Effect of Martensitic Transformation on Stress Evolution in Multi-Pass Butt-Welded 9%Cr Heat-Resistant Steel Pipes
Received date: 2017-02-13
Online published: 2017-04-19
Supported by
Supported by National Natural Science Foundation of China (Nos.51374153 and 51574181) and State Key Laboratory of Advanced Welding and Joining, Harbin Institute of Technology (No.AWJ-Z15-02)
It has been recognized that low temperature martensitic transformation can reduce harmful tensile stress and generate beneficial compressive stress in weld zone of single pass welded joints. The influence of martensitic transformation is even greater in 9%Cr steel because of its high hardenability and low transformation temperature (about 100~400 ℃). However, compressive stress was confined in certain parts of weld zone in multi-pass butt-welded 9%Cr steel pipes. In this work, stress evolution in a multi-pass butt-welded 9%Cr steel pipe was predicted using Abaqus software, and the effect of martensitic transformation was further investigated. The simulated results show that the overall pattern for the axial and hoop stresses appears to be similar, despite the lower magnitudes for axial stress. The maximum compressive stress was found in the final weld pass, and the maximum tensile stress was formed in the weld pass adjacent to the final weld pass. Stress in weld passes adjacent to weld root is relatively low. Tensile stress due to thermal contraction in the final weld pass was relieved by martensitic transformation and clear compressive stress was formed. However, little effect of martensitic transformation was found on the significant tensile residual stress in weld passes adjacent to the final weld pass. The final weld pass has the primary effect on the formation of residual stress. Compressive stress was indeed generated by martensitic transformation in former weld pass, however it was relieved by weld thermal cycle of latter weld pass. As a result, the effect of martensitic transformation appears to be confined to the final weld pass. The influence of martensitic transformation is greater around outer surface than that around inner surface.
Xue WANG , Lei HU , Dongxu CHEN , Songtao SUN , Liquan LI . Effect of Martensitic Transformation on Stress Evolution in Multi-Pass Butt-Welded 9%Cr Heat-Resistant Steel Pipes[J]. Acta Metall Sin, 2017 , 53(7) : 888 -896 . DOI: 10.11900/0412.1961.2017.00034
| [1] | Bugge J, Kj?r S, Blum R.High-efficiency coal-fired power plants development and perspectives[J]. Energy, 2006, 31: 1437 |
| [2] | Liu Z D, Cheng S C, Wang Q J, et al.Development of Boiler Steel Used for 600 ℃ Power Plants in China [M]. Beijing: Metallurgical Industry Press, 2011: 345 |
| [2] | (刘正东, 程世长, 王起江等. 中国600 ℃火电机组锅炉钢进展 [M]. 北京: 冶金工业出版社, 2011: 345) |
| [3] | Liang W, Murakawa H, Deng D A.Investigation of welding residual stress distribution in a thick-plate joint with an emphasis on the features near weld end-start[J]. Mater. Des., 2015, 67: 303 |
| [4] | Wang X, Pan Q G, Tao Y S, et al.Type IV creep rupture characteristics of P92 steel weldment[J]. Acta Metall. Sin., 2012, 48: 427 |
| [4] | (王学, 潘乾刚, 陶永顺等. P92钢焊接接头IV型蠕变断裂特性[J]. 金属学报, 2012, 48: 427) |
| [5] | Zhang G D, Zhou C Y, Xue J L.Finite element analysis of high temperature piping creep under inner pressure and welding residual stress[J]. Acta Metall. Sin., 2008, 44: 1271 |
| [5] | (张国栋, 周昌玉, 薛吉林. 内压与焊接残余应力共同作用下高温管道蠕变有限元分析[J]. 金属学报, 2008, 44: 1271) |
| [6] | Zhang G D, Zhou C Y.Finite element simulations of welding residual stress and creep damage for welded joint[J]. Acta Metall. Sin., 2008, 44: 848 |
| [6] | (张国栋, 周昌玉. 焊接接头残余应力及蠕变损伤的有限元模拟[J]. 金属学报, 2008, 44: 848) |
| [7] | Moat R J, Stone H J, Shirzadi A A, et al.Design of weld fillers for mitigation of residual stresses in ferritic and austenitic steel welds[J]. Sci. Technol. Weld. Join., 2011, 16: 279 |
