Evaluation of Fatigue Properties of CA6NM Martensite Stainless Steel Using Miniature Specimens
Received date: 2018-01-15
Online published: 2018-04-23
Supported by
Supported by National Natural Science Foundation of China (Nos.51771207 and 51501117)
Since structural components in the nuclear power plant are unable to be disassembled during their in service process, it is an urgent and key problem how to quickly and non-destructively evaluate fatigue reliability of these key structural components by using miniature specimens. Fatigue properties of miniature specimens of CA6NM martensite stainless steel for impellers in the nuclear pump were obtained by using symmetrically bending fatigue loading and uniaxial tension-tension fatigue loading, respectively. A comparison of fatigue properties between the miniature specimens and bulk specimens was conducted to examine feasibility for the evaluation of fatigue reliability of the CA6NM steel using miniature specimens. The results show that tensile strength of the 40 μm-thick CA6NM specimens is slightly higher than that of the bulk specimens, but elongation of the 40 μm-thick specimens is lower than that of the bulk counterparts. In low cycle fatigue regime, fatigue strength of the 40 μm-thick specimens subjected to uniaxial tension-tension fatigue loading is lower than that of the standard bulk counterparts. With decreasing the applied stress amplitude, the difference in fatigue properties gradually decreases, and the fatigue limit of the miniature specimen is close to that of the bulk counterparts. Fatigue strength of the 40 μm-thick specimens subjected to bending fatigue loading is much higher than that subjected to uniaxial tension-tension fatigue loading, and also higher than that of the bulk counterparts. Fatigue strength of the miniature specimens is related to the loading mode. The difference in the fatigue mechanism between the miniature specimens and the bulk counterparts is discussed, and the feasibility to evaluate fatigue reliability of the steel using miniature specimens is addressed.
Yefei MA , Zhuman SONG , Siqian ZHANG , Lijia CHEN , Guangping ZHANG . Evaluation of Fatigue Properties of CA6NM Martensite Stainless Steel Using Miniature Specimens[J]. Acta Metall Sin, 2018 , 54(10) : 1359 -1367 . DOI: 10.11900/0412.1961.2018.00023
| [1] | Lu Y G, Zhu R S, Wang X L, et al.Study on gas-liquid two-phase all-characteristics of CAP1400 nuclear main pump[J]. Nucl. Eng. Des., 2017, 319: 140 |
| [2] | Li Y.Study of unsteady flow and fatigue reliability of the reactor coolant pump's impeller [D]. Shanghai: Shanghai Jiao Tong University, 2009(李颖. 核主泵叶轮非定常流场及疲劳寿命可靠性分析 [D]. 上海: 上海交通大学, 2009) |
| [3] | Ma G J, Hu G J, Wu C W.Thermal fatigue analysis and life prediction of nuclear pump shaft surface[J]. Chin. J. Solid Mech., 2015, 36(suppl.1): 145(马国军, 胡光举, 吴承伟. 核主泵主轴表面热疲劳分析与寿命评估[J]. 固体力学学报, 2015, 36(增刊1): 145) |
| [4] | Liu S, Li Z L, Guan Z Q.Analysis on the mechanical-thermal coupling fatigue of the primary pump shaft[J]. China Nucl. Power, 2013, 6: 22(刘松, 李姿琳, 关振群. 核主泵主轴机械-热耦合疲劳分析[J]. 中国核电, 2013, 6: 22) |
| [5] | Trudel A, Lévesque M, Brochu M.Microstructural effects on the fatigue crack growth resistance of a stainless steel CA6NM weld[J]. Eng. Fract. Mech., 2014, 115: 60 |
| [6] | Mirakhorli F, Cao X, Pham X T, et al.Phase structures and morphologies of tempered CA6NM stainless steel welded by hybrid laser-arc process[J]. Mater. Charact., 2017, 123: 264 |
| [7] | Ma S Y, Chen R, He X C, et al.Shot peening induced strengthening of the surface layer of martensite stainless Steel 0Cr13Ni4Mo[J]. Acta Metall. Sin., 2005, 41: 28(马素媛, 陈瑞, 贺笑春等. 0Cr13Ni4Mo马氏体不锈钢表层的喷丸强化[J]. 金属学报, 2005, 41: 28) |
| [8] | Geng C W, He S S, Yu B.Development of martensitic stainless steel ZG0Cr13Ni4Mo[J]. Met. Phys. Examinat. Test., 1992, (4): 13(耿承伟, 何树生, 于波. ZG0Cr13Ni4Mo马氏体不锈钢研制[J]. 物理测试, 1992, (4): 13) |
| [9] | Wang S X, Jia W, Wang Y L.Effect of nitrogen on mechanical properties of martensitic stainless steel 0Cr13Ni4Mo[J]. Spec. Steel, 2001, 22(5): 23(王淑霞, 贾伟, 王毓麟. 氮对0Cr13Ni4 Mo马氏体不锈钢机械性能的影响[J]. 特殊钢, 2001, 22(5): 23) |
| [10] | Zhang T, Gao Y P, Tian F, et al.Failure analysis on fracture of 0Cr13Ni4Mo stainless steel shaft of a steam feed pump in a power unit[J]. Phys. Test. Chem. Anal.(Phys. Test.), 2015, 51: 725(张涛, 高云鹏, 田峰等. 电站汽动给水泵0Cr13Ni4Mo不锈钢主轴断裂失效分析[J]. 理化检验(物理分册), 2015, 51: 725) |
