A Review: Research on MR-Compatible Alloys in MRI
Received date: 2017-07-03
Online published: 2017-07-31
Supported by
Supported by National Natural Science Foundation of China (No.31370976)
Magnetic resonance imaging (MRI) is widely used in clinical applications. Metallic medical devices and implants used under MRI normally produce noticeable artifact which seriously affects image quality. Therefore, the artifact is an essential problem that should be solved for metallic biomaterials. Although artifact can be reduced by technical manipulation, it cannot be eliminated completely. This paper summarizes recent studies on MR-compatible alloys such as Zr alloys, Nb alloys and Cu alloys. Compared with normally clinical metallic materials, MR-compatible alloys described in this article can effectively reduce or eliminate artifacts under MRI. MR-compatibility will become an essential property to implant materials and devices. Thus developing metallic biomaterials with low magnetic susceptibility and excellent comprehensive performance becomes more important.
Key words: magnetic resonance imaging; metallic artifact; MR-compatibility; Zr alloy; Cu alloy
Yibin REN , Jun LI , Qingchuan WANG , Ke YANG . A Review: Research on MR-Compatible Alloys in MRI[J]. Acta Metall Sin, 2017 , 53(10) : 1323 -1330 . DOI: 10.11900/0412.1961.2017.00265
| [1] | Wang W D.Research on magnetic resonance imaging guided bone biopsy robot and key technologies [D]. Xi'an: Northwestern Polytechnical University, 2014(王文东. 磁共振图像向导的骨活检手术机器人关键技术研究 [D]. 西安: 西北工业大学, 2014) |
| [2] | Schenck J F.Safety of strong, static magnetic fields[J]. J. Magn. Reson. Imaging, 2000, 12: 2 |
| [3] | Tian J G, Liu M L, Xia Z F, et al.Safety factors of magnetic resonance imaging[J]. Chin. J. Magn. Reson., 2000, 17: 505(田建广, 刘买利, 夏照帆等. 磁共振成像的安全性[J]. 波谱学杂志, 2000, 17: 505) |
| [4] | Liu Y, Long D, Qian X M.Safety factors of magnetic resonance imaging and cardiac metal implants[J]. Chin. J. Misdiagn., 2007, 7: 7234(刘瑜, 龙丹, 钱晓明. 磁共振成像的安全性与心脏金属移植物[J]. 中国误诊学杂志, 2007, 7: 7234) |
| [5] | Luo M M.Research on the issues of fetal magnetic resonance safety [D]. Guangzhou: Southern Medical University, 2015(罗敏敏. 胎儿磁共振安全问题研究 [D]. 广州: 南方医科大学, 2015) |
| [6] | Syed M A, Mohiaddin R H.Magnetic Resonance Imaging of Congenital Heart Disease[M]. London: Springer, 2012: 39 |
| [7] | Schenck J F.The role of magnetic susceptibility in magnetic resonance imaging: MRI magnetic compatibility of the first and second kinds[J]. Med. Phys., 1996, 23: 815 |
| [8] | Lee M J, Kim S, Lee S A, et al.Overcoming artifacts from metallic orthopedic implants at high-field-strength MR imaging and multi-detector CT[J]. Radiographics, 2007, 27: 791 |
| [9] | Nitatori T, Hanaoka H, Hachiya J, et al.MRI artifacts of metallic stents derived from imaging sequencing and the ferromagnetic nature of materials[J]. Radiat. Med., 1999, 17: 329 |
| [10] | Bernstein M A, Huston J, Ward H A.Imaging artifacts at 3.0 T[J]. J. Magn. Reson. Imaging, 2006, 24: 735 |
| [11] | Bagheri M H, Hosseini M M, Emami M J, et al.Metallic artifact in MRI after removal of orthopedic implants[J]. Eur. J. Radiol., 2012, 81: 584 |