| [8] | Ramjaun T, Stone H J, Karlsson L, et al.Effect of interpass temperature on residual stresses in multi-pass welds produced using low transformation temperature filler alloy[J]. Sci. Technol. Weld. Join., 2014, 19: 44 |
| [9] | Ooi S W, Garnham J E, Ramjaun T I.Review: Low transformation temperature weld filler for tensile residual stress reduction[J]. Mater. Des., 2014, 56: 773 |
| [10] | Mochizuki M, Toyoda M.Strategy of considering microstructure effect on weld residual stress analysis[J]. J. Pressure Vessel Technol., 2006, 129: 619 |
| [11] | Francis J A, Bhadeshia H K D H, Withers P J. Welding residual stresses in ferritic power plant steels[J]. Mater. Sci. Technol., 2007, 23: 1009 |
| [12] | Lee C H, Chang K H.Prediction of residual stresses in high strength carbon steel pipe weld considering solid-state phase transformation effects[J]. Comput. Struct., 2011, 89: 256 |
| [13] | Deng D A, Zhang Y B, Li S, et al.Influence of solid-state phase transformation on residual stress in P92 steel welded joint[J]. Acta Metall. Sin., 2016, 52: 394 |
| [13] | (邓德安, 张彦斌, 李索等. 固态相变对P92钢焊接接头残余应力的影响[J]. 金属学报, 2016, 52: 394) |
| [14] | Yaghi A H, Hyde T H, Becker A A, et al.A comparison between measured and modeled residual stresses in a circumferentially butt-welded P91 steel pipe[J]. J. Pressure Vessel Technol., 2010, 132: 011206 |
| [15] | Deng D A, Murakawa H.Prediction of welding residual stress in multi-pass butt-welded modified 9Cr-1Mo steel pipe considering phase transformation effects[J]. Comp. Mater. Sci., 2006, 37: 209 |
| [16] | Yaghi A H, Hyde T H, Becke A A, et al.Finite element simulation of welding and residual stresses in a P91 steel pipe incorporating solid-state phase transformation and post-weld heat treatment[J]. J. Strain Anal. Eng. Des., 2008, 43: 275 |
| [17] | Ning B Q, Liu Y C, Qiao Z X, et al.Determination of critical cooling rates in undercooled austenite transformation process of T91 ferritic heat-resistant steel[J]. J. Mater. Eng., 2007, (9): 9 |
| [17] | (宁保群, 刘永长, 乔志霞等. T91铁素体耐热钢过冷奥氏体转变过程中临界冷却速度的研究[J]. 材料工程, 2007, (9): 9) |
| [18] | Koistinen D P, Marburger R E.A general equation prescribing the extent of the austenite-martensite transformation in pure iron-carbon alloys and plain carbon steels[J]. Acta Metall., 1959, 7: 59 |
| [19] | Karlsson R I, Josefson B L.Three-dimensional finite element analysis of temperatures and stresses in a single-pass butt-welded pipe[J]. J. Pressure Vessel Technol., 1990, 112: 76 |
| [20] | Paddea S, Francis J A, Paradowska A M, et al.Residual stress distributions in a P91 steel-pipe girth weld before and after post weld heat treatment[J]. Mater. Sci. Eng., 2012, A534: 663 |
| [21] | Zhang Y H, Li H Q, Xu Y.Reasons for metallography defect form and the formation of P91 steel main steam pipe welding seam[J]. Northeast Electr. Power Technol., 2009, (7): 1 |
| [21] | (张艳红, 李宏强, 徐昀. P91钢主蒸汽管道焊缝金相缺陷形态及其形成原因探讨[J]. 东北电力技术, 2009, (7): 1) |
| [22] | Wang Z Y, Li S J, Hao X J, et al.Ultrasonic testing of interlayer cracks in P91 butt weld[J]. Nondestr. Test., 2011, 33(5): 54 |
| [22] | (王志永, 李树军, 郝晓军等. P91钢管对接焊缝层间裂纹的超声波检测[J]. 无损检测, 2011, 33(5): 54) |
| [23] | Wang X, Hu L, Xu Q, et al.Influence of martensitic transformation on welding residual stress in plates and pipes[J]. Sci. Technol. Weld. Join., 2016, doi: 10.1080/13621718.2016.1263711 |
| [24] | Brickstad B, Josefson B L.A parametric study of residual stresses in multi-pass butt-welded stainless steel pipes[J]. Int. J. Pressure Vessels Piping, 1998, 75: 11 |
| [25] | Radaj D.Heat Effects of Welding: Temperature Field, Residual Stress, Distortion[M]. Berlin Heidelberg: Springer-Verlag, 1992: 204 |
/
| 〈 |
|
〉 |