Micromechanism of Cleavage Fracture of Weld Metals
Received date: 2017-04-24
Online published: 2017-08-14
Supported by
Supported by National Natural Science Foundation of China (Nos.51675255 and 51761027)
Cleavage fracture is the most dangerous form of fracture. Cleavage fracture usually happens well before general yielding at low nominal fracture stress and strain. Cleavage fracture is often spurred by low temperature and determines the toughness in the lower shelf temperature region. This paper describes a new framework for the micromechanism of cleavage fracture of high strength low alloy (HSLA) steel weld metals. Cleavage fracture not only determines the impact toughness in the lower shelf but also plays a decisive role on the impact toughness in the transition temperature region. The toughness is determined by the extending length of a preceding fibrous crack which is terminated by cleavage fracture. Three non-stop successive stages, i.e. crack nucleation, propagation of a second phase particle-sized crack across the particle/grain boundary, propagation of a grain-sized crack across the grain/grain boundary are explained. The "critical event" of cleavage fracture is emphasized which offers the greatest difficulty during crack formation and controls the cleavage process. The critical event indicates the weakest microstructural component and its critical size which specifies the local cleavage fracture stress σf for cleavage fracture. In toughness-study it is paramount important to reveal the critical events for various test specimens. Three criteria for crack nucleation, for preventing crack nucleus from blunting and for crack propagation are testified. An active region specified by these criteria is suggested where the combined stress and strain are sufficient to trigger the cleavage fracture. It can be used in statistical analyses. A case study, using the new framework of micromechanism for analyzing toughness of 8%Ni steel welding metals is presented to analyze the experimental results.
Key words: cleavage fracture; fracture process; critical event; fracture criteria
Jianhong CHEN , Rui CAO . Micromechanism of Cleavage Fracture of Weld Metals[J]. Acta Metall Sin, 2017 , 53(11) : 1427 -1444 . DOI: 10.11900/0412.1961.2017.00145
| [1] | Hahn G T.The influence of microstructure on brittle fracture toughness[J]. Metall. Trans., 1984, 15A: 947 |
| [2] | Stroh A N.The formation of cracks as a result of plastic flow[J]. Proc. Roy. Soc. Math. Phys. Eng. Sci., 1954, 223A: 404 |
| [3] | Knott J F.Some effects of hydrostatic tension on the fracture behaviour of mild steel[J]. J. Iron Steel Inst., 1966, 204: 104 |
| [4] | Brozzo P, Buzzichelli G, Mascanzoni A, et al.Microstructure and cleavage resistance of low-carbon bainitic steels[J]. Met. Sci., 1977, 11: 123 |
| [5] | Curry D A.Cleavage micromechanisms of crack extension in steels[J]. Met. Sci., 1980, 14: 319 |
| [6] | Yang W J, Lee B S, Oh Y T, et al.Microstructural parameters governing cleavage fracture behaviors in the ductile-brittle transition region in reactor pressure vessel steels[J]. Mater. Sci. Eng., 2004, A379: 17 |
| [7] | Ritchie R O, Knott J F, Rice J R.On the relationship between critical tensile stress and fracture toughness in mild steel[J]. J. Mech. Phys. Solids, 1973, 21: 395 |
| [8] | Chen J H, Cao R.Micromechanism of Cleavage Fracture of Metals—A Comprehensive Microphysical Model for Cleavage Cracking in Metals[M]. Waltham, MA, USA: Butterworth-Heinemann, 2014: 3 |
| [9] | Chen J H, Wang G Z, Wang H J.A statistical model for cleavage fracture of low alloy steel[J]. Acta Metall., 1996, 44: 3979 |
| [10] | Cao R, Yan Y J, Du W S, et al.Fracture behaviour of 8%Ni 980 MPa high strength steel at various temperatures Part 2—COD tests[J]. Mater. Sci. Technol., 2011, 27: 145 |
| [11] | Cao R, Li J, Liu D S, et al.Micromechanism of decrease of impact toughness in coarse-grain heat-affected zone of HSLA steel with increasing welding heat input[J]. Metall. Mater. Trans., 2015, 46A: 2999 |
| [12] | Griffiths J R, Owen D R J. An elastic-plastic stress analysis for a notched bar in plane strain bending[J]. J. Mech. Phys. Solids, 1971, 19: 419 |
| [13] | McMeeking R M. Finite deformation analysis of crack-tip opening in elastic-plastic materials and implications for fracture[J]. J. Mech. Phys. Solids, 1977, 25: 357 |
| [14] | Chen J H, Kikuta Y, Araki T, et al.Micro-fracture behaviour induced by M-A constituent (island martensite) in simulated welding heat affected zone of HT80 high strength low alloyed steel[J]. Acta Metall., 1984, 32: 1779 |
| [15] | Smith E.The nucleation and growth of cleavage microcracks in mild steel [A]. Proceedings of Conference on Physical Basis of Yield and Fracture[C]. London: Institute of Physics and Physical Society, 1996: 36 |
| [16] | Chen J H, Wang G Z, Wang Q.Change of critical events of cleavage fracture with variation of microscopic features of low-alloy steels[J]. Metall. Mater. Trans., 2002, 33A: 3393 |
| [17] | Chen J H, Zhu L, Ma H.On the scattering of the local fracture stress σf[J]. Acta Metall. Mater., 1990, 38: 2527 |
| [18] | Chen J H, Wang Q, Wang G Z, et al.Fracture behavior at crack tip—A new framework for cleavage mechanism of steel[J]. Acta Metall., 2003, 51: 1841 |
| [19] | Chen J H, Yan C, Sun J.Further study on the mechanism of cleavage fracture at low temperatures[J]. Acta Metall. Mater., 1994, 42: 251 |
| [20] | Chen J H, Cao R.Scatter of measured KIC related to the scatters of local parameters Xf, σf and εpc [A]. ICF2013[C]. Beijing: Chinese Society of Theoretical and Applied Mechanics, Chinese Society for Corrosion and Protection, China Mechanical Engineering Society, 2013: M10 |
| [21] | Cao R, Zhang X B, Wang Z, et al.Investigation of microstructural features determining the toughness of 980 MPa bainitic weld metal[J]. Metall. Mater. Trans., 2014, 45A: 815 |
/
| 〈 |
|
〉 |