Research on the Collaborative Effect of Plastic Deformation and Solution Treatment in the Intergranular Corrosion Property of Austenite Stainless Steel
Received date: 2016-07-05
Online published: 2017-03-31
Supported by
Supported by National Natural Science Foundation of China (No.51304186) and China Postdoctoral Science Foundation (No.2016M590454)
AISI 304 austenite stainless steel was applied extensively in the modern industry due to its good properties on mechanics and corrosion resistance. However, there is severe intergranular corrosion when the AISI 304 was working at the temperature 420~850 ℃ called sensitizing temperature. This phenomenon was more obvious with increase of strain. In addition, this effect can not be removed completely even with the heat treatment subsequently. In present work, the influence of solution treatment and plastic deformation on the intergranular corrosion property of AISI 304 was investigated. The specimens subjected to different strain were obtained by the uniaxial tensile tests at room temperature. XRD was used to measure the fraction of martensitic phase which was induced by deformation. Optical metal lographic microscope was applied to observe the evolution of microstructure. The influence of various deformation values, solution temperature and holding time on intergranular corrosion was quantitative analyzed by electrochemical potentiodynamic reactivation (EPR) method. Experimental results showed that the degree of the intergranular corrosion increased with the increase of deformation, and with the decrease of solution temperature and holding time. It is indicated that since the solubility of carbon in martensite and austenite is discrepant, the content of carbon in the grains recrystallized is discrepant too. The more martensite is transformed, the more chromium carbide is formed in the grain boundary after sensitization. This phenomenon causes poor intergranular corrosion resistance due to the lack of chromium. In addition, the carbon segregation which is caused by plastic deformation will relieve with the rise of solution temperature and holding time. It is because that the carbon atom is more active at higher temperature, and the distribution of carbon is more homogeneous with the extended holding time. Then the quantity of chromium carbide will decrease in solution treatment process. Consequently the chromium depletion will be mitigated. From the above, a uniform solution treatment condition is not suitable for austenite stainless steel with the effect of martensitic transformation in cold working. Flexible scheme can be employed to insure better combination property of products.
Xiaosong ZHANG , Yong XU , Shihong ZHANG , Ming CHENG , Yonghao ZHAO , Qiaosheng TANG , Yuexia DING . Research on the Collaborative Effect of Plastic Deformation and Solution Treatment in the Intergranular Corrosion Property of Austenite Stainless Steel[J]. Acta Metall Sin, 2017 , 53(3) : 335 -344 . DOI: 10.11900/0412.1961.2016.00284
| [1] | Li Z J, Chen X R, Sun Q Q, et al.Recent research and prospect of duplex stainless steel[J]. Foundry Technol., 2011, 32: 1320 |
| [1] | (李志军, 陈湘茹, 孙卿卿等. 双相不锈钢的研究与发展[J]. 铸造技术, 2011, 32: 1320) |
| [2] | Lo K H, Shek C H, Lai J K L. Recent developments in stainless steels[J]. Mater. Sci. Eng., 2009, R65: 39 |
| [3] | Xu Y, Zhang S H, Song H W, et al.The enhancement of transformation induced plasticity effect on austenitic stainless steels by cyclic tensile loading and unloading[J]. Mater. Lett., 2011, 65: 1545 |
| [4] | Ahn T H, Oh C S, Kim D H, et al.Investigation of strain-induced martensitic transformation in metastable austenite using nanoindentation[J]. Scr. Mater., 2010, 63: 540 |
| [5] | Wang L N, Yang P, Mao W M.Analysis of martensitic transformation during tension of high manganese trip steel at high strain rates[J]. Acta Metall. Sin., 2016, 52: 1045 |
| [5] | (王丽娜, 杨平, 毛卫民. 高锰TRIP钢高速拉伸时的马氏体转变行为分析[J]. 金属学报, 2016, 52: 1045) |
| [6] | Liu D X.Corrosion and Protection of Materials [M]. Xi'an: Northwestern Polytechnical University Press, 2005: 145 |
| [6] | (刘道新. 材料的腐蚀与防护[M]. 西安: 西北工业大学出版社, 2005: 145) |
