Three-Dimensional Characteristics and Morphological Evolution of Micro/Meso Pores inG20Mn5N Steel Castings
Received date: 2018-04-11
Revised date: 2018-11-07
Online published: 2018-11-19
Supported by
National Key Research and Development Program of China(2017YFC0805100);National Natural Science Foundation of China(51578137);Open Research Fund Program of Jiangsu Key Laboratory of Engineering Mechanics;Priority Academic Program Development of the Jiangsu Higher Education Institutions
Cast steel is an important metal material that is widely used in civil engineering due to its strength and ductility. However, a variety of casting defects such as micro/meso pores are usually present in the as-cast components and can lead to the degradation of mechanical properties. In this work, the initial micro/meso pores in the G20Mn5N low-alloy cast steel were investigated based on high resolution 3D X-ray tomography technology. Based on their formation mechanism and characteristics, pores were classified into gas, gas-shrinkage and shrinkage pores, and the parameters such as the number, size and sphericity of three types of pores have been counted and analyzed. Then the evolutionary behavior of micro/meso pores in G20Mn5N low-alloy cast steel specimens under monotonic tensile loading has also been studied. The results showed that the volume of gas pore was small and its sphericity coefficients were high. Compared with the gas pore, the shrinkage pore had large volume and more complex shape in space. The volume and sphericity coefficients of gas-shrinkage pore were between the gas pore and the shrinkage. Damage evolution to metallic materials can be divided into void nucleation, growth and coalescence. The void nucleation and growth law were investigated by statistical analysis, which showed that the evolution of the void density could be modeled by an empirical function, and the evolution of void average radius was not only related to void growth but also affected by void nucleation.
Key words: cast steel; micro/meso pore; morphological evolution; 3D X-ray tomography
Huadong YAN , Hui JIN . Three-Dimensional Characteristics and Morphological Evolution of Micro/Meso Pores inG20Mn5N Steel Castings[J]. Acta Metall Sin, 2019 , 55(3) : 341 -348 . DOI: 10.11900/0412.1961.2018.00131
| [1] | Bao W, Xing L T, Qiu J H. The use of cast steel in steel structure [J]. Adv. Mater. Res., 2011, 183-185: 1918 |
| [2] | Chen Y Y, Zhao X Z, Tong L W. Research and application of connections of structural steel casting [J]. Adv. Struct. Eng., 2010, 13: 441 |
| [3] | Lee P D, Hunt J D. Hydrogen porosity in directionally solidified aluminium-copper alloys: A mathematical model [J]. Acta Mater., 2001, 49: 1383 |
| [4] | Blair M, Monroe R, Beckermann C, et al. Predicting the occurrence and effects of defects in castings [J]. JOM, 2005, 57(5): 29 |
| [5] | Liu C Y, Wu X, Wu N, et al. Structural damage identification based on rough sets and artificial neural network [J]. Sci. World J., 2014, 2014: 193284 |
| [6] | Sigl K M, Hardin R A, Stephens R I, et al. Fatigue of 8630 cast steel in the presence of porosity [J]. Int. J. Cast Met. Res., 2004, 17: 130 |
| [7] | Hardin R A, Beckermann C. Prediction of the fatigue life of cast steel containing shrinkage porosity [J]. Metall. Mater. Trans., 2009, 40A: 581. |
| [8] | Hardin R A, Beckermann C. Effect of porosity on deformation, damage, and fracture of cast steel [J]. Metall. Mater. Trans., 2013, 44A: 5316 |
| [9] | Wang S G, Wang S C, Zhang L. Application of high resolution transmission X-ray tomography in material science [J]. Acta Metall. Sin., 2013, 49: 897 |
