Materials and Processes

Recent Progress on the Fabrication of TiAl-Based Composites Sheet by Reaction Annealingof Elemental Foils

  • Lin GENG ,
  • Hao WU ,
  • Xiping CUI ,
  • Guohua FAN
Expand
  • School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001, China

Received date: 2018-07-03

  Online published: 2018-07-23

Supported by

Supported by National Key Research and Development Program of China (No.2017YFB0703100) and National Natural Science Foundation of China (Nos.51701081, 51571070 and 51571071)

Abstract

This paper reviews the current progresses on the fabrication of TiAl-based composites produced by reaction annealing of elemental Ti and Al matrix composite foils. This technique includes deformation and reaction annealing of the multilayer Ti/Al metal matrix composite (MMC) sheet, which prevents traditionally direct deformation of brittle TiAl intermetallic, and TiAl-based composites sheets with good strength-ductility synergy have been produced. The research on microstructure evolution and forming mechanism of the TiAl-based composites sheet during reaction annealing has been summarized, with the focus on the reaction mechanism between Al-MMCs and Ti during reaction annealing, and the method to eliminate Kirkendall voids is proposed. A feasible proposal is provided to fabricate large scale TiAl-based composite sheets.

Cite this article

Lin GENG , Hao WU , Xiping CUI , Guohua FAN . Recent Progress on the Fabrication of TiAl-Based Composites Sheet by Reaction Annealingof Elemental Foils[J]. Acta Metall Sin, 2018 , 54(11) : 1625 -1636 . DOI: 10.11900/0412.1961.2018.00308