| [11] | Cai Q K, Song B, Gao W Q, et al.Hydrogen-induced failure of 0Cr13Ni4Mo casting steel by aquatic corrosion-fatigue[J]. J. Northeast Univ. Technol., 1987, (2): 202(才庆魁, 宋斌, 高文清等. ZG0Cr13Ni4Mo钢在水介质中腐蚀疲劳过程的氢致开裂分析[J]. 东北工学院学报, 1987, (2): 202) |
| [12] | Gao Y K, Yin Y F, Li X B.Influence of surface integrity on fatigue property for martensite stainless steel[J]. Heat Treat. Met., 2002, 27(8): 30(高玉魁, 殷源发, 李向斌. 表面完整性对马氏体不锈钢疲劳性能的影响[J]. 金属热处理, 2002, 27(8): 30) |
| [13] | Winck L B, Ferreira J L A, Araujo J A, et al. Surface nitriding influence on the fatigue life behavior of ASTM A743 steel type CA6NM[J]. Surf. Coat. Technol., 2013, 232: 844 |
| [14] | Da Silva B L, Oliveira F, Araújo J A, et al. The effect of mean stress on the fatigue behavior of ASTM A743 CA6NM alloy steel [A]. 20th International Congress of Mechanical Engineering[C]. RS: Gramado, 2009: 1 |
| [15] | Dymá?ek P.Recent developments in small punch testing: Applications at elevated temperatures[J]. Theor. Appl. Fract. Mec., 2016, 86: 25 |
| [16] | Zhang B, Lei L M, Yang J, et al.Fatigue properties of titanium alloy thin foils for MEMS applications[J]. Mater. Lett., 2012, 89: 302 |
| [17] | Zhang B, Song Z M, Lei L M, et al.Geometrical scale-sensitive fatigue properties of Ti-6.5Al-3.5Mo-1.5Zr-0.3Si alloys with α/β lamellar microstructures[J]. J. Mater. Sci. Technol., 2014, 30: 1284 |
| [18] | Zhang G P, Takashima K, Higo Y.Size effects on deformation and fatigue behavior of a micron-sized stainless steel[J]. Acta Metall. Sin., 2005, 41: 337(张广平, 高岛和希, 肥後矢吉. 微米尺寸不锈钢的形变与疲劳行为的尺寸效应[J]. 金属学报, 2005, 41: 337) |
| [19] | Zhang G P, Takashima K, Shimojo M, et al.Fatigue behavior of microsized austenitic stainless steel specimens[J]. Mater. Lett., 2003, 57: 1555 |
| [20] | Zhang G P, Wang Z G.Progress in fatigue of small dimensional materials[J]. Acta Metall. Sin., 2005, 41: 1(张广平, 王中光. 小尺度材料的疲劳研究进展[J]. 金属学报, 2005, 41: 1) |
| [21] | Li H X, Bo C Y, Yang B.Study on repairing process of casting defects for martensitic stainless steel turbine blade[J]. Foundry Eng., 2015, (5): 27(李红霞, 柏长友, 杨保. 马氏体不锈钢水轮机叶片铸造缺陷修补工艺的研究[J]. 铸造工程, 2015, (5): 27) |
| [22] | Dai C Y, Zhang G P, Yan C.Size effects on tensile and fatigue behaviour of polycrystalline metal foils at the micrometer scale[J]. Philos. Mag., 2011, 91: 932 |
| [23] | Xu J.Fatigue behavior of FCC-structured metals at micron scales: Effects of length scale and strain gradient [D]. Shenyang: Institute of Metal Research, Chinese Academy of Sciences, 2014(徐进. 微米尺度面心立方金属疲劳行为研究: 尺寸与应变梯度效应 [D]. 沈阳: 中国科学院金属研究所, 2014) |
| [24] | Suresh S.Fatigue of Materials [M]. 2nd Ed., London: Cambridge University Press, 1998: 161 |
| [25] | Da Silva B L, De Oliveira F, Sá M V C, et al. Characterization of ASTM A743 CA6NM alloy steel used in hydrogenator components [A]. 21th International Congress of Mechanical Engineering[C]. Natal, RN: Natal, 2007: 1 |
| [26] | Weiss B, Gr?ger V, Khatibi G, et al.Characterization of mechanical and thermal properties of thin Cu foils and wires[J]. Sen. Actuators, 2002, 99A: 172 |
| [27] | Demir E, Raabe D.Mechanical and microstructural single-crystal Bauschinger effects: Observation of reversible plasticity in copper during bending[J]. Acta Mater., 2010, 58: 6055 |
| [28] | Geers M G D, Brekelmans W A M, Janssen P J M. Size effects in miniaturized polycrystalline FCC samples: Strengthening versus weakening[J]. Int. J. Solids Struct., 2006, 43: 7304 |
| [29] | Fleck N A, Muller G M, Ashby M F, et al.Strain gradient plasticity: Theory and experiment[J]. Acta Metall. Mater., 1994, 42: 475 |
| [30] | Huang K Z, Qiu X M, Jiang H Q.Recent advances in strain gradient plasticity-II—Mechanism-based strain gradient (MSG) plasticity[J]. J. Mech. Strength, 1999, 21: 161(黄克智, 邱信明, 姜汉卿. 应变梯度理论的新进展(二)——基于细观机制的MSG应变梯度塑性理论[J]. 机械强度, 1999, 21: 161) |
| [31] | Fleck N A, Hutchinson J W.A Phenomenological theory for strain gradient effects in plasticity[J]. J. Mech. Phys. Solids, 1993, 41: 1825 |
| [32] | Yang J.Mechanical properties of microstructure units in lamellar structured α+β titanium alloys [D]. Shenyang: Institute of Metal Research, Chinese Academy of Sciences, 2017(杨佳. 片层组织α+β钛合金结构单元的力学性能研究 [D]. 沈阳: 中国科学院金属研究所, 2017) |
/
| 〈 |
|
〉 |