| [7] | Yu X F, Chen S H, Liu Y, et al.A study of intergranular corrosion of austenitic stainless steel by electrochemical potentiodynamic reactivation, electron back-scattering diffraction and cellular automaton[J]. Corros. Sci., 2010, 52: 1939 |
| [8] | Jha A K, Sreekumar K.Intergranular corrosion of a stud used in safety relief valve[J]. Eng. Fail. Anal., 2009, 16: 1379 |
| [9] | Chowdhury S G, Singh R.The influence of recrystallized structure and texture on the sensitization behaviour of a stable austenitic stainless steel (AISI 316L)[J]. Scr. Mater., 2008, 58: 1102 |
| [10] | Sidhom H, Amadou T, Sahlaoui H, et al.Quantitative evaluation of aged AISI 316L stainless steel sensitization to intergranular corrosion: comparison between microstructural electrochemical and analytical methods[J]. Metall. Mater. Trans., 2007, 38A: 1269 |
| [11] | Kina A Y, Souza V M, Tavares S S M et al. Microstructure and intergranular corrosion resistance evaluation of AISI 304 steel for high temperature service[J]. Mater. Charact., 2008, 59: 651 |
| [12] | Luo H, Gong M.On intergranular corrosion of austenitic stainless steel[J]. Corros. Sci. Protect. Technol., 2006, 18: 357 |
| [12] | (罗宏, 龚敏. 奥氏体不锈钢的晶间腐蚀[J]. 腐蚀科学与防护技术, 2006, 18: 357) |
| [13] | Zhang G Y, Wu Q F.Influence of solution treatment temperature on sensitization of 304 austenitic stainless steel[J]. Corros. Protect., 2012, 33: 695 |
| [13] | (张根元, 吴晴飞. 固溶处理温度对304奥氏体不锈钢敏化与晶间腐蚀的影响[J]. 腐蚀与防护, 2012, 33: 695) |
| [14] | Sun X Y, Liu X G, Wang L L, et al.Influence of solution annealing on intergranular corrosion resistance of 316L stainless steel[J]. Corros. Sci. Protect. Technol., 2014, 26: 228 |
| [14] | (孙小燕, 刘孝光, 汪列隆等. 固溶处理对316L不锈钢晶间腐蚀性能的影响[J]. 腐蚀科学与防护技术, 2014, 26: 228) |
| [15] | Garcia C, Martin F, De Tiedra P, et al.Effect of prior cold work on intergranular and transgranular corrosion in type 304 stainless steels: Quantitative discrimination by image analysis[J]. Corrosion, 2000, 56: 243 |
| [16] | Xu Y, Zhang S H, Cheng M, et al.Effect of loading modes on mechanical property and strain induced martensite transformation of austenitic stainless steels[J]. Acta Metall. Sin., 2013, 49: 775 |
| [16] | (徐勇, 张士宏, 程明等. 加载方式对奥氏体不锈钢力学性能和马氏体相变的影响[J]. 金属学报, 2013, 49: 775) |
| [17] | Moser N H, Gross T S, Korkolis Y P.Martensite formation in conventional and isothermal tension of 304 austenitic stainless steel measured by X-ray diffraction[J]. Metall. Mater. Trans., 2014, 45A: 4891 |
| [18] | Xu Y, Zhang S H, Cheng M, et al.In situ X-ray diffraction study of martensitic transformation in austenitic stainless steel during cyclic tensile loading and unloading[J]. Scr. Mater., 2012, 67: 771 |
| [19] | De A K, Murdock D C, Mataya M C, et al.Quantitative measurement of deformation-induced martensite in 304 stainless steel by X-ray diffraction[J]. Scr. Mater., 2004, 50: 1445 |
| [20] | Smallmann R E, Ngan A H W. Physical Metallurgy and Advanced Materials[M]. 7th Ed., Amsterdam: Butterworth Heinemann, 2007: 414 |
| [21] | Fultz B, Hown J M.Transmission Electron Microscopy and Diffractometry of Materials[M]. 3rd Ed., Berlin: Springer, 2008: 119 |
| [22] | Petit B, Gey N, Cherkaoui M, et al.Deformation behavior and microstructure/texture evolution of an annealed 304 AISI stainless steel sheet. Experimental and micromechanical modeling[J]. Int. J. Plasticity, 2007, 23: 323 |
| [23] | Dong H L.The effect of deformation on microstructure and properties of 304 austenitic stainless steel [D]. Nanjing: Nanjing University of Science and Technology, 2010 |
| [23] | (董红亮. 变形量对304奥氏体不锈钢组织和性能的影响 [D]. 南京: 南京理工大学, 2010) |
| [24] | Shi M T.Metal Material and Heat Treatment [M]. Shanghai: Shanghai Science and Technology Press, 1980: 28 |
| [24] | (史美堂. 金属材料及热处理 [M]. 上海: 上海科学技术出版社, 1980: 28) |
| [25] | Lee S L, Riehards N L.The effect of single-step low strain and annealing of nickel on grain boundary character[J]. Mater. Sci. Eng., 2005, A390: 81 |
| [26] | Xu Z Y.Martensitic Transformation and Martensite [M]. 2nd Ed., Beijing: Science Press, 1999: 253 |
| [26] | (徐祖耀. 马氏体相变与马氏体 [M]. 第2版, 北京: 科学出版社, 1999: 253) |
| [27] | Shimada M, Kokawa H, Wang Z J, et al.Optimization of grain boundary character distribution for intergranular corrosion resistant 304 stainless steel by twin-induced grain boundary engineering[J]. Acta Mater., 2002, 50: 2331 |
/
| 〈 |
|
〉 |