References

[1] Klassen T, Suryanarayana C, Bormann R.Low-temperature superplasticity in ultrafine-grained Ti5Si3-TiAl composites[J]. Scr. Mater., 2008, 59: 455
[2] Liu Y L, Liu L M, Wang S Q, et al.First-principles study of shear deformation in TiAl and Ti3Al[J]. Intermetallics, 2007, 15: 428
[3] Loria E A.Gamma titanium aluminides as prospective structural materials[J]. Intermetallics, 2000, 8: 1339
[4] Yu H L, Tieu A K, Lu C, et al.A deformation mechanism of hard metal surrounded by soft metal during roll forming[J]. Sci. Rep., 2014, 4: 5017
[5] Du Y, Fan G H, Yu T, et al.Effects of interface roughness on the annealing behaviour of laminated Ti-Al composite deformed by hot rolling[J]. IOP Conf. Ser.: Mater. Sci. Eng., 2015, 89: 012021
[6] Peng L M, Li Z, Li H.Effects of microalloying and ceramic particulates on mechanical properties of TiAl-based alloys[J]. J. Mater. Sci., 2006, 41: 7524
[7] Paul J D H, Appel F, Wagner R. The compression behaviour of niobium alloyed γ-titanium alumindies[J]. Acta Mater., 1998, 46: 1075
[8] Kawabata T, Tamura T, Izumi O.Effect of Ti/Al ratio and Cr, Nb, and Hf additions on material factors and mechanical properties in TiAl[J]. Metall. Trans., 1993, 24A: 141
[9] Park H S, Nam S W, Kim N J, et al.Refinement of the lamellar structure in TiAl-based intermetallic compound by addition of carbon[J]. Scr. Mater., 1999, 41: 1197
[10] Hecht U, Witusiewicz V, Drevermann A, et al.Grain refinement by low boron additions in niobium-rich TiAl-based alloys[J]. Intermetallics, 2008, 16: 969
[11] Muto S, Yamanaka T, Johnson D R, et al. Effects of refractory metals on microstructure and mechanical properties of directionally-solidified TiAl alloys [J]. Mater. Sci. Eng., 2002, A329-331: 424
[12] Ding X F, Lin J P, Zhang L Q, et al.Microstructural control of TiAl-Nb alloys by directional solidification[J]. Acta Mater., 2012, 60: 498
[13] Lasalmonie A.Intermetallics: Why is it so difficult to introduce them in gas turbine engines?[J]. Intermetallics, 2006, 14: 1123
[14] Fang W B, Hu L X, He W X, et al.Microstructure and properties of a TiAl alloy prepared by mechanical milling and subsequent reactive sintering[J]. Mater. Sci. Eng., 2005, A403: 186
[15] Luo J G, Acoff V L.Using cold roll bonding and annealing to process Ti/Al multi-layered composites from elemental foils[J]. Mater. Sci. Eng., 2004, A379: 164
[16] Pang J C, Fan G H, Cui X P, et al.Mechanical properties of Ti-(SiCp/Al) laminated composite with nano-sized TiAl3 interfacial layer synthesized by roll bonding[J]. Mater. Sci. Eng., 2013, A582: 294
[17] Pang J C, Fan G H, Cui X P, et al.Microstructure evolution of in situ (Ti3AlC + Ti5Si3)/Ti3Al composite sheet with a novel quasi-continuous chain reinforcement distribution architecture prepared by using roll bonding and reaction annealing[J]. J. Mater. Sci. Technol., 2013, 29: 1191
[18] Luo J G, Acoff V L.Processing gamma-based TiAl sheet materials by cyclic cold roll bonding and annealing of elemental titanium and aluminum foils[J]. Mater. Sci. Eng., 2006, A433: 334
[19] Wang Q W, Fan G H, Geng L, et al.A novel fabrication route to microlaminated TiB2-NiAl composite sheet with {111}<μνω> texture by roll bonding and annealing treatment[J]. Intermetallics, 2013, 37: 46
[20] Wu H, Cui X P, Geng L, et al.Fabrication and characterization of in-situ TiAl matrix composite with controlled microlaminated architecture based on SiC/Al and Ti system[J]. Intermetallics, 2013, 43: 8
[21] Wu H, Fan G H, Cui X P, et al.A novel approach to accelerate the reaction between Ti and Al[J]. Micron, 2014, 56: 49
[22] Mishin Y, Herzig C.Diffusion in the Ti-Al system[J]. Acta Mater., 2000, 48: 589
[23] He Y H, Jiang Y, Xu N P, et al.Fabrication of Ti-Al micro/nanometer-sized porous alloys through the Kirkendall effect[J]. Adv. Mater., 2007, 19: 2102
[24] Cui X P, Fan G H, Geng L, et al.Growth kinetics of TiAl3 layer in multi-laminated Ti-(TiB2/Al) composite sheets during annealing treatment[J]. Mater. Sci. Eng., 2012, A539: 337
