Received date: 2017-09-30
Online published: 2017-12-12
Supported by
Supported by National Natural Science Foundation of China (Nos.51771027 and 51271031), National Key Research and Development Program of China (No.2017YFB0702100) and Aeronautical Science Foundation of China (No.20165474001)
Beneficial from small-size effect, super-high specific surface area and a large amount of defects and dangling bonds on the surface, nanoscale metals exhibit superior chemical activities than traditional bulky counterparts. Nevertheless, it is the high reaction activities of nanoscale metals that in turn make them vulnerable to be oxidized and corroded, which is a main obstacle in their applications. In liquid solutions or liquid-involving multiphase environment, corrosion on nanoscale metals is ubiquitous so that it remains a crucial issue before nanoscale metals are widely employed in real applications. Due to the low-dimension and small-size of nanoscale metals, it is a huge challenge of studying their corrosion behaviors since the experimental and theoretical methods are significantly different from those on bulky metals. In the present paper, recent studies on environmental stability and corrosion behaviors of nanoscale noble metals (Pt, Ag), transition metals (Cu, Ni, Fe), active metals (Al, Mg) and semi-conductor metal (Ge) have been reviewed. Meanwhile, analysis and expectations of theoretical and experimental innovations have also been stated for the further study the corrosion on nanoscale metals.
Key words: low-dimension; nanoscale metal; oxidation; corrosion; environmental stability
Junsheng WU , Bowei ZHANG , Xiaogang LI , Yizhong HUANG . Corrosion of Nanoscale Metals[J]. Acta Metall Sin, 2018 , 54(8) : 1087 -1093 . DOI: 10.11900/0412.1961.2017.00415
| [1] | Sau T K, Rogach A L, Jackel F, et al.Properties and applications of colloidal nonspherical noble metal nanoparticles[J]. Adv. Mater., 2010, 22: 1805 |
| [2] | Ferrando R, Jellinek J, Johnston R L.Nanoalloys: From theory to applications of alloy clusters and nanoparticles[J]. Chem. Rev., 2008, 108: 845 |
| [3] | Rosei F.Nanostructured surfaces: Challenges and frontiers in nanotechnology[J]. J. Phys.: Condensed Matter, 2004, 16: S1373 |
| [4] | Dreizin E L.Metal-based reactive nanomaterials[J]. Prog. Energ. Combust. Sci., 2009, 35: 141 |
| [5] | Wang Q L, Lee S, Choi H.Aging study on the structure of Fe0-nanoparticles: Stabilization, characterization, and reactivity[J]. J. Phys. Chem., 2010, 114C: 2027 |
| [6] | Perez-Alonso F J, Elkj?r C F, Shim S S, et al. Identical locations transmission electron microscopy study of Pt/C electrocatalyst degradation during oxygen reduction reaction[J]. J. Power Sour., 2011, 196: 6085 |
| [7] | Cherevko S, Kulyk N, Mayrhofer K J J. Durability of platinum-based fuel cell electrocatalysts: Dissolution of bulk and nanoscale platinum[J]. Nano Energy, 2016, 29: 275 |
| [8] | Tang L, Han B C, Persson K, et al.Electrochemical stability of nanometer-scale Pt particles in acidic environments[J]. J. Am. Chem. Soc., 2010, 132: 596 |
| [9] | Tang L, Li X Q, Cammarata R C, et al.Electrochemical stability of elemental metal nanoparticles[J]. J. Am. Chem. Soc., 2010, 132: 1722 |
| [10] | Jinnouchi R, Suzuki K K T, Morimoto Y. DFT calculations on electro-oxidations and dissolutions of Pt and Pt-Au nanoparticles[J]. Catal. Today, 2016, 262: 100 |
| [11] | Ivanova O S, Zamborini F P.Size-dependent electrochemical oxidation of silver nanoparticles[J]. J. Am. Chem. Soc., 2010, 132: 70 |
| [12] | Liu Y, Lopes P P, Cha W, et al.Stability limits and defect dynamics in Ag nanoparticles probed by Bragg coherent diffractive imaging[J]. Nano Lett., 2017, 17: 1595 |
| [13] | Keast V J, Myles T A, Shahcheraghi N, et al.Corrosion processes of triangular silver nanoparticles compared to bulk silver[J]. J. Nanopart. Res., 2016, 18: 45 |
| [14] | Elechiguerra J L, Larios-Lopez L, Liu C, et al.Corrosion at the nanoscale: The case of silver nanowires and nanoparticles[J]. Chem. Mater., 2005, 17: 6042 |
| [15] | Taylor C D, Neurock M, Scully J R.First-principles investigation of the fundamental corrosion properties of a model Cu(38) nanoparticle and the (111), (113) surfaces[J]. J. Electrochem. Soc., 2008, 155: C407 |
| [16] | Xia X P, Xie C S, Cai S Z, et al.Corrosion characteristics of copper microparticles and copper nanoparticles in distilled water[J]. Corros. Sci., 2006, 48: 3924 |
| [17] | Zhang B W, Chen B S, Wu J S, et al.The electrochemical response of single crystalline copper nanowires to atmospheric air and aqueous solution[J]. Small, 2017, 13: 1603411 |
| [18] | D'Addato S, Grillo V, Altieri S, et al. Structure and stability of nickel/nickel oxide core-shell nanoparticles[J]. J. Phys.: Condensed Matter, 2011, 23: 175003 |
| [19] | Railsback J G, Johnston-Peck A C, Wang J W, et al. Size-dependent nanoscale Kirkendall effect during the oxidation of nickel nanoparticles[J]. ACS Nano, 2010, 4: 1913 |
| [20] | Zhang B W, Wu J S, Li X G, et al.Passivation of nickel nanoneedles in aqueous solutions[J]. J. Phys. Chem. , 2014, 118C: 9073 |
| [21] | Sarathy V, Tratnyek P G, Nurmi J T, et al.Aging of iron nanoparticles in aqueous solution: Effects on structure and reactivity[J]. J. Phys. Chem., 2008, 112C: 2286 |
| [22] | Reardon E J, Fagan R, Vogan J L, et al.Anaerobic corrosion reaction kinetics of nanosized iron[J]. Environ. Sci. Technol., 2008, 42: 2420 |
| [23] | Liu A R, Liu J, Han J H, et al.Evolution of nanoscale zero-valent iron (nZVI) in water: Microscopicand spectroscopic evidence on the formation of nano- andmicro-structured iron oxides[J]. J. Hazard. Mater., 2017, 322: 129 |
| [24] | Pullin H, Springell R, Parry S, et al.The effect of aqueous corrosion on the structure and reactivity of zero-valent iron nanoparticles[J]. Chem. Eng. J., 2017, 308: 568 |
| [25] | Hedberg Y S, Pradhan S, Cappellini F, et al.Electrochemical surface oxide characteristics of metal nanoparticles (Mn, Cu and Al) and the relation to toxicity[J]. Electrochim. Acta, 2016, 212: 360 |
| [26] | Gromov A A, Strokova Y I, Teipel U.Stabilization of metal nanoparticles—A chemical approach[J]. Chem. Eng. Technol., 2009, 32: 1049 |
| [27] | Lei J P, Huang H, Dong X L, et al.Oxidation and corrosion behaviors of Mg-based nanoparticles[J]. J. Nanosci. Nanotechnol., 2009, 9: 7503 |
| [28] | Hanrath T, Korgel B A.Chemical surface passivation of Ge nanowires[J]. J. Am. Chem. Soc., 2004, 126: 15466 |