Orginal Article

Study on Anisotropic Mechanical Properties of Cold Drawn Pearlitic Steel Wire

  • Peibei JI ,
  • Lichu ZHOU ,
  • Xuefeng ZHOU ,
  • Feng FANG ,
  • Jianqing JIANG
Expand
  • School of Materials Science and Engineering, Southeast University, Nanjing 211189, China

Received date: 2017-07-05

  Online published: 2017-10-23

Supported by

Supported by National Natural Science Foundation of China (No.51371050), Six Talent Peaks Program of Jiangsu Province (No.2015-XCL-004), Industry-University Strategic Research Fund of Jiangsu Province (No.BY2016076-08) and Key Research Project of Jiangsu Province (No.BE2015097)

Abstract

Cold drawn pearlitic steel wires with ultra-high strength are widely applied in industrial fields such as bridge cables, automobile tire and springs rope. In recent years, the strengthening mechanism and microstructure evolution have been profoundly studied. In order to investigate the influence of microstructure evolution on mechanical properties, the anisotropic mechanical properties of cold drawn pearlitic steel wires were investigated by tensile test, SEM and TEM. Results indicated that the distinctions of tensile strength between three directions (parallel to the tensile axis, inclined to the tensile axis (45°), vertical to the tensile axis) were amplified with increasing strain. The effect of strain strengthening was observed in parallel and inclined directions while the vertical direction remained strength stability in 1320 MPa. The wire rod was isotropic and the fracture mode was transgranular fracture; After cold drawing, the tensile strength reached peaks in parallel direction and valleys in vertical direction. The fracture mechanism of inclined and vertical directions remained transgranular or intergranular fracture while the fracture mechanism of parallel direction was converted into microvoid accumulation fracture. In TEM, the phenomenon was discovered that due to non-homogeneous distribution in vertical direction, dislocations piled up at the boundaries resulting in stress concentration. On the contrary, the dislocations were uniformly distributed which led to homogeneous transformation in parallel direction.

Cite this article

Peibei JI , Lichu ZHOU , Xuefeng ZHOU , Feng FANG , Jianqing JIANG . Study on Anisotropic Mechanical Properties of Cold Drawn Pearlitic Steel Wire[J]. Acta Metall Sin, 2018 , 54(4) : 494 -500 . DOI: 10.11900/0412.1961.2017.00274