[25] Wu H, Jin B C, Geng L, et al.Ductile-phase toughening in TiBw/Ti-Ti3Al metallic-intermetallic laminate composites[J]. Metall. Mater. Trans., 2015, 46A: 3803
[26] Van Loo F J J, Rieck G D. Diffusion in the titanium-aluminium system—I. Between solid Al and Ti or Ti-Al alloys[J]. Acta Metall., 1973, 21: 61
[27] Xu L, Cui Y Y, Hao Y L, et al. Growth of intermetallic layer in multi-laminated Ti/Al diffusion couples [J]. Mater. Sci. Eng., 2006, A435-436: 638
[28] Fu E K Y, Rawlings R D, McShane H B. Reaction synthesis of titanium aluminides[J]. J. Mater. Sci., 2001, 36: 5537
[29] Yao W, Wu A P, Zou G S, et al.Formation process of the bonding joint in Ti/Al diffusion bonding[J]. Mater. Sci. Eng., 2008, A480: 456
[30] Wu H, Fan G H, Jin B C, et al.Fabrication and mechanical properties of TiBw/Ti-Ti(Al) laminated composites[J]. Mater. Des., 2016, 89: 697
[31] Cui X P, Fan G H, Geng L, et al.Fabrication of fully dense TiAl-based composite sheets with a novel microlaminated microstructure[J]. Scr. Mater., 2012, 66: 276
[32] Wu H, Fan G H, Cui X P, et al.Mechanical properties of (Ti2AlC+Ti3AlC)-TiAl ceramic-intermetallic laminate (CIL) composites[J]. Mater. Sci. Eng., 2013, A585: 439
[33] Martin R, Kampe S L, Marte J S, et al.Microstructure/processing relationships in reaction-synthesized titanium aluminide intermetallic matrix composites[J]. Metall. Mater. Trans., 2002, 33A: 2747
[34] Yang R, Cui Y Y, Dong L M, et al.Alloy development and shell mould casting of gamma TiAl[J]. J. Mater. Process. Technol., 2003, 135: 179
[35] Perez-Bravo M, Madariaga I, Ostolaza K, et al.Microstructural refinement of a TiAl alloy by a two step heat treatment[J]. Scr. Mater., 2005, 53: 1141
[36] Wang J N, Xie K.Grain size refinement of a TiAl alloy by rapid heat treatment[J]. Scr. Mater., 2000, 43: 441
[37] Jakob A, Speidel M O.Microstructure and tensile properties of TiAl compounds formed by reactive foil metallurgy[J]. Mater. Sci. Eng., 1994, A189: 129
[38] Chaudhari G P, Acoff V L.Titanium aluminide sheets made using roll bonding and reaction annealing[J]. Intermetallics, 2010, 18: 472
[39] Court S A, Vasudevan V K, Fraser H L.Deformation mechanisms in the intermetallic compound TiAl[J]. Philos. Mag., 1990, 61A: 141
[40] Appel F, Wagner R.Microstructure and deformation of two-phase γ-titanium aluminides[J]. Mater. Sci. Eng., 1998, R22: 187
[41] Liu C T, Schneibel J H, Maziasz P J, et al.Tensile properties and fracture toughness of TiAl alloys with controlled microstructures[J]. Intermetallics, 1996, 4: 429
[42] Cui X P, Geng L, Fang K, et al.TiAl-based composite sheet with multi-layer distributed reinforcement prepared by solid-liquid reaction[J]. Acta Metall. Sin., 2013, 49: 1462(崔喜平, 耿林, 方堃等. 固液反应法制备增强体层状分布的TiAl基复合材料板[J]. 金属学报, 2013, 49: 1462)
[43] Bai H, Walsh F, Gludovatz B, et al.Bioinspired hydroxyapatite/poly(methyl methacrylate) composite with a nacre-mimetic architecture by a bidirectional freezing method[J]. Adv. Mater., 2016, 28: 50
[44] Bouville F, Maire E, Meille S, et al.Strong, tough and stiff bioinspired ceramics from brittle constituents[J]. Nat. Mater., 2014, 13: 508
[45] Koseki T, Inoue J, Nambu S.Development of multilayer steels for improved combinations of high strength and high ductility[J]. Mater. Trans., 2014, 55: 227
[46] Launey M E, Munch E, Alsem D H, et al.A novel biomimetic approach to the design of high-performance ceramic-metal composites[J]. J. Roy. Soc. Interface, 2010, 7: 741
[47] Launey M E, Ritchie R O.On the fracture toughness of advanced materials[J]. Adv. Mater., 2009, 21: 2103
[48] Froes F H, Suryanarayana C, Eliezer D.Synthesis, properties and applications of titanium aluminides[J]. J. Mater. Sci., 1992, 27: 5113
[49] Messerschmidt U, Bartsch M, Guder S, et al.Dynamic dislocation behaviour in the intermetallic compounds NiAl, TiAl and MoSi2[J]. Intermetallics, 1998, 6: 729
[50] Yamaguchi M, Inui H, Ito K.High-temperature structural intermetallics[J]. Acta Mater., 2000, 48: 307
Outlines

/