Study on Interface of Linear Friction Welded Joint Between TC11 and TC17 Titanium Alloy
Received date: 2018-11-13
Revised date: 2019-03-27
Online published: 2019-04-29
Supported by
National Natural Science Foundation of China(Nos.51675434);National Natural Science Foundation of China(10477017)
As a solid-state welding technology, linear friction welding has unique advantages in machining dissimilar titanium alloy blade disc. However, there still lacks sufficient support in basic applied research, and the mechanism of interface formation is still under study. In this work, the microstructure of the welded joint between TC11 and TC17 titanium alloys was analyzed by OM, SEM and TEM, respectively. The results showed that common grains and common grain boundaries are formed at the weld interface. In the common grain, a phase boundary is formed in the weld interface. Elements diffusion is observed on both sides of the common grain boundary and the phase boundary in the common grain. Under the action of rejection, adsorption and towing of solute elements in the formation of common grains and common grain boundary, the observed diffusion distance of elements in the phase boundary of the common grain is longer than the one in the common grain boundary. The composition change at the phase boundary of the weld zone is greater than the one inside the phase. A large number of small needle-like α phases are formed at the weld interface that has a large number of deformed twins. The structure of the interface in common grains consists of two interfaces (recrystallization growth interfaces of both sides) and two growth regions (ordered and disordered). The dynamic recrystallization also has an ordered and disordered crystallization process similar to that of solidification crystallization.
Key words: titanium alloy; linear friction welding; weld interface
Suigeng DU , Man GAO , Wanting XU , Xifeng WANG . Study on Interface of Linear Friction Welded Joint Between TC11 and TC17 Titanium Alloy[J]. Acta Metall Sin, 2019 , 55(7) : 885 -892 . DOI: 10.11900/0412.1961.2018.00512
| [1] | Zhang H Y, Zhang L F. Development overview of aeroengine integral blisk and its manufacturing technology at home and abroad [J]. Aero. Manuf. Technol., 2013, (23-24): 38 |
| [1] | (张海艳, 张连锋. 航空发动机整体叶盘制造技术国内外发展概述 [J]. 航空制造技术, 2013, (23-24): 38) |
| [2] | Han X F, Zhang L, Qian L Y. Application of solid state welding in civil aircraft aeroengine [J]. Aero. Manuf. Technol., 2012, (13): 55 |
| [2] | (韩秀峰, 张 露, 钱凌翼. 固态焊接在民用航空发动机中的应用 [J]. 航空制造技术, 2012, (13): 55) |
| [3] | Chen L, Li W Y, Ma T J. The state-of-the-art and perspectives of linear friction welding technology [J]. Adv. Aero. Sci. Eng., 2010, 1: 178 |
| [3] | (陈 亮, 李文亚, 马铁军等. 线性摩擦焊接技术研究进展与展望 [J]. 航空工程进展, 2010, 1: 178) |
| [4] | Su Y, Li W Y, Wang X Y, et al. Linear friction welding of titanium alloys: State-of-the-art and perspectives [J]. Mater. China, 2017, 36: 852 |
| [4] | (苏 宇, 李文亚, 王新宇等. 钛合金线性摩擦焊研究现状及展望 [J]. 中国材料进展, 2017, 36: 852) |
| [5] | Li W Y, Ma T, Zhang Y, et al. Microstructure characterization and mechanical properties of linear friction welded Ti-6Al-4V alloy [J]. Adv. Eng. Mater., 2008, 10: 89 |
| [6] | Li W Y, Ma T J, Yang S Q. Microstructure evolution and mechanical properties of linear friction welded Ti-5Al-2Sn-2Zr-4Mo-4Cr (Ti17) titanium alloy joints [J]. Adv. Eng. Mater., 2010, 12: 35 |
| [7] | Ji Y J, Zhang T C, Li X H, et al. Micro-area characteristic analysis of TC11/TC17 linear friction welding flash and weld [J]. Aero. Manuf. Technol., 2015, (11): 62 |
