Suppression Mechanism and Method of Vortex During Steel Teeming Process in Ladle
Received date: 2017-08-30
Online published: 2017-12-01
Supported by
Supported by National Natural Science Foundation of China (No.U1560207), Open Foundation of Stat Key Laboratory of Advanced Metallurgy, University of Science and Technology Beijing (No.KF12-07)
With the developments of science and technology, the performance of steel is required strictly and the quality of steel needs to improve continuously. In continuous casting process, there is an important flow phenomenon when the molten steel flows from ladle to tundish. It is that the rapidly rotating free surface vortex will form as the liquid level descending continuously. The surface vortex can cause the slag entrainment. In order to suppress slag entrainment by vortex during the steel teeming process, and to improve the cleanliness and quality of steel, the movement process of vortex and variation of flow field are studied through both numerical simulation and water model experiments. Since the eccentricity (eccentricity is the ratio of the nozzle distance and the ladle radius) has a large effect on the vortex formation, the vortex movement and flow field variation at different eccentricities are analyzed in details. And the mechanism of vortex suppression is found. It is that disturbing the velocity distribution of vortex formation or/and decreasing the tangential velocity value can suppress the movement and development of vortex. Thus the critical height of vortex can be decrease and the vortex can be availably suppressed. And then a method of vortex suppression is proposed according to this mechanism of vortex suppression. The method by blowing gas at the bottom of ladle is proposed. And the optimal gas flow rate and gas nozzle position are obtained.
Qiang WANG , Lianyu WANG , Hongxia LI , Jiawei JIANG , Xiaowei ZHU , Zhancheng GUO , Jicheng HE . Suppression Mechanism and Method of Vortex During Steel Teeming Process in Ladle[J]. Acta Metall Sin, 2018 , 54(7) : 959 -968 . DOI: 10.11900/0412.1961.2017.00365
| [1] | Niclas A, Andrey K, Par G J.The effect of different non-metallic inclusions on the machinability of steels[J]. Materials, 2015, 8: 751 |
| [2] | Holappa L E K, Helle A S. Inclusion control in high-performance steels[J]. J. Mater. Process. Technol., 1995, 53: 177 |
| [3] | Zhang L F, Thomas B G.State of the art in the control of inclusions during steel ingot casting[J]. Metall. Mater. Trans., 2006, 37B: 733 |
| [4] | Tripathi N N, Nzotta M, Sandberg A, et al.Effect of ladle age on formation of non-metallic inclusions in ladle treatment[J]. Ironmak. Steelmak., 2004, 31: 235 |
| [5] | Beskow K, Tripathi N N, Nzotta M, et al.Impact of slag-refractory lining reactions on the formation of inclusions in steel[J]. Ironmak. Steelmak., 2004, 31: 514 |
| [6] | Zhang S J, Zhu M Y, Zhang Y L, et al.Study on mechanism of entrapment in slab continuous casting mould with high casting speed and argon blowing[J]. Acta Metall. Sin., 2006, 42: 1087(张胜军, 朱苗勇, 张永亮等. 高拉速吹氩板坯连铸结晶器内的卷渣机理研究[J]. 金属学报, 2006, 42: 1087) |
| [7] | Riaz S, Mills K C, Bain K.Experimental examination of slag/refractory interface[J]. Ironmak. Steelmak., 2002, 29: 107 |
| [8] | Hassall G J, Bain K G, Jones N, et al.Modelling of ladle glaze interactions[J]. Ironmak. Steelmak., 2002, 29: 383 |