| [12] | Zhou F Y, Qiu K J, Li H F, et al.Screening on binary Zr-1X (X= Ti, Nb, Mo, Cu, Au, Pd, Ag, Ru, Hf and Bi) alloys with good in vitro cytocompatibility and magnetic resonance imaging compatibility[J]. Acta Biomater., 2013, 9: 9578 |
| [13] | Zhou D B, Wang S P, Wang S G, et al.Bulk metallic glasses: MRI compatibility and its correlation with magnetic susceptibility[J]. J. Mater. Sci. Technol., 2016, 32: 496 |
| [14] | Zhou F Y.Microstructure and property of novel Zr-based alloys for biomedical application [D]. Harbin: Harbin Harbin Engeering University, 2014(周飞宇. 新型医用锆基合金的组织结构与性能研究 [D]. 哈尔滨: 哈尔滨工程大学, 2014) |
| [15] | Salda?a L, Méndez-Vilas A, Jiang L, et al.In vitro biocompatibility of an ultrafine grained zirconium[J]. Biomaterials, 2007, 28: 4343 |
| [16] | Kondo R, Nomura N, Suyalatu, et al. Microstructure and mechanical properties of as-cast Zr-Nb alloys[J]. Acta Biomater., 2011, 7: 4278 |
| [17] | Kondo R, Shimizu R, Nomura N, et al.Effect of cold rolling on the magnetic susceptibility of Zr-14Nb alloy[J]. Acta Biomater., 2013, 9: 5795 |
| [18] | Suyalatu, Nomura N, Oya K, et al. Microstructure and magnetic susceptibility of as-cast Zr-Mo alloys[J]. Acta Biomater., 2010, 6: 1033 |
| [19] | Suyalatu, Kondo R, Tsutsumi Y, et al. Effects of phase constitution on magnetic susceptibility and mechanical properties of Zr-rich Zr-Mo alloys[J]. Acta Biomater., 2011, 7: 4259 |
| [20] | Imai H, Tanaka Y, Nomura N, et al.Magnetic susceptibility, artifact volume in MRI, and tensile properties of swaged Zr-Ag composites for biomedical applications[J]. J. Mech. Behav. Biomed. Mater., 2017, 66: 152 |
| [21] | Zhou D B, Wang S G, Wang S P, et al.MRI compatibility of several early transition metal based alloys and its influencing factors[J]. J. Biomed. Mater. Res. Part B, 2017, doi: 10.1002/jbm.b.33832 |
| [22] | O'Brien B, Stinson J, Carroll W. Development of a new niobium-based alloy for vascular stent applications[J]. J. Mech. Behav. Biomed. Mater., 2008, 1: 303 |
| [23] | O'Brien B J, Stinson J S, Boismier D A, et al. Characterization of an NbTaWZr alloy designed for magnetic resonance angiography compatible stents[J]. Biomaterials, 2008, 29: 4540 |
| [24] | Li H Z, Xu J.MRI compatible Nb-Ta-Zr alloys used for vascular stents: Optimization for mechanical properties[J]. J. Mech. Behav. Biomed. Mater., 2014, 32: 166 |
| [25] | Li H Z, Zhao X, Xu J.MRI-compatible Nb-60Ta-2Zr alloy for vascular stents: Electrochemical corrosion behavior in simulated plasma solution[J]. Mater. Sci. Eng., 2015, C56: 205 |
| [26] | Li X M, Li H Z, Wang S P, et al.MRI-compatible Nb-60Ta-2Zr alloy used for vascular stents: Haemocompatibility and its correlation with protein adsorption[J]. Mater. Sci. Eng., 2014, C42: 385 |
| [27] | van Dijk L C, van Holten J, van Dijk B P, et al. A precious metal alloy for construction of MR imaging-compatible balloon-expandable vascular stents[J]. Radiology, 2001, 219: 284 |
| [28] | Wataha J C, Shor K.Palladium alloys for biomedical devices[J]. Expert Rev. Med. Devices, 2010, 7: 489 |
| [29] | Liu Y B, Hu D Y, Xia L M, et al.Research about interventional magnetic resonance imaging[J]. Radiol. Pract., 2003, 18: 611(刘于宝, 胡道予, 夏黎明等. 介入性磁共振器械的研究[J]. 放射学实践, 2003, 18: 611) |
