Effect of Cooling Rate on Microstructure and Properties ofa Cu-Containing Titanium Alloy
Received date: 2017-07-03
Online published: 2017-08-04
Supported by
Supported by National Natural Science Foundation of China (No.51631009), National Key Research and Development Program of China (No.2016YFC1100600), Youth Innovation Promotion Association, CAS (No.2014168), Natural Science Foundation of Guangdong Province (No.2015A030312004), and Joint Foundation of Natural Science Foundation of Liaoning Province and Shenyang National Laboratory for Materials Science (No.2015021004)
The Cu-containing titanium alloy has been proved to possess excellent antibacterial performance, which has great potential for clinical application. In this work, the effect of cooling rate on the microstructure, mechanical properties, corrosion resistance and antibacterial property of a Ti6Al4V-5Cu alloy was investigated. Results showed that the furnace-cooled alloy exhibited the best ductility because of the maximum size and volume fraction of the primary α phase in microstructure. The alloys water quenched from 740 and 820 ℃ respectively demonstrated low hardness and yield strength due to the existence of orthorhombic α′′ phase in microstructure. The alloy quenched at 910 ℃ showed the highest hardness and tensile strength, but the lowest plasticity because of the presence of acicular hcp α′ phase. With the increase of heating temperature, the elemental distribution in the alloy became more uniform, and therefore the corrosion resistance increased gradually. However, the cooling rate did not obviously change the antibacterial property of the alloy. The Ti6Al4V-5Cu alloy showed excellent antibacterial property under different cooling rates.
Cong PENG , Shuyuan ZHANG , Ling REN , Ke YANG . Effect of Cooling Rate on Microstructure and Properties ofa Cu-Containing Titanium Alloy[J]. Acta Metall Sin, 2017 , 53(10) : 1377 -1384 . DOI: 10.11900/0412.1961.2017.00267
| [1] | Navarro M, Michiardi A, Casta?o O, et al.Biomaterials in orthopaedics[J]. J. R. Soc. Interface, 2008, 5: 1137 |
| [2] | Arciola C R, Alvi F I, An Y H, et al.Implant infection and infection resistant materials: A mini review[J]. Int. J. Artif. Organs, 2005, 28: 1119 |
| [3] | Deysine M.Infections associated with surgical implants[J]. New Engl. J. Med., 2004, 351: 193 |
| [4] | Hu H, Zhang W, Qiao Y, et al.Antibacterial activity and increased bone marrow stem cell functions of Zn-incorporated TiO2 coatings on titanium[J]. Acta Biomater., 2012, 8: 904 |
| [5] | Zhao L Z, Wang H R, Huo K F, et al.Antibacterial nano-structured titania coating incorporated with silver nanoparticles[J]. Biomaterials, 2011, 32: 5706 |
| [6] | Ren L, Xu L, Feng J W, et al.In vitro study of role of trace amount of Cu release from Cu-bearing stainless steel targeting for reduction of in-stent restenosis[J]. J. Mater. Sci. Mater. Med., 2012, 23: 1235 |
| [7] | Liu J, Li F B, Liu C, et al.Effect of Cu content on the antibacterial activity of titanium-copper sintered alloys[J]. Mater. Sci. Eng., 2014, C35: 392 |
| [8] | Ren L, Memarzadeh K, Zhang S Y, et al.A novel coping metal material CoCrCu alloy fabricated by selective laser melting with antimicrobial and antibiofilm properties[J]. Mater. Sci. Eng., 2016, C67: 461 |
| [9] | Ren L, Ma Z, Li M, et al.Antibacterial properties of Ti-6Al-4V-xCu alloys[J]. J. Mater. Sci. Technol., 2014, 30: 699 |
| [10] | Filip R, Kubiak K, Ziaja W, et al.The effect of microstructure on the mechanical properties of two-phase titanium alloys[J]. J. Mater. Process. Technol., 2003, 133: 84 |