| [9] | Lei H, Zhu M Y, He J C.Mathematical modeling of slag entrapment in continuous casting mould[J]. Acta Metall. Sin., 2000, 36: 1113(雷洪, 朱苗勇, 赫冀成. 连铸结晶器内卷渣过程的数学模型[J]. 金属学报, 2000, 36: 1113) |
| [10] | Piva M, Iglesias M, Bissio P, et al.Experiments on vortex funnel formation during drainage[J]. Physica, 2003, 329A: 1 |
| [11] | Sankaranarayanan R, Guthrie R I L. Slag entraining vortexing funnel formation during ladle teeming: Similarity criteria and scale-up relationships[J]. Ironmak. Steelmak., 2002, 29: 147 |
| [12] | Kuwana K, Hassan M I, Signh P K, et al.Scale-model experiment and numerical simulation of a steel teeming process[J]. Mater. Manuf. Process., 2008, 23: 407 |
| [13] | Hammerschmid P, Tacke K H, Popper H, et al.Vortex formation during drainage of metallurgical vessels[J]. Ironmak. Steelmak., 1984, 11: 332 |
| [14] | Sucker D, Reinecke J, Hage-Jewainski H.Flow investigations for melting metallurgical processes[J]. Stahl Eisen, 1985, 105: 765 |
| [15] | Lin R, Yan Z G, Liu T, et al.Modeling formation mechanism of vortex during steel casting in a 60 t LADLE[J]. Chin. J. Process. Eng., 2010, 10: 655(蔺瑞, 颜正国, 刘涛等. 60 t钢包浇注过程中汇流旋涡形成机理[J]. 过程工程学报, 2010, 10: 655) |
| [16] | Pierre V.Récipient métallurgique de coulee [P]. France Pat, No2443892, 1978 |
| [17] | Dardick I I, Kapusta A K, Mikhailovich B M, et al.Methods and facilities for suppressing vortices arising in tundishes or ladles during their respective discharge [P]. Eur Pat, EP1791665, 2007 |
| [18] | Suh J W, Park J, Kim H, et al.Suppression of the vortex in ladle by static magnetic field[J]. ISIJ Int., 2001, 41: 689 |
| [19] | Ono-Nakazato H, Taguchi K, Usui T, et al.Prevention method of swirling flow generation in discharging liquid in the reactor vessel[J]. J. Jpn. Soc. Exp. Mech., 2007, 8: S147 |
| [20] | Mazzaferro G M, Piva M, Ferro S P, et al.Experimental and numerical analysis of ladle teeming process[J]. Ironmak. Steelmak., 2004, 31: 503 |
| [21] | Lin R, Yan Z G, Liu T, et al. Water modelling on the effect of trapezoidal nozzle on vortex during teeming in ladle [J]. Adv. Mater. Res., 2011, 295-297: 716 |
| [22] | Labate M D.Slag retaining device with vortex inhibitor [P]. US Pat, 4799650, 1989 |
| [23] | Huang Y, Ye S F, Su T S, et al.Technology of preventing slag down in casting process[J]. Jiangxi Metall, 1999, 19(6): 1(黄晔, 叶树峰, 苏天森等. 浇注过程的防下渣技术[J]. 江西冶金, 1999, 19(6): 1) |
| [24] | Li H X, Wang Q, Lei H, et al.Mechanism analysis of free-surface vortex formation during steel teeming[J]. ISIJ Int., 2014, 54: 1592 |
| [25] | Li H X, Wang Q, Jiang J W, et al.Analysis of factors affecting free surface vortex formation during steel teeming[J]. ISIJ Int., 2016, 56: 94 |
| [26] | Centerra Resource park 10 Cavendish court Lebanon. User's Guide for Fluent version 6. 3, 2006 |
| [27] | Sankaranarayanan R, Guthrie R I L. Slag entraining vortexing funnel formation during ladle teeming: Similarity criteria and scale-up relationships[J]. Ironmak. Steelmak., 2002, 29: 147 |
| [28] | Jain A K, Ranga R, Kittur G, et al.Vortex formation at vertical pipe intake[J]. J. Hydraulics Division, 1978, 104: 1429 |
| [29] | Aubert J, Brito D, Nataf H C, et al.A systematic experimental study of rapidly rotating spherical convection in water and liquid gallium[J]. Phys. Earth Planet. Int., 2001, 128: 51 |
/
| 〈 |
|
〉 |