| [30] | Liu P, Ren F Z, Jia S G.Copper Alloy and Its Application [M]. Beijing: Chemical Industry Press, 2007: 1(刘平, 任凤章, 贾淑果. 铜合金及其应用 [M]. 北京: 化学工业出版社, 2007: 1) |
| [31] | Spuentrup E, Ruebben A, Stuber M, et al.Metallic renal artery MR imaging stent: Artifact-free lumen visualization with projection and standard renal MR angiography[J]. Radiology, 2003, 227: 897 |
| [32] | Li J, Ren Y B, Ibrahim M, et al.MR-compatible silicon brass for magnetic resonance guided biopsy application[J]. Mater. Lett., 2017, 202: 162 |
| [33] | Imai H, Tanaka Y, Nomura N, et al.Three-dimensional quantification of susceptibility artifacts from various metals in magnetic resonance images[J]. Acta Biomater., 2013, 9: 8433 |
| [34] | Buecker A, Spuentrup E, Ruebben A, et al.Artifact-free in-stent lumen visualization by standard magnetic resonance angiography using a new metallic magnetic resonance imaging stent[J]. Circulation, 2002, 105: 1772 |
| [35] | Spuentrup E, Ruebben A, Mahnken A, et al.Artifact-free coronary magnetic resonance angiography and coronary vessel wall imaging in the presence of a new, metallic, coronary magnetic resonance imaging stent[J]. Circulation, 2005, 111: 1019 |
| [36] | Astary G W, Peprah M K, Fisher C R, et al.MR measurement of alloy magnetic susceptibility: Towards developing tissue-susceptibility matched metals[J]. J. Magn. Reson., 2013, 233: 49 |
| [37] | Weiss C R, Nour S G, Lewin J S.MR-guided biopsy: A review of current techniques and applications[J]. J. Magn. Reson. Imaging, 2008, 27: 311 |
| [38] | Dogan B E, Le-Petross C H, Stafford J R, et al. MRI-guided vacuum-assisted breast biopsy performed at 3 T with a 9-gauge needle: preliminary experience[J]. Am. J. Roentgenol., 2012, 199: W651 |
| [39] | Shafiei F, Honda E, Takahashi H, et al.Artifacts from dental casting alloys in magnetic resonance imaging[J]. J. Dent. Res., 2003, 82: 602 |
| [40] | Taniyama T, Sohmura T, Etoh T, et al.Metal artifacts in MRI from non-magnetic dental alloy and its FEM analysis[J]. Dent. Mater. J., 2010, 29: 297 |
| [41] | Silvestri Z, Davis R S, Genevès G, et al.Volume magnetic susceptibility of gold-platinum alloys: Possible materials to make mass standards for the watt balance experiment[J]. Metrologia, 2003, 40: 172 |
| [42] | Uyama E, Inui S, Hamada K, et al.Magnetic susceptibility and hardness of Au-xPt-yNb alloys for biomedical applications[J]. Acta Biomater., 2013, 9: 8449 |
| [43] | Li Q Y, Zhang S.Nutritionist Handbook [M]. Beijing: People's Military Medical Press, 2009: 46(李清亚, 张松. 营养师手册 [M]. 北京: 人民军医出版社, 2009: 46) |
| [44] | Bowen P K, Drelich J, Goldman J.Zinc exhibits ideal physiological corrosion behavior for bioabsorbable stents[J]. Adv. Mater., 2013, 25: 2577 |
| [45] | Vojtěch D, Kubásek J, ?erák J, et al.Mechanical and corrosion properties of newly developed biodegradable Zn-based alloys for bone fixation[J]. Acta Biomater., 2011, 7: 3515 |
| [46] | Ren Y B, Li J, Dong J H, et al.Magnetic compatibility zinc alloy and application thereof [P]. Chin. Pat., 20150542175.X, 2017(任伊宾, 李俊, 东家慧等. 一种磁兼容锌合金及其应用 [P]. 中国专利, 20150542175.X, 2017) |
/
| 〈 |
|
〉 |