuG H, , et al. Hot deformation behavior and micro-structure evolution of superalloy GH742 [J]. Acta Metall. Sin., 2005, 41: 1207
[39] 张北江, 赵光普, 胥国华等. GH742合金热变形行为与微观组织演化 [J]. 金属学报, 2005, 41: 1207
[40] SchafrikR E. Materials for a non-steady-state world [J]. Metall. Mater. Trans., 2016, 47B: 1505
[41] SunX F, YinF S, LiJ G, , et al. Solidification behavior of a cast nickel-base superalloy [J]. Acta Metall. Sin., 2003, 39: 27
[41] 孙晓峰, 殷凤仕, 李金国等. 一种铸造镍基高温合金的凝固行为 [J]. 金属学报, 2003, 39: 27
[42] ZhangJ, HuangT W, LiuL, , et al. Advances in solidification characteristics and typical casting defects in nickel-based single crystal superalloys [J]. Acta Metall. Sin., 2015, 51: 1163
[42] 张 军, 黄太文, 刘 林等. 单晶高温合金凝固特性与典型凝固缺陷研究 [J]. 金属学报, 2015, 51: 1163
[43] ZhangJ, LouL H. Basic research in development and application of cast superalloy [J]. Acta Metall. Sin., 2018, 54: 1637
[43] 张 健, 楼琅洪. 铸造高温合金研发中的应用基础研究 [J]. 金属学报, 2018, 54: 1637
[44] Carter JrW T, JonesR M F. Nucleated casting for the production of large superalloy ingots [J]. JOM, 2005, 57(4): 52
[45] MonajatiH, TaheriA K, JahaziM, , et al. Deformation characteristics of isothermally forged UDIMET 720 nickel-base superalloy [J]. Metall. Mater. Trans., 2005, 36A: 895
[46] RobsonJ D. Modeling competitive continuous and discontinuous precipitation [J]. Acta Mater., 2013, 61: 7781
[47] CantwellP R, TangM, DillonS J, , et al. Grain boundary complexions [J]. Acta Mater., 2014, 62: 1
[48] BondB J, O'BrienC M, RussellJ L, , et al. René 65 billet material for forged turbine components [A]. 8th International Symposium on Superalloy 718 and Derivatives [C]. Pittsburgh: TMS, 2014: 107
[49] LarrouyB, VillechaiseP, CormierJ, , et al. Influence of both temperature and γ' distribution on the development of strain incompatibilities at grain boundaries at low temperature in the UdimetTM 720 Li superalloy [A]. 8th International Symposium on Superalloy 718 and Derivatives [C]. Pittsburgh: TMS, 2014: 713
[50] ValitovV A. Formation of nanocrystalline structure upon severe thermomechanical processing and its effect on the superplastic properties of nickel base alloys [A]. 8th International Symposium on Superalloy 718 and Derivatives [C]. Pittsburgh: TMS, 2014: 739
[51] TileyJ, ViswanathanG B, SrinivasanR, , et al. Coarsening kinetics of γ' precipitates in the commercial nickel base Superalloy René 88 DT [J]. Acta Mater., 2009, 57: 2538
[52] MacSleyneJ, UchicM D, SimmonsJ P, , et al. Three-dimensional analysis of secondary γ' precipitates in René-88 DT and UMF-20 superalloys [J]. Acta Mater., 2009, 57: 6251
[53] RadisR, SchafferM, AlbuM, , et al. Multimodal size distributions of γ' precipitates during continuous cooling of UDIMET 720 Li [J]. Acta Mater., 2009, 57: 5739
Outlines

/