| [11] | Gil F J, Ginebra M P, Manero J M, et al.Formation of α-Widmanst?tten structure: Effects of grain size and cooling rate on the Widmanst?tten morphologies and on the mechanical properties in Ti6Al4V alloy[J]. J. Alloys Compd., 2001, 329: 142 |
| [12] | Osório W R, Cremasco A, Andrade P N, et al.Electrochemical behavior of centrifuged cast and heat treated Ti-Cu alloys for medical applications[J]. Electrochim. Acta, 2010, 55: 759 |
| [13] | Koike M, Cai Z, Oda Y, et al.Corrosion behavior of cast Ti-6Al-4V alloyed with Cu[J]. J. Biomed. Mater. Res., 2005, 73B: 368 |
| [14] | Kikuchi M, Takada Y, Kiyosue S, et al.Mechanical properties and microstructures of cast Ti-Cu alloys[J]. Dent. Mater., 2003, 19: 174 |
| [15] | Aoki T, Okafor I C I, Watanabe I, et al. Mechanical properties of cast Ti-6Al-4V-XCu alloys[J]. J. Oral Rehabil., 2004, 31: 1109 |
| [16] | Ma Z, Ren L, Liu R, et al.Effect of heat treatment on Cu distribution, antibacterial performance and cytotoxicity of Ti-6Al-4V-5Cu alloy[J]. J. Mater. Sci. Technol., 2015, 31: 723 |
| [17] | Cao C N.Principles of Electrochemistry of Corrosion [M]. 3rd Ed., Beijing: Chemical Industry Press, 2008: 74(曹楚南. 腐蚀电化学原理 [M]. 第3版. 北京: 化学工业出版社, 2008: 74) |
| [18] | Matsumoto H, Yoneda H, Sato K, et al.Room-temperature ductility of Ti-6Al-4V alloy with α′ martensite microstructure[J]. Mater. Sci. Eng., 2011, A528: 1512 |
| [19] | Colins P C, Koduri S, Welk B, et al.Neural networks relating alloy composition, microstructure, and tensile properties of α/β-processed TIMETAL 6-4[J]. Metall. Mater. Trans., 2012, 44A: 1441 |
| [20] | Jovanovi? M T, Tadi? S, Zec S, et al.The effect of annealing temperatures and cooling rates on microstructure and mechanical properties of investment cast Ti-6Al-4V alloy[J]. Mater. Des., 2006, 27: 192 |
| [21] | Tarzimoghadam Z, Sandl?bes S, Pradeep K G, et al.Microstructure design and mechanical properties in a near-α Ti-4Mo alloy[J]. Acta Mater., 2015, 97: 291 |
| [22] | Sun Y, Zeng W D, Han Y F, et al.Modeling the correlation between microstructure and the properties of the Ti-6Al-4V alloy based on an artificial neural network[J]. Mater. Sci. Eng., 2011, A528: 8757 |
| [22] | Li C F, Li G P, Yang Y, et al.Influence of quenching temperature on martensite type in Ti-4Al-4.5Mo alloy[J]. Acta Metall. Sin., 2010, 46: 1061(李长富, 李阁平, 杨义等. 淬火温度对Ti-4Al-4.5Mo合金马氏体类型的影响[J]. 金属学报, 2010, 46: 1061) |
| [24] | Jiang X J, Jing R, Ma M Z, et al.The orthorhombic α″ martensite transformation during water quenching and its influence on mechanical properties of Ti-41Zr-7.3Al alloy[J]. Intermetallics, 2014, 52: 32 |
| [25] | Yu Z T, Zhou L. Influence of martensitic transformation on mechanical compatibility of biomedical β type titanium alloy TLM [J]. Mater. Sci. Eng., 2006, A438-440: 391 |
| [26] | Moiseev V N, Polyak é V, Sokolova A Y.Martensite strengthening of titanium alloys[J]. Met. Sci. Heat Treat., 1975, 17: 687 |
| [27] | Bai Y, Gai X, Li S J, et al.Improved corrosion behaviour of electron beam melted Ti-6Al-4V alloy in phosphate buffered saline[J]. Corros. Sci., 2017, 123: 289 |
| [28] | Liu R, Memarzadeh K, Chang B, et al.Antibacterial effect of copper-bearing titanium alloy (Ti-Cu) against Streptococcus mutans and Porphyromonas gingivalis[J]. Sci. Rep., 2016, 6: 29985 |
| [29] | Zhang E L, Wang X Y, Chen M, et al.Effect of the existing form of Cu element on the mechanical properties, bio-corrosion and antibacterial properties of Ti-Cu alloys for biomedical application[J]. Mater. Sci. Eng., 2016, C69: 1210 |
| [30] | Ma Z, Ren L, Liu R, et al.Effect of heat treatment on cu distribution, antibacterial performance and cytotoxicity of Ti-6Al-4V-5Cu alloy[J]. J. Mater. Sci. Technol., 2015, 31: 723 |
/
| 〈 |
|
〉 |