| [7] | (季亚娟, 张田仓, 李晓红等. TC11/TC17线性摩擦焊飞边及焊缝微区特征分析 [J]. 航空制造技术2015, (11): 62) |
| [8] | Zhao P K, Fu L, Chen H Y. Low cycle fatigue properties of linear friction welded joint of TC11 and TC17 titanium alloys [J]. J. Alloys Compd., 2016, 675: 248 |
| [9] | Zhao P K, Fu L. Strain hardening behavior of linear friction welded joints between TC11 and TC17 dissimilar titanium alloys [J]. Mater. Sci. Eng., 2015, A621: 149 |
| [10] | Dalgaard E, Wanjara P, Gholipour J, et al. Linear friction welding of a near-β titanium alloy [J]. Acta Mater., 2012, 60: 770 |
| [11] | Li W Y, Suo J D, Ma T J, et al. Abnormal microstructure in the weld zone of linear friction welded Ti-6.5Al-3.5Mo-1.5Zr-0.3Si titanium alloy joint and its influence on joint properties [J]. Mater. Sci. Eng., 2014, A599: 38 |
| [12] | Guo Y N, Attallah M M, Chiu Y, et al. Spatial variation of microtexture in linear friction welded Ti-6Al-4V [J]. Mater. Charact., 2017, 127: 342 |
| [13] | Karadge M, Preuss M, Lovell C, et al. Texture development in Ti-6Al-4V linear friction welds [J]. Mater. Sci. Eng., 2007, A459: 182 |
| [14] | Wanjara P, Jahazi M. Linear friction welding of Ti-6Al-4V: Processing, microstructure, and mechanical-property inter-relationships [J]. Metall. Mater. Trans., 2005, 36A: 2149 |
| [15] | Turner R, Gebelin J C, Ward R M, et al. Linear friction welding of Ti-6Al-4V: Modelling and validation [J]. Acta Mater., 2011, 59: 3792 |
| [16] | Zhang C C, Zhang T C, Ji Y J, et al. Formation process and mechanism of linear friction welding joint [J]. J. Mater. Eng., 2015, 43(11): 39 |
| [16] | (张传臣, 张田仓, 季亚娟等. 线性摩擦焊接头形成过程及机理 [J]. 材料工程, 2015, 43(11): 39) |
| [17] | Lang B, Zhang T C, Tao J, et al. Microstructure in linear friction welded dissimillar titanium alloy joint [J]. Trans. China Weld. Inst., 2012, 33(7): 105 |
| [17] | (郎 波, 张田仓, 陶 军等. 异质钛合金线性摩擦焊接头微观组织 [J]. 焊接学报, 2012, 33(7): 105) |
| [18] | Lang B, Zhang T C, Tao J, et al. Formation mechanism of linear friction welded titanium alloy joint [J]. Trans. China Weld. Inst., 2012, 35(9): 37 |
| [18] | (郎 波, 张田仓, 陶 军等. 钛合金线性摩擦焊接头形成机制 [J]. 焊接学报, 2014, 35(9): 37) |
| [19] | Lang B, Zhang T C, Li X H, et al. Microstructural evolution of a TC11 titanium alloy during linear friction welding [J]. J. Mater. Sci., 2010, 45: 6218 |
| [20] | Wen G D, Ma T J, Li W Y, et al. Cyclic deformation behavior of linear friction welded Ti6Al4V joints [J]. Mater. Sci. Eng., 2014, A597: 408 |
| [21] | Ma T J, Tang L F, Li W Y, et al. Linear friction welding of a solid-solution strengthened Ni-based superalloy: Microstructure evolution and mechanical properties studies [J]. J. Manuf. Processes, 2018, 34: 442 |
| [22] | Ma T J, Chen T, Li W Y, et al. Formation mechanism of linear friction welded Ti-6Al-4V alloy joint based on microstructure observation [J]. Mater. Charact., 2011, 62: 130 |
| [23] | Chen Y. Study on the microstructure of TC4 joints welded by linear friction welding [D]. Dalian: Dalian Jiaotong University, 2012 |
| [23] | (陈 燕. TC4钛合金线性摩擦焊接头组织结构分析 [D]. 大连: 大连交通大学, 2012) |
| [24] | Wang X Y, Li W Y, Ma T J. Research status of microstructure of linear friction welded titanium alloy [J]. Aero. Manuf. Technol., 2015, (20): 56 |
| [24] | (王新宇, 李文亚, 马铁军. 钛合金线性摩擦焊接界面组织研究现状 [J]. 航空制造技术, 2015, (20): 56) |
| [25] | Editiorial Committee of China Aeronautical Materials Handbook. China Aeronautical Materials Handbook (Book 4) [M]. 2nd Ed., Beijing: China Standard Press, 2002: 152 |
| [25] | (《中国航空材料手册》编辑委员会. 中国航空材料手册(第4卷) [M]. 第2版. 北京: 中国标准出版社, 2002: 152) |
/
| 〈 |
|
〉 |