| [9] | 王绍钢, 王苏程, 张 磊. 高分辨透射X射线三维成像在材料科学中的应用 [J]. 金属学报, 2013, 49: 897 |
| [10] | Wan Q, Zhao H D, Zou C. Three-dimensional characterization and distribution of micropores in aluminum alloy high pressure die castings [J]. Acta Metall. Sin., 2013, 49: 284 |
| [10] | 万 谦, 赵海东, 邹 纯. 铝合金压铸件微观孔洞三维特征及分布的研究 [J]. 金属学报, 2013, 49: 284 |
| [11] | Yu C, Wu S C, Hu Y N, et al. Three-dimensional imaging of gas pores in fusion welded Al alloys by synchrotron radiation X-ray microtomography [J]. Acta Metall. Sin., 2015, 51: 159 |
| [11] | 喻 程, 吴圣川, 胡雅楠等. 铝合金熔焊微气孔的三维同步辐射X射线成像 [J]. 金属学报, 2015, 51: 159 |
| [12] | Maire E. X-ray tomography applied to the characterization of highly porous materials [J]. Annu. Rev. Mater. Res., 2012, 42: 163 |
| [13] | Cao T S, Maire E, Verdu C, et al. Characterization of ductile damage for a high carbon steel using 3D X-ray micro-tomography and mechanical tests-application to the identification of a shear modified GTN model [J]. Comput. Mater. Sci., 2014, 84: 175 |
| [14] | Lee S G, Gokhale A M, Patel G R, et al. Effect of process parameters on porosity distributions in high-pressure die-cast AM50 Mg-alloy [J]. Mater. Sci. Eng., 2006, A427: 99 |
| [15] | Zió?kowski G, Chlebus E, Szymczyk P, et al. Application of X-ray CT method for discontinuity and porosity detection in 316L stainless steel parts produced with SLM technology [J]. Arch. Civ. Mech. Eng., 2014, 14: 608 |
| [16] | Balasundaram A, Gokhale A M. Quantitative characterization of spatial arrangement of shrinkage and gas (air) pores in cast magnesium alloys [J]. Mater. Charact., 2001, 46: 419 |
| [17] | Fansi J, Balan T, Lemoine X, et al. Numerical investigation and experimental validation of physically based advanced GTN model for DP steels [J]. Mater. Sci. Eng., 2013, A569: 1 |
| [18] | Russell K C. The theory of void nucleation in metals [J]. Acta Metall., 1978, 26: 1615 |
| [19] | Bieler T R, Crimp M A, Yang Y, et al. Strain heterogeneity and damage nucleation at grain boundaries during monotonic deformation in commercial purity titanium [J]. JOM, 2009, 61(12): 45 |
| [20] | Landron C, Bouaziz O, Maire E, et al. Characterization and modeling of void nucleation by interface decohesion in dual phase steels [J]. Scr. Mater., 2010, 63: 973 |
| [21] | Bouaziz O, Maire E, Giton M, et al. A model for initiation and growth of damage in dualphase steels identified by X-ray micro-tomography [J]. Metall. Res. Technol., 2008, 105: 102 |
| [22] | Maire E, Bouaziz O, Di Michiel M, et al. Initiation and growth of damage in a dual-phase steel observed by X-ray microtomography [J]. Acta Mater., 2008, 56: 4954 |
| [23] | Chu C C, Needleman A. Void nucleation effects in biaxially stretched sheets [J]. J. Eng. Mater. Technol., 1980, 102: 249 |
| [24] | Zhao C F. Analysis method and application of multi-scale damage evolution of weld specimen with meso-defects [D]. Nanjing: Southeast University, 2016 |
| [24] | 赵超凡. 含细观缺陷的焊接构件损伤跨尺度演化分析方法及其应用 [D]. 南京: 东南大学, 2016 |
| [25] | Zhong Q P, Zhao Z H, Zhang Z. Development of "fractography" and research of fracture micromechanism [J]. J. Mech. Strength, 2005, 27: 358 |
| [25] | 钟群鹏, 赵子华, 张 峥. 断口学的发展及微观断裂机理研究 [J]. 机械强度, 2005, 27: 358 |
| [26] | Wang H. Evolution of microvoid and inclusion in metal materials [D]. Shanghai: Shanghai Jiao Tong University, 2005 |
| [26] | 王 华. 金属中微孔洞和夹杂的演变 [D]. 上海: 上海交通大学, 2005 |
| [27] | Xin R S, Ma Q X, Li W Q. Microstructure and mechanical properties of internal crack healing in a low carbon steel [J]. Mater. Sci. Eng., 2016, A662: 65 |
| [28] | Hu Z, Zhang Y, Teng H, et al. Research progress and prospect of crack healing in metal material [J]. Mater. Rev., 2014, 28(17): 47 |