References

[1] Zelin M.Microstructure evolution in pearlitic steels during wire drawing[J]. Acta Mater., 2002, 50: 4431
[2] Li Y J, Choi P, Goto S, et al.Evolution of strength and microstructure during annealing of heavily cold-drawn 6.3 GPa hypereutectoid pearlitic steel wire[J]. Acta Mater., 2012, 60: 4005
[3] Read H G, Reynolds Jr W T, Hono K, et al. APFIM and TEM studies of drawn pearlitic wire[J]. Scr. Mater., 1997, 37: 1221
[4] Zhang X D, Godfrey A, Huang X X, et al.Microstructure and strengthening mechanisms in cold-drawn pearlitic steel wire[J]. Acta Mater., 2011, 59: 3422
[5] Embury J D, Fisher R M.The structure and properties of drawn pearlite[J]. Acta Metall., 1966, 14: 147
[6] Buono V T L, Gonzalez B M, Lima T M, et al. Measurement of fine pearlite interlamellar spacing by atomic force microscopy[J]. J. Mater. Sci., 1997, 32: 1005
[7] Zhou L C, Hu X J, Ma C, et al.Effect of pearlitic lamella orientation on deformation of pearlite steel wire during cold drawing[J]. Acta Metall. Sin., 2015, 51: 897(周立初, 胡显军, 马驰等. 珠光体层片取向对冷拔珠光体钢丝形变的影响[J]. 金属学报, 2015, 51: 897)
[8] Fang F, Zhao Y F, Liu P P, et al.Deformation of cementite in cold drawn pearlitic steel wire[J]. Mater. Sci. Eng., 2014, A608: 11
[9] Lamontagne A, Massardier V, Kléber X, et al.Comparative study and quantification of cementite decomposition in heavily drawn pearlitic steel wires[J]. Mater. Sci. Eng., 2015, A644: 105
[10] Li Y J, Choi P, Borchers C, et al.Atom probe tomography characterization of heavily cold drawn pearlitic steel wire[J]. Ultramicroscopy, 2011, 111: 628
[11] Li Y J, Choi P, Borchers C, et al.Atomic-scale mechanisms of deformation-induced cementite decomposition in pearlite[J]. Acta Mater., 2011, 59: 3965
[12] Zhou L C, Fang F, Zhou X F, et al.Cementite nano-crystallization in cold drawn pearlitic wires instigated by low temperature annealing[J]. Scr. Mater., 2016, 120: 5
[13] Li Y J, Raabe D, Herbig M, et al.Segregation stabilizes nanocrystalline bulk steel with near theoretical strength[J]. Phys. Rev. Lett., 2014, 113: 106104
[14] Fang F, Zhou L C, Hu X J, et al.Microstructure and mechanical properties of cold-drawn pearlitic wires affect by inherited texture[J]. Mater. Des., 2015, 79: 60
[15] Zhang X D, Godfrey A, Hansen N, et al.Hierarchical structures in cold-drawn pearlitic steel wire[J]. Acta Mater., 2013, 61: 4898
[16] Zhao T Z, Song H W, Zhang G L, et al.The texture evolution at the center of pearlitic steel wire during drawing and its influence on the mechanical properties[J]. Acta Metall. Sin., 2014, 50: 667(赵天章, 宋鸿武, 张光亮等. 拉拔过程中珠光体钢丝心部的织构演化规律及其对力学性能的影响[J]. 金属学报, 2014, 50: 667)
[17] Zhang X D, Godfrey A, Liu W, et al.Evolutions of microstructure and ferritic micro-orientation and texture in a pearlitic steel wire during cold drawing[J]. Acta Metall. Sin., 2010, 46: 141(张晓丹, Godfrey A, 刘伟等. 珠光体钢丝冷拉拔过程中微观组织及铁素体微区取向与织构演变[J]. 金属学报, 2010, 46: 141)
[18] Kapp M W, Hohenwarter A, Wurster S, et al.Anisotropic deformation characteristics of an ultrafine-and nanolamellar pearlitic steel[J]. Acta Mater., 2016, 106: 239
[19] Kammerhofer C, Hohenwarter A, Scheriau S, et al.Influence of morphology and structural size on the fracture behavior of a nanostructured pearlitic steel[J]. Mater. Sci. Eng., 2013, A585: 190
[20] Hohenwarter A, Taylor A, Stock R, et al.Effect of large shear deformations on the fracture behavior of a fully pearlitic steel[J]. Metall. Mater. Trans., 2011, 42A: 1609
[21] He Y, Xiang S, Shi W, et al.Effect of microstructure evolution on anisotropic fracture behaviors of cold drawing pearlitic steels[J]. Mater. Sci. Eng., 2017, A683: 153
[22] Toribio J, Ayaso F J.Anisotropic fracture behaviour of cold drawn steel: A materials science approach[J]. Mater. Sci. Eng., 2003, A343: 265
[23] Suzuki T, Tomota Y, Isaka M, et al.Strength anisotropy and residual stress in drawn pearlite steel wire[J]. ISIJ Int., 2004, 44: 1426
[24] Zhang X D, Hansen N, Godfrey A, et al.Dislocation-based plasticity and strengthening mechanisms in sub-20 nm lamellar structures in pearlitic steel wire[J]. Acta Mater., 2016, 114: 176
[25] Ju H L, Li B H, Wu Z F, et al.Perpendicular magnetic anisotropy in Co/Ni multilayers studied by anomalous Hall effect[J]. Acta Phys. Sin., 2015, 64: 097501(俱海浪, 李宝河, 吴志芳等. Co/Ni多层膜垂直磁各向异性的研究[J]. 物理学报, 2015, 64: 097501)
[26] Chen Z Y, Cai H N, Wang F C, et al.Investigation on anisotropy of dynamic compressive mechanical properties of cold-rolled Cu sheet[J]. Acta Metall. Sin., 2009, 45: 143(陈志永, 才鸿年, 王富耻等. 冷轧Cu板动态压缩力学性能各向异性的研究[J]. 金属学报, 2009, 45: 143)
[27] Xu Y B, Liu M Z.An in situ study of crack nucleation and propagation in pearlite during deformation[J]. Acta Metall. Sin., 1982, 18: 58(徐永波, 刘民治. 珠光体组织的形变、裂纹形核与扩展微观过程的动态研究[J]. 金属学报, 1982, 18: 58)
Outlines

/