Orginal Article

A First-Principles Study on Basal/Prismatic Reorientation-Induced Twinning Path and Alloying Effect in Hexagonal Metals

  • Gang ZHOU ,
  • Lihua YE ,
  • Hao WANG ,
  • Dongsheng XU ,
  • Changgong MENG ,
  • Rui YANG
Expand
  • 1 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    2 School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024, China

Received date: 2017-06-27

  Online published: 2017-08-22

Supported by

Supported by National Key Research and Development Program of China (No.2016YFB0701304) and National Natural Science Foundation of China (No.51671195)

Abstract

In hexagonal metals and alloys, deformation twinning plays an important role, because it is closely relevant to the mechanical behaviors. Recent studies have proposed a new twinning mode via direct lattice reorientation, which results in the basal/prismatic boundary, however, some important details remain unanswered, e.g., the twinning path and alloying effect. In this work, first principles calculations were employed to systematically study the reorientation process from basal to prismatic orientation in hexagonal metals and corresponding alloying effect. The result indicates that different activation energies are required to reorient in various hexagonal metals, and among them, the energy in Mg is the lowest and Os is the highest. Shear and shuffle components compose the reorientation process, where the shuffle component always contributes a significant part of the activation energy in Mg, whereas in Ti with sufficient shear strain, subsequent transition becomes energy-downhill. The pure shear was effected by alloying elements in Mg alloys, but pure shuffle in Ti alloys. Under certain shear or shuffle, subsequent activation energy has a complex dependence on alloying elements.

Cite this article

Gang ZHOU , Lihua YE , Hao WANG , Dongsheng XU , Changgong MENG , Rui YANG . A First-Principles Study on Basal/Prismatic Reorientation-Induced Twinning Path and Alloying Effect in Hexagonal Metals[J]. Acta Metall Sin, 2018 , 54(4) : 603 -612 . DOI: 10.11900/0412.1961.2017.00252

References

[1] Biget M P, Saada G.Low-temperature plasticity of high purity α-titanium single crystals[J]. Philos. Mag., 1989, 59A: 747
[2] Ostapovets A, Molnár P, Gr?eger R. On basal-prismatic twinning interfaces in magnesium [J]. 6th International Conference on Nanomaterials by Severe Plastic Deformation [C]. Bristol: IOP Publishing, 2014: 012134
[3] Zhang X Y, Lou C, Tu J, et al.Plasticity induced by twin lamellar structure in magnesium alloy[J]. J. Mater. Sci. Technol., 2013, 29: 1123
[4] Lou C, Zhang X Y, Wang R H, et al.Effects of untwinning and {1012} twin lamellar structure on the mechanical properties of Mg alloy[J]. Acta Metall. Sin., 2013, 49: 291(娄超, 张喜燕, 汪润红等. 退孪生行为以及{1012}孪晶片层结构对镁合金力学性能的影响[J]. 金属学报, 2013, 49: 291)
[5] Wang Y N, Huang J C.Texture analysis in hexagonal materials[J]. Mater. Chem. Phys., 2003, 81: 11
[6] Yoo M H, Wei C T.Slip modes of hexagonal-close-packed metals[J]. J. Appl. Phys., 1967, 38: 4317
[7] Shan Z W, Liu B Y.The mechanism of {1012} deformation twinning in magnesium[J]. Acta Metall. Sin., 2016, 52: 1267(单智伟, 刘博宇. Mg的{1012}形变孪晶机制[J]. 金属学报, 2016, 52: 1267)
[8] Liu B Y, Wang J, Li B, et al.Twinning-like lattice reorientation without a crystallographic twinning plane[J]. Nat. Commun., 2014, 5: 3297
[9] Zong H X, Ding X D, Lookman T, et al.Collective nature of plasticity in mediating phase transformation under shock compression[J]. Phys. Rev., 2014, 89B: 220101
[10] Kumar A, Wang J, Tomé C N.First-principles study of energy and atomic solubility of twinning-associated boundaries in hexagonal metals[J]. Acta Mater., 2015, 85: 144
[11] Ishii A, Li J, Ogata S.Shuffling-controlled versus strain-controlled deformation twinning: The case for HCP Mg twin nucleation[J]. Int. J. Plast., 2016, 82: 32
[12] Zhang X Y, Li B, Tu J, et al.Non-classical twinning behavior in dynamically deformed cobalt[J]. Mater. Res. Lett., 2015, 3: 142
[13] Li B, Zhang X Y.Twinning with zero twinning shear[J]. Scr. Mater., 2016, 125: 73
[14] Wu W, Gao Y F, Li N, et al.Intragranular twinning, detwinning, and twinning-like lattice reorientation in magnesium alloys[J]. Acta Mater., 2016, 121: 15
[15] Kresse G, Hafner J.Ab initio molecular-dynamics simulation of the liquid-metal amorphous-semiconductor transition in germanium[J]. Phys. Rev., 1994, 49B: 14251
[16] Kresse G, Furthmüller J.Efficient iterative schemes for Ab initio total-energy calculations using a plane-wave basis set[J]. Phys. Rev., 1996, 54B: 11169
[17] Bl?chl P E.Projector augmented-wave method[J]. Phys. Rev., 1994, 50B: 17953
[18] Kresse G, Joubert D.From ultrasoft pseudopotentials to the projector augmented-wave method[J]. Phys. Rev., 1999, 59B: 1758
[19] Perdew J P, Burke K, Ernzerhof M.Generalized gradient approximation made simple[J]. Phys. Rev. Lett., 1996, 77: 3865
[20] Sheppard D, Xiao P H, Chemelewski W, et al.A generalized solid-state nudged elastic band method[J]. J. Chem. Phys., 2012, 136: 074103
[21] Martienssen W, Warlimont H.Springer Handbook of Condensed Matter and Materials Data[M]. Berlin: Springer, 2005: 54
[22] Park J S, Chang Y W. The effect of alloying elements on the c/a ratio of magnesium binary alloys [J]. Adv. Mater. Res., 2007, 26-28: 95
[23] Kim H L, Park J S, Chang Y W.Effects of lattice parameter changes on critical resolved shear stress and mechanical properties of magnesium binary single crystals[J]. Mater. Sci. Eng., 2012, A540: 198
[24] Minárik P, Král R, ?i?ek J, et al.Effect of different c/a ratio on the microstructure and mechanical properties in magnesium alloys processed by ECAP[J]. Acta Mater., 2016, 107: 83
[25] Zheng-Johansson J X, Eriksson O, Johansson B. Systematic behavior of the hexagonal axial ratio for the d transition metals[J]. Phys. Rev., 1999, 59B: 6131
[26] Nan X L, Wang H Y, Zhang L, et al.Calculation of schmid factors in magnesium: Analysis of deformation behaviors[J]. Scr. Mater., 2012, 67: 443
[27] Kwasniak P, Muzyk M, Garbacz H, et al.Influence of oxygen content on the mechanical properties of hexagonal Ti-first principles calculations[J]. Mater. Sci. Eng., 2014, A590: 74
Outlines

/